Progress and Perspectives on Metallic Bipolar Plates in Fuel Cells
Received date: 2025-05-27
Revised date: 2025-09-25
Online published: 2026-01-04
Supported by
China Baowu Low Carbon Metallurgy Innovation Foundation(BWLCF202213)
With the advancement of the global carbon neutrality strategy, proton exchange membrane fuel cells (PEMFCs), a typical type of low-temperature fuel cell, have been widely applied in transportation power systems, portable power equipment, and distributed energy systems because of their notable technical advantages, including high energy conversion efficiency (> 60%), low operating temperatures (60-80 oC), and near-zero carbon dioxide emissions. As a key fuel cell component, the bipolar plate serves several essential functions, including gas distribution, electron conduction, and management of reactant flow fields. The corrosion resistance and electrical conductivity of bipolar plates directly determine overall fuel cell performance, including energy conversion efficiency, durability, and manufacturing cost. Therefore, bipolar plates with high corrosion resistance and high conductivity for PEMFCs have recently been the focus of intensive research. This study reviews various metallic bipolar plates, their surface modification strategies, and the resulting performance, including Al/Ti alloys and austenitic/ferritic stainless steels. Both Al and Ti alloys require noble metal coatings, such as Au/Ni-P and CrN, to balance corrosion resistance and conductivity, leading to high costs and complex fabrication processes that hinder commercialization. Although the corrosion resistance of austenitic stainless steels can be enhanced through synergistic Cr/Mo alloying, the rapid thickening of the passivation layer leads to excessively high interfacial contact resistance during service. In contrast, ferritic stainless steels are prone to intergranular corrosion; however, this can be mitigated through ultralow carbon content and stabilization by Ti/Nb microalloying. Their application in bipolar plates remains constrained because of poor formability and corrosion current densities in the uncoated state that often exceed the target values set by the United States Department of Energy. Although surface coating technologies, such as CrN and conductive polymers, can improve corrosion resistance and conductivity, process complexity and coating durability remain major concerns. Furthermore, this paper introduces a novel alloying strategy for high-Cr ferritic stainless steels used as coating-free bipolar plates, which simultaneously achieves excellent ductility, high corrosion resistance, and high electrical conductivity under simulated PEMFC conditions. Finally, future development directions for PEMFC bipolar plate materials are discussed.
LUO Haiwen , LIN Xiong , LIU Gaoyang , HU Bin . Progress and Perspectives on Metallic Bipolar Plates in Fuel Cells[J]. Acta Metall Sin, 2026 , 62(2) : 263 -274 . DOI: 10.11900/0412.1961.2025.00142
| [1] | Du Z Z, Wang J, Wang J, et al. Research progress of key materials in proton exchange membrane fuel cell [J]. J. Mater. Eng., 2022, 50(12): 35 |
| 杜真真, 王 珺, 王 晶 等. 质子交换膜燃料电池关键材料的研究进展 [J]. 材料工程, 2022, 50(12): 35 | |
| [2] | Hermann A, Chaudhuri T, Spagnol P. Bipolar plates for PEM fuel cells: A review [J]. Int. J. Hydrogen Energy, 2005, 30: 1297 |
| [3] | U.S. Department of Energy. Targets for bipolar plates [R]. DOE/GO-102020-5486, 2020 |
| [4] | Hung Y, Tawfik H, Mahajan D. Durability and characterization studies of polymer electrolyte membrane fuel cell’s coated aluminum bipolar plates and membrane electrode assembly [J]. J. Power Sources, 2009, 186: 123 |
| [5] | André J, Antoni L, Petit J P. Corrosion resistance of stainless steel bipolar plates in a PEFC environment: A comprehensive study [J]. Int. J. Hydrogen Energy, 2010, 35: 3684 |
| [6] | Wilkinson D P, Zhang J J, Hui R, et al. Proton Exchange Membrane Fuel Cells: Materials Properties and Performance [M]. Boca Raton: CRC Press, 2009: 1 |
| [7] | Wang H, Turner J A. Reviewing metallic PEMFC bipolar plates [J]. Fuel Cells, 2010, 10: 510 |
| [8] | Hamilton P J, Pollet B G. Polymer electrolyte membrane fuel cell (PEMFC) flow field plate: Design, materials and characterisation [J]. Fuel Cells, 2010, 10: 489 |
| [9] | Lee D, Lim J W, Lee D G. Cathode/anode integrated composite bipolar plate for high-temperature PEMFC [J]. Compos. Struct., 2017, 167: 144 |
| [10] | Barranco J, Barreras F, Lozano A, et al. Influence of CrN-coating thickness on the corrosion resistance behaviour of aluminium-based bipolar plates [J]. J. Power Sources, 2011, 196: 4283 |
| [11] | Fetohi A E, Hameed R M A, El-Khatib K M, et al. Study of different aluminum alloy substrates coated with Ni-Co-P as metallic bipolar plates for PEM fuel cell applications [J]. Int. J. Hydrogen Energy, 2012, 37: 10807 |
| [12] | Mawdsley J R, Carter J D, Wang X P, et al. Composite-coated aluminum bipolar plates for PEM fuel cells [J]. J. Power Sources, 2013, 231: 106 |
| [13] | Tsai S Y, Lin C H, Jian Y J, et al. The fabrication and characteristics of electroless nickel and immersion Au-polytetrafluoroethylene composite coating on aluminum alloy 5052 as bipolar plate [J]. Surf. Coat. Technol., 2017, 313: 151 |
| [14] | Hou K H, Lin C H, Ger M D, et al. Analysis of the corrosion behavior of Al alloy bipolar plate for proton exchange membrane fuel cell (PEMFC) under operating thermal conditions [J]. Int. J. Green Energy, 2012, 9: 71 |
| [15] | Tsai S Y, Bai C Y, Lin C H, et al. The characteristics and performance of electroless nickel and immersion Au plated aluminum alloy bipolar plates in polymer electrolyte membrane fuel cells [J]. J. Power Sources, 2012, 214: 51 |
| [16] | Aukland N, Boudina A, Eddy D S, et al. Alloys that form conductive and passivating oxides for proton exchange membrane fuel cell bipolar plates [J]. J. Mater. Res., 2004, 19: 1723 |
| [17] | Dincer I. Technical, environmental and exergetic aspects of hydrogen energy systems [J]. Int. J. Hydrogen Energy, 2002, 27: 265 |
| [18] | Zhang D M, Duan L T, Guo L, et al. TiN-coated titanium as the bipolar plate for PEMFC by multi-arc ion plating [J]. Int. J. Hydrogen Energy, 2011, 36: 9155 |
| [19] | Qian Y, Xu J. Properties of ZrC nanocrystalline coating on Ti alloy bipolar plates in simulated PEMFC environments [J]. Rare Met. Mater. Eng., 2017, 46: 1033 |
| 钱 阳, 徐 江. 模拟PEMFC环境下纳米晶ZrC涂层钛合金双及板的性能研究 [J]. 稀有金属材料与工程, 2017, 46: 1033 | |
| [20] | Qian Y, Xu J. Properties of Zr nanocrystalline coating on Ti alloy bipolar plates in simulated PEMFC environments [J]. Acta Phys.-Chim. Sin., 2015, 31: 291 |
| [21] | Xu J, Huang H J, Li Z Y, et al. Corrosion behavior of a ZrCN coated Ti alloy with potential application as a bipolar plate for proton exchange membrane fuel cell [J]. J. Alloys Compd., 2016, 663: 718 |
| [22] | Hsieh S S, Huang C F, Feng C L. A novel design and micro-fabrication for copper (Cu) electroforming bipolar plates [J]. Micron, 2008, 39: 263 |
| [23] | Tran T Q, Lee J K Y, Chinnappan A, et al. High-performance carbon fiber/gold/copper composite wires for lightweight electrical cables [J]. J. Mater. Sci. Technol., 2020, 42: 46 |
| [24] | Lee H Y, Lee S H, Kim J H, et al. Thermally nitrided Cu-5.3Cr alloy for application as metallic separators in PEMFCs [J]. Int. J. Hydrogen Energy, 2008, 33: 4171 |
| [25] | Pan T J, Zuo X W, Wang T, et al. Electrodeposited conductive polypyrrole/polyaniline composite film for the corrosion protection of copper bipolar plates in proton exchange membrane fuel cells [J]. J. Power Sources, 2016, 302: 180 |
| [26] | Ashok Kumar P, Vasanth Kumar D, Davis Hans S J, et al. Investigation of stainless steel 316 coated with nickel [J]. Mater. Today Proc., 2022, 62: 2376 |
| [27] | Mohanty S, Kumar Senapati A. Study on wear behavior of low nickel austenitic stainless steel by using ball on disc [J]. Mater. Today Proc., 2022, 66: 1961 |
| [28] | Song S, Yu L, Xiao X, et al. Outstanding oxygen evolution reaction performance of nickel iron selenide/stainless steel mat for water electrolysis [J]. Mater. Today Phys., 2020, 13: 100216 |
| [29] | Ghorbani M M, Taherian R, Bozorg M. Investigation on physical and electrochemical properties of TiN-coated Monel alloy used for bipolar plates of proton exchange membrane fuel cell [J]. Mater. Chem. Phys., 2019, 238: 121916 |
| [30] | Ben Jadi S, El Jaouhari A, Aouzal Z, et al. Electropolymerization and corrosion resistance of polypyrrole on nickel bipolar plate for PEM fuel cell application [J]. Mater. Today Proc., 2020, 22: 52 |
| [31] | Sun Y T, Tan X, Lei L L, et al. Revisiting the effect of molybdenum on pitting resistance of stainless steels [J]. Tungsten, 2021, 3: 329 |
| [32] | Malik A U, Siddiqi N A, Ahmad S, et al. The effect of dominant alloy additions on the corrosion behavior of some conventional and high alloy stainless steels in seawater [J]. Corros. Sci., 1995, 37: 1521 |
| [33] | Kim J K, Kim Y H, Lee B H, et al. New findings on intergranular corrosion mechanism of stabilized stainless steels [J]. Electrochim. Acta, 2011, 56: 1701 |
| [34] | Davies D P, Adcock P L, Turpin M, et al. Stainless steel as a bipolar plate material for solid polymer fuel cells [J]. J. Power Sources, 2000, 86: 237 |
| [35] | Davies D P, Adcock P L, Turpin M, et al. Bipolar plate materials for solid polymer fuel cells [J]. J. Appl. Electrochem., 2000, 30: 101 |
| [36] | Wang H L, Sweikart M A, Turner J A. Stainless steel as bipolar plate material for polymer electrolyte membrane fuel cells [J]. J. Power Sources, 2003, 115: 243 |
| [37] | Chanda U K, Behera A, Roy S, et al. Evaluation of Ni-Cr-P coatings electrodeposited on low carbon steel bipolar plates for polymer electrolyte membrane fuel cell [J]. Int. J. Hydrogen Energy, 2018, 43: 23430 |
| [38] | Zhang M, Kim K H, Shao Z G, et al. Effects of Mo content on microstructure and corrosion resistance of arc ion plated Ti-Mo-N films on 316L stainless steel as bipolar plates for polymer exchange membrane fuel cells [J]. J. Power Sources, 2014, 253: 201 |
| [39] | Peng S, Xu J, Xie Z H, et al. Titanium bipolar plates augmented by nanocrystalline TiZrHfMoW coatings for application in proton exchange membrane fuel cells [J]. Appl. Surf. Sci., 2022, 591: 153200 |
| [40] | Kumagai M, Myung S T, Katada Y, et al. Stability of type 310S stainless steel bipolar plates tested at various current densities in proton exchange membrane fuel cells [J]. Electrochim. Acta, 2016, 211: 754 |
| [41] | Myung S T, Kumagai M, Asaishi R, et al. Nanoparticle TiN-coated type 310S stainless steel as bipolar plates for polymer electrolyte membrane fuel cell [J]. Electrochem. Commun., 2008, 10: 480 |
| [42] | Wang Z Y, Feng K, Li Z G, et al. Self-passivating carbon film as bipolar plate protective coating in polymer electrolyte membrane fuel cell [J]. Int. J. Hydrogen Energy, 2016, 41: 5783 |
| [43] | Joseph S, McClure J C, Chianelli R, et al. Conducting polymer-coated stainless steel bipolar plates for proton exchange membrane fuel cells (PEMFC) [J]. Int. J. Hydrogen Energy, 2005, 30: 1339 |
| [44] | Lee S H, Kakati N, Maiti J, et al. Corrosion and electrical properties of CrN- and TiN-coated 316L stainless steel used as bipolar plates for polymer electrolyte membrane fuel cells [J]. Thin Solid Films, 2013, 529: 374 |
| [45] | Mani S P, Rajendran N. Corrosion and interfacial contact resistance behavior of electrochemically nitrided 316L SS bipolar plates for proton exchange membrane fuel cells [J]. Energy, 2017, 133: 1050 |
| [46] | Fu Y, Lin G, Hou M, et al. Optimized Cr-nitride film on 316L stainless steel as proton exchange membrane fuel cell bipolar plate [J]. Int. J. Hydrogen Energy, 2009, 34: 453 |
| [47] | Mendizabal L, Oedegaard A, Kongstein O E, et al. TaN x coatings deposited by HPPMS on SS316L bipolar plates for polymer electrolyte membrane fuel cells: Correlation between corrosion current, contact resistance and barrier oxide film formation [J]. Int. J. Hydrogen Energy, 2017, 42: 3259 |
| [48] | Turner J A, Wang H L, Brady M P. Corrosion protection of metallic bipolar plates for fuel cells [R]. Golden: National Renewable Energy Lab. (NREL), 2005 |
| [49] | Zhang D M, Duan L T, Guo L, et al. Corrosion behavior of TiN-coated stainless steel as bipolar plate for proton exchange membrane fuel cell [J]. Int. J. Hydrogen Energy, 2010, 35: 3721 |
| [50] | Wang L X, Sun J C, Kang B, et al. Electrochemical behaviour and surface conductivity of niobium carbide-modified austenitic stainless steel bipolar plate [J]. J. Power Sources, 2014, 246: 775 |
| [51] | Wang S L, Hou M, Zhao Q, et al. Ti/(Ti, Cr)N/CrN multilayer coated 316L stainless steel by arc ion plating as bipolar plates for proton exchange membrane fuel cells [J]. J. Energy Chem., 2017, 26: 168 |
| [52] | Bi F F, Peng L F, Yi P Y, et al. Multilayered Zr-C/a-C film on stainless steel 316L as bipolar plates for proton exchange membrane fuel cells [J]. J. Power Sources, 2016, 314: 58 |
| [53] | Allahkaram S R, Mohammadi N. Corrosion behavior of two candidate PEMFC's bipolar plate materials [J]. Anti-Corros. Methods Mater., 2017, 64: 293 |
| [54] | Wu B, Lin G Q, Fu Y, et al. Chromium-containing carbon film on stainless steel as bipolar plates for proton exchange membrane fuel cells [J]. Int. J. Hydrogen Energy, 2010, 35: 13255 |
| [55] | Fu Y, Lin G, Hou M, et al. Carbon-based films coated 316L stainless steel as bipolar plate for proton exchange membrane fuel cells [J]. Int. J. Hydrogen Energy, 2009, 34: 405 |
| [56] | Ujiro T, Yoshioka K, Staehle R W. Differences in corrosion behavior of ferritic and austenitic stainless steels [J]. Corrosion, 1994, 50: 953 |
| [57] | Jun S, Hong Y B, Xin L, et al. The effect of copper and molybdenum on pitting corrosion and stress corrosion cracking behavior of ultra-pure ferritic stainless steels [J]. Corros. Sci., 2012, 57: 89 |
| [58] | Wang H L, Turner J A. Ferritic stainless steels as bipolar plate material for polymer electrolyte membrane fuel cells [J]. J. Power Sources, 2004, 128: 193 |
| [59] | ASTM. ASTM A240/A240M-08 Standard specification for chromium and chromium-nickel stainless steel plate, sheet, and strip for pressure vessels and for general applications [S]. West Conshohocken: ASTM, 2008 |
| [60] | Kim K M, Kim S N, Kim J H, et al. Study on surface topography of 446M stainless steel as a bipolar plate on interfacial contact resistance of polymer electrolyte membrane fuel cell [J]. J. Power Sources, 2012, 220: 42 |
| [61] | Kim J, Jo K, Kim Y, et al. Stainless steel for polymer fuel cell separator and method for preparing same [P]. U.S. Pat, 20110294042, 2011 |
| [62] | Brady M P, Abd Elhamid M, Dadheech G, et al. Manufacturing and performance assessment of stamped, laser welded, and nitrided FeCrV stainless steel bipolar plates for proton exchange membrane fuel cells [J]. Int. J. Hydrogen Energy, 2013, 38: 4734 |
| [63] | Moretti G, Quartarone G, Tassan A, et al. Pitting corrosion behavior of superferritic stainless steel in waters containing chloride [J]. Mater. Corros., 1993, 44: 24 |
| [64] | Clayton C R, Lu Y C. A bipolar model of the passivity of stainless steel: The role of Mo addition [J]. J. Electrochem. Soc., 1986, 133: 2465 |
| [65] | Sun J L, Tang H J, Wang C L, et al. Effects of alloying elements and microstructure on stainless steel corrosion: A review [J]. Steel Res. Int., 2022, 93: 2100450 |
| [66] | Olsson C O A, Landolt D. Passive films on stainless steels—Chemistry, structure and growth [J]. Electrochim. Acta, 2003, 48: 1093 |
| [67] | Sun Y L, Xie Z P, Li Y W. Enhanced lithium storage performance of V2O5 with oxygen vacancy [J]. RSC Adv., 2018, 8: 39371 |
| [68] | Kim K M, Park J H, Kim J H, et al. Effect of chemical and heat treatment on the interfacial contact resistance and corrosion resistance of 446M ferritic stainless steel as a bipolar plate for polymer electrolyte membrane fuel cells [J]. Int. J. Hydrogen Energy, 2011, 36: 9926 |
| [69] | Cui J L, Yao Z D, Cui Y F, et al. Electrochemical properties of tungsten-alloying-modified AISI 430 stainless steel as bipolar plates for PEMFCs used in marine environment [J]. Acta Metall. Sin. (Engl. Lett.), 2016, 29: 920 |
| [70] | Wang H L, Turner J A, Li X N, et al. Process modification for coating SnO2: F on stainless steels for PEM fuel cell bipolar plates [J]. J. Power Sources, 2008, 178: 238 |
| [71] | Luo H W, Lin X. Ferritic stainless steel for bipolar plate of fuel cell and preparation method of ferritic stainless steel [P]. Chin Pat, 202510151353.X, 2025 |
| 罗海文, 林 雄. 一种燃料电池双极板用铁素体不锈钢及其制备方法 [P]. 中国专利, 202510151353.X, 2025 |
/
| 〈 |
|
〉 |