Ordering Process of Interfacial Intermetallic Compounds and Strengthening Mechanism of QAl10-5-5/TC6 Bimetals Adding Ag Interlayer
Received date: 2025-05-27
Revised date: 2026-01-08
Online published: 2026-01-15
Supported by
National Natural Science Foundation of China(U2341271);National Natural Science Foundation of China(52104385);Innovation Research team of Shaanxi(2025RS-CXTD-020);Distinguished Young Scholars of Shaanxi Province(2025ZC-KJXX-33);Key Research and Development Projects of Shaanxi Province(2023GXLH-037);Foundation of Aviation Science(202400070T6001)
Structural-functional integrated Cu-alloy/Ti-alloy bimetals combine the advantageous properties of both constituents and therefore exhibit considerable potential for multifunctional applications. However, controlling the interfacial microstructure and achieving sufficient interfacial strength remain significant challenges in Cu-alloy/Ti-alloy systems. This study investigates the evolution of the interfacial microstructure, the ordering behavior of interfacial intermetallic compounds (IMCs), and the relationship between interfacial structure and mechanical performance, aiming to clarify the formation pathway of IMCs and its effect on the interface strength of Cu-alloy/Ti-alloy bimetals. QAl10-5-5/TC6 bimetals were fabricated via diffusion bonding using Ag interlayer (adding Ag foil as interlayer or electrodeposited Ag interlayer on QAl10-5-5 alloy). The resulting interfacial microstructures and shear strengths were systematically characterized, and the corresponding strengthening mechanism was clarified. For the QAl10-5-5/Ag foil/TC6 bimetals, the interfacial strength reached a maximum of 200 MPa at a bonding temperature of 850 oC. Meanwhile, for the Ag layer deposited QAl10-5-5/TC6 bimetals, the fine-grained structure of the electrodeposited Ag layer promoted metallurgical bonding, and the QAl10-5-5/TC6 bimetals achieved maximum interfacial strength of 217 MPa at a bonding temperature of 835 oC. Moreover, an “affected zone” formed on the TC6 alloy side of Ag layer deposited QAl10-5-5/TC6 bimetals, consisting of a TiAlCu2 reaction layer with a thickness of ~1 μm, and submicron scale Ti2Cu and Ti3Al phases, in which a semi-coherent interface occurred between Ti3Al and α-Ti. Theoretical strengthening analysis of Ag layer deposited QAl10-5-5/TC6 bimetal revealed that the grain refinement strengthening and precipitation strengthening enhanced the property of the “affected zone” on the TC6 alloy side.
Key words: Cu alloy; Ti alloy; bimetal; intermetallic compounds; interface strengthening
SUN Lixing , XUE Hangyu , LIANG Shuhua , YANG Qian , JIANG Qi , ZOU Juntao . Ordering Process of Interfacial Intermetallic Compounds and Strengthening Mechanism of QAl10-5-5/TC6 Bimetals Adding Ag Interlayer[J]. Acta Metall Sin, 2026 , 62(8) : 1454 -1466 . DOI: 10.11900/0412.1961.2025.00144
| [1] | Li J, Zhou P, Hui Y Y. Microstructure and properties of dissimilar materials Ti/Cu welding joint by arc welding [J]. Chin. J. Nonferrous Met., 2021, 31: 2419 |
| 李 杰, 周 鹏, 惠媛媛. 钛/铜异种金属电弧焊焊接接头界面组织与力学性能 [J]. 中国有色金属学报, 2021, 31: 2419 | |
| [2] | Wu B S, Dong H G, Ma Y T, et al. Bonding mechanism of TC4 titanium alloy/T2 copper vacuum diffusion bonded joint with nickel as transition interlayer [J]. J. Manuf. Processes, 2024, 131: 1309 |
| [3] | Zhou J, Guo S, Deng Z H C, et al. Microstructural features and mechanical properties of in-situ remelting welding of TC4 titanium alloy and T2 copper welded joint by electron beam [J]. J. Mater. Res. Technol., 2024, 33: 6853 |
| [4] | Jiang S, Peng R L, Jia N, et al. Microstructural and textural evolutions in multilayered Ti/Cu composites processed by accumulative roll bonding [J]. J. Mater. Sci. Technol., 2019, 35: 1165 |
| [5] | Wu B S, Li P, Ma Y T, et al. Vacuum diffusion bonding of TC4 titanium alloy to T2 copper with VCrNi1.8 eutectic medium entropy alloy interlayer [J]. Mater. Charact., 2024, 214: 114125 |
| [6] | Fang Y J, Jiang X S, Mo D F, et al. A review on dissimilar metals' welding methods and mechanisms with interlayer [J]. Int. J. Adv. Manuf. Technol., 2019, 102: 2845 |
| [7] | Cai X P, Li K E, Sang C C, et al. Interfacial microstructure and mechanical properties of Ti/Cu joint manufactured by Ni-Al thermal explosion reaction [J]. J. Manuf. Processes, 2020, 57: 919 |
| [8] | Zhao Y, Wang W Y, Yan K, et al. Microstructure and properties of Cu/Ti laser welded joints [J]. J. Mater. Process. Technol., 2018, 257: 244 |
| [9] | Chen G Q, Zhang B G, Liu W, et al. Influence of electron-beam superposition welding on intermetallic layer of Cu/Ti joint [J]. Trans. Nonferrous Met. Soc. China, 2012, 22: 2416 |
| [10] | Xu Y, Ke L M, Nie H, et al. Precipitation behavior of intermetallic compounds at the interface of thick plate friction stir welded Al alloy/Mg alloy joints under local strong cooling [J]. Acta Metall. Sin., 2024, 60: 777 |
| 徐 洋, 柯黎明, 聂 浩 等. 局部强冷作用下厚板铝合金/镁合金搅拌摩擦焊界面金属间化合物的析出行为 [J]. 金属学报, 2024, 60: 777 | |
| [11] | Li B B, Wang B, Li P, et al. Solid diffusion bonding of Ti2AlNb-based alloy [J]. Chin. J. Nonferrous Met., 2015, 25: 662 |
| 李贝贝, 王 斌, 李 萍 等. Ti2AlNb基合金固态扩散连接工艺 [J]. 中国有色金属学报, 2015, 25: 662 | |
| [12] | Tong J C, Yuan Y, Tong D M, et al. Effect of dynamic recrystallization on healing at pure nickel joint interface during hot compression bonding [J]. Chin. J. Nonferrous Met., 2024, 34: 2708 |
| 仝珏川, 袁 瑶, 仝大明 等. 动态再结晶对纯镍热压连接界面结合率的影响 [J]. 中国有色金属学报, 2024, 34: 2708 | |
| [13] | Yuan J J, Fan Q B, Liu W F, et al. Interface evolution mechanism and mechanical properties of Ti311/TC4 laminated composites during hot-pressing diffusion bonding [J]. Mater. Charact., 2024, 211: 113900 |
| [14] | Ayd?n K, Kaya Y, Kahraman N. Experimental study of diffusion welding/bonding of titanium to copper [J]. Mater. Des., 2012, 37: 356 |
| [15] | Shen Q, Xiang H Y, Luo G Q, et al. Microstructure and mechanical properties of TC4/oxygen-free copper joint with silver interlayer prepared by diffusion bonding [J]. Mater. Sci. Eng., 2014, A596: 45 |
| [16] | Lin T, Li C, Si X Q, et al. An investigation on di?usion bonding of Cu/Cu using various grain size of Ni interlayers at low temperature [J]. Materialia, 2020, 14: 100882 |
| [17] | Guo H C, Rao M, Zhang J, et al. Electromigration-enhanced Kirkendall effect of Cu/Ti direct diffusion welding by sparking plasma sintering [J]. J. Mater. Process. Technol., 2023, 315: 117933 |
| [18] | Sun L X, Zhang R Y, Liang S H, et al. Effect of multi-component alloy interlayer on interfacial microstructure and shear strength of titanium/bronze bimetal [J]. JOM, 2024, 76: 5258 |
| [19] | Fukamachi K. Kinetics and thermodynamics associated with age hardening of Cu-4at% Ti alloy [J]. Mater. Sci. Eng., 2020, A788: 139411 |
| [20] | Liao Y M, Guo C J, Zhou C Y, et al. Stability of the metastable β'-Cu4Ti phase in Cu-Ti alloys: Role of the Ti content [J]. Mater. Charact., 2023, 203: 113164 |
| [21] | Souza S A, Afonso C R M, Ferrandini P L, et al. Effect of cooling rate on Ti-Cu eutectoid alloy microstructure [J]. Mater. Sci. Eng., 2009, C29: 1023 |
| [22] | Vilardell A M, Yadroitsev I, Yadroitsava I, et al. Manufacturing and characterization of in-situ alloyed Ti6Al4V (ELI)-3 at.% Cu by laser powder bed fusion [J]. Addit. Manuf., 2020, 36: 101436 |
| [23] | Wu B S, Dong H G, Li P, et al. Vacuum diffusion bonding of TC4 titanium alloy and T2 copper by a slow cooling heat treatment [J]. J. Mater. Process. Technol., 2022, 305: 117595 |
| [24] | Sun L X, Li M Q, Li L. Characterization of crystal structure in the bonding interface between TC17 and TC4 alloys [J]. Mater. Charact., 2019, 153: 169 |
| [25] | Seyring M, Rettenmayr M. Impact of crystallography at Ni/NiAl interfaces on the nucleation of Ni3Al [J]. Acta Mater., 2021, 208: 116713 |
| [26] | Hou Z Q, Zhang J Y, Li J, et al. Phase transformation-induced strength softening in Ti/Ta nanostructured multilayers: Coherent interface vs phase boundary [J]. Mater. Sci. Eng., 2017, A684: 78 |
| [27] | Supakul S, Jain M, Yaddanapudi K, et al. Synthesis, microstructure and micro-mechanical characterization of metal (Nb, Ti)-MAX ph-ase (Ti2AlC) nanolaminates [J]. Mater. Sci. Eng., 2024, A910: 146905 |
| [28] | Yamaguchi M, Umakoshi Y. The deformation behaviour of intermetallic superlattice compounds [J]. Prog. Mater. Sci., 1990, 34: 1 |
| [29] | Lai A, Bhanumurthy K, Kale G B, et al. Diffusion characteristics in the Cu-Ti system [J]. Int. J. Mater. Res., 2012, 103: 661 |
| [30] | Liu C, Song Z Y, Fan Y G, et al. Growth kinetics of intermetallic compounds in Cu-Ti diffusion couples [J]. Intermetallics, 2024, 168: 108261 |
| [31] | Deng Y Q, Sheng G M, Xu C. Evaluation of the microstructure and mechanical properties of diffusion bonded joints of titanium to stainless steel with a pure silver interlayer [J]. Mater. Des., 2013, 46: 84 |
| [32] | Kim Y K, Pouraliakbar H, Hong S I. Effect of interfacial intermetallic compounds evolution on the mechanical response and fracture of layered Ti/Cu/Ti clad materials [J]. Mater. Sci. Eng., 2020, A772: 138802 |
| [33] | Han Q, Di X, Zheng Y, et al. Interface interlocking enhances mechanical strength of wire-arc directed energy deposited Mg-Al-Si/Mg-Gd-Y-Zn bimetals [J]. Mater. Sci. Eng., 2025, A932: 148254 |
| [34] | Jiang S, Peng R L, Heged?s Z, et al. Micromechanical behavior of multilayered Ti/Nb composites processed by accumulative roll bonding: An in-situ synchrotron X-ray diffraction investigation [J]. Acta Mater., 2021, 205: 116546 |
| [35] | Hong X, Qin Z, Jiang X, et al. Compositional and structural control toward boosting inner-grain prestress and releasing the inter-lattice strain of an FGH99 diffusion-bonded superalloy [J]. Mater. Horiz., 2026, 13: 1939 |
| [36] | Liu F, Lin J, Hu X Q, et al. Relationship of microstructure and mechanical properties of 2195-T8 aluminum-lithium alloy TIG welded joint [J]. Mater. Charact., 2026, 232: 115951 |
| [37] | Taylor G I. The mechanism of plastic deformation of crystals. Part I.—Theoretical [J]. Proc. R. Soc. London, 1934, 145A: 362 |
| [38] | Zhang R, Wang S, Lu W H, et al. Enhancing microstructure refinement and strengthening efficiency of TiBw/near α-Ti composites by combining solid-solution treatment with hot processing [J]. Composites, 2023, B257: 110696 |
| [39] | Li L, Ma P P, Zhang L, et al. Fabrication of TiB whiskers reinforced Ti6242 matrix composites by direct laser deposition: Powder preparation, microstructure and mechanical property [J]. Composites, 2024, 268B: 111068 |
| [40] | Fu Y L, Xie G L, Zhao F, et al. Precipitation behaviors and property variations of Cu-3.0 wt% Ti fabricated by a novel short-processing non-vacuum heating-cooling combined mold continuous casting [J]. J. Alloys Compd., 2022, 921: 166059 |
/
| 〈 |
|
〉 |