Review of the Formation Mechanism and Control Technology for Freckle Defects in Directionally Solidified Superalloys
Received date: 2025-04-14
Revised date: 2025-07-23
Online published: 2025-10-15
Supported by
National Key Research and Development Program of China(2024YFB3713805);Basic Research Program(JCKY-C102)
Freckles severely degrade the crystalline integrity and high-temperature mechanical properties of superalloy blades, posing a critical barrier to the fabrication of large-sized directionally solidified blades for heavy-duty gas turbines. This paper reviews the research progress on freckles over the past several decades, both domestically and internationally. It summarizes investigations of elemental segregation, thermo-solutal convection, and dendrite arm fragmentation during freckle formation using techniques such as atom probe tomography, synchrotron radiation, and numerical simulation. Freckle formation criteria based on temperature fields or mushy-zone density have been described, and the influences of blade geometry and solidification parameters on freckle distribution have been elucidated. Moreover, freckle control techniques and methods are comprehensively reviewed. At present, most studies on freckles focus on cases involving “small-sized specimens, low withdrawal rates (≤ 1.5 mm/min), and alloys with high W/Re contents”, which exhibit relatively significant differences from the freckle solidification conditions and occurrence patterns of “large blades, high withdrawal rates (≥ 2.0 mm/min), and alloys with low W/Re content” in the engineering practice of heavy-duty gas turbines. Therefore, developing rapid freckle prediction methods and effective control technologies specifically suited to the solidification conditions of large blades in heavy-duty gas turbines has become a critical need and a key research direction for the present and future.
JIA Yuliang , ZHANG Yongjia , SHI Zekai , SHEN Xu , YIN Yajun , SHI Changkun , ZHOU Jianxin , LYU Zhigang . Review of the Formation Mechanism and Control Technology for Freckle Defects in Directionally Solidified Superalloys[J]. Acta Metall Sin, 2026 , 62(2) : 309 -327 . DOI: 10.11900/0412.1961.2025.00109
| [1] | Broomfield R W, Ford D A, Bhangu J K, et al. Development and turbine engine performance of three advanced rhenium containing superalloys for single crystal and directionally solidified blades and vanes [J]. J. Eng. Gas. Turbines Power, 1998, 120: 595 |
| [2] | Reed R C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 1 |
| [3] | Pollock T M, Argon A S. Creep resistance of CMSX-3 nickel base superalloy single crystals [J]. Acta Metall. Mater., 1992, 40: 1 |
| [4] | Versnyder F I, Shank M E. The development of columnar grain and single crystal high temperature materials through directional solidification [J]. Mater. Sci. Eng., 1970, 6: 213 |
| [5] | Quested P N, Osgerby S. Mechanical properties of conventionally cast, directionally solidified, and single-crystal superalloys [J]. Mater. Sci. Technol., 1986, 2: 461 |
| [6] | Szeliga D, Kubiak K, Sieniawski J. Control of liquidus isotherm shape during solidification of Ni-based superalloy of single crystal platforms [J]. J. Mater. Process. Technol., 2016, 234: 18 |
| [7] | Mathur H N, Panwisawas C, Jones C N, et al. Nucleation of recrystallisation in castings of single crystal Ni-based superalloys [J]. Acta Mater., 2017, 129: 112 |
| [8] | Tin S, Pollock T M, Murphy W. Stabilization of thermosolutal convective instabilities in Ni-based single-crystal superalloys: Carbon additions and freckle formation [J]. Metall. Mater. Trans., 2001, 32A: 1743 |
| [9] | Giamei A F, Kear B H. On the nature of freckles in nickel base superalloys [J]. Metall. Trans., 1970, 1: 2185 |
| [10] | Pollock T M, Murphy W H. The breakdown of single-crystal solidification in high refractory nickel-base alloys [J]. Metall. Mater. Trans., 1996, 27A: 1081 |
| [11] | Copley S M, Giamei A F, Johnson S M, et al. The origin of freckles in unidirectionally solidified castings [J]. Metall. Trans., 1970, 1: 2193 |
| [12] | Amouyal Y, Seidman D N. An atom-probe tomographic study of freckle formation in a nickel-based superalloy [J]. Acta Mater., 2011, 59: 6729 |
| [13] | Reinhart G, Grange D, Abou-Khalil L, et al. Impact of solute flow during directional solidification of a Ni-based alloy: In-situ and real-time X-radiography [J]. Acta Mater., 2020, 194: 68 |
| [14] | Felicelli S D, Heinrich J C, Poirier D R. Three-dimensional simulations of freckles in binary alloys [J]. J. Cryst. Growth, 1998, 191: 879 |
| [15] | Pollock T M, Murphy W H, Goldman E H, et al. Grain defect formation during directional solidification of nickel base single crystals [A]. Superalloys 1992 [C]. Pennsylvania: TMS, 1992: 125 |
| [16] | Wang S, Jia Y L, Wang Y Z, et al. New vision of convection induced freckle formation theory in nickel-based superalloys by electron microscopy [J]. Microstructures, 2024, 4: 2024006 |
| [17] | Tin S, Pollock T M, King W T. Carbon additions and grain defect formation in high refractory nickel-base single crystal superalloys [A]. Proceedings of the 9th International Symposium on Superalloys [C]. Pennsylvania: TMS, 2000: 201 |
| [18] | Hobbs R A, Tin S, Rae C M F. A castability model based on elemental solid-liquid partitioning in advanced nickel-base single-crystal superalloys [J]. Metall. Mater. Trans., 2005, 36A: 2761 |
| [19] | Amouyal Y, Seidman D N. The role of hafnium in the formation of misoriented defects in Ni-based superalloys: An atom-probe tomographic study [J]. Acta Mater., 2011, 59: 3321 |
| [20] | Bao C J, Li Z F, Liu F, et al. Modeling of constituent-based freckle predictor for nickel-base superalloys [J]. Chin. J. Nonferrous Met., 2019, 29: 998 |
| 包超君, 李振锋, 刘 锋 等. 一种基于镍基高温合金成分的雀斑预测模型 [J]. 中国有色金属学报, 2019, 29: 998 | |
| [21] | Sarazin J R, Hellawell A. Channel formation in Pb-Sn, Pb-Sb, and Pb-Sn-Sb alloy ingots and comparison with the system NH4Cl-H2O [J]. Metall. Trans., 1988, 19A: 1861 |
| [22] | Shevchenko N, Boden S, Eckert S, et al. Observation of segregation freckle formation under the influence of melt convection [J]. IOP Conf. Ser.: Mater. Sci. Eng., 2012, 27: 012085 |
| [23] | Schneider M C, Gu J P, Beckermann C, et al. Modeling of micro- and macrosegregation and freckle formation in single-crystal nickel-base superalloy directional solidification [J]. Metall. Mater. Trans., 1997, 28A: 1517 |
| [24] | Saad A, Gandin C A, Bellet M, et al. Simulation of channel segregation during directional solidification of In-75 wt pct Ga. qualitative comparison with in situ observations [J]. Metall. Mater. Trans., 2015, 46A: 4886 |
| [25] | Felicelli S D. Simulation of freckles during vertical solidification of binary alloys [D]. Arizona: The University of Arizona, 1991 |
| [26] | Frueh C, Poirier D R, Felicelli S D. Predicting freckle-defects in directionally solidified Pb-Sn alloys [J]. Mater. Sci. Eng., 2002, A328: 245 |
| [27] | Gu J P, Beckermann C, Giamei A F. Motion and remelting of dendrite fragments during directional solidification of a nickel-base superalloy [J]. Metall. Mater. Trans., 1997, 28A: 1533 |
| [28] | Ren N, Li J, Panwisawas C, et al. Thermal-solutal-fluid flow of channel segregation during directional solidification of single-crystal nickel-based superalloys [J]. Acta Mater., 2021, 206: 116620 |
| [29] | Ren N, Li J, Panwisawas C, et al. Insight into the sensitivities of freckles in the directional solidification of single-crystal turbine blades [J]. J. Manuf. Processes, 2022, 77: 219 |
| [30] | Zhang H J, Liu X S, Ma D X, et al. Digital twin for directional solidification of a single-crystal turbine blade [J]. Acta Mater., 2023, 244: 118579 |
| [31] | Wu M, Ludwig A. Using a three-phase deterministic model for the columnar-to-equiaxed transition [J]. Metall. Mater. Trans., 2007, 38A: 1465 |
| [32] | Zhang H J, Zhao Y X, Xiong W, et al. Modelling freckles and spurious grain formation in directionally solidified superalloy castings [J]. Commun. Mater., 2024, 5: 232 |
| [33] | Liu Y, Wang F, Ma D X, et al. Freckle prediction model incorporating geometrical effects for Ni-based single-crystal superalloy components [J]. Acta Mater., 2024, 266: 119702 |
| [34] | Yuan L, Lee P D. A new mechanism for freckle initiation based on microstructural level simulation [J]. Acta Mater., 2012, 60: 4917 |
| [35] | Kao A, Shevchenko N, Alexandrakis M, et al. Thermal dependence of large-scale freckle defect formation [J]. Philos. Trans. Roy. Soc., 2019, 377A: 20180206 |
| [36] | Karagadde S, Yuan L, Shevchenko N, et al. 3-D microstructural model of freckle formation validated using in situ experiments [J]. Acta Mater., 2014, 79: 168 |
| [37] | Takaki T, Rojas R, Sakane S, et al. Phase-field-lattice Boltzmann studies for dendritic growth with natural convection [J]. J. Cryst. Growth, 2017, 474: 146 |
| [38] | Ohno M, Takaki T, Shibuta Y. Numerical testing of quantitative phase-field models with different polynomials for isothermal solidification in binary alloys [J]. J. Comput. Phys., 2017, 335: 621 |
| [39] | Rojas R, Takaki T, Ohno M. A phase-field-lattice Boltzmann method for modeling motion and growth of a dendrite for binary alloy solidification in the presence of melt convection [J]. J. Comput. Phys., 2015, 298: 29 |
| [40] | Sakane S, Takaki T, Ohno M, et al. Acceleration of phase-field lattice Boltzmann simulation of dendrite growth with thermosolutal convection by the multi-GPUs parallel computation with multiple mesh and time step method [J]. Modell. Simul. Mater. Sci. Eng., 2019, 27: 054004 |
| [41] | Takaki T, Sakane S, Ohno M, et al. Large-scale phase-field lattice Boltzmann study on the effects of natural convection on dendrite morphology formed during directional solidification of a binary alloy [J]. Comput. Mater. Sci., 2020, 171: 109209 |
| [42] | Watanabe S, Aoki T. Large-scale flow simulations using lattice Boltzmann method with AMR following free-surface on multiple GPUs [J]. Comput. Phys. Commun., 2021, 264: 107871 |
| [43] | Sakane S, Aoki T, Takaki T. Parallel GPU-accelerated adaptive mesh refinement on two-dimensional phase-field lattice Boltzmann simulation of dendrite growth [J]. Comput. Mater. Sci., 2022, 211: 111507 |
| [44] | Guo Z, Mi J, Grant P S. An implicit parallel multigrid computing scheme to solve coupled thermal-solute phase-field equations for dendrite evolution [J]. J. Comput. Phys., 2012, 231: 1781 |
| [45] | Guo Z, Mi J, Xiong S, et al. Phase field study of the tip operating state of a freely growing dendrite against convection using a novel parallel multigrid approach [J]. J. Comput. Phys., 2014, 257: 278 |
| [46] | Yang C, Xu Q Y, Liu B C. Study of dendrite growth with natural convection in superalloy directional solidification via a multiphase-field-lattice Boltzmann model [J]. Comput. Mater. Sci., 2019, 158: 130 |
| [47] | Steinbach I, Pezzolla F, Nestler B, et al. A phase field concept for multiphase systems [J]. Physica, 1996, 94D: 135 |
| [48] | Eiken J, B?ttger B, Steinbach I. Multiphase-field approach for multicomponent alloys with extrapolation scheme for numerical application [J]. Phys. Rev., 2006, 73E: 066122 |
| [49] | Yang C, Xu Q Y, Liu B C. A high precision extrapolation method in multiphase-field model for simulating dendrite growth [J]. J. Cryst. Growth, 2018, 490: 25 |
| [50] | Yasuda H, Yamamoto Y, Nakatsuka N, et al. In situ observation of nucleation, fragmentation and microstructure evolution in Sn-Bi and Al-Cu alloys [J]. Int. J. Cast Met. Res., 2008, 21: 125 |
| [51] | Ruvalcaba D, Mathiesen R H, Eskin D G, et al. In situ observations of dendritic fragmentation due to local solute-enrichment during directional solidification of an aluminum alloy [J]. Acta Mater., 2007, 55: 4287 |
| [52] | Shevchenko N, Boden S, Gerbeth G, et al. Chimney formation in solidifying Ga-25wt pct in alloys under the influence of thermosolutal melt convection [J]. Metall. Mater. Trans., 2013, 44A: 3797 |
| [53] | Soar P, Kao A, Djambazov G, et al. The integration of structural mechanics into microstructure solidification modelling [J]. IOP Conf. Ser.: Mater. Sci. Eng., 2020, 861: 012054 |
| [54] | Ren N, Panwisawas C, Li J, et al. Solute enrichment induced dendritic fragmentation in directional solidification of nickel-based superalloys [J]. Acta Mater., 2021, 215: 117043 |
| [55] | Rutter J W, Chalmers B. A Prismatic substructure formed during the solidification of metals [J]. Canadian Journal of Physics. 1952, 3: 15 |
| [56] | Schadt R, Wagner I, Preuhs J, et al. New aspects of freckle formation during single crystal solidification of CMSX-4 [A]. Superalloys 2000 [C]. Pennsylvania: TMS, 2000: 211 |
| [57] | Li Q D, Shen J, Xiong Y L, et al. Prediction of freckle formation in directionally solidified CMSX-4 superalloy [J]. Mater. Lett., 2018, 228: 281 |
| [58] | Ma D X, Wu Q, Bührig-Polaczek A. Some new observations on freckle formation in directionally solidified superalloy components [J]. Metall. Mater. Trans., 2012, 43B: 344 |
| [59] | Han D Y, Jiang W G, Xiao J H, et al. Investigation on freckle formation and evolution of single-crystal nickel-based superalloy specimens with different thicknesses and abrupt cross-section changes [J]. J. Alloys Compd., 2019, 805: 218 |
| [60] | Wu H Z, Xuan W D, Zhang X Y, et al. Investigation of mechanism for formation of freckle during directional solidification of Ni base single crystal superalloy [J]. Hot Work. Technol., 2025, 54(3): 120 |
| 吴怀洲, 玄伟东, 张翔宇 等. 镍基单晶高温合金定向凝固雀斑形成机理研究 [J]. 热加工工艺, 2025, 54(3): 120 | |
| [61] | Tin S, Pollock T M. Predicting freckle formation in single crystal Ni-base superalloys [J]. J. Mater. Sci., 2004, 39: 7199 |
| [62] | Worster M G. Instabilities of the liquid and mushy regions during solidification of alloys [J]. J. Fluid Mech., 1992, 237: 649 |
| [63] | Beckermann C, Gu J P, Boettinger W J. Development of a freckle predictor via Rayleigh number method for single-crystal nickel-base superalloy castings [J]. Metall. Mater. Trans., 2000, 31A: 2545 |
| [64] | Madison J, Spowart J E, Rowenhorst D J, et al. Fluid flow and defect formation in the three-dimensional dendritic structure of nickel-based single crystals [J]. Metall. Mater. Trans., 2012, 43A: 369 |
| [65] | Hong J P, Ma D X, Wang J, et al. Freckle defect formation near the casting interfaces of directionally solidified superalloys [J]. Materials, 2016, 9: 929 |
| [66] | Ma D X. Freckle formation during directional solidification of complex castings of superalloys [J]. Acta Metall. Sin., 2016, 52: 426 |
| 马德新. 定向凝固的复杂形状高温合金铸件中的雀斑形成 [J]. 金属学报, 2016, 52: 426 | |
| [67] | Monde A D, Shrivastava A, Jakhar A, et al. Binary alloy solidification and freckle formation: effect of shrinkage induced flow on solutal instability and macro-segregation [J]. Phys. Fluids, 2021, 33: 037108 |
| [68] | Zhang H J, Wu M H, Tewari S N, et al. Geometrical effect on macrosegregation formation during unidirectional solidification of Al-Si alloy [J]. J. Mater. Process. Technol., 2021, 288: 116913 |
| [69] | Ma D X, Bührig-Polaczek A. The influence of surface roughness on freckle formation in directionally solidified superalloy samples [J]. Metall. Mater. Trans., 2012, 43B: 671 |
| [70] | Zhang Y J, Jia Y L, Zhou J X, et al. Effect of withdrawal rate on freckle formation of large-size directional solidified nickel-based superalloy blades [J]. J. Mater. Res. Technol., 2024, 30: 1518 |
| [71] | Qin L, Shen J, Yang G X, et al. A design of non-uniform thickness mould for controlling temperature gradient and S/L interface shape in directionally solidified superalloy blade [J]. Mater. Des., 2017, 116: 565 |
| [72] | Ren Y. Numerical simulation of freckle defects in nickel-based superalloys [D]. Harbin: Harbin University of Science and Technology, 2019 |
| 任 莹. 镍基高温合金雀斑缺陷数值模拟研究 [D]. 哈尔滨理工大学, 2019 | |
| [73] | Qin L, Shen J, Li Q D, et al. Effects of convection patterns on freckle formation of directionally solidified nickel-based superalloy casting with abruptly varying cross-sections [J]. J. Cryst. Growth, 2017, 466: 45 |
| [74] | Zhang J, Lou L H, Li H. Material and processing technology of directionally solidified blade in heavy duty industrial gas turbines [J]. Mater. China, 2013, 32(1): 12 |
| 张 健, 楼琅洪, 李 辉. 重型燃气轮机定向结晶叶片的材料与制造工艺 [J]. 中国材料进展, 2013, 32(1): 12 | |
| [75] | Elliott A J, Pollock T M, Tin S, et al. Directional solidification of large superalloy castings with radiation and liquid-metal cooling: A comparative assessment [J]. Metall. Mater. Trans., 2004, 35A: 3221 |
| [76] | Song J S, Wang F, Jia S, et al. Liquid metal cooling furnace for large-sized single crystal blades [J]. Vacuum. 2025, 62(01): 67 |
| 宋静思, 王 富, 贾 石 等. 用于大尺寸叶片的液态金属冷却单晶炉 [J]. 真空. 2025, 62(01): 67 | |
| [77] | Wang Z C, Li J R, Liu S Z, et al. Effects of shell mold heating temperature on microstructures and freckle formation of single crystal superalloys [J]. Trans. Nonferrous Met. Soc. China, 2024, 34: 1191 |
| [78] | Li Q D, Shen J, Qin L, et al. Investigation on local cooling in reducing freckles for directionally solidified superalloy specimens with abruptly varying cross-sections [J]. Mater. Charact., 2017, 130: 139 |
| [79] | Wang F, Ma D X, Zhang J, et al. Investigation of segregation and density profiles in the mushy zone of CMSX-4 superalloys solidified during downward and upward directional solidification processes [J]. J. Alloys Compd., 2015, 620: 24 |
| [80] | Li Z F, Hu B, Zhong W H, et al. Study on formation mechanism of casting defects in directionally solidified blades of DZ22B superalloy [J]. Aeron. Manuf. Technol., 2020, 63(16): 45 |
| 李振锋, 胡 兵, 钟文惠 等. DZ22B高温合金定向凝固叶片铸造缺陷的形成机理研究 [J]. 航空制造技术, 2020, 63(16): 45 | |
| [81] | Li Q D, Shen J, Qin L, et al. Effect of traveling magnetic field on freckle formation in directionally solidified CMSX-4 superalloy [J]. J. Mater. Process. Technol., 2019, 274: 116308 |
| [82] | Zhang Y J, Zhou J X, Yin Y J, et al. Numerical simulation of dendrite growth and solute convection during directional solidification of superalloy [J]. J. Netshape Forming Eng., 2023, 15(10): 13 |
| 张勇佳, 周建新, 殷亚军 等. 高温合金定向凝固过程中枝晶生长与溶质对流数值模拟 [J]. 精密成形工程, 2023, 15(10): 13 | |
| [83] | Richter A R, Scholz F, Eggeler G, et al. Microstructure informatics: using computer vision for the characterization of dendrite growth phenomena in Ni-base single crystal Superalloys [J]. Mater. Charact., 2025, 223: 114878 |
| [84] | Kavousi S, Asle Zaeem M. Integration of multiscale simulations and machine learning for predicting dendritic microstructures in solidification of alloys [J]. Acta Mater., 2025, 289: 120860 |
/
| 〈 |
|
〉 |