High-Entropy Alloys in Extreme Environments: A Perspective on Advantages, Challenges, and Breakthroughs
Received date: 2025-10-15
Revised date: 2025-12-20
Online published: 2025-12-30
Supported by
National Natural Science Foundation of China(52201171);National Natural Science Foundation of China(52225103);National Natural Science Foundation of China(52322102);National Natural Science Foundation of China(U2441262);National Natural Science Foundation of China(W2412068);National Key Research and Development Program of China(2022-YFB4602101);Fundamental Research Funds for the Central Universities(FRF-IDRY-23-020);State Key Laboratory for Advanced Metals and Materials(2025-S11)
Extreme environments, such as ultra-high temperatures, extremely low temperatures, and intense irradiation, impose growing demands on structural materials for next-generation engineering applications. Conventional single-principal-element alloys are approaching their performance limits because of insufficient phase stability, low-temperature ductile-to-brittle transitions, and uncontrolled defect evolution. Conversely, high-entropy alloys (HEAs), characterized by multi-principal elements, exhibit high configurational entropy, severe lattice distortion, and chemical short-range order. These intrinsic characteristics enable exceptional thermal-mechanical stability, cryogenic toughness, and irradiation resistance, rendering them promising candidates for applications in extreme environments. Focusing on three representative conditions, this work summarizes the potentials and challenges of HEAs as structural materials, clarifies the underlying high-entropy-driven mechanisms, and identifies key technological barriers. Furthermore, we report perspectives on future research directions and propose pathways to accelerate the transition of HEAs from laboratory-scale research to practical engineering applications.
LU Zhaoping , SHEN Yaozu , WANG Xianzhen , CHEN Qiang , TANG Jianguo , ZHANG Xiaobin , YU Yong , JIANG Suihe , LIU Xiongjun , WANG Hui , WU Yuan . High-Entropy Alloys in Extreme Environments: A Perspective on Advantages, Challenges, and Breakthroughs[J]. Acta Metall Sin, 2026 , 62(5) : 743 -755 . DOI: 10.11900/0412.1961.2025.00322
| [1] | Yeh J W, Chen S K, Lin S J, et al. Nanostructured high-entropy alloys with multiple principal elements: Novel alloy design concepts and outcomes [J]. Adv. Eng. Mater., 2004, 6: 299 |
| [2] | Cantor B, Chang I T H, Knight P, et al. Microstructural development in equiatomic multicomponent alloys [J]. Mater. Sci. Eng., 2004, A375-377: 213 |
| [3] | Senkov O N, Miller J D, Miracle D B, et al. Accelerated exploration of multi-principal element alloys with solid solution phases [J]. Nat. Commun., 2015, 6: 6529 |
| [4] | Senkov O N, Wilks G B, Scott J M, et al. Mechanical properties of Nb25Mo25Ta25W25 and V20Nb20Mo20Ta20W20 refractory high entropy alloys [J]. Intermetallics, 2011, 19: 698 |
| [5] | Han J C, Song B, Xu P, et al. Multiscale synthesis and performance regulation mechanisms of high-entropy materials [J]. Acta Metall Sin, 2026, 62: 397 |
| 韩杰才, 宋 波, 徐 平 等. 高熵材料的多尺度制备及性能调控机制 [J]. 金属学报, 2026, 62: 397 | |
| [6] | Senkov O N, Scott J M, Senkova S V, et al. Microstructure and room temperature properties of a high-entropy TaNbHfZrTi alloy [J]. J. Alloys Compd., 2011, 509: 6043 |
| [7] | George E P, Raabe D, Ritchie R O. High-entropy alloys [J]. Nat. Rev. Mater., 2019, 4: 515 |
| [8] | Wu Y, Zhang F, Yuan X Y, et al. Short-range ordering and its effects on mechanical properties of high-entropy alloys [J]. J. Mater. Sci. Technol., 2021, 62: 214 |
| [9] | Wang Y H, Jiao M Y, Wu Y, et al. Enhancing properties of high-entropy alloys via manipulation of local chemical ordering [J]. J. Mater. Sci. Technol., 2024, 180: 23 |
| [10] | Han X D, An Z B, Mao S H, et al. Negative mixing enthalpy alloying to promote the development of alloys with high strength and ductility [J]. Acta Metall. Sin., 2025, 61: 953 |
| 韩晓东, 安子冰, 毛圣成 等. 负混合焓合金化推动高强韧合金发展 [J]. 金属学报, 2025, 61: 953 | |
| [11] | Jiao M Y, Lei Z F, Wu Y, et al. Manipulating the ordered oxygen complexes to achieve high strength and ductility in medium-entropy alloys [J]. Nat. Commun., 2023, 14: 806 |
| [12] | Ma E, Liu C. Achieving alloys with concurrent high strength and high ductility [J]. Acta Metall. Sin., 2025, 61: 665 |
| 马 恩, 刘 畅. 如何使合金兼具高强度与高塑性 [J]. 金属学报, 2025, 61: 665 | |
| [13] | Eswarappa Prameela S, Pollock T M, Raabe D, et al. Materials for extreme environments [J]. Nat. Rev. Mater., 2023, 8: 81 |
| [14] | Han L L, Zhu S Y, Rao Z Y, et al. Multifunctional high-entropy materials [J]. Nat. Rev. Mater., 2024, 9: 846 |
| [15] | Qi H, Chen L, Deng S Q, et al. High-entropy ferroelectric materials [J]. Nat. Rev. Mater., 2023, 8: 355 |
| [16] | Yang T, Zhao Y L, Tong Y, et al. Multicomponent intermetallic nanoparticles and superb mechanical behaviors of complex alloys [J]. Science, 2018, 362: 933 |
| [17] | Lee C, Song G, Gao M C, et al. Lattice distortion in a strong and ductile refractory high-entropy alloy [J]. Acta Mater., 2018, 160: 158 |
| [18] | Chen H, Xu Y J, Liu L H, et al. Lattice distortion tuning resistivity Invar effect in high-entropy alloys [J]. Phys. Rev., 2025, 111B: 094209 |
| [19] | Lei Z F, Liu X J, Wu Y, et al. Enhanced strength and ductility in a high-entropy alloy via ordered oxygen complexes [J]. Nature, 2018, 563: 546 |
| [20] | Ding J, Yu Q, Asta M, et al. Tunable stacking fault energies by tailoring local chemical order in CrCoNi medium-entropy alloys [J]. Proc. Natl. Acad. Sci. U.S.A., 2018, 115: 8919 |
| [21] | Perepezko J H. The hotter the engine, the better [J]. Science, 2009, 326: 1068 |
| [22] | Zhao J C, Westbrook J H. Ultrahigh-temperature materials for jet engines [J]. MRS Bull., 2003, 28: 622 |
| [23] | Senkov O N, Miracle D B, Chaput K J, et al. Development and exploration of refractory high entropy alloys—A review [J]. J. Mater. Res., 2018, 33: 3092 |
| [24] | Shen Y Z, Wang X Z, Zhang X B, et al. Research progress on mechanical properties of ultra-high temperature WTa-containing refractory multi-principal element alloys [J]. Tungsten, 2025, 7: 680 |
| [25] | Chen B, Li S Z, Ding J, et al. Correlating dislocation mobility with local lattice distortion in refractory multi-principal element alloys [J]. Scr. Mater., 2023, 222: 115048 |
| [26] | Wang X Y, Maresca F, Cao P H. The hierarchical energy landscape of screw dislocation motion in refractory high-entropy alloys [J]. Acta Mater., 2022, 234: 118022 |
| [27] | Maresca F, Curtin W A. Mechanistic origin of high strength in refractory BCC high entropy alloys up to 1900 K [J]. Acta Mater., 2020, 182: 235 |
| [28] | Yin S, Zuo Y X, Abu-Odeh A, et al. Atomistic simulations of dislocation mobility in refractory high-entropy alloys and the effect of chemical short-range order [J]. Nat. Commun., 2021, 12: 4873 |
| [29] | Tsuru T, Han S, Matsuura S, et al. Intrinsic factors responsible for brittle versus ductile nature of refractory high-entropy alloys [J]. Nat. Commun., 2024, 15: 1706 |
| [30] | Belcher C H, MacDonald B E, Apelian D, et al. The role of interstitial constituents in refractory complex concentrated alloys [J]. Prog. Mater. Sci., 2023, 137: 101140 |
| [31] | Wang Z Q, Wu H H, Wu Y, et al. Solving oxygen embrittlement of refractory high-entropy alloy via grain boundary engineering [J]. Mater. Today, 2022, 54: 83 |
| [32] | Han Z D, Luan H W, Liu X, et al. Microstructures and mechanical properties of Ti x NbMoTaW refractory high-entropy alloys [J]. Mater. Sci. Eng., 2018, A712: 380 |
| [33] | Li T X, Jiao W N, Miao J W, et al. A novel ZrNbMoTaW refractory high-entropy alloy with in-situ forming heterogeneous structure [J]. Mater. Sci. Eng., 2021, A827: 142061 |
| [34] | Sun Y P, Hou C, Li Y R, et al. Ultrafine-grained refractory high-entropy alloy with oxygen control and high mechanical performance [J]. J. Mater. Sci. Technol., 2025, 215: 45 |
| [35] | Golla B R, Mukhopadhyay A, Basu B, et al. Review on ultra-high temperature boride ceramics [J]. Prog. Mater. Sci., 2020, 111: 100651 |
| [36] | Wei Q Q, Xu X D, Shen Q, et al. Metal-carbide eutectics with multiprincipal elements make superrefractory alloys [J]. Sci. Adv., 2022, 8: eabo2068 |
| [37] | Wan Y X, Wang X, Zhang Z B, et al. Structures and properties of the (NbMoTaW)100 - x C x high-entropy composites [J]. J. Alloys Compd., 2021, 889: 161645 |
| [38] | Wu S Y, Qiao D X, Zhang H T, et al. Microstructure and mechanical properties of C x Hf0.25NbTaW0.5 refractory high-entropy alloys at room and high temperatures [J]. J. Mater. Sci. Technol., 2022, 97: 229 |
| [39] | Wei Q Q, Luo G Q, Zhang J, et al. Designing high entropy alloy-ceramic eutectic composites of MoNbRe0.5TaW(TiC) x with high compressive strength [J]. J. Alloys Compd., 2020, 818: 152846 |
| [40] | He H T, Wang J X, Cao Y, et al. Effect of Re and C on mechanical properties of NbTaW0.4 refractory medium-entropy alloy at elevated temperature [J]. J. Alloys Compd., 2023, 931: 167421 |
| [41] | Wu S Y, Qiao D X, Zhao H L, et al. A novel NbTaW0.5 (Mo2C) x refractory high-entropy alloy with excellent mechanical properties [J]. J. Alloys Compd., 2021, 889: 161800 |
| [42] | Shen Y Z, Wang Z Q, Wang X Z, et al. Enhancing mechanical properties of refractory multi-principal element alloys via compositionally complex carbides [J]. J. Mater. Sci. Technol., 2025, 232: 191 |
| [43] | Tanaka M, Tarleton E, Roberts S G. The brittle-ductile transition in single-crystal iron [J]. Acta Mater., 2008, 56: 5123 |
| [44] | Liu J P, Chen H, Zhang C, et al. Progress of cryogenic deformation and strengthening-toughening mechanisms of high-entropy alloys [J]. Acta Metall. Sin., 2023, 59: 727. |
| 刘俊鹏, 陈 浩, 张 弛 等. 高熵合金的低温塑性变形机制及强韧化研究进展 [J]. 金属学报, 2023, 59: 727 | |
| [45] | Gludovatz B, Hohenwarter A, Catoor D, et al. A fracture-resistant high-entropy alloy for cryogenic applications [J]. Science, 2014, 345: 1153 |
| [46] | Gludovatz B, Hohenwarter A, Thurston K V S, et al. Exceptional damage-tolerance of a medium-entropy alloy CrCoNi at cryogenic temperatures [J]. Nat. Commun., 2016, 7: 10602 |
| [47] | Liu D, Yu Q, Kabra S, et al. Exceptional fracture toughness of CrCoNi-based medium- and high-entropy alloys at 20 kelvin [J]. Science, 2022, 378: 978 |
| [48] | Jo Y H, Jung S, Choi W M, et al. Cryogenic strength improvement by utilizing room-temperature deformation twinning in a partially recrystallized VCrMnFeCoNi high-entropy alloy [J]. Nat. Commun., 2017, 8: 15719 |
| [49] | Seol J B, Bae J W, Kim J G, et al. Short-range order strengthening in boron-doped high-entropy alloys for cryogenic applications [J]. Acta Mater., 2020, 194: 366 |
| [50] | Lu Y P, Gao X Z, Jiang L, et al. Directly cast bulk eutectic and near-eutectic high entropy alloys with balanced strength and ductility in a wide temperature range [J]. Acta Mater., 2017, 124: 143 |
| [51] | Sung M Y, Jang T J, Song S Y, et al. Ultrahigh strength with suppressed flow instability at liquid helium temperature via coherent nanoprecipitation in a medium-entropy alloy [J]. Adv. Funct. Mater., 2025, 36: e15593 |
| [52] | Wang F, Song M, Elkot M N, et al. Shearing brittle intermetallics enhances cryogenic strength and ductility of steels [J]. Science, 2024, 384: 1017 |
| [53] | Yang T, Zhao Y L, Luan J H, et al. Nanoparticles-strengthened high-entropy alloys for cryogenic applications showing an exceptional strength-ductility synergy [J]. Scr. Mater., 2019, 164: 30 |
| [54] | Sohail Y, Zhang C L, Gao S H, et al. A complex concentrated alloy with record-high strength-toughness at 77 K [J]. Adv. Mater., 2025, 37: 2410923. |
| [55] | Lu T W, Sun B H, Li Y, et al. Dual-scale chemical ordering for cryogenic properties in CoNiV-based alloys [J]. Nature, 2025, 645: 385 |
| [56] | Wang S B, Wu M X, Shu D, et al. Mechanical instability and tensile properties of TiZrHfNbTa high entropy alloy at cryogenic temperatures [J]. Acta Mater., 2020, 201: 517 |
| [57] | Wen X C, Wu Y, Huang H L, et al. Effects of Nb on deformation-induced transformation and mechanical properties of HfNbxTa0.2-TiZr high entropy alloys [J]. Mater. Sci. Eng., 2021, A805: 140798 |
| [58] | Cook D H, Kumar P, Payne M I, et al. Kink bands promote exceptional fracture resistance in a NbTaTiHf refractory medium-entropy alloy [J]. Science, 2024, 384: 178 |
| [59] | Zinkle S J, Was G S. Materials challenges in nuclear energy [J]. Acta Mater., 2013, 61: 735 |
| [60] | Murty K L, Charit I. Structural materials for Gen-IV nuclear reactors: Challenges and opportunities [J]. J. Nucl. Mater., 2008, 383: 189 |
| [61] | Johnston W G, Rosolowski J H, Turkalo A M, et al. An experimental survey of swelling in commercial Fe-Cr-Ni alloys bombarded with 5 MeV Ni ions [J]. J. Nucl. Mater., 1974, 54: 24 |
| [62] | Nagase T, Rack P D, Noh J H, et al. In-situ TEM observation of structural changes in nano-crystalline CoCrCuFeNi multicomponent high-entropy alloy (HEA) under fast electron irradiation by high voltage electron microscopy (HVEM) [J]. Intermetallics, 2015, 59: 32 |
| [63] | Zhang Y W, Stocks G M, Jin K, et al. Influence of chemical disorder on energy dissipation and defect evolution in concentrated solid solution alloys [J]. Nat. Commun., 2015, 6: 8736 |
| [64] | Granberg F, Nordlund K, Ullah M W, et al. Mechanism of radiation damage reduction in equiatomic multicomponent single phase alloys [J]. Phys. Rev. Lett., 2016, 116: 135504 |
| [65] | Lu C Y, Niu L L, Chen N J, et al. Enhancing radiation tolerance by controlling defect mobility and migration pathways in multicomponent single-phase alloys [J]. Nat. Commun., 2016, 7: 13564 |
| [66] | Li D, Jia N, Huang H, et al. Helium ion irradiation enhanced precipitation and the impact on cavity formation in a HfNbZrTi refractory high entropy alloy [J]. J. Nucl. Mater., 2021, 552: 153023 |
| [67] | Xia X C, Zhang E K, Ding J, et al. Research progress on laser cladding of refractory high-entropy alloy coatings [J]. Acta Metall Sin, 2025, 61: 59 |
| 夏兴川, 张恩宽, 丁 俭 等. 激光熔覆难熔高熵合金涂层研究进展 [J]. 金属学报, 2025, 61: 59 | |
| [68] | Jin K, Bei H B. Single-phase concentrated solid-solution alloys: Bridging intrinsic transport properties and irradiation resistance [J]. Front. Mater., 2018, 5: 26 |
| [69] | Jin K, Zhang C, Zhang F, et al. Influence of compositional complexity on interdiffusion in Ni-containing concentrated solid-solution alloys [J]. Mater. Res. Lett., 2018, 6: 293 |
| [70] | Zhao S J, Egami T, Stocks G M, et al. Effect of d electrons on defect properties in equiatomic NiCoCr and NiCoFeCr concentrated solid solution alloys [J]. Phys. Rev. Mater., 2018, 2: 013602 |
| [71] | Ding J, Wang Z J. Local chemical order in high-entropy alloys [J]. Acta Metall Sin, 2021, 57: 413 |
| 丁 俊, 王章洁. 高熵合金中的局域化学有序 [J]. 金属学报, 2021, 57: 413 | |
| [72] | Zhang Z R, Armstrong D E J, Grant P S. The effects of irradiation on CrMnFeCoNi high-entropy alloy and its derivatives [J]. Prog. Mater. Sci., 2022, 123: 100807 |
| [73] | Liu L Q, Liu X J, Du Q, et al. Local chemical ordering and its impact on radiation damage behavior of multi-principal element alloys [J]. J. Mater. Sci. Technol., 2023, 135: 13 |
| [74] | Su Z X, Ding J, Song M, et al. Enhancing the radiation tolerance of high-entropy alloys via solute-promoted chemical heterogeneities [J]. Acta Mater., 2023, 245: 118662 |
| [75] | Ullah M W, Aidhy D S, Zhang Y W, et al. Damage accumulation in ion-irradiated Ni-based concentrated solid-solution alloys [J]. Acta Mater., 2016, 109: 17 |
| [76] | Liu L Q. Radiation damage behavior and the underlying mechanism of NiFeCr-based multi-principal element alloys by molecular dynamics simulations [D]. Beijing: University of Science and Technology Beijing, 2024 |
| 刘乐青. NiFeCr系多主元合金辐照损伤行为及其机理的分子动力学研究 [D]. 北京: 北京科技大学, 2024 | |
| [77] | Tan L Z, Ali K, Ghosh P S, et al. Design principles of low-activation high entropy alloys [J]. J. Alloys Compd., 2022, 907: 164526 |
| [78] | Pu G, Lin L W, Ang R, et al. Outstanding radiation tolerance and mechanical behavior in ultra-fine nanocrystalline Al1.5CoCrFeNi high entropy alloy films under He ion irradiation [J]. Appl. Surf. Sci., 2020, 516: 146129 |
| [79] | Zhao Y F, Chen H H, Zhang D D, et al. Unusual He-ion irradiation strengthening and inverse layer thickness-dependent strain rate sensitivity in transformable high-entropy alloy/metal nanolaminates: A comparison of Fe50Mn30Co10Cr10/Cu vs Fe50Mn30Co10Ni10/Cu [J]. J. Mater. Sci. Technol., 2022, 116: 199 |
| [80] | Du J L, Jiang S H, Cao P P, et al. Superior radiation tolerance via reversible disordering-ordering transition of coherent superlattices [J]. Nat. Mater., 2023, 22: 442 |
| [81] | Cao P P. Tuning mechanical properties and irradiation resistance of FCC-based multi-principal element alloys via nano-precipitation [D]. Beijing: University of Science and Technology Beijing, 2022 |
| 曹培培. 基于纳米析出调控FCC系多主元合金的力学性能和辐照性能 [D]. 北京: 北京科技大学, 2022 | |
| [82] | Peng X Y, Cao P P, Liu D, et al. On the origin of superior stability of coherent nanoparticles under ion irradiation [J]. Mater. Des., 2024, 247: 113393 |
| [83] | Yang C, Wang B Y, Shen G Y, et al. High-throughput design of a light and strong refractory eutectic medium entropy alloy with outstanding He-ion irradiation resistance [J]. Sci. Adv., 2025, 11: eadq6828 |
/
| 〈 |
|
〉 |