Research paper

Nanoscale Carbide Precipitates and Residual Stress Evolution in Cryogenically Treated M50 Aeroengine Bearing Steel Investigated Using Advanced Neutron Methods

  • CAO Yanfei ,
  • ZHANG Xiao ,
  • LIU Hongwei ,
  • WANG Leitao ,
  • KE Yubin ,
  • HE Lunhua ,
  • XIE Zhenhua ,
  • WANG Pei ,
  • LI Dianzhong
Expand
  • 1.Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2.Spallation Neutron Source Science Center, Dongguan 523803, China
    3.Institute of High Energy Physics, Chinese Academy of Sciences, Beijing 100049, China
WANG Pei, professor, Tel: (024)83970106, E-mail: pwang@imr.ac.cn;
LI Dianzhong, professor, Tel: (024)83970106, E-mail: dzli@imr.ac.cn

Received date: 2024-08-27

  Revised date: 2025-03-12

  Online published: 2025-10-10

Supported by

National Natural Science Foundation of China(52031013);National Natural Science Foundation of China(52321001);National Natural Science Foundation of China(52201150)

Abstract

Aeroengine bearings, often referred to as the “joints” of the critical aeroengine components, are essential to engine performance, operating under extreme conditions of high temperatures, rapid rotation, and heavy mechanical loads. M50 high-carbon, high-alloy steel, renowned for its exceptional high-temperature stability, hardness, wear resistance, and fatigue resistance, has long been the material of choice for aerospace bearings. Although advances in purification, homogenization, and grain refinement have improved the fatigue life of M50 steel, challenges remain. Notably, microstructural heterogeneities within the matrix, such as coarse carbides, can act as crack initiators under cyclic loading, highlighting the need for advanced microstructural control strategies. This study systematically investigates the evolution of nanoscale carbides in M50 bearing steel during a novel treatment process combining quenching, direct cryogenic treatment, and subsequent tempering, as well as the evolution of residual stress under service conditions. The analyses employed the following methods: small angle neutron scattering and general purpose powder diffraction at the China Spallation Neutron Source, complemented by aberration-corrected high-resolution transmission electron microscopy and residual stress profiling using the contour method. The results demonstrate that elliptical and rod-shaped nanoscale carbides are predominant in the cryogenically treated M50 steel. After tempering, the density of rod-shaped nanoscale carbides increases while the average size decreases, enhancing secondary hardening through the strengthening of carbide dispersion. Remarkably, atomically thin lamellar carbides, with a face-centered cubic structure and bulk enrichment in elements C, Cr, Mo, and V, were identified as precursors to geometrically anisotropic carbides. This novel treatment promotes finer, more uniformly distributed nanoscale carbides comparing to the typical tempering after cryogenically treated microstructure, synergistically improving fatigue strength and hardness while ensuring uniform residual stress distribution in bearing rings. The residual stresses in aeroengine bearing rings under precision and fine grinding conditions are comparable and remain at low levels. Under various service conditions, comparisons between domestically developed and imported bearing rings reveal that after service, transverse residual stress shifts from compressive to tensile, with domestically developed bearings exhibiting residual stress states similar to imported bearings.

Cite this article

CAO Yanfei , ZHANG Xiao , LIU Hongwei , WANG Leitao , KE Yubin , HE Lunhua , XIE Zhenhua , WANG Pei , LI Dianzhong . Nanoscale Carbide Precipitates and Residual Stress Evolution in Cryogenically Treated M50 Aeroengine Bearing Steel Investigated Using Advanced Neutron Methods[J]. Acta Metall Sin, 2026 , 62(3) : 467 -476 . DOI: 10.11900/0412.1961.2024.00300

References

[1] Bhadeshia H K D H. Steels for bearings [J]. Prog. Mater. Sci., 2012, 57: 268
[2] Jelita Rydel J, Toda-Caraballo I, Guetard G, et al. Understanding the factors controlling rolling contact fatigue damage in VIM-VAR M50 steel [J]. Int. J. Fatigue, 2018, 108: 68
[3] Torkamani H, Raygan S, Garcia Mateo C, et al. Contributions of rare earth element (La, Ce) addition to the impact toughness of low carbon cast niobium microalloyed steels [J]. Met. Mater. Int., 2018, 24: 773
[4] Yang C Y, Luan Y K, Li D Z, et al. Very high cycle fatigue behavior of bearing steel with rare earth addition [J]. Int. J. Fatigue, 2020, 131: 105263
[5] Liu H H, Ma H, Du N Y, et al. Probing rare earth segregation in steels [J]. Scr. Mater., 2023, 230: 115407
[6] Cao Y F, Miao Y Y, Li D Z, et al. On the mechanism of steel homogenization via rare earth addition: Experimental characterization and numerical simulation [J]. Metall. Mater. Trans., 2022, 53B: 1858
[7] Guan J, Liu D R, Cao Y F, et al. Macro and micro segregations and prediction of carbide equivalent size in vacuum arc remelting of M50 steel via simulations and experiments [J]. Metall. Mater. Trans., 2024, 55A: 1081
[8] Liu H H, Fu P X, Sun C, et al. Primary carbide refinement in AISI M50 steel by dislocation engineering via pre-deformation treatment [J]. Metall. Mater. Trans., 2023, 54A: 783
[9] Du N Y, Liu H H, Cao Y F, et al. In situ investigation of the fracture of primary carbides and its mechanism in M50 steel [J]. Mater. Charact., 2022, 186: 111822
[10] Liu W F, Guo Y F, Cao Y F, et al. Transformation behavior of primary MC and M2C carbides in Cr4Mo4V steel [J]. J. Alloys Compd., 2021, 889: 161755
[11] Yang L Q, Xue W H, Gao S Y, et al. Effects of primary carbide size and type on the sliding wear and rolling contact fatigue properties of M50 bearing steel [J]. Acta Metall. Sin. (Engl. Lett.), 2023, 36: 1336
[12] Fu H W, Wang W J, Lu Y Y, et al. The origin of microstructural alterations in M50 bearing steel undergoing rolling contact fatigue [J]. Int. J. Fatigue, 2023, 175: 107807
[13] Harish S, Bensely A, Lal D M, et al. Microstructural study of cryogenically treated En 31 bearing steel [J]. J. Mater. Process. Technol., 2009, 209: 3351
[14] Gunes I, Cicek A, Aslantas K, et al. Effect of deep cryogenic treatment on wear resistance of AISI 52100 bearing steel [J]. Trans. Indian Inst. Met., 2014, 67: 909
[15] Sonar T, Lomte S, Gogte C. Cryogenic treatment of metal—A review [J]. Mater. Today: Proc., 2018, 5: 25219
[16] Cajner F, Leskov?ek V, Landek D, et al. Effect of deep-cryogenic treatment on high speed steel properties [J]. Mater. Manuf. Processes, 2009, 24: 743
[17] Mazor G, Ladizhensky I, Shapiro A. Influence of cryogenic cooling rate on mechanical properties of tool steels [J]. IOP Conf. Ser.: Mater. Sci. Eng., 2017, 244: 012005
[18] Singh L P, Singh J. Effects of cryogenic treatment on the cutting tool durability [J]. Int. J. Des. Manuf. Technol., 2012, 3: 11
[19] Akhbarizadeh A, Shafyei A, Golozar M A. Effects of cryogenic treatment on wear behavior of D6 tool steel [J]. Mater. Des., 2009, 30: 3259
[20] ?zbek N A, ?i?ek A, Gülesin M, et al. Investigation of the effects of cryogenic treatment applied at different holding times to cemented carbide inserts on tool wear [J]. Int. J. Mach. Tools Manuf., 2014, 86: 34
[21] Das D, Ray K K, Dutta A K. Influence of temperature of sub-zero treatments on the wear behaviour of die steel [J]. Wear, 2009, 267: 1361
[22] Gavriljuk V G, Theisen W, Sirosh V V, et al. Low-temperature martensitic transformation in tool steels in relation to their deep cryogenic treatment [J]. Acta Mater., 2013, 61: 1705
[23] Sri Siva R, Mohan Lal D, Kesavan Nair P, et al. Influence of cryogenic treatment on the wear characteristics of 100Cr6 bearing steel [J]. Int. J. Miner., Metall., Mater., 2014, 21: 46
[24] Weng Z J, Gu K X, Zheng J P, et al. Cryogenically martensitic transformation and its effects on tempering behaviors of bearing steel [J]. Mater. Charact., 2022, 190: 112066
[25] Cai X, Hu X Q, Lu X Y, et al. Exploring the ultrahigh rolling contact fatigue life of M50 bearing steel by adjusting the cryogenic sequence [J]. J. Mater. Sci. Technol., 2024, 169: 243
[26] Ke Y B, Li B, Duan H P. Morphology and chemical composition of nanoprecipitate in AerMet100 steel by separation of the nuclear and magnetic small-angle neutron scattering data [J]. Acta Metall Sin, 2024, 60: 1109
  柯于斌, 李 彬, 段辉平. 利用小角中子核磁散射分离研究AerMet100钢中纳米析出相的形貌和成分 [J]. 金属学报, 2024, 60: 1109
[27] He L H, Chen J, Lu H L, et al. First experimental results from the GPPD diffractometer at the CSNS [J]. Neutron News, 2018, 29: 7
[28] Brown D W, Bernardin J D, Carpenter J S, et al. Neutron diffraction measurements of residual stress in additively manufactured stainless steel [J]. Mater. Sci. Eng., 2016, A678: 291
[29] Zhou L N, Tang G Z, Ma X X, et al. Relationship between microstructure and mechanical properties of M50 ultra-high strength steel via quenching-partitioning-tempering process [J]. Mater. Charact., 2018, 146: 258
Outlines

/