Effect of Hot Rolling Process on Mechanical Property and Corrosion Behavior of Rapidly Degrading Mg-Li Alloy
PANG Mengyao, WU Ruizhi, MA Xiaochun, JIN Siyuan, YU Zhe, Boris Krit
Acta Metall Sin . 2025, (
3
): 509 -520 . DOI: 10.11900/0412.1961.2024.00324