Hierarchical Lamellar Heterostructure Design Renders Metallic Materials with Ultrahigh Strength-Ductility Combinations
Received date: 2025-08-13
Revised date: 2025-09-10
Online published: 2025-11-07
Supported by
National Natural Science Foundation of China(U23A20607);National Key Research and Development Program of China(2022YFC2904900)
“Heterogeneous structures” or “heterostructures” have emerged as a cutting-edge paradigm in the field of mechanical strengthening and toughening, promising to overcome the long-standing trade-offs among strength, ductility, and toughness in metallic materials. Inspired by the multiscale design principle of natural materials, researchers have proposed a synergistic design of bioinspired “hierarchical lamellar heterostructures”, enabling exceptional and simultaneous enhancements in the strength, ductility, and toughness of metallic materials. This study reviews the theoretical foundations, design principles, and strengthening-toughening mechanisms underpinning several archetypal hierarchical lamellar heterostructures: bionic herringbone type, micro-lamellar heredity pattern, and cocoon-like dislocation network model. This review focuses on how these hierarchical lamellar heterostructures effectively overcome the strength-ductility trade-off limitations imposed by uncontrolled crack propagation, ultrafine grain structures, and high-density dislocations. It also elucidates how this heterostructure strategy and its remarkable efficacy have been successfully extended to multiple metal systems, enabling the design and fabrication of a new generation of key high-speed railway contact wires with internationally leading comprehensive performance. Finally, the review discusses the prospects for developing more advanced hierarchical lamellar heterostructured materials and explores their potential future directions.
ZHONG Yunbo , SHI Peijian . Hierarchical Lamellar Heterostructure Design Renders Metallic Materials with Ultrahigh Strength-Ductility Combinations[J]. Acta Metall Sin, 2025 , 61(11) : 1593 -1602 . DOI: 10.11900/0412.1961.2025.00234
| [1] | Kim S H, Kim H, Kim N J. Brittle intermetallic compound makes ultrastrong low-density steel with large ductility [J]. Nature, 2015, 518: 77 |
| [2] | Ritchie R O. Toughening materials: Enhancing resistance to fracture [J]. Philos. Trans. Roy. Soc., 2021, 379A: 20200437 |
| [3] | Gludovatz B, Hohenwarter A, Catoor D, et al. A fracture-resistant high-entropy alloy for cryogenic applications [J]. Science, 2014, 345: 1153 |
| [4] | Zhang M Z, Zhang K, Song K K, et al. Enhanced mechanical performance of gradient-structured CoCrFeMnNi high-entropy alloys induced by industrial shot-blasting [J]. Rare Met., 2023, 42: 982 |
| [5] | Ma E, Liu C. Achieving alloys with concurrent high strength and high ductility [J]. Acta Metall. Sin., 2025, 61: 665 |
| 马 恩, 刘 畅. 如何使合金兼具高强度与高塑性 [J]. 金属学报, 2025, 61: 665 | |
| [6] | Shi P J, Ren W L, Zheng T X, et al. Enhanced strength-ductility synergy in ultrafine-grained eutectic high-entropy alloys by inheriting microstructural lamellae [J]. Nat. Commun., 2019, 10: 489 |
| [7] | Li Y, Shi P J, Wen Y B, et al. Hierarchically heterogeneous eutectic high-entropy alloy with high strength and high ductility fabricated by directional solidification [J]. Shanghai Met., 2021, 43(5): 79 |
| 李 毅, 时培建, 温跃波 等. 定向凝固法制备高强塑性多级异构共晶高熵合金 [J]. 上海金属, 2021, 43(5): 79 | |
| [8] | Lü Z P, Jiang S H, He J Y, et al. Second phase strengthening in advanced metal materials [J]. Acta Metall. Sin., 2016, 52: 1183 |
| 吕昭平, 蒋虽合, 何骏阳 等. 先进金属材料的第二相强化 [J]. 金属学报, 2016, 52: 1183 | |
| [9] | Zhu Y T, Liao X Z. Retaining ductility [J]. Nat. Mater., 2004, 3: 351 |
| [10] | Lu L, Zhao H Z. Progress in strengthening and toughening mechanisms of heterogeneous nanostructured metals [J]. Acta Metall. Sin., 2022, 58: 1360 |
| 卢 磊, 赵怀智. 异质纳米结构金属强化韧化机理研究进展 [J]. 金属学报, 2022, 58: 1360 | |
| [11] | Huang X X. Size effects on the strength of metals [J]. Acta Metall. Sin., 2014, 50: 137 |
| 黄晓旭. 金属强度的尺寸效应 [J]. 金属学报, 2014, 50: 137 | |
| [12] | Koch C C, Morris D G, Lu K, et al. Ductility of nanostructured materials [J]. MRS Bull., 1999, 24: 54 |
| [13] | Shahmir H, He J Y, Lu Z P, et al. Effect of annealing on mechanical properties of a nanocrystalline CoCrFeNiMn high-entropy alloy processed by high-pressure torsion [J]. Mater. Sci. Eng., 2016, A676: 294 |
| [14] | He B B, Hu B, Yen H W, et al. High dislocation density-induced large ductility in deformed and partitioned steels [J]. Science, 2017, 357: 1029 |
| [15] | Wani I S, Bhattacharjee T, Sheikh S, et al. Ultrafine-grained AlCoCrFeNi2.1 eutectic high-entropy alloy [J]. Mater. Res. Lett., 2016, 4: 174 |
| [16] | Bhattacharjee T, Wani I S, Sheikh S, et al. Simultaneous strength-ductility enhancement of a nano-lamellar AlCoCrFeNi2.1 eutectic high entropy alloy by cryo-rolling and annealing [J]. Sci. Rep., 2018, 8: 3276 |
| [17] | Zhu Y T, Ameyama K, Anderson P M, et al. Heterostructured materials: Superior properties from hetero-zone interaction [J]. Mater. Res. Lett., 2020, 9: 1 |
| [18] | Wu X L, Yang M X, Yuan F P, et al. Heterogeneous lamella structure unites ultrafine-grain strength with coarse-grain ductility [J]. Proc. Natl. Acad. Sci. USA, 2015, 112: 14501 |
| [19] | Wu X L, Zhu Y T. Heterogeneous materials: A new class of materials with unprecedented mechanical properties [J]. Mater. Res. Lett., 2017, 5: 527 |
| [20] | Romero-Resendiz L, El-Tahawy M, Zhang T, et al. Heterostructured stainless steel: Properties, current trends, and future perspectives [J]. Mater. Sci. Eng., 2022, R150: 100691 |
| [21] | Wu X L, Zhu Y T. Heterostructured metallic materials: Plastic deformation and strain hardening [J]. Acta Metall. Sin., 2022, 58: 1349 |
| 武晓雷, 朱运田. 异构金属材料及其塑性变形与应变硬化 [J]. 金属学报, 2022, 58: 1349 | |
| [22] | Zhu Y T, Wu X L. Heterostructured materials [J]. Prog. Mater. Sci., 2023, 131: 101019 |
| [23] | Shi P J, Zhong Y B, Li Y, et al. Multistage work hardening assisted by multi-type twinning in ultrafine-grained heterostructural eutectic high-entropy alloys [J]. Mater. Today, 2020, 41: 62 |
| [24] | Shi P J, Li R G, Li Y, et al. Hierarchical crack buffering triples ductility in eutectic herringbone high-entropy alloys [J]. Science, 2021, 373: 912 |
| [25] | Shi P J, Shen Z, Wang H G, et al. Bioinspired, heredity-derived hierarchical bulk multifunctional copper alloys [J]. Mater. Today, 2023, 71: 22 |
| [26] | Shi P J, Li Y, Jiang X, et al. Strong-yet-ductile eutectic alloys employing cocoon‐like nanometer‐sized dislocation cells [J]. Adv. Mater., 2024, 36: 2405459 |
| [27] | Shi P J, Li Y, Li Z, et al. Strong, ductile, and hierarchical hetero-lamellar-structured alloys through microstructural inheritance and refinement [J]. Proc. Natl. Acad. Sci. USA, 2025, 122: e2409317121 |
| [28] | Ritchie R O. The conflicts between strength and toughness [J]. Nat. Mater., 2011, 10: 817 |
| [29] | Koyama M, Zhang Z, Wang M M, et al. Bone-like crack resistance in hierarchical metastable nanolaminate steels [J]. Science, 2017, 355: 1055 |
| [30] | Lu Y P, Dong Y, Guo S, et al. A promising new class of high-temperature alloys: Eutectic high-entropy alloys [J]. Sci. Rep., 2014, 4: 6200 |
| [31] | Jain S, Jain R, Kumar V, et al. Design strategies and mechanical behaviour of high-strength eutectic high-entropy alloys: A comprehensive review [J]. J. Alloys Compd., 2025, 1022: 180000 |
| [32] | Shi P J, Li Y, Wen Y B, et al. A precipitate-free AlCoFeNi eutectic high-entropy alloy with strong strain hardening [J]. J. Mater. Sci. Technol., 2021, 89: 88 |
| [33] | Lee J, Kim S, Kwon T, et al. Strengthening mechanisms analysis and tailoring of bimodal grain structures for enhanced strength in CoCrFeMnNi high-entropy alloys [J]. Rare Met., 2024, 43: 3893 |
| [34] | Edalati P, Fuji M, Edalati K. Superfunctional high-entropy alloys and ceramics by severe plastic deformation [J]. Rare Met., 2023, 42: 3246 |
| [35] | Ren J, Zhang Y, Zhao D X, et al. Strong yet ductile nanolamellar high-entropy alloys by additive manufacturing [J]. Nature, 2022, 608: 62 |
| [36] | Ma H W, Zhao Y C, Feng L, et al. Achieving strength-ductility synergy in novel paramagnetic Fe-based medium-entropy alloys through deep cryogenic deformation [J]. Rare Met., 2024, 43: 4493 |
| [37] | Li Y, Shi P J, Wang M Y, et al. Unveiling microstructural origins of the balanced strength-ductility combination in eutectic high-entropy alloys at cryogenic temperatures [J]. Mater. Res. Lett., 2022, 10: 602 |
| [38] | Natonal Raiway Administration of the People's Republic of China. Copper and copper alloy contact wires for electrified railway [S]. Beijing: China Railway Publishing House, 2017 |
| 国家铁路局. 电气化铁路用铜及铜合金接触线 [S]. 北京: 中国铁道出版社, 2017 |
/
| 〈 |
|
〉 |