Effect of Heat Treatment on Microstructural Evolution and Mechanical Properties of Inertial Friction Welded Joints for FGH96 Superalloy
Received date: 2025-10-31
Revised date: 2025-12-15
Online published: 2026-03-16
Supported by
National Natural Science Foundation of China(52375313);National Natural Science Foundation of China(51605075)
Aero engines serve as a critical indicator of national comprehensive strength and technological advancement. However, their performance enhancement poses considerable challenges to the manufacturing technologies of hot-end components. Hot-end structures undergo inertial friction welding, which effectively avoids the defects associated with fusion welding and has been widely adopted for high-quality joining of these structures. This study addresses the inherent process limitations of inertial friction welded joints, including strengthening phase dissolution within the welding zone (WZ), along with axial and radial microstructural heterogeneity, and proposes a customized post-weld heat treatment (PWHT) strategy for inertial friction welded joints of FGH96 superalloys. A systematic investigation was conducted on the effects of solution aging and double aging on microstructural evolution and mechanical properties. The results indicated that increasing the solution temperature leads to grain coarsening and enhanced recrystallization, accompanied by pronounced precipitation and growth of the γ′ strengthening phase, a more uniform carbide distribution, and intensified grain boundary serration within the WZ compared to joints at low solution temperature. At a solution temperature of 1140 oC, abnormal grain growth occurred, along with coarsening and inhomogeneous distribution of the γ′ strengthening phase. After solution aging, the impact toughness of the joints improved with increasing solution temperature, whereas the tensile strength initially increased and then decreased. At the solution temperature of 1080 oC, the grain size and γ′ strengthening phase were moderate and uniformly distributed, the degree of recrystallization and grain boundary serration were relatively high, carbides were uniformly dispersed, and microstructural inhomogeneity was notably improved. Under this condition, the ultimate tensile strengths of the joints at room temperature and 750 °C were 1455 and 1042 MPa, respectively; and the impact toughness reached 41 J/cm2, demonstrating an optimal strength-toughness synergy. Double aging promoted the uniform precipitation of tertiary γ′ strengthening phase in the WZ, resulting in tensile strengths of 1574 and 1279 MPa at room temperature and 750 oC, respectively, approaching base metal levels. Meanwhile, the hardness was considerably enhanced beyond the base metal, although the impact toughness was slightly reduced compared with the as-welded joints.
WANG Bin , ZHAO Peng , LIU Jiawei , ZHANG Chunbo , QIN Zhiwei , DONG Honggang , LI Peng . Effect of Heat Treatment on Microstructural Evolution and Mechanical Properties of Inertial Friction Welded Joints for FGH96 Superalloy[J]. Acta Metall Sin, 2026 , 62(6) : 1043 -1058 . DOI: 10.11900/0412.1961.2025.00350
| [1] | Bai R S, Tan Y, Cui H Y, et al. Effect of electron beam smelting power on microstructure, segregation, and γ′ phase precipitation behavior of GH4068 alloy[J]. Acta Metall. Sin., 2024, 60: 1189 |
| 白如圣, 谭 毅, 崔弘阳 等. 电子束熔炼功率对GH4068合金微观组织、偏析和γ′相析出行为的影响[J]. 金属学报, 2024, 60: 1189 | |
| [2] | Peng Z C, Luo J P, Zhao Y, et al. Evolution of microstrucutre during static recrystallization in FGH96 superalloy[J]. Acta Metall. Sin., 2025, 61: 235 |
| 彭子超, 罗俊鹏, 赵 宇 等. FGH96合金静态再结晶过程的显微组织演化[J]. 金属学报, 2025, 61: 235 | |
| [3] | Zhou Q, Ding Q Q, Liu D Y, et al. The grain boundary brittleness at intermediate temperature in a precipitation strengthened Ni-based polycrystalline alloy[J]. Acta Mater., 2025, 285: 120681 |
| [4] | Zhou Y, Fang X W, Xi N Y, et al. Enhanced strength and ductility of laser-directed energy deposition repaired IN718 superalloy via a novel tailored heat treatment[J]. J. Mater. Sci. Technol., 2024, 199: 86 |
| [5] | Li C A, Qin G L, Fu B L, et al. Simulation of interfacial friction regime transition in inertia friction welding[J]. Int. J. Mech. Sci., 2025, 303: 110643 |
| [6] | Liu Y, Liu Y F, Zhang S R, et al. Diffusion behavior of oxygen in FGH96 superalloys during consolidation process[J]. Corros. Sci., 2024, 238: 112357 |
| [7] | Liu Y, Zhang S, Zhang L, et al. A new perspective about the surface structure of FGH96 superalloys powders[J]. Vacuum, 2024, 220: 112838 |
| [8] | Qin Z W, Zhao Q, Zhang L, et al. Research progress on inertial friction welding of nickel-based superalloy GH4065A and IN718[J]. J. Net. Form. Eng., 2024, 16(10): 28 |
| 秦志伟, 赵 强, 张 露 等. 镍基高温合金GH4065A与IN718惯性摩擦焊接研究进展[J]. 精密成形工程, 2024, 16(10): 28 | |
| [9] | Wang J W, Wang H M, Gao H W, et al. Microstructure characteristics and failure mechanisms of hybrid manufacturing of FGH96 and IC10 bimetal component using laser directed energy deposition[J]. Mater. Sci. Eng., 2024, A889: 145965 |
| [10] | Xu X X, You G Q, Ding Y H, et al. Microstructure and mechanical properties of inertia friction welded joints between high-strength low-alloy steel and medium carbon steel[J]. J. Mater. Process. Technol., 2020, 286: 116811 |
| [11] | Wang B, Liu J W, Qin Z W, et al. Cumulative strain-induced gradient heterostructure for synchronously boosting mechanical properties and corrosion resistance[J]. J. Mater. Sci. Technol., 2026, 270: 1 |
| [12] | Tang T X, Shi Q Y, Zhang C B, et al. Elucidating the in-process interfacial friction regime and thermal responses during inertia friction welding of dissimilar superalloys[J]. J. Mater. Res. Technol., 2024, 30: 1650 |
| [13] | Li C A, Qin G L, Wang H. Omnidirectional simulation analysis of thermo-mechanical coupling mechanism in inertia friction welding of Ni-based superalloy[J]. Chin. J. Aeronaut., 2025, 38: 103047 |
| [14] | Cao K, Fan J K, Liu X D, et al. Microstructure and mechanical properties of nickel-based wrought superalloys under thermal-mechanical coupling: A review with Inconel 718, 625 as main cases[J]. Prog. Nat. Sci., 2025, 35: 65 |
| [15] | Zhang C B, Liang W, Zhou J, et al. Effect of heat treatment on microstructure and microhardness of FGH96 inertia friction welding[J]. Trans. China Weld. Inst., 2023, 44(8): 57 |
| 张春波, 梁 武, 周 军 等. 热处理工艺对FGH96合金惯性摩擦焊组织与显微硬度的影响[J]. 焊接学报, 2023, 44(8): 57 | |
| [16] | Li Y M, Liu C X, Yu L M, et al. Effect of high-temperature ageing on microstructure and mechanical properties of linear friction welded S31042 steel joint[J]. Acta Metall. Sin., 2018, 54: 981 |
| 李彦默, 刘晨曦, 余黎明 等. 高温时效对S31042钢线性摩擦焊接头组织和力学性能的影响[J]. 金属学报, 2018, 54: 981 | |
| [17] | Gai Y C, Zhang R, Yang J X, et al. Effects of heat treatment on γ′ precipitates and tensile properties of a Ni-base superalloy[J]. Mater. Sci. Eng., 2022, A842: 143079 |
| [18] | Li H Y, Sun J F, Hardy M C, et al. Effects of microstructure on high temperature dwell fatigue crack growth in a coarse grain PM nickel based superalloy[J]. Acta Mater., 2015, 90: 355 |
| [19] | Semiatin S L, Levkulich N C, Saurber A E, et al. The kinetics of precipitate dissolution in a nickel-base superalloy[J]. Metall. Mater. Trans., 2017, 48A: 5567 |
| [20] | Liu J T, Liu G Q, Hu B F, et al. Study on grain growth of P/M FGH96 superalloy[J]. Trans. Mater. Heat Treat., 2004, 25(6): 25 |
| 刘建涛, 刘国权, 胡本芙 等. FGH96合金晶粒长大规律的研究[J]. 材料热处理学报, 2004, 25(6): 25 | |
| [21] | Yang J, Li J L, Xiong J T, et al. Effect of solution treatment temperature on the γ′ precipitation distribution, high temperature tensile and fatigue properties of FGH96 joints prepared by inertia friction welding[J]. Mater. Res. Express, 2019, 6: 1165g9 |
| [22] | Han X F, Zhu G L, Tan Q B, et al. Effect of semi-aging heat treatment on microstructure and mechanical properties of an inertia friction welded joint of FGH96 powder metallurgy superalloy[J]. Metals, 2023, 13: 632 |
| [23] | Hao Z B, Tian T, Peng S Q, et al. Effect of heat treatment on microstructure and properties of FGH4096M superalloy processed by selective laser melting[J]. Met. Mater. Int., 2020, 26: 1270 |
| [24] | Fang B, Ji Z, Tian G F, et al. Investigation on complete solution temperature of γ' in the P/M superalloy of FGH96[J]. Powder Metall. Technol., 2013, 31(02): 89 |
| 方 彬, 纪 箴, 田高峰 等. FGH96高温合金中γ'相完全溶解温度的研究[J]. 粉末冶金技术, 2013, 31(02): 89 | |
| [25] | Zhang C, Shen W F, Zhang L W, et al. The microstructure and gamma prime distributions in inertia friction welded joint of P/M superalloy FGH96[J]. J. Mater. Eng. Perform., 2017, 26: 1581 |
| [26] | Yang J, Li J L, Jin F. Effect of welding parameters on high-temperature tensile and fatigue properties of FGH96 inertia friction welded joints[J]. Weld. World, 2019, 63: 1033 |
| [27] | Senkov O N, Mahaffey D W, Semiatin S L. Effect of process parameters on process efficiency and inertia friction welding behavior of the superalloys LSHR and Mar-M247[J]. J. Mater. Process. Technol., 2017, 250: 156 |
| [28] | Zheng K K, Yang Z K, Mou G. Effect of inertia friction welding speed on microstructure and mechanical properties of 2205/316L stainless steel joints[J]. Mater. Today Commun., 2023, 35: 106226 |
| [29] | Liu Y Y, Tian W T, Yang Q H, et al. Inertia radial friction welding of Ti60(near-α)/TC18(near-β) bimetallic components: Interfacial bon-ding mechanism, heterogenous microstructure and mechanical properties[J]. Mater. Charact., 2024, 208: 113598 |
| [30] | Pan L W, Li P, Hao X H, et al. Inhomogeneity of microstructure and mechanical properties in radial direction of aluminum/copper friction welded joints[J]. J. Mater. Process. Technol., 2018, 255: 308 |
| [31] | Mishra N K, Manikandan S G K, Shrivastava A. Interfacial inhomogeneous plastic deformation during rotary friction welding of dissimilar AA2219-SS321 joint combination with AA6061 interlayer[J]. J. Adv. Join. Process., 2024, 10: 100245 |
| [32] | Zhao P, Li P, Ding Z J, et al. Microstructural characterization and mechanical properties of inertia friction welded FGH96 joints[J]. Mater. Today Commun., 2025, 42: 111194 |
/
| 〈 |
|
〉 |