Research and Application Progress of SiCp-Reinforced Aluminum-Based Composite Brake Discs for Rail Transit Vehicles
Received date: 2025-12-16
Revised date: 2026-01-26
Online published: 2026-07-14
Supported by
National Key Research and Development Program of China(2023YFB3710602);National Nat-ural Science Foundation of China(U24A2026)
Driven by the “dual-carbon” strategy, the lightweighting of rail transit equipment has become a dominant industry trend. Among the key components, the brake disc—critical to the braking system—faces particularly stringent weight-reduction requirements. SiCp-reinforced aluminum-based composites (SiCp/Al), known for their low density, high thermal conductivity, and superior wear resistance, are now regarded as the prime candidate to replace conventional cast-iron discs. In recent years, SiCp/Al brake discs have been implemented in urban rail transit vehicles operating at 120 km/h. However, their high-temperature stability remains a technical challenge, and no breakthroughs have been achieved for operation on suburban railways at speed ≥ 140 km/h. This study systematically reviews the research progress and engineering applications of SiCp/Al brake discs in rail transit, focusing on its fabrication methods, core performance, in-service behavior, and evaluation standards. Future development directions are discussed to guide technological innovation and the industrial deployment of advanced rail transit equipment.
Key words: aluminum-based composites; brake disc; rail transit; lightweighting
TAN Dong , WU Liukun , FU Kangxi , XIA Shaohua , LI Chong , CUI Lei , LIU Yongchang , ZAN Yuning . Research and Application Progress of SiCp-Reinforced Aluminum-Based Composite Brake Discs for Rail Transit Vehicles[J]. Acta Metall Sin, 2026 , 62(7) : 1163 -1174 . DOI: 10.11900/0412.1961.2025.00409
| [1] | Wang W L, Wu J H, Zhang G D. The tribological and wear behavior of aluminum matrix composites [J]. Acta Metall. Sin., 1998, 34: 1178 |
| 王文龙, 吴军华, 张国定. 铝基复合材料的摩擦磨损性能 [J]. 金属学报, 1998, 34: 1178 | |
| [2] | Xu H Y, Huang L J, Geng L, et al. Effects of Cu content on the wear properties of Al2O3·SiO2sf/Al-Cu composites [J]. Acta Metall. Sin., 2013, 49: 1131 |
| 许虹宇, 黄陆军, 耿 林 等. Cu含量对Al2O3·SiO2sf/Al-Cu复合材料耐磨性能的影响 [J]. 金属学报, 2013, 49: 1131 | |
| [3] | Liu C X, Luo R, Xie Y, et al. Research progress on particle reinforced aluminum matrix composites for brake discs in rail transit [J]. Mod. Urban Transit, 2022, (7): 11 |
| 刘春轩, 罗 任, 谢 屹 等. 轨道交通制动盘用颗粒增强铝基复合材料研究及进展 [J]. 现代城市轨道交通, 2022, (7): 11 | |
| [4] | Zhang R, Zhu S Z, Liu Z Y, et al. Influence of aging temperatures on precipitation behaviors of SiC/Al-Zn-Mg-Cu composites [J]. Acta Metall. Sin., 2024, 60: 1043 |
| 张 冉, 朱士泽, 刘振宇 等. 时效温度对SiC/Al-Zn-Mg-Cu复合材料时效析出行为的影响 [J]. 金属学报, 2024, 60: 1043 | |
| [5] | Ramanathan A, Krishnan P K, Muraliraja R. A review on the production of metal matrix composites through stir casting—Furnace design, properties, challenges, and research opportunities [J]. J. Manuf. Process., 2019, 42: 213 |
| [6] | Chen Z P, Chen W P, Liu F F. Research progress on casting Al matrix composites [J]. Cast. Equip. Technol., 2020, (1): 42 |
| 陈志平, 陈维平, 刘方方. 铸造铝基复合材料的研究进展 [J]. 铸造设备与工艺, 2020, (1): 42 | |
| [7] | Hashim J, Looney L, Hashmi M S J. Metal matrix composites: Production by the stir casting method [J]. J. Mater. Process. Technol., 1999, 92-93: 1 |
| [8] | Zhang Z L. Investigation on semi-solid stir casting technology of SiCp/A357 composite [D]. Beijing: University of Science and Technology Beijing, 2017 |
| 张桢林. SiCp/A357复合材料半固态搅拌铸造工艺研究 [D]. 北京: 北京科技大学, 2017 | |
| [9] | Pan L W, Lin W J, Tang J F, et al. Preparation methods and research status of particles-reinforced aluminum matrix composites [J]. Mater. Rev., 2016, 30(suppl.1) : 511 |
| 潘利文, 林维捐, 唐景凡 等. 颗粒增强铝基复合材料制备方法及研究现状 [J]. 材料导报, 2016, 30(): 511 | |
| [10] | Pan L K, Han J M, Zhang Y X, et al. Microstructure and properties of derived material for high content SiCp/A356 composites [J]. Chin. J. Nonferrous Met., 2016, 26: 2078 |
| 潘利科, 韩建民, 张颖骁 等. 高含量SiCp/A356复合材料衍生材料的组织与性能 [J]. 中国有色金属学报, 2016, 26: 2078 | |
| [11] | Zhang Z L, Zhang Z F, Xu J, et al. Properties of SiCp/A357 composites fabricated by double-deck mechanical stirring casting [J]. Spec. Cast. Nonferrous Alloys, 2017, 37: 598 |
| 张桢林, 张志峰, 徐 骏 等. 双级机械搅拌铸造SiCp/A357复合材料的工艺及性能 [J]. 特种铸造及有色合金, 2017, 37: 598 | |
| [12] | Zhang Z L, Xu J, Xiang J, et al. Application of electromagnetic stirring suction casting in aluminum matrix composite brake disc [J]. Spec. Cast. Nonferrous Alloys, 2022, 42: 171 |
| 张桢林, 徐 骏, 向 俊 等. 电磁搅拌吸铸技术及其在铝陶制动盘铸造中的应用 [J]. 特种铸造及有色合金, 2022, 42: 171 | |
| [13] | Tong W B. Study on structure and forming process of aluminum matrix composites axial brake disc for urban rail [D]. Beijing: Beijing Jiaotong University, 2019 |
| 童卫兵. 城轨铝基复合材料轴装制动盘结构与成型工艺研究 [D]. 北京: 北京交通大学, 2019 | |
| [14] | Zhao H Q, Yang Z Y, Zhang X F, et al. Casting process design and defect prediction of SiCp/A356 brake disc [J]. Foundry Technol., 2019, 40: 671 |
| 赵海芹, 杨智勇, 张雄飞 等. SiCp/A356制动盘铸造成形工艺设计和缺陷预测 [J]. 铸造技术, 2019, 40: 671 | |
| [15] | Qin Q, Hua J J. Preparation of powder metallurgy submicron SiC particle reinforced Al based composites and mechanical properties [J]. Spec. Cast. Nonferrous Alloys, 2017, 37: 411 |
| 覃 群, 华建杰. 粉末冶金制备SiCp增强Al基复合材料及其性能 [J]. 特种铸造及有色合金, 2017, 37: 411 | |
| [16] | Cao L X, Zhang X Y, Huo S H, et al. Progress of study on powder metallurgical aluminum-based composite brake disc for urban rail transit [J]. Roll. Stock, 2024, 62(6): 87 |
| 曹柳絮, 张晓泳, 霍树海 等. 城市轨道交通粉末冶金铝基复合材料制动盘研究进展 [J]. 铁道车辆, 2024, 62(6): 87 | |
| [17] | Fu K X, Tan D, Zhang S Q, et al. Friction and wear behavior of SiCp/Al brake disk sliding against semimetallic brake pad under the braking condition of urban rail vehicles [J]. Tribol. Trans., 2024, 67: 875 |
| [18] | Tan D, Xia S H, Yob A, et al. Evaluation of the wear resistance of aluminium-based hybrid composite brake discs under relevant city rail environments [J]. Mater. Des., 2022, 215: 110504 |
| [19] | Viswanatha B M, Kumar M P, Basavarajappa S, et al. Effect of ageing on dry sliding wear behaviour of Al-MMC for disc brake [J]. Tribol. Ind., 2014, 36: 40 |
| [20] | Hong S J, Kim H M, Huh D, et al. Effect of clustering on the mechanical properties of SiC particulate-reinforced aluminum alloy 2024 metal matrix composites [J]. Mater. Sci. Eng., 2003, A347: 198 |
| [21] | Wang R, Zhang C. Research on friction and wear properties of aluminum matrix composites for brake discs with SiCp/A357 contents [J]. China Rail., 2023, (2): 74 |
| 王 瑞, 张 臣. 制动盘用SiCp/A357铝基复合材料摩擦磨损性能研究 [J]. 中国铁路, 2023, (2): 74 | |
| [22] | Tan D, Fu K X, Zhang S Q, et al. Friction and wear behavior of different volume fraction SiCp/Al composites by stir casting combined with friction stir processing [J]. Mater. Mech. Eng., 2024, 48(9): 59 |
| 谭 东, 付康习, 张士琦 等. 搅拌铸造结合搅拌摩擦加工制备不同体积分数SiCp/Al复合材料的摩擦磨损行为 [J]. 机械工程材料, 2024, 48(9): 59 | |
| [23] | Lee T, Lee J, Lee D, et al. Effects of particle size and surface modification of SiC on the wear behavior of high volume fraction Al/SiCp composites [J]. J. Alloys Compd., 2020, 831: 154647 |
| [24] | Ye C T, Jia L N, Qi Y, et al. Strengthening effects of Mg-Si precipitates on wear resistance of SiCp/Al-Si-Mg composites [J]. Wear, 2025, 564-565: 205716 |
| [25] | Du A D, Lattanzi L, Jarfors A E W, et al. Role of matrix alloy, reinforcement size and fraction in the sliding wear behaviour of Al-SiCp MMCs against brake pad material [J]. Wear, 2023, 530-531: 204969 |
| [26] | Lattanzi L, Awe S A. Thermophysical properties of Al-based metal matrix composites suitable for automotive brake discs [J]. J. Alloys Metall. Syst., 2024, 5: 100059 |
| [27] | Rong Z Z. Study on high temperature mechanical properties of nano-Al2O3/6061 aluminum matrix composites [D]. Zhengzhou: Zhengzhou University of Aeronautics, 2023 |
| 荣智峥. 纳米氧化铝颗粒增强6061铝基复合材料的高温力学性能研究 [D]. 郑州: 郑州航空工业管理学院, 2023 | |
| [28] | Lyu Y, Wahlstr?m J, Tu M, et al. A friction, wear and emission tribometer study of non-asbestos organic pins sliding against AlSiC MMC discs [J]. Tribol. Ind., 2018, 40: 274 |
| [29] | Yang Z Y, Zang J J, Fang D L, et al. Thermal fatigue crack propagation mechanism of SiCp/A356 composites for urban rail train brake disc [J]. J. Mater. Eng., 2022, 50(7): 165 |
| 杨智勇, 臧家俊, 方丹琳 等. 城轨列车制动盘SiCp/A356复合材料热疲劳裂纹扩展机理 [J]. 材料工程, 2022, 50(7): 165 | |
| [30] | Chen A L, Arai Y, Tsuchida E. An experimental study on effect of thermal cycling on monotonic and cyclic response of cast aluminium alloy-SiC particulate composites [J]. Composites, 2005, 36B: 319 |
| [31] | Pal S, Bhanuprasad V V, Mitra R. Damage evaluation in discontinuously reinforced aluminum matrix composites subjected to thermal cycling [J]. Mater. Sci. Eng., 2008, A489: 11 |
| [32] | Nam T H, Requena G, Degischer P. Thermal expansion behaviour of aluminum matrix composites with densely packed SiC particles [J]. Composites, 2008, 39A: 856 |
| [33] | Requena G, Yubero D C, Corrochano J, et al. Stress relaxation during thermal cycling of particle reinforced aluminium matrix composites [J]. Composites, 2012, 43A: 1981 |
| [34] | Song P L, Yang Z Y, Zang J J, et al. Effects of thermal cycling treatment on load bearing and friction behavior of SiCp/A356 composites [J]. Eng. Fail. Anal., 2024, 156: 107828 |
| [35] | Pan L K, Han J M, Yang Z Y, et al. Thermal fatigue crack behavior of SiCp/A356 composites prepared by stirring casting [J]. Results Phys., 2017, 7: 927 |
| [36] | Zhou K L, Cai W B, Chi M R, et al. Dynamic performance analysis of aluminum matrix composite brake disc for linear metro vehicle [J]. Electr. Drive Locomot., 2021, (1): 53 |
| 周开磊, 蔡吴斌, 池茂儒 等. 直线电机地铁车辆铝基复合材料制动盘动力学性能分析 [J]. 机车电传动, 2021, (1): 53 | |
| [37] | Gou Q B, Zhang N, Meng F H, et al. Development and experimental study of new brake friction pairs for standard metro train [J]. Electr. Drive Locomot., 2022, (2): 67 |
| 苟青炳, 张 宁, 孟繁辉 等. 标准地铁车辆用新型制动摩擦副设计与试验研究 [J]. 机车电传动, 2022, (2): 67 | |
| [38] | Zhao F. Application of aluminum matrix composite brake disc on subway vehicles [J]. Machinery, 2023, 50(10): 33 |
| 赵 锋. 铝基复合材料制动盘在地铁车辆上的应用研究 [J]. 机械, 2023, 50(10): 33 | |
| [39] | Cao J H, Liang H, Xue J, et al. Research on brake disc lightweight technology based on improving train running quality [J]. Mod. Urban Transit, 2019, (11): 47 |
| 曹建行, 梁 洪, 薛 江 等. 基于提高列车运行品质的制动盘轻量化技术研究 [J]. 现代城市轨道交通, 2019, (11): 47 | |
| [40] | Zhao N Q, Liu X H, Pu B W. Progress on multi-dimensional carbon nanomaterials reinforced aluminum matrix composites: A review [J]. Acta Metall. Sin., 2019, 55: 1 |
| 赵乃勤, 刘兴海, 蒲博闻. 多维度碳纳米相增强铝基复合材料研究进展 [J]. 金属学报, 2019, 55: 1 | |
| [41] | Zhang X X, Zheng Z, Gao Y, et al. Progress in high throughput fabrication and characterization of metal matrix composites [J]. Acta Metall. Sin., 2019, 55: 109 |
| 张学习, 郑 忠, 高 莹 等. 金属基复合材料高通量制备及表征技术研究进展 [J]. 金属学报, 2019, 55: 109 | |
| [42] | Bi S, Li Z C, Sun H X, et al. Microstructure and mechanical properties of carbon nanotubes-reinforced 7055Al composites fabricated by high-energy ball milling and powder metallurgy processing [J]. Acta Metall. Sin., 2021, 57: 71 |
| 毕 胜, 李泽琛, 孙海霞 等. 高能球磨结合粉末冶金法制备碳纳米管增强7055Al复合材料的微观组织和力学性能 [J]. 金属学报, 2021, 51: 71 | |
| [43] | Zhou L, Zhang M Y, Yang X S, et al. Simulation of thermal expansion coefficient of configurational GNPs/2009Al composites [J]. Acta Metall. Sin., 2024, 60: 977 |
| 周 丽, 张明远, 杨欣盛 等. 构型化石墨烯纳米片/2009Al复合材料热膨胀系数模拟 [J]. 金属学报, 2024, 60: 977 | |
| [44] | Kukutschová J, Roubí?ek V, Malachová K, et al. Wear mechanism in automotive brake materials, wear debris and its potential environmental impact [J]. Wear, 2009, 267: 807 |
| [45] | Yuan Z W, Tian C, Zhang D Q, et al. Development and testing of pad for brake disc of aluminum matrix composites [J]. J. Tongji Univ. (Nat. Sci. Ed.), 2019, 47: 201 |
| 袁泽旺, 田 春, 张定权 等. 铝基复合制动盘闸片开发及试验 [J]. 同济大学学报(自然科学版), 2019, 47: 201 | |
| [46] | Gao H M, Wang G S, Yang H S, et al. Application and development of organic friction materials in rail transit field [J]. Rail Transit Mater., 2024, 3(1): 32 |
| 高红梅, 汪贵松, 杨火顺 等. 合成摩擦材料在轨道交通领域的应用与发展 [J]. 轨道交通材料, 2024, 3(1): 32 | |
| [47] | Li S C. Performance research of organic composite friction materials matching Al-MMC brake discs [D]. Nanning: Guangxi University for Nationalities, 2024 |
| 李尚谌. 匹配铝基制动盘的有机复合摩擦材料性能研究 [D]. 南宁: 广西民族大学, 2024 |
/
| 〈 |
|
〉 |