Research Status and Development Trend of Precipitation Phase Regulation and Strengthening Mechanism in Ultra-High Strength Steel
Received date: 2025-11-03
Revised date: 2025-12-10
Online published: 2026-05-13
Supported by
National Natural Science Foundation of China(52574422)
As a key structural material for aviation, aerospace, and major equipment, the lightweight and high-performance development of ultra-high strength (UHS) steel is essential for the advancement of related fields. However, traditional UHS steels have long faced critical challenges: the difficulty in achieving a synergistic combination of high strength, high toughness, good weldability, and corrosion resistance, along with the constraint of high alloy costs that limit their widespread application. To address these issues, we systematically review the development history, composition, microstructure, and performance characteristics of traditional UHS steels, including low-alloy UHS, secondary hardening, maraging, and precipitation-hardening stainless steels. We also review the research progress in developing novel UHS steels through two main pathways: the regulation of composite nanoprecipitates and the design of multiphase composite microstructures. Special attention is paid to exploring the potential and preliminary practices of the “hybrid” design concept, which breaks the boundaries of traditional steel classifications and integrates multiple strengthening mechanisms to develop cost-effective, high-performance, and easily weldable “all-round” UHS steels. The current research status regarding the evolution laws of precipitates and strengthening mechanisms in UHS steels is detailed. Finally, the future development directions of UHS steels are proposed, particularly regarding the synergistic control of complex precipitates, high-temperature stability, and industrial application.
ZHANG Chaolei , PAN Xiaokun , GAO Junheng , WU Honghui , MAO Xinping . Research Status and Development Trend of Precipitation Phase Regulation and Strengthening Mechanism in Ultra-High Strength Steel[J]. Acta Metall Sin, 2026 , 62(7) : 1207 -1227 . DOI: 10.11900/0412.1961.2025.00354
| [1] | Luo H W, Shen G H. Progress and perspective of ultra-high strength steels having high toughness [J]. Acta Metall. Sin., 2020, 56: 494 |
| 罗海文, 沈国慧. 超高强高韧化钢的研究进展和展望 [J]. 金属学报, 2020, 56: 494 | |
| [2] | Li H F, Wang S G, Zhang P, et al. Crack propagation mechanisms of AISI 4340 steels with different strength and toughness [J]. Mater. Sci. Eng., 2018, A729: 130 |
| [3] | Liu F G, Lin X, Song M H, et al. Effect of tempering temperature on microstructure and mechanical properties of laser solid formed 300M steel [J]. J. Alloys Compd., 2016, 689: 225 |
| [4] | Zhang Y P, Zhan D P, Qi X W, et al. Effect of solid-solution temperature on the microstructure and properties of ultra-high-strength ferrium S53? steel [J]. Mater. Sci. Eng., 2018, A730: 41 |
| [5] | Daymond B T, Binot N, Schmidt M L, et al. Development of custom 465? corrosion-resisting steel for landing gear applications [J]. J. Mater. Eng. Perform., 2016, 25: 1539 |
| [6] | Li Y C, Yan W, Cotton J D, et al. A new 1.9 GPa maraging stainless steel strengthened by multiple precipitating species [J]. Mater. Des., 2015, 82: 56 |
| [7] | Maloney J L, Garrison W M. The effect of sulfide type on the fracture behavior of HY180 steel [J]. Acta Mater., 2005, 53: 533 |
| [8] | Li Y F, Cheng X, Liu D, et al. Influence of last stage heat treatment on microstructure and mechanical properties of laser additive manufactured AF1410 steel [J]. Mater. Sci. Eng., 2018, A713: 75 |
| [9] | Manigandan K, Srivatsan T S, Tammana D, et al. Influence of microstructure on strain-controlled fatigue and fracture behavior of ultra high strength alloy steel AerMet 100 [J]. Mater. Sci. Eng., 2014, A601: 29 |
| [10] | Prasad N E, Wanhill R J H. Aerospace Materials and Material Technologies [M]. Singapore: Springer, 2017: 173 |
| [11] | Morris J W. Making steel strong and cheap [J]. Nat. Mater., 2017, 16: 787 |
| [12] | He Y, Yang K, Kong F Y, et al. Mechanical properties of ultra-high-strength 18Ni cobalt-free maraging steel [J]. Acta Metall. Sin., 2002, 38: 278 |
| 何 毅, 杨 柯, 孔凡亚 等. 超高强度18Ni无钴马氏体时效钢的力学性能 [J]. 金属学报, 2002, 38: 278 | |
| [13] | Gao Y H, Liu S Z, Hu X B, et al. A novel low cost 2000 MPa grade ultra-high strength steel with balanced strength and toughness [J]. Mater. Sci. Eng., 2019, A759: 298 |
| [14] | Liu Z B, Yang Z, Wang X H, et al. Enhanced strength-ductility synergy in a new 2.2 GPa grade ultra-high strength stainless steel with balanced fracture toughness: Elucidating the role of duplex aging treatment [J]. J. Alloys Compd., 2022, 928: 167135 |
| [15] | Niu G, Zurob H S, Misra R D K, et al. Superior fracture toughness in a high-strength austenitic steel with heterogeneous lamellar microstructure [J]. Acta Mater., 2022, 226: 117642 |
| [16] | Leo D W, Varadarajan A S. Simulation of surface milling of hardened AISI 4340 steel with minimal fluid application using artificial neural network [J]. Adv. Prod. Eng. Manag., 2012, 1: 51 |
| [17] | Kasana, S S, Sharma S, Pandey O P. Influence of heat treatment (routes) on the microstructure and mechanical properties of 300M ultra high strength steel [J]. Arch. Civ. Mech. Eng., 2022, 22: 126 |
| [18] | Feng D Y, Liu S C, Wang S L, et al. Effect of heat treatment on microstructure and mechanical properties of electron beam welding joint of 30CrMnSiNi2A steel [J]. Mater. Rep., 2025, 39(14): 132 |
| 冯殿远, 刘诗超, 王善林 等. 热处理对30CrMnSiNi2A钢电子束焊接头组织和性能的影响 [J]. 材料导报, 2025, 39(14): 132 | |
| [19] | Chen D M, Kang M K, Tan R B. Fatigue properties of meta-bainite in steel 40CrMnSiMoVA [J]. Acta Metall. Sin., 1991, 27: A458 |
| 陈大明, 康沫狂, 谭若兵. 40CrMnSiMoVA钢准贝氏体的疲劳性能 [J]. 金属学报, 1991, 27: A458 | |
| [20] | Tikhe O, Doiphode P, Nichul U, et al. Development of optimized mechanical properties of AISI 4340 steel: Role of quenching and partitioning process [J]. Met. Mater. Int., 2023, 29: 2216 |
| [21] | Liu X M, Hua F, Liu R, et al. Effect of heat treatment on the mechanical properties of steel 30CrMnSiNi2A [J]. Iron Steel, 2003, 38(1): 43 |
| 刘宪民, 花 峰, 刘 蕤 等. 热处理对30CrMnSiNi2A钢力学性能的影响 [J]. 钢铁, 2003, 38(1): 43 | |
| [22] | Khodamorad A, Hassan S, Shahram K. Bainite-martensite microstructure in D6AC steel effect of bainite morphology on mechanical properties of the mixed [J]. J. Mater. Sci. Technol., 2012, 28: 336 |
| [23] | Maloney J L, Garrison W M. The effect of sulfide type on the fracture behavior of HY180 steel [J]. Acta Mater., 2005, 53: 533 |
| [24] | Handerhan K J, Garrison W M, Moody N R. A comparison of the fracture behavior of two heats of the secondary hardening steel AF1410 [J]. Metall. Trans., 1989, 20A: 105 |
| [25] | Thomas R L S, Li D M, Gangloff R P, et al. Trap-governed hydrogen diffusivity and uptake capacity in ultrahigh-strength AERMET100 steel [J]. Metall. Mater. Trans., 2002, 33A: 1991 |
| [26] | Morikawa H, Komatsu H, Tanino M. Effect of chromium upon co‐herency between M2C precipitates and α-iron matrix in 0.1C-10Ni-8Co-lMo-Cr steels [J]. J. Electron. Microsc., 1973, 22: 99 |
| [27] | Li K, Shan J G, Wang C X, et al. Strength and toughness of T250 maraging steel joint hybrid-treated with laser welding and aging [J]. Acta Metall. Sin., 2015, 51: 904 |
| 李 坤, 单际国, 王春旭 等. T250马氏体时效钢激光焊接-时效处理接头的强韧性 [J]. 金属学报, 2015, 51: 904 | |
| [28] | Liu Z B, Liang J X, Su J, et al. Research and application progress in ultra-high strength stainless steel [J]. Acta Metall. Sin., 2020, 56: 549 |
| 刘振宝, 梁剑雄, 苏 杰 等. 高强度不锈钢的研究及发展现状 [J]. 金属学报, 2020, 56: 549 | |
| [29] | Anoop C R, Prakash A, Narayana Murty S V S, et al. Origin of low temperature toughness in a 12Cr-10Ni martensitic precipitation hardenable stainless steel [J]. Mater. Sci. Eng., 2018, A709: 1 |
| [30] | Bray J W, Maloney J L, Raghavan K S, et al. A comparison of the fracture behavior of two commercially produced heats of HY180 steel differing in sulfide type [J]. Metall. Trans., 1991, 22A: 2277 |
| [31] | Luo H, Yin Z D, Zhu J C, et al. Influence of grain size on mechanical properties of 18Ni maraging steel [J]. Mater. Sci. Technol., 2000, 8(1): 59 |
| 罗 鸿, 尹钟大, 朱景川 等. 晶粒尺寸对18Ni马氏体时效钢力学性能的影响 [J]. 材料科学与工艺, 2000, 8(1): 59 | |
| [32] | Kim Y G, Kim G S, Lee C S, et al. Microstructure and mechanical properties of a cobalt-free tungsten-bearing maraging steel [J]. Mater. Sci. Eng., 1986, 79: 133 |
| [33] | Yang W Y. Investigation on strength-toughness mechanism of low nickel, cobalt free maraging steel [D]. Taiyuan: North University of China, 2009 |
| 杨维宇. 低Ni无Co马氏体时效钢强韧化研究 [D]. 太原: 中北大学, 2009 | |
| [34] | Kuehmann C, Tufts B, Trester P. Computational design for ultra high-strength alloy [J]. AMP Tech. Artic., 2008, 166: 37 |
| [35] | Niu Y E, Zhao P P, Li N, et al. Research status and application of ultra-high strength steel at home and abroad [J]. J. Ordnance Equip. Eng., 2021, 42(7): 274 |
| 牛艳娥, 赵芃沛, 李 宁 等. 国内外超高强度钢的研究现状及应用 [J]. 兵器装备工程学报, 2021, 42(7): 274 | |
| [36] | Zhou C, Ye Q B, Tian Y, et al. Research and application progress of ultra-high strength structural steel [J]. Trans. Mater. Heat Treat., 2021, 42(1): 14 |
| 周 成, 叶其斌, 田 勇 等. 超高强度结构钢的研究及发展 [J]. 材料热处理学报, 2021, 42(1): 14 | |
| [37] | Yin H, Li J X, Su Y J, et al. Current situation and development of maraging steel [J]. J. Iron Steel Res., 2014, 26(3): 1 |
| 尹 航, 李金许, 宿彦京 等. 马氏体时效钢的研究现状与发展 [J]. 钢铁研究学报, 2014, 26(3): 1 | |
| [38] | Jiang S H, Wang H, Wu Y, et al. Ultrastrong steel via minimal lattice misfit and high-density nanoprecipitation [J]. Nature, 2017, 544: 460 |
| [39] | Olson G B. Genomic materials design: The ferrous frontier [J]. Acta Mater., 2013, 61: 771 |
| [40] | Xu W, Rivera-Díaz-del-Castillo P E J, Yan W, et al. A new ultrahigh-strength stainless steel strengthened by various coexisting nanoprecipitates [J]. Acta Mater., 2010, 58: 4067 |
| [41] | Jiao Z B, Luan J H, Miller M K, et al. Precipitation mechanism and mechanical properties of an ultra-high strength steel hardened by nanoscale NiAl and Cu particles [J]. Acta Mater., 2015, 97: 58 |
| [42] | Jiao Z B, Luan J H, Miller M K, et al. Co-precipitation of nanoscale particles in steels with ultra-high strength for a new era [J]. Mater. Today, 2017, 20: 142 |
| [43] | Niu M C, Yin L C, Yang K, et al. Synergistic alloying effects on nanoscale precipitation and mechanical properties of ultrahigh-strength steels strengthened by Ni3Ti, Mo-enriched, and Cr-rich co-precipitates [J]. Acta Mater., 2021, 209: 116788 |
| [44] | Wang L J, Jiang S H, Peng B, et al. Ultrastrong steel strengthened by multiple shearable nanostructures [J]. J. Mater. Sci. Technol., 2023, 161: 245 |
| [45] | Raabe D, Ponge D, Dmitrieva O, et al. Nanoprecipitate-hardened 1.5 GPa steels with unexpected high ductility [J]. Scr. Mater., 2009, 60: 1141 |
| [46] | Sun L, Simm T H, Martin T L, et al. A novel ultra-high strength maraging steel with balanced ductility and creep resistance achieved by nanoscale β-NiAl and Laves phase precipitates [J]. Acta Mater., 2018, 149: 285 |
| [47] | Sun M X, Zhang W N, Liu Z Y, et al. Direct observations on the crystal structure evolution of nano Cu-precipitates in an extremely low carbon steel [J]. Mater. Lett., 2017, 187: 49 |
| [48] | Bhadeshia H K D H, Edmonds D V. The bainite transformation in a silicon steel [J]. Metall. Trans., 1979, 10A: 895 |
| [49] | Hodgson P, Timokhina I, Xiong X Y, et al. Understanding of the bainite transformation in a nano-structured bainitic steel [J]. Solid State Phenom., 2011, 172-174: 123 |
| [50] | He B B, Hu B, Yen H W, et al. High dislocation density-induced large ductility in deformed and partitioned steels [J]. Science, 2017, 357: 1029 |
| [51] | Qin S W, Liu Y, Hao Q G, et al. High carbon microalloyed martensitic steel with ultrahigh strength-ductility [J]. Mater. Sci. Eng., 2016, A663: 151 |
| [52] | Gao G H, Zhang H, Gui X L, et al. Enhanced ductility and toughness in an ultrahigh-strength Mn-Si-Cr-C steel: The great potential of ultrafine filmy retained austenite [J]. Acta Mater., 2014, 76: 425 |
| [53] | Yin C C, Hu F, Zheng H, et al. Research progress on retained austenite refinement and controlling of mechanical properties of nanostructured bainitic steel [J]. Trans. Mater. Heat Treat., 2021, 42(1): 1 |
| 尹朝朝, 胡 锋, 郑 花 等. 纳米贝氏体钢残奥细化及其力学性能调控研究进展 [J]. 材料热处理学报, 2021, 42(1): 1 | |
| [54] | Wilms M B, Rittinghaus S K, Go?ling M, et al. Additive manufacturing of oxide-dispersion strengthened alloys: Materials, synthesis and manufacturing [J]. Prog. Mater. Sci., 2023, 133: 101049 |
| [55] | Romero-Resendiz L, El-Tahawy M, Zhang T, et al. Heterostructured stainless steel: Properties, current trends, and future perspectives [J]. Mater. Sci. Eng., 2022, R150: 100691 |
| [56] | Nagarajan B, Hu Z H, Song X, et al. Development of micro selective laser melting: The state of the art and future perspectives [J]. Engineering, 2019, 5: 702 |
| [57] | Yadroitsev I, Smurov I. Selective laser melting technology: From the single laser melted track stability to 3D parts of complex shape [J]. Phys. Proc., 2010, 5: 551 |
| [58] | Thompson S M, Bian L K, Shamsaei N, et al. An overview of Direct Laser Deposition for additive manufacturing; Part I: Transport phenomena, modeling and diagnostics [J]. Addit. Manuf., 2015, 8: 36 |
| [59] | Ding D H, Pan Z X, Cuiuri D, et al. Wire-feed additive manufacturing of metal components: Technologies, developments and future interests [J]. Int. J. Adv. Manuf. Technol., 2015, 81: 465 |
| [60] | Wu W W, Xiang C, Zhang T, et al. Effect of heat treatment on microstructure and mechanical properties of 18Ni300 maraging steel fabricated by selective laser melting [J]. Acta Metall. Sin., 2025, 61: 1515 |
| 吴文伟, 向 超, 张 涛 等. 热处理工艺对选区激光熔化成型18Ni300马氏体时效钢微观组织及力学性能的影响 [J]. 金属学报, 2025, 61: 1515 | |
| [61] | Tan C L, Zhou K S, Ma W Y, et al. Microstructural evolution, nanoprecipitation behavior and mechanical properties of selective laser melted high-performance grade 300 maraging steel [J]. Mater. Des., 2017, 134: 23 |
| [62] | Tan C L, Zhou K S, Kuang M, et al. Microstructural characterization and properties of selective laser melted maraging steel with different build directions [J]. Sci. Technol. Adv. Mater., 2018, 19: 746 |
| [63] | J?gle E A, Choi P P, Van Humbeeck J, et al. Precipitation and austenite reversion behavior of a maraging steel produced by selective laser melting [J]. J. Mater. Res., 2014, 29: 2072 |
| [64] | Becker T H, Dimitrov D. The achievable mechanical properties of SLM produced maraging Steel 300 components [J]. Rapid Prototyping J., 2016, 22: 487 |
| [65] | Suryawanshi J, Prashanth K G, Ramamurty U. Tensile, fracture, and fatigue crack growth properties of a 3D printed maraging steel through selective laser melting [J]. J. Alloys Compd., 2017, 725: 355 |
| [66] | Tan C L, Zhou K S, Ma W Y, et al. Interfacial characteristic and mechanical performance of maraging steel-copper functional bimetal produced by selective laser melting based hybrid manufacture [J]. Mater. Des., 2018, 155: 77 |
| [67] | Cyr E, Asgari H, Shamsdini S, et al. Fracture behaviour of additively manufactured MS1-H13 hybrid hard steels [J]. Mater. Lett., 2018, 212: 174 |
| [68] | Wang B X, Cui W W, Zhang Y, et al. Effect of tempering temperature on microstructure and mechanical properties of 300M steel [J]. Foundry Technol., 2021, 42: 719 |
| 王丙旭, 崔威威, 张 宇 等. 回火温度对300M钢组织和性能的影响 [J]. 铸造技术, 2021, 42: 719 | |
| [69] | Wen C F, Xiao A D, Liu X H, et al. Effect of tempering temperature on microstructure and mechanical properties of low alloy ultra-high strength steel Q1300 [J]. Heat Treat. Met., 2019, 44(2): 172 |
| 温长飞, 肖爱达, 刘旭辉 等. 回火温度对低合金超高强钢Q1300组织与性能的影响 [J]. 金属热处理, 2019, 44(2): 172 | |
| [70] | Abdollah-Zadeh A, Jafari-Pirlari A, Barzegari M. Tempered martensite embrittlement in a 32NiCrMoV125 steel [J]. J. Mater. Eng. Perform., 2005, 14: 569 |
| [71] | Kim S H, Kim H, Kim N J. Brittle intermetallic compound makes ultrastrong low-density steel with large ductility [J]. Nature, 2015, 518: 77 |
| [72] | Li X Y, Lu K. Improving sustainability with simpler alloys [J]. Science, 2019, 364: 733 |
| [73] | Jan-Erik A, Lindberg F, Patrik ?. Hybrid steel enhances component performance at reduced weight [J]. Lightweight Des. Worldw., 2019, 12: 34 |
| [74] | Ma X L, Zhang C C, Zhang C L, et al. Microstructure and properties of sorbite stainless steel designed by “hybrid” idea [J]. Mater. Rep., 2020, 34: 4103 |
| 马潇磊, 张成成, 张朝磊 等. 基于“混杂”设计的索氏体新型不锈钢的组织和性能 [J]. 材料导报, 2020, 34: 4103 | |
| [75] | Pan X K, Huang B Y, Zhang C L, et al. Strengthening mechanism and precipitate evolution of a multi-application special engineering steel designed based on a hybrid idea [J]. J. Alloys Compd., 2023, 942: 169053 |
| [76] | Lee J Y, Jeong H B, Jo W H, et al. Hydrogen desorption mechanism associated with ε carbide decomposition in martensitic medium-Mn steel [J]. J. Mater. Res. Technol., 2025, 37: 3832 |
| [77] | Chen J Y, Jin P F, Wang S J, et al. A novel Ni-Mo-W-V martensitic steel for hot working dies: Improved elevated-temperature mechanical properties and wear resistance via thermally stable MC nanoprecipitates [J]. Tribol. Int., 2025, 207: 110618 |
| [78] | Hong C W, Youn K T, Kim S H, et al. Investigation of V-rich MC (M = V, Mo) carbide behavior related to thermal fatigue property in commercial hot work tool steel processing [J]. Mater. Charact., 2024, 214: 114025 |
| [79] | Ghosh G, Olson G B. Precipitation of paraequilibrium cementite: Experiments, and thermodynamic and kinetic modeling [J]. Acta Mater., 2002, 50: 2099 |
| [80] | Dyson D J, Keown S R, Raynor D, et al. The orientation relationship and growth direction of Mo2C in ferrite [J]. Acta Metall., 1966, 14: 867 |
| [81] | Wang C C. Alloy design of high Co-Ni secondary hardening steel by multi-scale simulation [D]. Beijing: Tsinghua University, 2017 |
| 王晨充. 基于多尺度模拟的高Co-Ni二次硬化钢合金设计 [D]. 北京: 清华大学, 2017 | |
| [82] | Kamikawa N, Abe Y, Miyamoto G, et al. Tensile behavior of Ti, Mo-added low carbon steels with interphase precipitation [J]. ISIJ Int., 2014, 54: 212 |
| [83] | Jain D, Isheim D, Hunter A H, et al. Multicomponent high-strength low-alloy steel precipitation-strengthened by sub-nanometric Cu precipitates and M2C carbides [J]. Metall. Mater. Trans., 2016, 47A: 3860 |
| [84] | Inoue A, Masumoto T. Carbide reactions (M3C→M7C3→M23C6→M6C) during tempering of rapidly solidified high carbon Cr-W and Cr-Mo steels [J]. Metall. Trans., 1980, 11A: 739 |
| [85] | Kapoor M, Isheim D, Ghosh G, et al. Aging characteristics and mechanical properties of 1600MPa body-centered cubic Cu and B2-NiAl precipitation-strengthened ferritic steel [J]. Acta Mater., 2014, 73: 56 |
| [86] | Li C N, Duan R, Fu W, et al. Improvement of mechanical properties for low carbon ultra-high strength steel strengthened by Cu-rich multistructured precipitation via modification to bainite [J]. Mater. Sci. Eng., 2021, A817: 141337 |
| [87] | Moshka O, Pinkas M, Brosh E, et al. Addressing the issue of precipitates in maraging steels—Unambiguous answer [J]. Mater. Sci. Eng., 2015, A638: 232 |
| [88] | Simm T H, Sun L, Galvin D R, et al. A SANS and APT study of precipitate evolution and strengthening in a maraging steel [J]. Mater. Sci. Eng., 2017, A702: 414 |
| [89] | Ruan T T, Shen J J, Li B, et al. High-temperature strengthening mechanism and thermal stability of Laves phase in ferritic matrix [J]. Mater. Sci. Eng., 2022, A859: 144183 |
| [90] | Zhang C X, Gao Q Z, Ma Q S, et al. Variety of yield strength caused by precipitations of L12-Ni3Al and B2-NiAl phases in alumina-forming austenitic steel [J]. Mater. Sci. Eng., 2024, A894: 146177 |
| [91] | Jiao Z B, Luan J H, Miller M K, et al. Group precipitation and age hardening of nanostructured Fe-based alloys with ultra-high strengths [J]. Sci. Rep., 2016, 6: 21364 |
| [92] | Leitner H, Schober M, Schnitzer R. Splitting phenomenon in the precipitation evolution in an Fe-Ni-Al-Ti-Cr stainless steel [J]. Acta Mater., 2010, 58: 1261 |
| [93] | Schnitzer R, Schober M, Zinner S, et al. Effect of Cu on the evolution of precipitation in an Fe-Cr-Ni-Al-Ti maraging steel [J]. Acta Mater., 2010, 58: 3733 |
| [94] | Liebscher C H, Radmilovi? V R, Dahmen U, et al. A hierarchical microstructure due to chemical ordering in the bcc lattice: Early stages of formation in a ferritic Fe-Al-Cr-Ni-Ti alloy [J]. Acta Mater., 2015, 92: 220 |
| [95] | Millán J, Sandl?bes S, Al-Zubi A, et al. Designing Heusler nanoprecipitates by elastic misfit stabilization in Fe-Mn maraging steels [J]. Acta Mater., 2014, 76: 94 |
| [96] | Delagnes D, Pettinari-Sturmel F, Mathon M H, et al. Cementite-free martensitic steels: A new route to develop high strength/high toughness grades by modifying the conventional precipitation sequence during tempering [J]. Acta Mater., 2012, 60: 5877 |
| [97] | Wang Y X, Guo X F, Hu C D, et al. Industrially produced 2.4 GPa ultra-strong steel via nanoscale dual-precipitates co-configuration [J]. Mater. Charact., 2024, 208: 113646 |
| [98] | Wang Y X, Li A J, Wang T, et al. Effects of NiAl on precipitation behavior and mechanical properties of M2C strengthened secondary hardening steel [J]. J. Mater. Res. Technol., 2025, 35: 3107 |
| [99] | Zhu H F, Xiong Z P, Mao J W, et al. Effect of ageing temperature on the microstructural evolution and mechanical properties in M2C and NiAl co-precipitation secondary hardening ultrahigh-strength steel [J]. J. Mater. Res. Technol., 2024, 30: 3522 |
| [100] | Liu X Q, Wang C C, Zhang Y F, et al. Design of a 2.7 GPa ultra-high-strength high Co-Ni secondary hardening steel by two-step nano-size precipitation tailoring [J]. J. Mater. Res. Technol., 2024, 28: 4212 |
| [101] | Xiao C J, Zhang Y P, Zhan D P, et al. Effect of Cu addition on the precipitation behavior of M2C carbides in maraging steel [J]. Mater. Charact., 2024, 210: 113846 |
| [102] | Peng R Z, Wu X C, Chen S N, et al. Evolution mechanism of Mo-rich, B2-NiAl, and Cu-rich particles under aging and its influence on strength and elongation in a maraging hot work steel SDH88 [J]. Mater. Sci. Eng., 2024, A916: 147317 |
| [103] | Galindo-Nava E I, Rainforth W M, Rivera-Díaz-del-Castillo P E J. Predicting microstructure and strength of maraging steels: Elemental optimisation [J]. Acta Mater., 2016, 117: 270 |
| [104] | Galindo-Nava E I, Rivera-Díaz-del-Castillo P E J. A model for the microstructure behaviour and strength evolution in lath martensite [J]. Acta Mater., 2015, 98: 81 |
| [105] | Follansbee P S, Kocks U F. A constitutive description of the deformation of copper based on the use of the mechanical threshold stress as an internal state variable [J]. Acta Metall., 1988, 36: 81 |
| [106] | Fleischer R L. Substitutional solution hardening [J]. Acta Metall., 1963, 11: 203 |
| [107] | Labusch R. A statistical theory of solid solution hardening [J]. Phys. Satus Solidi, 1970, 41b: 659 |
| [108] | Li Y J, Yuan G, Li L L, et al. Ductile 2-GPa steels with hierarchical substructure [J]. Science, 2023, 379: 168 |
| [109] | Kimura Y, Inoue T, Yin F X, et al. Inverse temperature dependence of toughness in an ultrafine grain-structure steel [J]. Science, 2008, 320: 1057 |
| [110] | Li Y Z, Huang M X. A method to calculate the dislocation density of a TWIP steel based on neutron diffraction and synchrotron X-ray diffraction [J]. Acta Metall. Sin., 2020, 56: 487 |
| 李亦庄, 黄明欣. 基于中子衍射和同步辐射X射线衍射的TWIP钢位错密度计算方法 [J]. 金属学报, 2020, 56: 487 | |
| [111] | Cong Z H, Murata Y. Dislocation density of lath martensite in 10Cr-5W heat-resistant steels [J]. Mater. Trans., 2011, 52: 2151 |
| [112] | Blankenship C P, Hornbogen E, Starke E A. Predicting slip behavior in alloys containing shearable and strong particles [J]. Mater. Sci. Eng., 1993, A169: 33 |
| [113] | Yong Q L. Secondary Phases in Steel [M]. Beijing: Metallurgical Industry Press, 2006: 442 |
| 雍岐龙. 钢铁材料中的第二相 [M]. 北京: 冶金工业出版社, 2006: 442 | |
| [114] | Ma K K, Wen H M, Hu T, et al. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy [J]. Acta Mater., 2014, 62: 141 |
| [115] | G?tz G, Blum W. Influence of thermal history on precipitation of hardening phases in tempered martensite 10%Cr-steel X12CrMo-WVNbN 10-1-1 [J]. Mater. Sci. Eng., 2003, A348: 201 |
| [116] | Wang F, Song M, Elkot M N, et al. Shearing brittle intermetallics enhances cryogenic strength and ductility of steels [J]. Science, 2024, 384: 1017 |
| [117] | Kapoor M. Design and development of bcc-copper- and B2 nickel-aluminium-precipitation-strengthened ferritic steel [D]. Evanston: Northwestern University, 2013 |
| [118] | Aghajani A, Somsen C, Eggeler G. On the effect of long-term creep on the microstructure of a 12% chromium tempered martensite ferritic steel [J]. Acta Mater., 2009, 57: 5093 |
| [119] | Zhang T Y, Zhang B, Xiao N, et al. Effect of austenitizing temperature on the microstructure and mechanical properties of a 2 GPa ultra-high strength steel [J]. Acta Metall. Sin., 2025, 61: 1353 |
| 张天宇, 张 鹏, 肖 娜 等. 奥氏体化温度对2 GPa超高强钢显微组织和力学性能的影响 [J]. 金属学报, 2025, 61: 1353 | |
| [120] | Baird J D. The effects of strain-ageing due to interstitial solutes on the mechanical properties of metals [J]. Metall. Rev., 1971, 16: 1 |
| [121] | Zener C. Theory of growth of spherical precipitates from solid solution [J]. J. Appl. Phys., 1949, 20: 950 |
| [122] | Gladman T. On the theory of the effect of precipitate particles on grain growth in metals [J]. Proc. Roy. Soc., 1966, 294A: 298 |
| [123] | Baldan A. Review Progress in Ostwald ripening theories and their applications to nickel-base superalloys Part I: Ostwald ripening theories [J]. J. Mater. Sci., 2002, 37: 2171 |
| [124] | Lifshitz I M, Slyozov V V. The Kinetics of precipitation from supersaturated solid solutions [J]. J. Phys. Chem. Solids, 1961, 19: 35 |
| [125] | Wagner C. Theorie der alterung von niederschl?gen durch uml?sen (Ostwald-Reifung) [J]. Z. Electrochemie, Ber. Bunsen. Phys. Chem., 1961, 65: 581 |
| [126] | Speight M V. Growth kinetics of grain-boundary precipitates [J]. Acta Metall., 1968, 16: 133 |
| [127] | Kirchner H O K. Coarsening of grain-boundary precipitates [J]. Metall. Trans., 1971, 2: 2861 |
| [128] | Ardell A J. On the coarsening of grain boundary precipitates [J]. Acta Metall., 1972, 20: 601 |
/
| 〈 |
|
〉 |