Mechanical and Conductive Properties of Cu/1060Al/Cu Three-Layer Composite Prepared by High-Temperature Oxygen-Free Rolling
JIANG Zhida, XU Yangyang, YU Jiaxin, LIU Wencai, ZHU Haowen, WU Guohua, SHANG Zhengping
Acta Metall Sin . 2026, (
3
): 431 -444 . DOI: 10.11900/0412.1961.2025.00057