Microstructure and High-Temperature Oxidation Behavior of Silicide-Boride Composite Coatings on the Surface of Mo
Received date: 2025-05-08
Revised date: 2026-01-23
Online published: 2026-02-10
Supported by
National Natural Science Foundation of China(51805069)
Mo and its alloys exhibit considerable potential for aerospace high-temperature components, electronic thermal management systems, and high-temperature power-generation structures due to their high melting point, excellent elevated-temperature mechanical strength, and good creep resistance. However, their application is severely limited by rapid oxidation at temperatures above 700 oC, where the formation and volatilization of MoO3 lead to accelerated material loss and structural degradation. This oxidation susceptibility can ultimately result in disintegration and catastrophic failure under extreme service conditions. The application of silicide-based coatings is an effective strategy to mitigate high-temperature oxidation by forming a protective barrier that isolates the substrate from the environment. Nevertheless, monolithic silicide coatings often suffer from premature failure caused by thermal expansion mismatch with the substrate and inward silicon diffusion during prolonged high-temperature exposure. In this context, silicide-boride composite coatings have emerged as a promising alternative for further improving oxidation resistance. Despite their potential, the mechanisms governing gradient microstructure formation and the origins of performance variability in such composite coatings remain insufficiently understood. In this study, silicide and silicide-boride composite coatings were fabricated on pure Mo substrates using halide-activated pack cementation, and their microstructural evolution and high-temperature oxidation behavior were systematically investigated. The results demonstrate that B element incorporation promotes the formation of a silicide-boride composite coating with a five-layer graded structure: MoSi2/(MoSi2 + MoB)/Mo5Si3/MoB/Mo2B. Notably, B facilitates the preferential formation of an initial MoB interlayer at the coating-substrate interface. This interlayer not only inhibits the directional diffusion of Si but also induces a displacement reaction between Si and MoB to form MoSi2, thereby suppressing the (001) preferred growth orientation of MoSi2. In addition, volume contraction associated with MoB formation within the MoSi2 + MoB mixed layer generates pores and a roughened interface, which act as high-density nucleation sites and significantly refine the surface MoSi2 grain structure. The refined grain structure accelerated the formation of a dense and continuous SiO2 protective film, thereby effectively inhibiting O diffusion. After 30 h of oxidation at 1200 oC, the silicide-boride composite coating exhibited an oxidation mass gain of 1.28 mg/cm2 and an oxidation rate constant of 0.29 mg/(cm2·h), representing a 53% reduction relative to the silicide coating. Moreover, the MoB interlayer suppressed inward Si diffusion into the substrate, thereby enhancing long-term stability under high-temperature oxidative conditions.
WU Zhou , WU Fan , WANG Yiming , GAN Youliang , FU Xuesong , CHEN Guoqing , ZHOU Wenlong , ZU Yufei . Microstructure and High-Temperature Oxidation Behavior of Silicide-Boride Composite Coatings on the Surface of Mo[J]. Acta Metall Sin, 2026 , 62(6) : 1069 -1081 . DOI: 10.11900/0412.1961.2025.00127
| [1] | Ding H Y, Yin Y J, Guan J R, et al. Research progress on additively manufactured refractory metals[J]. Rare Met. Mater. Eng., 2021, 50: 2237 |
| 丁红瑜, 尹衍军, 关杰仁 等. 难熔金属增材制造研究进展[J]. 稀有金属材料与工程, 2021, 50: 2237 | |
| [2] | Kamata S Y, Kanekon D, Lu Y Y, et al. Ultrahigh-temperature tensile creep of TiC-reinforced Mo-Si-B-based alloy[J]. Sci. Rep., 2018, 8: 10487 |
| [3] | Depka T, Somsen C, Eggeler G, et al. Microstructures of Co-Re-Cr, Mo-Si and Mo-Si-B high-temperature alloys[J]. Mater. Sci. Eng., 2009, A510-511: 337 |
| [4] | Cai Z Y, Zhao X J, Zhang D X, et al. Microstructure and oxidation resistance of a YSZ modified silicide coating for Ta-W alloy at 1800 oC[J]. Corros. Sci., 2018, 143: 116 |
| [5] | Yu L H, Shen F Q, Fu T, et al. Microstructure and oxidation behavior of metal-modified Mo-Si-B alloys: A review[J]. Coatings, 2021, 11: 1256 |
| [6] | Ding Z Y, Brouwer J C, Kwakernaak C, et al. Selective oxidation of aluminium in Mo(Al, Si)2[J]. Corros. Sci., 2023, 211: 110884 |
| [7] | Lemberg J A, Ritchie R O. Mo-Si-B alloys for ultrahigh-temperature structural applications[J]. Adv. Mater., 2012, 24: 3445 |
| [8] | An L, Gao C Q, Jia J G, et al. Review on metal silicide anti-oxidation coatings[J]. J. Chin. Soc. Corros. Prot., 2021, 41: 298 |
| 安 亮, 高昌琦, 贾建刚 等. 金属硅化物抗氧化涂层的研究进展[J]. 中国腐蚀与防护学报, 2021, 41: 298 | |
| [9] | Yi Z Q, Tan D Q, Tang Y, et al. Characterization of microstructure and oxidation resistance of Y modified silicide composite coating on Mo-Cr-W-Al-Ti substrate[J]. Ceram. Int., 2022, 48: 9848 |
| [10] | Zhang Y Y, Cui K K, Fu T, et al. Synthesis WSi2 coating on W substrate by HDS method with various deposition times[J]. Appl. Surf. Sci., 2020, 511: 145551 |
| [11] | Yan J H, Lin Y Z, Wang Y, et al. Refractory WMoNbVTa high-entropy alloy as a diffusion barrier between a molybdenum substrate and MoSi2 ceramic coating[J]. Ceram. Int., 2022, 48: 11410 |
| [12] | Xiao L R, Zhou X J, Wang Y F, et al. Formation and oxidation behavior of Ce-modified MoSi2-NbSi2 coating on niobium alloy[J]. Corros. Sci., 2020, 173: 108751 |
| [13] | Fu T, Shen F Q, Zhang Y Y, et al. Oxidation protection of high-temperature coatings on the surface of Mo-based alloys—A review[J]. Coatings, 2022, 12: 141 |
| [14] | Szajna E, Moskal G, Stryczniewicz W, et al. Microstructure and high-temperature oxidation behaviour of MoSi2 protective coatings on Mo-based combustion chamber in rocket engines[J]. Surf. Coat. Technol., 2023, 473: 129896 |
| [15] | Wang K, Reeber R R. The role of defects on thermophysical properties: Thermal expansion of V, Nb, Ta, Mo and W[J]. Mater. Sci. Eng., 1998, R23: 101 |
| [16] | Engstr?m I, L?nnberg B. Thermal expansion studies of the group IV-VII transition-metal disilicides[J]. J. Appl. Phys., 1988, 63: 4476 |
| [17] | Xiao L R, Zhang B, Cai Z Y, et al. Thermal shock behavior and crack propagation of MoSi2 coating on molybdenum alloy[J]. Rare Met. Mater. Eng., 2018, 47: 3387 |
| 肖来荣, 张 贝, 蔡圳阳 等. 钼合金MoSi2涂层高温热震行为与裂纹扩展[J]. 稀有金属材料与工程, 2018, 47: 3387 | |
| [18] | Yoon J K, Kim G H. Isothermal and cyclic oxidation behavior of in-situ grown MoSi2-SiC coating on Mo substrate at 1300 oC[J]. Surf. Coat. Technol., 2023, 464: 129582 |
| [19] | Zhang Y F, Xiao L R, Zeng D L, et al. A novel niobium based oxidation protective coating with three lines of defense at ultra-high temperature[J]. Corros. Sci., 2022, 206: 110515 |
| [20] | Zhang Y F, Liu S N, Zhou X J, et al. Ultra-high temperature oxidation behavior of ZrB2/YSZ modified Si-Mo-W coating with a diffusion barrier on niobium alloy[J]. Corros. Sci., 2022, 195: 109977 |
| [21] | Wang Y, Wang D Z, Yan J H. Preparation and characterization of MoSi2/MoB composite coating on Mo substrate[J]. J. Alloys Compd., 2014, 589: 384 |
| [22] | Chen Z, Yu W P, Wen S H, et al. First principles study on effect of B addition on oxidation resistance of MoSi2-based compound[J]. J. Chin. Soc. Corros. Prot., 2025, 45: 224 |
| 陈 郑, 宇文佩, 温思涵 等. B添加对MoSi2基化合物抗氧化性能影响的第一性原理研究[J]. 中国腐蚀与防护学报, 2025, 45: 224 | |
| [23] | Zhao H L, Kramer M J, Akinc M. Thermal expansion behavior of intermetallic compounds in the Mo-Si-B system[J]. Intermetallics, 2004, 12: 493 |
| [24] | Shan X, Cai H Y, Luo L R, et al. Influence of pore characteristics of air plasma sprayed thermal barrier coatings on calcia-magnesia-alumino-silicate (CMAS) attack behavior[J]. Corros. Sci., 2021, 190: 109636 |
| [25] | Scrivani A, Rizzi G, Berndt C C. Enhanced thick thermal barrier coatings that exhibit varying porosity[J]. Mater. Sci. Eng., 2008, A476: 1 |
| [26] | Cockeram B, Rapp R A. Development and growth of boron-modified and germanium-doped titanium-silicide diffusion coatings by the halide-activated, pack-cementation method[J]. Oxid. Met., 1996, 45: 375 |
| [27] | Cai Z Y, Liu S N, Xiao L R, et al. Oxidation behavior and microstructural evolution of a slurry sintered Si-Mo coating on Mo alloy at 1650 oC[J]. Surf. Coat. Technol., 2017, 324: 182 |
| [28] | Spear K E, Liao P K. The B-Mo (boron-molybdenum) system[J]. Bull. Alloy Phase Diagr., 1988, 9: 457 |
| [29] | Yang Y, Chang Y A. Thermodynamic modeling of the Mo-Si-B system[J]. Intermetallics, 2005, 13: 121 |
| [30] | Tang Z H, Thom A J, Kramer M J, et al. Characterization and oxidation behavior of silicide coating on multiphase Mo-Si-B alloy[J]. Intermetallics, 2008, 16: 1125 |
| [31] | Hayashi T, Ito K, Numakura H. Reaction diffusion of MoSi2 and Mo5SiB2[J]. Intermetallics, 2005, 13: 93 |
| [32] | Yoon J K, Doh J M, Byun J Y, et al. Formation of MoSi2-SiC composite coatings by chemical vapor deposition of Si on the surface of Mo2C layer formed by carburizing of Mo substrate[J]. Surf. Coat. Technol., 2003, 173: 39 |
| [33] | Grosfils P, Lutsko J F. Impact of surface roughness on crystal nucleation[J]. Crystals, 2020, 11: 4 |
| [34] | Zhang G J, Kou H, Dang Q, et al. Microstructure and oxidation resistance behavior of lanthanum oxide-doped Mo-12Si-8.5B alloys[J]. Int. J. Refract. Met. Hard Mater., 2012, 30: 6 |
| [35] | Rioult F A, Imhoff S D, Sakidja R, et al. Transient oxidation of Mo-Si-B alloys: Effect of the microstructure size scale[J]. Acta Mater., 2009, 57: 4600 |
| [36] | Zhang Y F, Zhou X J, Cheng H C, et al. Fabrication and oxidation resistance of a novel MoSi2-ZrB2-based coating on Mo-based alloy[J]. Materials, 2023, 16: 5634 |
| [37] | Rodríguez-Viejo J, Sibieude F, Clavaguera-Mora M T, et al. 18O diffusion through amorphous SiO2 and cristobalite[J]. Appl. Phys. Lett., 1993, 63: 1906 |
| [38] | Chatilyan H A, Kharatyan S L, Harutyunyan A B. Diffusion annealing of Mo/MoSi2 couple and silicon diffusivity in Mo5Si3 layer[J]. Mater. Sci. Eng., 2007, A459: 227 |
/
| 〈 |
|
〉 |