Research Status and Future Directions of Pure Mo and Mo-Based Biodegradable Metals
Received date: 2025-10-20
Revised date: 2026-02-11
Online published: 2026-03-24
Supported by
National Natural Science Foundation of China(52531008)
Mo, a trace element in the human body, has attracted increasing attention owing to its excellent mechanical properties, uniform degradation behavior, and favorable biocompatibility. The highlighted features make it a promising candidate for various biodegradable medical devices, including cardiovascular and neurovascular stents, cardiac pacemakers, gastrointestinal anastomotic staples, and wearable bioelectronic devices. Currently, Mo and its alloys have been developed as industrial materials and are well-established in aerospace, electronics, and chemical engineering. However, research on Mo and its alloys as biomaterials is an emerging field of study and faces several critical scientific challenges. In this review, we highlight Mo's intrinsic material characteristics, summarize traditional manufacturing methods and performance advantages, and outline its degradation mechanisms and biological responses in physiological environments. Furthermore, we propose design strategies for Mo-based biodegradable metals that consider biodegradability, biocompatibility, and the functional requirements of biodegradable implants, focusing on composition, microstructure, plastic deformation, and additive manufacturing. Finally, we discuss the future applications and developmental directions of Mo-based biodegradable metals in the field of biomaterials.
ZHENG Yufeng , SHEN Yunong . Research Status and Future Directions of Pure Mo and Mo-Based Biodegradable Metals[J]. Acta Metall Sin, 2026 , 62(5) : 905 -922 . DOI: 10.11900/0412.1961.2025.00323
| [1] | Lasheen T A, El-Ahmady M E, Hassib H B, et al. Molybdenum metallurgy review: Hydrometallurgical routes to recovery of molybdenum from ores and mineral raw materials [J]. Miner. Process. Extr. Metall. Rev., 2015, 36: 145 |
| [2] | Novotny J A, Peterson C A. Molybdenum [J]. Adv. Nutr., 2018, 9: 272 |
| [3] | Outteridge T, Kinsman N, Ronchi G, et al. Editorial: Industrial relevance of molybdenum in China [J]. Adv. Manuf., 2020, 8: 35 |
| [4] | Braithwaite E R, Haber J. Molybdenum: An Outline of Its Chemistry and Uses: Vol.19[M]. Amsterdam: Elsevier, 2013: 13 |
| [5] | Morales R, Aune R E, Seetharaman S, et al. The powder metallurgy processing of refractory metals and alloys [J]. JOM, 2003, 55(10): 20 |
| [6] | Lalik E. Kinetic analysis of reduction of MoO3 to MoO2 [J]. Catal. Today, 2011, 169: 85 |
| [7] | Tkachenko S, Oliver-Urrutia C, Ksenzova O, et al. Production of spherical Mo and Mo-Si powders by spray drying of Si suspension in a water-soluble Mo precursor [J]. Adv. Powder Technol., 2024, 35: 104313 |
| [8] | Garg P, Park S J, German R M. Effect of die compaction pressure on densification behavior of molybdenum powders [J]. Int. J. Refract. Met. Hard Mater., 2007, 25: 16 |
| [9] | Solodkyi I, Petrusha V, Grigoroscuta M A, et al. Efficient sintering of Mo matrix composites—A study of temperature dependences and the use of the sinter additive Ni [J]. Metals, 2023, 13: 1715 |
| [10] | Huang H S, Hwang K S. Deoxidation of molybdenum during vacuum sintering [J]. Metall. Mater. Trans., 2002, 33A: 657 |
| [11] | Tanvir G, Karim M A, Jadhav S, et al. Effect of hot isostatic pressing on porosity of wire-arc directed energy deposited TZM/NbZr1 bimetallic structure [J]. Virtual Phys. Prototy., 2024, 19: e2404989 |
| [12] | Atkinson H V, Davies S. Fundamental aspects of hot isostatic pressing: An overview [J]. Metall. Mater. Trans., 2000, 31A: 2981 |
| [13] | Mouawad B, Soueidan M, Fabrègue D, et al. Full densification of molybdenum powders using spark plasma sintering [J]. Metall. Mater. Trans., 2012, 43A: 3402 |
| [14] | Liu Z W, Wang A Q, Zhang Q F, et al. Microstructure evolution and process optimization of molybdenum rods during loose tooling forging [J]. Int. J. Refract. Met. Hard Mater., 2022, 108: 105926 |
| [15] | Primig S, Clemens H, Knabl W, et al. Orientation dependent recovery and recrystallization behavior of hot-rolled molybdenum [J]. Int. J. Refract. Met. Hard Mater., 2015, 48: 179 |
| [16] | Bian D, Tong Z P, Gong G C, et al. Additive manufacturing of biodegradable molybdenum—From powder to vascular stent [J]. Adv. Mater., 2024, 36: 2401614 |
| [17] | Zhao C, Shi B, Chen S L, et al. Laser melting modes in metal powder bed fusion additive manufacturing [J]. Rev. Mod. Phys., 2022, 94: 045002 |
| [18] | Wang D Z, Yu C F, Ma J, et al. Densification and crack suppression in selective laser melting of pure molybdenum [J]. Mater. Des., 2017, 129: 44 |
| [19] | Ramakrishnan T, Espiritu E R L, Kwon S, et al. Laser powder bed fusion additive manufacturing of molybdenum using a nitrogen build atmosphere [J]. Int. J. Refract. Met. Hard Mater., 2024, 119: 106555 |
| [20] | Leclercq A, Mouret T, Brailovski V. Laser powder bed fusion of molybdenum: Density, structure and mechanical properties at room and elevated temperatures [J]. Mater. Sci. Eng., 2025, A929: 148004 |
| [21] | Rebesan P, Ballan M, Bonesso M, et al. Pure molybdenum manufactured by laser powder bed fusion: Thermal and mechanical characterization at room and high temperature [J]. Add. Manuf., 2021, 47: 102277 |
| [22] | Yan A R, Atif A M, Wang X B, et al. The microstructure and cracking behaviors of pure molybdenum fabricated by selective laser melting [J]. Materials, 2022, 15: 6230 |
| [23] | Fu Z W, K?rner C. Actual state-of-the-art of electron beam powder bed fusion [J]. Eur. J. Mater., 2022, 2: 54 |
| [24] | Dejene N D, Lemu H G. Current status and challenges of powder bed fusion-based metal additive manufacturing: Literature review [J]. Metals, 2023, 13: 424 |
| [25] | B?hm J, Breuning C, Markl M, et al. A new approach of preheating and powder sintering in electron beam powder bed fusion [J]. Int. J. Adv. Manuf. Technol., 2024, 133: 3769 |
| [26] | Fernandez-Zelaia P, Ledford C, Ellis E A I, et al. Crystallographic texture evolution in electron beam melting additive manufacturing of pure molybdenum [J]. Mater. Des., 2021, 207: 109809 |
| [27] | Di Sturco S, Marchese G, Bondioli F, et al. Understanding the processability, microstructure, and mechanical properties of molybdenum processed by electron beam powder bed fusion [J]. Int. J. Refract. Met. Hard Mater., 2025, 129: 107091 |
| [28] | Gr?ger R, Bailey A G, Vitek V. Multiscale modeling of plastic deformation of molybdenum and tungsten: I. Atomistic studies of the core structure and glide of 1/2<111> screw dislocations at 0 K [J]. Acta Mater., 2008, 56: 5401 |
| [29] | Gr?ger R, Vitek V. Multiscale modeling of plastic deformation of molybdenum and tungsten. III. Effects of temperature and plastic strain rate [J]. Acta Mater., 2008, 56: 5426 |
| [30] | Kraych A, Clouet E, Dezerald L, et al. Non-glide effects and dislocation core fields in BCC metals [J]. npj Comput. Mater., 2019, 5: 109 |
| [31] | Zhang G, Chen G Q, Panwisawas C, et al. First-principles study of oxygen segregation and its effect on the embrittlement of molybdenum symmetrical tilt grain boundaries [J]. Acta Mater., 2023, 261: 119387 |
| [32] | Mueller A J, Bianco R, Buckman R W. Evaluation of oxide dispersion strengthened (ODS) molybdenum and molybdenum-rhenium alloys [J]. Int. J. Refract. Met. Hard Mater., 2000, 18: 205 |
| [33] | Tammas-Williams S, Withers P J, Todd I, et al. The influence of porosity on fatigue crack initiation in additively manufactured titanium components [J]. Sci. Rep., 2017, 7: 7308 |
| [34] | Cockeram B V. The role of stress state on the fracture toughness and toughening mechanisms of wrought molybdenum and molybdenum alloys [J]. Mater. Sci. Eng., 2010, A528: 288 |
| [35] | Pourbaix M. Atlas of Electrochemical Equilibria in Aqueous Solutions [M]. Brussels: Pergamon Press, 1966: 272 |
| [36] | Shen Y N, Cheng Y, Zheng Y F. Insight into the biodegradation behavior of pure molybdenum under simulated inflammatory condition [J]. Corros. Sci., 2024, 228: 111816 |
| [37] | Tong Z P, Gong G C, Huang H, et al. In vitro corrosion and biocompatibility of additively manufactured biodegradable molybdenum [J]. Acta Biomater., 2025, 191: 66 |
| [38] | Yin L, Cheng H Y, Mao S M, et al. Dissolvable metals for transient electronics [J]. Adv. Funct. Mater., 2014, 24: 645 |
| [39] | Hixson H, Sherwood P M A. Valence-band and core photoelectron spectroscopic studies of molybdenum aqueous oxidation and the influence of argon-ion etching [J]. J. Chem. Soc., Faraday Trans., 1995, 91: 3593 |
| [40] | Okonkwo I A, Doff J, Baron-Wieche? A, et al. Oxidation states of molybdenum in oxide films formed in sulphuric acid and sodium hydroxide [J]. Thin Solid Films, 2012, 520: 6318 |
| [41] | Petrova M, Bojinov M, Zanna S, et al. Mechanism of anodic oxidation of molybdenum in nearly-neutral electrolytes studied by electrochemical impedance spectroscopy and X-ray photoelectron spectroscopy [J]. Electrochim. Acta, 2011, 56: 7899 |
| [42] | Novotny J A, Turnlund J R. Molybdenum intake influences molybdenum kinetics in men [J]. J. Nutr., 2007, 137: 37 |
| [43] | Institute of Medicine. Dietary Reference Intakes for Vitamin A, Vitamin K, Arsenic, Boron, Chromium, Copper, Iodine, Iron, Manganese, Molybdenum, Nickel, Silicon, Vanadium, and Zinc [M]. Washington: National Academies Press, 2001: 420 |
| [44] | Novotny J A. Molybdenum nutriture in humans [J]. J. Evid. Based Complementary Altern. Med., 2011, 16: 164 |
| [45] | Brewer G J, Askari F, Dick R B, et al. Treatment of Wilson’s disease with tetrathiomolybdate: V. Control of free copper by tetrathiomolybdate and a comparison with trientine [J]. Transl. Res., 2009, 154: 70 |
| [46] | Harrison R. Structure and function of xanthine oxidoreductase: Where are we now? [J]. Free Radical Biol. Med., 2002, 33: 774 |
| [47] | Polito L, Bortolotti M, Battelli M G, et al. Xanthine oxidoreductase: A leading actor in cardiovascular disease drama [J]. Redox Biol., 2021, 48: 102195 |
| [48] | Battelli M G, Bortolotti M, Polito L, et al. The role of xanthine oxidoreductase and uric acid in metabolic syndrome [J]. Biochim. Biophys. Acta Mol. Basis Dis., 2018, 1864: 2557 |
| [49] | Kelley E E. Biochemistry of molybdopterin nitrate/nitrite reductases [A]. Nitric Oxide: Biology and Pathobiology [M]. London: Elsevier, 2017: 173 |
| [50] | Terao M, Rom?o M J, Leimkühler S, et al. Structure and function of mammalian aldehyde oxidases [J]. Arch. Toxicol., 2016, 90: 753 |
| [51] | Shintani Y, Maruoka S, Gon Y, et al. Nuclear factor erythroid 2-related factor 2 (Nrf2) regulates airway epithelial barrier integrity [J]. Allergol. Int., 2015, 64(suppl.) : S54 |
| [52] | Shaw S, Jayatilleke E. The role of aldehyde oxidase in ethanol-induced hepatic lipid peroxidation in the rat [J]. Biochem. J., 1990, 268: 579 |
| [53] | Burzlaff A, Beevers C, Pearce H, et al. New studies on the in vitro genotoxicity of sodium molybdate and their impact on the overall assessment of the genotoxicity of molybdenum substances [J]. Regul. Toxicol. Pharm., 2017, 86: 279 |
| [54] | Barceloux D G, Barceloux D. Molybdenum [J]. J. Toxicol.: Clin. Toxicol., 1999, 37: 231 |
| [55] | Vysko?il A, Viau C. Assessment of molybdenum toxicity in humans [J]. J. Appl. Toxicol., 1999, 19: 185 |
| [56] | Murray F J, Sullivan F M, Tiwary A K, et al. 90-day subchronic toxicity study of sodium molybdate dihydrate in rats [J]. Regul. Toxicol. Pharm., 2014, 70: 579 |
| [57] | Bandyopadhyay S K, Chatterjee K, Tiwari R K, et al. Biochemical studies on molybdenum toxicity in rats: Effects of high protein feeding [J]. Int. J. Vitam. Nutr. Res., 1981, 51: 401 |
| [58] | Bompart G, Pécher C, Prévot D, et al. Mild renal failure induced by subchronic exposure to molybdenum: urinary kallikrein excretion as a marker of distal tubular effect [J]. Toxicol. Lett., 1990, 52: 293 |
| [59] | Ott H C, Prior C, Herold M, et al. Respiratory symptoms and bronchoalveolar lavage abnormalities in molybdenum exposed workers [J]. Wien. Klin. Wochenschr., 2004, 116(suppl.): 25 |
| [60] | National Toxicology Program. Toxicology and carcinogenesis studies of molybdenum trioxide [R]. Research Triangle Park, NC: U.S. Dept. of Health and Human Services, Public Health Service, National Institutes of Health, 1997 |
| [61] | Shiue I, Hristova K. Higher urinary heavy metal, phthalate and arsenic concentrations accounted for 3-19% of the population attributable risk for high blood pressure: US NHANES, 2009-2012 [J]. Hypertens. Res., 2014, 37: 1075 |
| [62] | Schroeder H A, Kraemer L A. Cardiovascular mortality, municipal water, and corrosion [J]. Arch. Environ. Health: Int. J., 1974, 28: 303 |
| [63] | Bortolotti M, Polito L, Battelli M G, et al. Xanthine oxidoreductase: One enzyme for multiple physiological tasks [J]. Redox Biol., 2021, 41: 101882 |
| [64] | He W L, Kwesiga M P, Gebreyesus E, et al. Nitric oxide and oxidative stress-mediated cardiovascular functionality: From molecular mechanism to cardiovascular disease [A]. Vascular Biology-Selection of Mechanisms and Clinical Applications [M]. London: IntechOpen, 2019: 78 |
| [65] | Byon C H, Heath J M, Chen Y B. Redox signaling in cardiovascular pathophysiology: A focus on hydrogen peroxide and vascular smooth muscle cells [J]. Redox Biol, 2016, 9: 244 |
| [66] | Beckman J S, Koppenol W H. Nitric oxide, superoxide, and peroxynitrite: The good, the bad, and ugly [J]. Am. J. Physiol. Cell Physiol., 1996, 271: C1424 |
| [67] | White C R, Brock T A, Chang L Y, et al. Superoxide and peroxynitrite inatherosclerosis. [J]. Proc. Natl. Acad. Sci. USA, 1994, 91: 1044 |
| [68] | Leeuwenburgh C, Hardy M M, Hazen S L, et al. Reactive nitrogen intermediates promote low density lipoprotein oxidation in human atherosclerotic intima [J]. J. Biol. Chem., 1997, 272: 1433 |
| [69] | Patetsios P, Song M, Shutze W P, et al. Identification of uric acid and xanthine oxidase in atherosclerotic plaque [J]. Am. J. Cardiol., 2001, 88: 188 |
| [70] | Nomura J, Busso N, Ives A, et al. Xanthine oxidase inhibition by febuxostat attenuates experimental atherosclerosis in mice [J]. Sci. Rep., 2014, 4: 4554 |
| [71] | Koval’Skii V V, Iarovaia G A, Shmavonian D M. Modification of human and animal purine metabolism in conditions of various molybdenum bio-geochemical areas [J]. Zh. Obshch. Biol., 1961, 22: 179 |
| [72] | Yan Z Y, Liu Z X, Yang B W, et al. Long-term exposure of molybdenum disulfide nanosheets leads to hepatic lipid accumulation and atherogenesis in apolipoprotein E deficient mice [J]. NanoImpact, 2023, 30: 100462 |
| [73] | Sikora-Jasinska M, Morath L M, Kwesiga M P, et al. In-vivo evaluation of molybdenum as bioabsorbable stent candidate [J]. Bioact. Mater., 2022, 14: 262 |
| [74] | Schauer A, Redlich C, Scheibler J, et al. Biocompatibility and degradation behavior of molybdenum in an in vivo rat model [J]. Materials, 2021, 14: 7776 |
| [75] | Shen Y N, Huang Y M, Zhang Y, et al. Ultrafine molybdenum wire braided neurointerventional implants: Bridging biodegradability and neurovascular safety for stroke treatment [J]. Adv. Sci., 2026, 13: e11466 |
| [76] | Curry E J, Ke K, Chorsi M T, et al. Biodegradable piezoelectric force sensor [J]. Proc. Natl. Acad. Sci. USA, 2018, 115: 909 |
| [77] | Kang S K, Murphy R K J, Hwang S W, et al. Bioresorbable silicon electronic sensors for the brain [J]. Nature, 2016, 530: 71 |
| [78] | Yin L, Huang X, Xu H X, et al. Materials, designs, and operational characteristics for fully biodegradable primary batteries [J]. Adv. Mater., 2014, 26: 3879 |
| [79] | Yu K J, Kuzum D, Hwang S W, et al. Bioresorbable silicon electronics for transient spatiotemporal mapping of electrical activity from the cerebral cortex [J]. Nat. Mater., 2016, 15: 782 |
| [80] | Yang Q S, Liu T L, Xue Y G, et al. Ecoresorbable and bioresorbable microelectromechanical systems [J]. Nat. Electron., 2022, 5: 526 |
| [81] | Song J W, Ryu H, Bai W B, et al. Bioresorbable, wireless, and battery-free system for electrotherapy and impedance sensing at wound sites [J]. Sci. Adv., 2023, 9: eade4687 |
| [82] | Hu P, Yang F, Wang K S, et al. Preparation and ductile-to-brittle transition temperature of the La-TZM alloy plates [J]. Int. J. Refract. Met. Hard Mater., 2015, 52: 131 |
| [83] | Chen X C, Wang C, Ju H J, et al. Microstructure, room-temperature mechanical properties, and oxidation resistance of Ti-added Mo-Si-B alloys fabricated via hot pressing sintering [J]. J. Alloys Compd., 2025, 1010: 177634 |
| [84] | Cheng P M, Yang C, Zhang P, et al. Enhancing the high-temperature creep properties of Mo alloys via nanosized La2O3 particle addition [J]. J. Mater. Sci. Technol., 2022, 130: 53 |
| [85] | Hu W Q, Du Z F, Dong Z Z, et al. The synthesis of TiC dispersed strengthened Mo alloy by freeze-drying technology and subsequent low temperature sintering [J]. Scr. Mater., 2021, 198: 113831 |
| [86] | Chen Y J, Fang Y, Cheng P M, et al. The origin of exceptionally large ductility in molybdenum alloys dispersed with irregular-shaped La2O3 nano-particles [J]. Nat. Commun., 2024, 15: 4105 |
| [87] | Liu Y, Zheng Y F, Chen X H, et al. Fundamental theory of biodegradable metals—Definition, criteria, and design [J]. Adv. Funct. Mater., 2019, 29: 1805402 |
| [88] | Ashby M F, Cebon D. Materials selection in mechanical design [J]. J. Phys. IV France, 1993, 3: C7-1 |
| [89] | Dang W T, Wang X Y, Li J Y, et al. 3D printing of Mo-containing scaffolds with activated anabolic responses and bi-lineage bioactivities [J]. Theranostics, 2018, 8: 4372 |
| [90] | Tian B M, Li X, Zhang J J, et al. A 3D-printed molybdenum-containing scaffold exerts dual pro-osteogenic and anti-osteoclastogenic effects to facilitate alveolar bone repair [J]. Int. J. Oral Sci., 2022, 14: 45 |
| [91] | He X T, Li X, Zhang M, et al. Role of molybdenum in material immunomodulation and periodontal wound healing: Targeting immunometabolism and mitochondrial function for macrophage modulation [J]. Biomaterials, 2022, 283: 121439 |
| [92] | Liu D Y, Chen J H, Zhou J N, et al. Macrophage-related inflammatory responses to degradation products of biodegradable molybdenum implants [J]. Mater. Today Bio, 2025, 31: 101519 |
| [93] | Jing K, Liu R, Xie Z M, et al. Excellent high-temperature strength and ductility of the ZrC nanoparticles dispersed molybdenum [J]. Acta Mater., 2022, 227: 117725 |
| [94] | Liu G, Zhang G J, Jiang F, et al. Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility [J]. Nat. Mater., 2013, 12: 344 |
| [95] | Shi C X, Li H D, Zhou L. Materials Science and Engineering Handbook [M]. Beijing: Chemical Industry Press, 2004: 16 |
| 师昌绪, 李恒德, 周 廉. 材料科学与工程手册 [M]. 北京: 化学工业出版社, 2004: 16 |
/
| 〈 |
|
〉 |