Overview

Fatigue Small Crack Behavior of TiAl Alloys

  • XIANG Henggao ,
  • Song Weidong ,
  • JIA Luyi ,
  • QI Zhixiang ,
  • CHEN Yang ,
  • ZHOU Bing ,
  • ZHENG Gong ,
  • YING Pan ,
  • CHEN Guang
Expand
  • 1 State Key Laboratory of Light Superalloys, Nanjing Research Base, Nanjing University of Science and Technology, Nanjing 210094, China
    2 National Key Laboratory of Advanced Casting Technologies, Nanjing University of Science and Technology, Nanjing 210094, China
    3 Nanjing Belight Laboratory, Nanjing 210094, China
CHEN Yang, professor, Tel: (025)84315159, E-mail: yang.chen@njust.edu.cn

Received date: 2025-11-12

  Revised date: 2026-01-12

  Online published: 2026-03-13

Supported by

National Natural Science Foundation of China(12202201);National Natural Science Foundation of China(52571145);National Natural Science Foundation of China(92463301);National Natural Science Foundation of China(52433016);National Natural Science Foundation of China(92163215);National Natural Science Foundation of China(52305379);National Natural Science Foundation of China(52174364);National Natural Science Foundation of China(52595663);Jiangsu Provincial Natural Science Foundation(BK20243066);Jiangsu Provincial Natural Science Foundation(BE2023024);State Key Laboratory of Light Superalloys(Sysjj2025203);State Key Laboratory of Light Superalloys(Sysjj2025101)

Abstract

TiAl alloys are important lightweight materials for aerospace propulsion systems owing to their low density, creep resistance, corrosion resistance, and other properties. Fatigue is the primary failure mode of aeroengine blades. Once a long crack forms in a blade, rapid fracture can occur. The initiation and propagation of small fatigue cracks therefore directly determine the service life of blades. Focusing on the issue of small fatigue cracks in TiAl alloys, this paper systematically reviews the definition and characteristics of small fatigue cracks and summarizes the mechanisms of crack initiation and propagation in TiAl alloys. In addition, the propagation models of small fatigue cracks, together with their applicability and limitations, are discussed. Finally, future perspectives are presented regarding the characterization of fatigue small-crack initiation and propagation behavior and the development of unified life prediction methods for TiAl alloys.

Cite this article

XIANG Henggao , Song Weidong , JIA Luyi , QI Zhixiang , CHEN Yang , ZHOU Bing , ZHENG Gong , YING Pan , CHEN Guang . Fatigue Small Crack Behavior of TiAl Alloys[J]. Acta Metall Sin, 2026 , 62(5) : 721 -732 . DOI: 10.11900/0412.1961.2025.00367

References

[1] Chen G, Peng Y B, Zheng G, et al. Polysynthetic twinned TiAl single crystals for high-temperature applications [J]. Nat. Mater., 2016, 15: 876
[2] Kear B H, Thompson E R. Aircraft gas turbine materials and processes [J]. Science, 1980, 208: 847
[3] Lasalmonie A. Intermetallics: Why is it so difficult to introduce them in gas turbine engines? [J]. Intermetallics, 2006, 14: 1123
[4] Chen Y Y, Shi G H, Du Z M, et al. Research progress on additive manufacturing TiAl alloy [J]. Acta Metall. Sin., 2024, 60: 1
  陈玉勇, 时国浩, 杜之明 等. 增材制造TiAl合金的研究进展 [J]. 金属学报, 2024, 60: 1
[5] Chen G, Chen F R, Zhu D M, et al. Polysynthetic twinned high-performance TiAl alloy with ordered structures of functional units [J]. Acta Metall. Sin., 2026, 62: 541
  陈 光, 陈奉锐, 朱德民 等. 聚片孪生功能基元序构的高性能TiAl合金 [J]. 金属学报, 2026, 62: 541
[6] Bewlay B P, Nag S, Suzuki A, et al. TiAl alloys in commercial aircraft engines [J]. Mater. High Temp., 2016, 33: 549
[7] Ma N N, Tao C H, He Y H, et al. Research progress of multiaxial fatigue test methods on blades of aviation engine [J]. J. Aeronaut. Mater., 2012, 32(6): 44
  马楠楠, 陶春虎, 何玉怀 等. 航空发动机叶片多轴疲劳试验研究进展 [J]. 航空材料学报, 2012, 32(6): 44
[8] Miller K J. The behaviour of short fatigue cracks and their initiation part II—A general summary [J]. Fatigue Fract. Eng. Mater. Struct., 1987, 10: 93
[9] Xu L, Huang S J, Hui L, et al. Small fatigue crack growth behavior of TB6 titanium alloy [J]. J. Mater. Eng., 2019, 47(11): 171
  许 良, 黄双君, 回 丽 等. TB6钛合金疲劳小裂纹扩展行为 [J]. 材料工程, 2019, 47(11): 171
[10] Meyers M A, Chawla K K, translated by Zhang Z F, Lu L. Mechanical Behavior of Materials [M]. 2nd Ed., Beijing: Higher Education Press, 2017: 787
  Meyers M A, Chawla K K著, 张哲峰, 卢 磊 译. 材料的力学行为 [M]. 第2版. 北京: 高等教育出版社, 2017: 787
[11] Kruzic J J, Campbell J P, Ritchie R O. On the fatigue behavior of γ-based titanium aluminides: Role of small cracks [J]. Acta Mater., 1999, 47: 801
[12] Pearson S. Initiation of fatigue cracks in commercial aluminium alloys and the subsequent propagation of very short cracks [J]. Eng. Fract. Mech., 1975, 7: 235
[13] Wu X R, Newman J C, Zhao W, et al. Small‐crack growth and fatigue life predictions for high‐strength aluminium alloys. Part II: Crack closure and fatigue analyses [J]. Fatigue Fract. Eng. Mater. Struct., 2000, 23: 59
[14] Findley K O, Evans J L, Saxena A. A critical assessment of fatigue crack nucleation and growth models for Ni- and Ni,Fe-based superalloys [J]. Int. Mater. Rev., 2011, 56: 49
[15] Hironobu N, Masahiro G, Norio K. A small-crack growth law and its related phenomena [J]. Eng. Fract. Mech., 1992, 41(4): 499
[16] Hanlon T, Tabachnikova E D, Suresh S. Fatigue behavior of nanocrystalline metals and alloys [J]. Int. J. Fatigue, 2005, 27: 1147
[17] Yang Q Z, Yang X G, Huang W Q, et al. Propagation behaviors of small cracks in powder metallurgy nickel-based superalloy FGH4096 [J]. Acta Metall. Sin., 2022, 58: 683
  杨秦政, 杨晓光, 黄渭清 等. 粉末高温合金FGH4096的疲劳小裂纹扩展行为 [J]. 金属学报, 2022, 58: 683
[18] Tokaji K, Ogawa T, Harada Y. The growth of small fatigue cracks in a low carbon steel; the effect of microstructure and limitations of linear elastic fracture mechanics [J]. Fatigue Fract. Eng. Mater. Struct., 1986, 9: 205
[19] Shibanuma K, Ueda K, Ito H, et al. Model for predicting fatigue life and limit of steels based on micromechanics of small crack growth [J]. Mater. Des., 2018, 139: 269
[20] Jiao Z H, Yu H C, Dong C L, et al. Propagation behavior of small and long fatigue cracks in TiAl alloy at elevated temperature [J]. Rare Met. Mater. Eng., 2019, 48: 538
  焦泽辉, 于慧臣, 董成利 等. TiAl合金高温疲劳小裂纹与长裂纹扩展行为 [J]. 稀有金属材料与工程, 2019, 48: 538
[21] Zhu S J, Peng L M, Moriya T, et al. Effect of stress ratio on fatigue crack growth in TiAl intermetallics at room and elevated temperatures [J]. Mater. Sci. Eng., 2000, A290: 198
[22] Wang C H, Miller K J. Short fatigue crack growth under mean stress, uniaxial loading [J]. Fatigue Fract. Eng. Mater. Struct., 1993, 16: 181
[23] Suresh S, Ritchie R O. Propagation of short fatigue cracks [J]. Int. Met. Rev., 1984, 29: 445
[24] Zhao G L, Qi H Y, Li S L, et al. Effects of tensile load hold time on the fatigue and corrosion-fatigue behavior of turbine blade materials [J]. Int. J. Fatigue, 2021, 152: 106448
[25] Pippan R, Hageneder P, Knabl W, et al. Fatigue threshold and crack propagation in γ-TiAl sheets [J]. Intermetallics, 2001, 9: 89
[26] Zhao G L, Qi H Y, Li S L, et al. Review of fatigue small cracks in key components of gas turbine engines [J]. Adv. Mech., 2023, 53: 819
  赵高乐, 齐红宇, 李少林 等. 燃气涡轮发动机关键部件疲劳小裂纹研究进展 [J]. 力学进展, 2023, 53: 819
[27] Hong Y S, Fang B. Microscopic process and description for the initiation and propagation of short fatigue cracks [J]. Adv. Mech., 1993, 23: 468
  洪友士, 方 飚. 疲劳短裂纹萌生及发展的细观过程和理论 [J]. 力学进展, 1993, 23: 468
[28] Ritchie R O, Lankford J. Small fatigue cracks: A statement of the problem and potential solutions [J]. Mater. Sci. Eng., 1986, 84: 11
[29] ASTM International. ASTM E1823-24a Standard terminology relating to fatigue and fracture testing [S]. West Conshohocken: ASTM International, 2024
[30] Mutoh Y, Moriya T, Zhu S J, et al. Initiation and growth of small fatigue crack in TiAl intermetallics at elevated and room temperatures [J]. J. Soc. Mater. Sci., Jpn., 1998, 47: 19
[31] Li T R, Xu Y Q, Wu W P, et al. Effects of V and B on the microstructure evolution and deformation mechanisms of Ti-44Al-5Nb-1Mo alloys [J]. Acta Metall. Sin., 2024, 60: 650
  李天瑞, 许瑜倩, 吴文平 等. V和B元素对Ti-44Al-5Nb-1Mo合金显微组织及热变形机制的影响 [J]. 金属学报, 2024, 60: 650
[32] Zuo Z B, Hu R, Luo X, et al. Solidification behavior and microstructures characteristics of Ti-48Al-3Nb-1.5Ta powder produced by supreme-speed plasma rotating electrode process [J]. Acta Metall. Sin. (Engl. Lett.), 2023, 36: 1221
[33] Chan K S, Shih D S. Fundamental aspects of fatigue and fracture in a TiAl sheet alloy [J]. Metall. Mater. Trans., 1998, 29A: 73
[34] Wessel W, Zeismann F, Brueckner-Foit A. Short fatigue cracks in intermetallic γ-TiAl-alloys [J]. Fatigue Fract. Eng. Mater. Struct., 2015, 38: 1507
[35] Edwards T E J. Recent progress in the high-cycle fatigue behaviour of γ-TiAl alloys [J]. Mater. Sci. Eng., 2018, 34: 1919
[36] Zhang M, Song X P, Yu L, et al. Fatigue small crack growth threshold determination of a high-Nb TiAl alloy at different temperatures by in-situ observation [J]. Int. J. Miner., Metall., Mater., 2013, 20: 1192
[37] Wang L, Huang X Y, Zhao P T, et al. Investigation of fatigue small crack propagation of TiAl alloy at 750 oC [J]. Failure Anal. Prev., 2018, 13: 159
  王 亮, 黄新跃, 赵澎涛. TiAl合金750 ℃下疲劳小裂纹行为研究 [J]. 失效分析与预防, 2018, 13: 159
[38] Cottrell A H. Theory of brittle fracture in steel and similar metals [J]. Trans. Metall. Soc. AIME, 1958, 212: 192
[39] Huang Z W, Bowen P. Persistent microslip bands in the lamellar TiAl structure subjected to room temperature fatigue [J]. Scr. Mater., 2001, 45: 931
[40] Ding R G, Li H Y, Hu D W, et al. Features of fracture surface in a fully lamellar TiAl-base alloy [J]. Intermetallics, 2015, 58: 36
[41] Yang J, Li H, Hu D, et al. Microstructural characterisation of fatigue crack growth fracture surfaces of lamellar Ti45Al2Mn2Nb1B [J]. Intermetallics, 2014, 45: 89
[42] Bode B, Wessel W, Brueckner-Foit A, et al. Local deformation at micro‐notches and crack initiation in an intermetallic γ‐TiAl‐alloy [J]. Fatigue Fract. Eng. Mater. Struct., 2016, 39: 227
[43] Tanaka K, Mura T. A dislocation model for fatigue crack initiation [J]. J. Appl. Mech., 1981, 48: 97
[44] Motoyashiki Y, Brückner-Foit A, Sugeta A. Investigation of small crack behaviour under cyclic loading in a dual phase steel with an FIB tomography technique [J]. Fatigue Fract. Eng. Mater. Struct., 2007, 30: 556
[45] Santus C, Taylor D. Physically short crack propagation in metals during high cycle fatigue [J]. Int. J. Fatigue, 2009, 31: 1356
[46] Pippan R, Hohenwarter A. Fatigue crack closure: A review of the physical phenomena [J]. Fatigue Fract. Eng. Mater. Struct., 2017, 40: 471
[47] Li W, Sun C W, Li C, et al. In-situ experimental investigation on fatigue crack growth behavior and crack tip plastic zone evolution of laser powder bed fused TiC/Ti6Al4V composites [J]. Mater. Today Commun., 2025, 49: 113731
[48] Chan K S, Shih D S. Fatigue and fracture behavior of a fine-grained lamellar TiAl alloy [J]. Metall. Mater. Trans., 1997, 28A: 79
[49] Panwar S, Adams J F, Allison J E, et al. A grain boundary interaction model for microstructurally short fatigue cracks [J]. Int. J. Fatigue, 2018, 113: 401
[50] Wen W, Zhai T G. Quantification of resistance of grain boundaries to short-fatigue crack growth in three dimensions in high-strength Al alloys [J]. Metall. Mater. Trans., 2012, 43A: 2743
[51] Zhai T, Jiang X P, Li J X, et al. The grain boundary geometry for optimum resistance to growth of short fatigue cracks in high strength Al-alloys [J]. Int. J. Fatigue, 2005, 27: 1202
[52] Zhang X X, Dunne F P E. 3D CP-XFEM modelling of short crack propagation interacting with twist/tilt nickel grain boundaries [J]. J. Mech. Phys. Solids, 2022, 168: 105028
[53] Schmiedel A, Burkhardt C, Rudolph S M, et al. Very high cycle fatigue properties at 973 K of additively manufactured and conventionally processed intermetallic TiAl 48-2-2 alloy [J]. Mater. Sci. Eng., 2023, A862: 144507
[54] Wang S C, Yang B, Liao Z, et al. Research on short fatigue crack initiation and propagation of metallic materials: A review [J]. J. Mech. Eng., 2023, 59(16): 32
  王栓程, 杨 冰, 廖 贞 等. 金属材料疲劳短裂纹萌生与扩展研究综述 [J]. 机械工程学报, 2023, 59(16): 32
[55] Antunes F V, Branco R, Prates P A, et al. Fatigue crack growth modelling based on CTOD for the 7050-T6 alloy [J]. Fatigue Fract. Eng. Mater. Struct., 2017, 40: 1309
[56] Zheng X L, Hirt M A. Fatigue crack propagation in steels [J]. Eng. Fract. Mech., 1983, 18: 965
[57] Chan K S, Lankford J. A crack-tip strain model for the growth of small fatigue cracks [J]. Scr. Metall., 1983, 17: 529
[58] Shyam A, Allison J E, Jones J W. A small fatigue crack growth relationship and its application to cast aluminum [J]. Acta Mater., 2005, 53: 1499
[59] Wang X Y, Zhao Y, Wang L B, et al. In-situ SEM investigation and modeling of small crack growth behavior of additively manufactured titanium alloy [J]. Int. J. Fatigue, 2021, 149: 106303
[60] Chai L D, Han L, Ren L P, et al. A unified threshold model for physically small and long crack based on CTOD [J]. Theor. Appl. Fract. Mech., 2025, 139: 105002
[61] Dowling N E, Begley J A. Fatigue crack growth during gross plasticity and the J-integral [R]. Philadelphia, PA: American Society for Testing and Materials, 1976: 82
[62] Polák J, Zezulka P. Short crack growth and fatigue life in austenitic-ferritic duplex stainless steel [J]. Fatigue Fract. Eng. Mater. Struct., 2005, 28: 923
[63] D?ring R, Hoffmeyer J, Seeger T, et al. Short fatigue crack growth under nonproportional multiaxial elastic-plastic strains [J]. Int. J. Fatigue, 2006, 28: 972
[64] Chapetti M D. Fatigue propagation threshold of short cracks under constant amplitude loading [J]. Int. J. Fatigue, 2003, 25: 1319
[65] Newman Jr J C. A crack-closure model for predicting fatigue-crack growth under aircraft spectrum loading [R]. Hampton, VA: NASA Langley Research Center, 1981
[66] Newman Jr J C, Phillips E P, Swain M H. Fatigue-life prediction methodology using small-crack theory [J]. Int. J. Fatigue, 1999, 21: 109
[67] Newman Jr J C, Annigeri B S. Fatigue-life prediction method based on small-crack theory in an engine material [J]. J. Eng. Gas Turbines Power, 2012, 124: 032501
[68] Chan K S, Lankford J, Davidson D L. A comparison of crack-tip field parameters for large and small fatigue cracks [J]. J. Eng. Mater. Technol., 1986, 108: 206
[69] Tada H, Paris P C, Irwin G R. The Stress Analysis of Cracks Handbook [M]. Hellertown: Del Research Corporation, 1973: 602
[70] Ye S, Zhang X C, Gong J G, et al. Multi‐scale fatigue crack propagation in 304 stainless steel: Experiments and modelling [J]. Fatigue Fract. Eng. Mater. Struct., 2017, 40: 1928
[71] Shamir M, Zhang X, Syed A K. Characterising and representing small crack growth in an additive manufactured titanium alloy [J]. Eng. Fract. Mech., 2021, 253: 107876
[72] Jones R, Michopoulos J G, Iliopoulos A P, et al. Representing crack growth in additively manufactured Ti-6Al-4V [J]. Int. J. Fatigue, 2018, 116: 610
[73] Iliopoulos A, Jones R, Michopoulos J, et al. Crack growth in a range of additively manufactured aerospace structural materials [J]. Aerospace, 2018, 5: 118
[74] Jones R, Rans C, Iliopoulos A P, et al. Modelling the variability and the anisotropic behaviour of crack growth in SLM Ti-6Al-4V [J]. Materials, 2021, 14: 1400
[75] Hartman A, Schijve J. The effects of environment and load frequency on the crack propagation law for macro fatigue crack growth in aluminium alloys [J]. Eng. Fract. Mech., 1970, 1: 615
[76] Markham M J, Fatemi A, Phan N. Mixed-mode small fatigue crack growth rates and modeling in additively manufactured metals [J]. Int. J. Fatigue, 2024, 183: 108258
Outlines

/