Abstract

With growing emphasis on energy saving and emission reduction, lightweight structures have become a key development focus in vehicle manufacturing. Mg and Al alloys, as lightweight materials with excellent properties, have broad applications in aerospace, automobile manufacturing, 3C products, and other fields. Mg/Al composite components can fully leverage the advantages of both alloys. Therefore, achieving high-quality and high-efficiency joints of Mg/Al dissimilar alloys has become a critical challenge in the manufacturing industry. Among the important structural types of Mg/Al thin-plate dissimilar welded joints, lap joints have attracted considerable attention. Friction stir welding (FSW), a solid-state joining process, offers distinct advantages for producing high-quality, defect-free Mg/Al joints. Ultrasonic-assisted FSW can further broaden the process window and enhance joint strength. However, the mechanism by which ultrasound influences joint formation during welding remains unclear. In this study, ultrasonic vibration enhanced friction stir lap welding experiments were conducted on Mg alloy and Al alloy sheets. The optimal process parameters were determined to be a rotation speed of 800 r/min and a welding speed of 90 mm/min. During welding, the keyhole region of the lap joint was subjected to a sudden stop + freezing treatment. Material flow behavior was characterized on vertical cross-sections at various angles around the keyhole and on horizontal cross-sections. Microstructures of the characteristic regions on the horizontal cross-section around the keyhole and along the weld centerline passing through keyhole center near the Mg alloy side were characterized. The influence of ultrasonic vibration on the mechanical properties of the lap joints was also evaluated. The results show that introducing ultrasonic vibration during friction stir lap welding enhanced both the tensile shear strength and the effective sheet thickness of the Mg/Al lap joints. Furthermore, ultrasonic vibration increased the volume of material driven by the tool, promoting enhanced material flow and mixing. During joint formation, the grain size distribution around the keyhole on the Mg alloy side became more uniform, and the grains behind the tool underwent a significantly higher degree of recrystallization.

Cite this article

YIN Jialin , SHI Lei , WU Chuansong . Effect of Ultrasonic Vibration on Microstructure Evolution at the Mg/Al Dissimilar Alloy Friction Stir Welded Lap Joint Interface[J]. Acta Metall Sin, 2026 , 62(1) : 133 -147 . DOI: 10.11900/0412.1961.2025.00198

References

[1] Zhang W, Xu J. Advanced lightweight materials for Automobiles: A review [J]. Mater. Des., 2022, 221: 110994
[2] Lyu R, Jiang X, Minoru O, et al. Lightweight design of automobile frame based on magnesium alloy [J]. IOP Conf. Ser. Mater. Sci. Eng., 2018, 372: 012047
[3] Ahmed M M Z, El-Sayed Seleman M M, Fydrych D, et al. Friction stir welding of aluminum in the aerospace industry: The current progress and state-of-the-art review [J]. Materials, 2023, 16: 2971
[4] Pantelakis S G, Alexopoulos N D, Chamos A N. Mechanical performance evaluation of cast magnesium alloys for automotive and aeronautical applications [J]. J. Eng. Mater. Technol., 2007, 129: 422
[5] Liu J Z, Zhao Y H, Song L, et al. Study on the AZ31B magnesium alloy in the application on high-speed trains [J]. Adv. Mater. Res., 2012, 535-537: 875
[6] Song L, Zhao Y H, Liu J Z, et al. Study on the ZK60A and AZ31B magnesium-alloy in the application on high-speed train seats [J]. Adv. Mater. Res., 2013, 690-693: 53
[7] Yan Y, Zhang D T, Qiu C, et al. Dissimilar friction stir welding between 5052 aluminum alloy and AZ31 magnesium alloy [J]. Trans. Nonferrous Met. Soc. China, 2010, 20: S619
[8] Firouzdor V, Kou S. Al-to-Mg friction stir welding: Effect of positions of Al and Mg with respect to the welding tool [J]. Weld. J., 2009, 88: 213S
[9] Lv X Z, Liu L M, Song G. Laser welding of AZ31Mg alloy with 6061Al alloy via Ti interlayer based on two kinds of bonding mechanisms [J]. J. Manuf. Process., 2022, 83: 678
[10] Xu Y, Ke L M, Nie H, et al. Precipitation behavior of intermetallic compounds at the interface of thick plate friction stir welded Al Alloy/Mg alloy joints under local strong cooling [J]. Acta Metall. Sin., 2024, 60: 777
  徐 洋, 柯黎明, 聂 浩 等. 局部强冷作用下厚板铝合金/镁合金搅拌摩擦焊界面金属间化合物的析出行为 [J]. 金属学报, 2024, 60: 777
[11] Singh V P, Patel S K, Ranjan A, et al. Recent research progress in solid state friction-stir welding of aluminium-magnesium alloys: A critical review [J]. J. Mater. Res. Technol., 2020, 9: 6217
[12] Zhai M, Wu C S, Shi L. Influence of tool pin length and dissimilar material configuration on friction stir lap welding of Al and Mg alloys [J]. Int. J. Adv. Manuf. Technol., 2022, 122: 1567
[13] Heidarzadeh A, Mironov S, Kaibyshev R, et al. Friction stir welding/processing of metals and alloys: A comprehensive review on microstructural evolution [J]. Prog. Mater. Sci., 2021, 117: 100752
[14] Wen T, Wei L, Chen X, et al. Effects of ultrasonic vibration on plastic deformation of AZ31 during the tensile process [J]. Int. J. Miner. Metall. Mater., 2011, 18: 70
[15] Li S L, Zhao Y X, Cui J H, et al. Ultrasonic energy attenuation characteristics in plastic deformation of 2219-O aluminum alloy [J]. Int. J. Adv. Manuf. Technol., 2023, 125: 267
[16] Hu X J, Li X H, Qin Q Y. Influence of ultrasonic vibration on metal plastic forming [J]. Appl. Mech. Mater., 2013, 470: 162
[17] Liu X C, Wu C S. Material flow in ultrasonic vibration enhanced friction stir welding [J]. J. Mater. Process. Technol., 2015, 225: 32
[18] Liu X C, Wu C S, Padhy G K. Characterization of plastic deformation and material flow in ultrasonic vibration enhanced friction stir welding [J]. Scr. Mater., 2015, 102: 95
[19] Wu C S, Wang T, Su H. Material flow velocity, strain and strain rate in ultrasonic vibration enhanced friction stir welding of dissimilar Al/Mg alloys [J]. J. Manuf. Process., 2022, 75: 13
[20] Ji S D, Niu S Y, Liu J G, et al. Friction stir lap welding of Al to Mg assisted by ultrasound and a Zn interlayer [J]. J. Mater. Process. Technol., 2019, 267: 141
[21] Zhao J J, Wu C S, Shi L, et al. Evolution of microstructures and intermetallic compounds at bonding interface in friction stir welding of dissimilar Al/Mg alloys with/without ultrasonic assistance [J]. J. Mater. Sci. Technol., 2023, 139: 31
[22] Zhao J J, Wu C S, Shi L. Effect of ultrasonic field on microstructure evolution in friction stir welding of dissimilar Al/Mg alloys [J]. J. Mater. Res. Technol., 2022, 17: 1
[23] Zhai M, Shi L, Wu C S. Elucidating the process mechanism in Mg-to-Al friction stir lap welding enhanced by ultrasonic vibration [J]. J. Magnes. Alloys, 2025, 13: 338
[24] Chen Y C, Nakata K. Friction stir lap joining aluminum and magnesium alloys [J]. Scr. Mater., 2008, 58: 433
[25] Deng H K, Xie Y M, Meng X C, et al. Improving tensile-shear strength of friction stir lap welded joints of light-weight Mg-Li/Mg-Al-Zn alloys [J]. Weld. World, 2022, 66: 1775
[26] Prangnell P B, Heason C P. Grain structure formation during friction stir welding observed by the ‘stop action technique’ [J]. Acta Mater., 2005, 53: 3179
[27] Shi L. Numerical analysis of thermal process and plastic material flow in ultrasonic vibration enhanced friction stir welding [D]. Jinan: Shandong University, 2016
  石 磊. 超声振动强化搅拌摩擦焊接热过程及材料流动的数值分析 [D]. 济南: 山东大学, 2016
[28] Shi L, Wu C S, Gao S, et al. Modified constitutive equation for use in modeling the ultrasonic vibration enhanced friction stir welding process [J]. Scr. Mater., 2016, 119: 21
[29] Zhai M. Numerical simulation and experimental investigation of Al-to-Mg FSLW/UVeFSLW process [D]. Jinan: Shandong University, 2023
  翟 明. 铝/镁异质合金FSLW/UVeFSLW焊接过程的数值模拟与实验研究 [D]. 济南: 山东大学, 2023
Outlines

/