Quantitative Relationships Between the Strength-Plasticity and Strength-Electrical Conductivity of Metallic Materials
Received date: 2025-08-25
Revised date: 2025-10-04
Online published: 2025-11-03
Supported by
National Natural Science Foundation of China(52321001);National Natural Science Foundation of China(52130002);National Natural Science Foundation of China(52322105);National Natural Science Foundation of China(52571160);National Natural Science Foundation of China(52401122);Strategic Priority Research Program of the Chinese Academy of Sciences(XDB1420000)
A general mutual constraint exists between the strength-plasticity and the strength-electrical conductivity of metallic materials. This study proposes an independent space model of dislocation motion to show that the trade-off relation between the strength and plasticity of metallic materials is controlled by the independent spatial size of dislocation motion. Furthermore, the model is used to show that the metal type, alloy composition, deformation temperature, and strain rate are the key factors regulating the spatial size, whereas the microstructure or grain size distribution has a limited influence on it. This finding explains why it is difficult to simultaneously improve strength and plasticity through microstructure or grain size optimization when the metal type, composition, and deformation parameters are fixed. Further, based on the grain size dependence of dislocation piling-up in single-phase alloys, a quantitative trade-off model between tensile strength and uniform elongation is established and experimentally verified in a variety of metal alloy systems. Three high-strength and high-electrical conductivity principles for metal wires are proposed by analyzing the differentiated effects of grain boundaries, orientation, and nanoprecipitation relative dislocation piling-up and electron scattering: elongated grains, strong texture orientation, and nanoprecipitate regulation. Based on the three principles, a quantitative model describing the relationship between strength and electrical conductivity is constructed, and the underlying mechanisms of typical phenomena, such as the synergistic improvement and mutual constraint of strength and electrical conductivity in different metal wires, are systematically explained. Finally, high-performance conductors based on three principles, with performance that breaks through the existing strength-electrical conductivity constraint, are developed. Establishing quantitative models describing the relationships between strength and plasticity, as well as between the strength and electrical conductivity of metallic materials, can efficiently guide material selection, composition design, and microstructure process control, ensuring the service safety of components.
ZHANG Zhefeng , HOU Jiapeng , LIU Rui , LI Xiaotao , ZHANG Zhenjun , ZHANG Peng . Quantitative Relationships Between the Strength-Plasticity and Strength-Electrical Conductivity of Metallic Materials[J]. Acta Metall Sin, 2026 , 62(2) : 253 -262 . DOI: 10.11900/0412.1961.2025.00248
| [1] | Anderson P M, Hirth J P, Lothe J. Theory of Dislocations [M]. 3rd Ed., Cambridge: Cambridge University Press, 2017: 58 |
| [2] | Meyers M, Chawla K, translated by Zhang Z F, Lu L. Mechanical Behavior of Materials [M]. Beijing: Higher Education Press, 2017: 255 |
| Meyers M, Chawla K著, 张哲峰, 卢 磊 译. 材料力学行为 [M]. 北京: 高等教育出版社, 2017: 255 | |
| [3] | Jiang S H, Wang H, Wu Y, et al. Ultrastrong steel via minimal lattice misfit and high-density nanoprecipitation [J]. Nature, 2017, 544: 460 |
| [4] | An X H, Wu S D, Wang Z G, et al. Significance of stacking fault energy in bulk nanostructured materials: Insights from Cu and its binary alloys as model systems [J]. Prog. Mater. Sci., 2019, 101: 1 |
| [5] | Zhang D Y, Qiu D, Gibson M A, et al. Additive manufacturing of ultrafine-grained high-strength titanium alloys [J]. Nature, 2019, 576: 91 |
| [6] | Ma K K, Wen H M, Hu T, et al. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy [J]. Acta Mater., 2014, 62: 141 |
| [7] | Sohrabi M J, Kalhor A, Mirzadeh H, et al. Tailoring the strengthening mechanisms of high-entropy alloys toward excellent strength-ductility synergy by metalloid silicon alloying: A review [J]. Prog. Mater. Sci., 2024, 144: 101295 |
| [8] | Wu H, Fan G H. An overview of tailoring strain delocalization for strength-ductility synergy [J]. Prog. Mater. Sci., 2020, 113: 100675 |
| [9] | Wang Y M, Chen M W, Zhou F H, et al. High tensile ductility in a nanostructured metal [J]. Nature, 2002, 419: 912 |
| [10] | Lu L, Shen Y F, Chen X H, et al. Ultrahigh strength and high electrical conductivity in copper [J]. Science, 2004, 304: 422 |
| [11] | Wu X L, Yuan F P, Yang M X, et al. Nanodomained nickel unite nanocrystal strength with coarse-grain ductility [J]. Sci. Rep., 2015, 5: 11728 |
| [12] | Liu G, Zhang G J, Jiang F, et al. Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility [J]. Nat. Mater., 2013, 12: 344 |
| [13] | Gao J H, Jiang S H, Zhang H R, et al. Facile route to bulk ultrafine-grain steels for high strength and ductility [J]. Nature, 2021, 590: 262 |
| [14] | He B B, Hu B, Yen H W, et al. High dislocation density-induced large ductility in deformed and partitioned steels [J]. Science, 2017, 357: 1029 |
| [15] | Li Z M, Pradeep K G, Deng Y, et al. Metastable high-entropy dual-phase alloys overcome the strength-ductility trade-off [J]. Nature, 2016, 534: 227 |
| [16] | Pan Q S, Zhang L X, Feng R, et al. Gradient cell-structured high-entropy alloy with exceptional strength and ductility [J]. Science, 2021, 374: 984 |
| [17] | Sakai Y, Schneider-Muntau H J. Ultra-high strength, high conductivity Cu-Ag alloy wires [J]. Acta Mater., 1997, 45: 1017 |
| [18] | Zhang H T, Fu H D, He X Q, et al. Dramatically enhanced combination of ultimate tensile strength and electric conductivity of alloys via machine learning screening [J]. Acta Mater., 2020, 200: 803 |
| [19] | Liu R, Li K Q, Zhang Z J, et al. Independent dislocation space model for synchronous improvement of strength and plasticity in fcc metals [J]. J. Mater. Sci. Technol., 2025, 224: 239 |
| [20] | Li X T, Liu R, Hou J P, et al. Trade-off model for strength-ductility relationship of metallic materials [J]. Acta Mater., 2025, 289: 120942 |
| [21] | Hou J P, Li R, Wang Q, et al. Three principles for preparing Al wire with high strength and high electrical conductivity [J]. J. Mater. Sci. Technol., 2019, 35: 742 |
| [22] | Hou J P, Li X T, Wang S, et al. Quantitative model for grain boundary effects on strength-electrical conductivity relation [J]. Acta Mater., 2024, 281: 120390 |
| [23] | Ashby M F. Materials Selection in Mechanical Design [M]. 4th Ed., Amsterdam: Elsevier, 2011: 31 |
| [24] | Qu S, An X H, Yang H J, et al. Microstructural evolution and mechanical properties of Cu-Al alloys subjected to equal channel angular pressing [J]. Acta Mater., 2009, 57: 1586 |
| [25] | Shao C W, Zhang P, Zhu Y K, et al. Simultaneous improvement of strength and plasticity: Additional work-hardening from gradient microstructure [J]. Acta Mater., 2018, 145: 413 |
| [26] | Li G D, Jiang J X, Ma H C, et al. Superior strength-ductility synergy in three-dimensional heterogeneous-nanostructured metals [J]. Acta Mater., 2023, 256: 119143 |
| [27] | Hirth J P, Lothe J. Theory of Dislocations [M]. 2nd Ed., New York: John Wiley & Sons, Inc., 1982: 764 |
| [28] | Mishin Y, Mehl M J, Papaconstantopoulos D A, et al. Structural stability and lattice defects in copper: Ab initio, tight-binding, and embedded-atom calculations [J]. Phys. Rev., 2001, 63B: 224106 |
| [29] | Li K Q, Zhang Z J, Li L L, et al. Effective stacking fault energy in face-centered cubic metals [J]. Acta Metall. Sin. (Engl. Lett.), 2018, 31: 873 |
| [30] | Vegge T, Rasmussen T, Leffers T, et al. Determination of the of rate cross slip of screw dislocations [J]. Phys. Rev. Lett., 2000, 85: 3866 |
| [31] | Püschl W, Schoeck G. Calculation of cross-slip parameters in f.c.c. crystals [J]. Mater. Sci. Eng., 1993, A164: 286 |
| [32] | Kocks U F, Mecking H. Physics and phenomenology of strain hardening: The FCC case [J]. Prog. Mater. Sci., 2003, 48: 171 |
| [33] | Zhang Z J, Qu Z, Xu L, et al. A general physics-based hardening law for single phase metals [J]. Acta Mater., 2022, 231: 117877 |
| [34] | Han D, Wang Z Y, Yan Y, et al. A good strength-ductility match in Cu-Mn alloys with high stacking fault energies: Determinant effect of short range ordering [J]. Scr. Mater., 2017, 133: 59 |
| [35] | Otto F, Dlouhy A, Somsen C, et al. The influences of temperature and microstructure on the tensile properties of a CoCrFeMnNi high-entropy alloy [J]. Acta Mater., 2013, 61: 5743 |
| [36] | Yang H K, Zhang Z J, Dong F Y, et al. Strain rate effects on tensile de-formation behaviors for Fe-22Mn-0.6C-(1.5Al) twinning-induced plasticity steel [J]. Mater. Sci. Eng., 2014, A607: 551 |
| [37] | Wang F, Song M, Elkot M N, et al. Shearing brittle intermetallics enhances cryogenic strength and ductility of steels [J]. Science, 2024, 384: 1017 |
| [38] | Ma E, Liu C. Chemical inhomogeneities in high-entropy alloys help mitigate the strength-ductility trade-off [J]. Prog. Mater. Sci., 2024, 143: 101252 |
| [39] | Watanabe T, Tsurekawa S. The control of brittleness and development of desirable mechanical properties in polycrystalline systems by grain boundary engineering [J]. Acta Mater., 1999, 47: 4171 |
| [40] | Khalajhedayati A, Pan Z L, Rupert T J. Manipulating the interfacial structure of nanomaterials to achieve a unique combination of strength and ductility [J]. Nat. Commun., 2016, 7: 10802 |
| [41] | Zhang Z F, Li K Q, Cai T, et al. Effects of stacking fault energy on the deformation mechanisms and mechanical properties of face-centered cubic metals [J]. Acta Metall. Sin., 2023, 59: 467 |
| 张哲峰, 李克强, 蔡 拓 等. 层错能对面心立方金属形变机制与力学性能的影响 [J]. 金属学报, 2023, 59: 467 | |
| [42] | Carlton C E, Ferreira P J. What is behind the inverse Hall-Petch effect in nanocrystalline materials? [J]. Acta Mater., 2007, 55: 3749 |
| [43] | Hall E O. The deformation and ageing of mild steel: III Discussion of results [J]. Proc. Phys. Soc., 1951, 64B: 747 |
| [44] | Miyajima Y, Komatsu S Y, Mitsuhara M, et al. Change in electrical resistivity of commercial purity aluminium severely plastic deformed [J]. Philos. Mag., 2010, 90: 4475 |
| [45] | Schmid E, Boas W. Plasticity of Crystals [M]. London: F. A. Hughes & Co. Limited, 1950: 77 |
| [46] | Sauvage X, Bobruk E V, Murashkin M Y, et al. Optimization of electrical conductivity and strength combination by structure design at the nanoscale in Al-Mg-Si alloys [J]. Acta Mater., 2015, 98: 355 |
| [47] | Bardel D, Perez M, Nelias D, et al. Coupled precipitation and yield strength modelling for non-isothermal treatments of a 6061 aluminium alloy [J]. Acta Mater., 2014, 62: 129 |
| [48] | Zhang Z, Chen D. Consideration of Orowan strengthening effect in particulate-reinforced metal matrix nanocomposites: A model for predicting their yield strength [J]. Scr. Mater., 2006, 54: 1321 |
| [49] | Seidman D N, Marquis E A, Dunand D C. Precipitation strengthening at ambient and elevated temperatures of heat-treatable Al(Sc) alloys [J]. Acta Mater., 2002, 50: 4021 |
| [50] | Booth-Morrison C, Dunand D C, Seidman D N. Coarsening resistance at 400 oC of precipitation-strengthened Al-Zr-Sc-Er alloys [J]. Acta Mater., 2011, 59: 7029 |
| [51] | Ziman J M. Electrons and Phonons: The Theory of Transport Phenomena in Solids [M]. Oxford: Clarendon Press, 1960: 4 |
| [52] | Myhr O R, Grong ?, Andersen S J. Modelling of the age hardening behaviour of Al-Mg-Si alloys [J]. Acta Mater., 2001, 49: 65 |
| [53] | Perez M. Gibbs-Thomson effects in phase transformations [J]. Scr. Mater., 2005, 52: 709 |
| [54] | Simar A, Bréchet Y, de Meester B, et al. Sequential modeling of local precipitation, strength and strain hardening in friction stir welds of an aluminum alloy 6005A-T6 [J]. Acta Mater., 2007, 55: 6133 |
| [55] | Ma E, Liu C. Achieving alloys with concurrent high strength and high ductility [J]. Acta Metall. Sin., 2025, 61: 665 |
| 马 恩, 刘 畅. 如何使合金兼具高强度与高塑性 [J]. 金属学报, 2025, 61: 665 |
/
| 〈 |
|
〉 |