Research paper

Molecular Dynamics Simulations of Tensile Deformation of Cu/Ta Nano-Bilayer Films and the Effect of Al and W Atoms Doping on the Deformation

  • SHI Tenglong ,
  • CHEN Juan ,
  • ZHAO Bin ,
  • SHI Junqin
Expand
  • 1 Center of Advanced Lubrication and Seal Materials, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi'an 710072, China
    2 School of Materials Science and Engineering, Taiyuan University of Science and Technology, Taiyuan 030024, China
    3 Xi'an Surface Material Protection Co. Ltd., Xi'an 710200, China
SHI Junqin, associate professor, Tel: (029)88460311, E-mail: junqin.shi@nwpu.edu.cn

Received date: 2024-09-11

  Revised date: 2025-03-10

  Online published: 2025-09-17

Supported by

National Science and Technology Major Project(2025ZD0618600);Science and Technology Plan Project of Xi'an(24ZDCYJSGG0050)

Abstract

Nano-multilayers composed of immiscible metals have been widely investigated over the past decades due to their exceptional microstructural stability. The Cu/Ta system, which is also immiscible, is particularly notable because Ta offers higher melting point, strength, and superior wear and corrosion resistance compared to metals like Nb. Cu/Ta nano-bilayer films are extensively used in the electronics industry for semiconductors, microelectronic devices, optical systems, and magnetic applications. However, the presence of interfaces and the distinct deformation responses of the Cu and Ta layers during processing, fabrication, and service conditions make mechanical deformation and subsequent failure inevitable, potentially compromising the performance of microscale devices. Therefore, understanding the deformation mechanisms and enhancing the mechanical strength of Cu/Ta nano-bilayer films at the microscopic scale is essential. In this study, molecular dynamics simulations were employed to investigate the tensile behavior and deformation mechanisms of Cu/Ta nano-bilayer films. In addition, the effects of Al and W doping in the Cu layer on the deformation behavior were analyzed. The results indicate that tensile loading direction significantly influences the plastic deformation mode. When the bilayer films were stretched parallel to the interface, both Cu and Ta layers exhibited sequential plastic deformation. In contrast, when the loading was applied perpendicular to the interface, only the Cu layer deformed plastically, while the Ta layer remained elastically constrained throughout. Doping with Al or W atoms enhanced the overall hardness and yield strength of the nano-bilayer films. Furthermore, W doping induced stacking faults in both loading directions when stretched parallel to the interface, and a martensitic transformation from fcc to bcc structure occurred in the Cu layer under perpendicular tension.

Cite this article

SHI Tenglong , CHEN Juan , ZHAO Bin , SHI Junqin . Molecular Dynamics Simulations of Tensile Deformation of Cu/Ta Nano-Bilayer Films and the Effect of Al and W Atoms Doping on the Deformation[J]. Acta Metall Sin, 2026 , 62(7) : 1297 -1309 . DOI: 10.11900/0412.1961.2024.00322

References

[1] Chen H B. Fabrication and property of Ta-based diffusion barrier for Cu interconnection in new generation IC [D]. Changsha: Central South University, 2007
  陈海波. 新一代集成电路Cu互连用Ta基扩散阻挡层的制备及特性研究 [D]. 长沙: 中南大学, 2007
[2] Holloway K, Fryer P M, Cabral Jr C, et al. Tantalum as a diffusion barrier between copper and silicon: Failure mechanism and effect of nitrogen additions [J]. J. Appl. Phys., 1992, 71: 5433
[3] Fullwood D T, Niezgoda S R, Adams B L, et al. Microstructure sensitive design for performance optimization [J]. Prog. Mater. Sci., 2010, 55: 477
[4] Mondal S, Polley D, Pattabi A, et al. Single-shot switching in Tb/Co-multilayer based nanoscale magnetic tunnel junctions [J]. J. Magn. Magn. Mater., 2023, 581: 170960
[5] Sakhonenkov S S, Filatova E O. Nanoscale W/Be multilayers: Intermixing during magnetron sputtering deposition and effect of heat treatment [J]. Appl. Surf. Sci., 2022, 571: 151265
[6] Tran A S, Fang T H. Dislocation interaction and fracture of Cu/Ta bilayer interfaces [J]. Phys. Scr., 2019, 94: 095402
[7] Feng X T, Lin Z J, Xin K, et al. The deformation mechanisms and mechanical properties of Cu/Fe multilayer during compression process [J]. J. Mater. Res., 2021, 36: 3203
[8] Zhang R F, Wang J, Beyerlein I J, et al. Dislocation nucleation mechanisms from fcc/bcc incoherent interfaces [J]. Scr. Mater., 2011, 65: 1022
[9] Chen Y, Li N, Hoagland R G, et al. Effects of three-dimensional Cu/Nb interfaces on strengthening and shear banding in nanoscale metallic multilayers [J]. Acta Mater., 2020, 199: 593
[10] Wang Y, Zhu X Y, Liu G M, et al. Strain rate sensitivity of Cu/Ni and Cu/Nb nanoscale multilayers [J]. Acta Metall. Sin., 2017, 53: 183
  王 尧, 朱晓莹, 刘贵民 等. Cu/Ni和Cu/Nb纳米多层膜的应变率敏感性 [J]. 金属学报, 2017, 53: 183
[11] Zhang R F, Wang J, Beyerlein I J, et al. Atomic-scale study of nucleation of dislocations from fcc-bcc interfaces [J]. Acta Mater., 2012, 60: 2855
[12] Lu L, Huang C, Pi W L, et al. Molecular dynamics simulation of effects of interface imperfections and modulation periods on Cu/Ta multilayers [J]. Comp. Mater. Sci., 2018, 143: 63
[13] Shi T L, Xu L L, Chen J, et al. Influence of grain boundary and twin boundary on the stretching deformation behaviors of Cu/Ta interface material [J]. Mater. Today Commun., 2024, 39: 108633
[14] Tu A D, Teng C Y, Wang H, et al. Molecular dynamics simulation of the structure and deformation behavior of γ/α2 interface in TiAl alloys [J]. Acta Metall. Sin., 2019, 55: 291
  涂爱东, 滕春禹, 王 皞 等. Ti-Al合金γ/α2界面结构及拉伸变形行为的分子动力学模拟 [J]. 金属学报, 2019, 55: 291
[15] Karimzadeh A, Rouhaghdam A S, Aliofkhazraei M, et al. Sliding wear behavior of Ni-Co-P multilayer coatings electrodeposited by pulse reverse method [J]. Tribol. Int., 2020, 141: 105914
[16] Major L, Lackner J M, Kot M, et al. Nanostructural aspects of the wear process of multilayer tribological coatings [J]. Tribol. Int., 2020, 151: 106411
[17] Shi J Q, Li L L, Wang J Y, et al. Alloy strengthening toward improving mechanical and tribological performances of Cu x Ni100 - x /Ta nano multilayer materials [J]. Tribol. Int., 2023, 190: 109039
[18] Bai Z W, Ding Z G, Zhou A L, et al. Molecular dynamics simulation of thermo-kinetics of tensile deformation of α-Fe single crystal [J]. Acta Metall. Sin., 2024, 60: 848
  柏智文, 丁志刚, 周爱龙 等. α-Fe单晶拉伸变形热-动力学的分子动力学模拟 [J]. 金属学报, 2024, 60: 848
[19] Zhang J Y, Qu Q M, Wang Y Q, et al. Research progress on irradiation effects and mechanical properties of metal/high-entropy alloy nanostructured multilayers [J]. Acta Metall. Sin., 2022, 58: 1371
  张金钰, 屈启蒙, 王亚强 等. 金属/高熵合金纳米多层膜的力学性能及其辐照效应研究进展 [J]. 金属学报, 2022, 58: 1371
[20] Abraham F F. Computational statistical mechanics methodology, applications and supercomputing [J]. Adv. Phys., 1986, 35: 1
[21] Stukowski A. Structure identification methods for atomistic simulations of crystalline materials [J]. Modell. Simul. Mater. Sci. Eng., 2012, 20: 045021
[22] Choudhuri D, Srinivasan S G, Mishra R S. Deformation of lamellar FCC-B2 nanostructures containing Kurdjumov-Sachs interfaces: Relation between interfacial structure and plasticity [J]. Int. J. Plast., 2020, 125: 191
[23] Zhou Q, Ren Y, Du Y, et al. Cracking and toughening mechanisms in nanoscale metallic multilayer films: A brief review [J]. Appl. Sci., 2018, 8: 1821
[24] Mendelev M I, Han S, Srolovitz D J, et al. Development of new interatomic potentials appropriate for crystalline and liquid iron [J]. Philos. Mag., 2003, 83: 3977
[25] Wei M Z, Cao Z H, Shi J, et al. Anomalous plastic deformation in nanoscale Cu/Ta multilayers [J]. Mater. Sci. Eng., 2014, A598: 355
[26] Zhao X, Lu C, Tieu A K, et al. Deformation mechanisms and slip-twin interactions in nanotwinned body-centered cubic iron by molecular dynamics simulations [J]. Comput. Mater. Sci., 2018, 147: 34
[27] An M R, Song H Y, Deng Q, et al. Influence of interface with mismatch dislocations on mechanical properties of Ti/Al nanolaminate [J]. J. Appl. Phys., 2019, 125: 165307
[28] Liu Y, Yang K M, Hay J, et al. The effect of coherent interface on strain-rate sensitivity of highly textured Cu/Ni and Cu/V multilayers [J]. Scr. Mater., 2019, 162: 33
[29] Yin F X, Zhao Y Z, Yu S Y, et al. Molecular dynamics studies on the interface evolution characteristics and deformation mechanisms of Cu/Al multilayers during compression process [J]. J. Appl. Phys., 2019, 125: 025112
[30] Eder S J, Rodríguez Ripoll M, Cihak-Bayr U, et al. Unraveling and mapping the mechanisms for near-surface microstructure evolution in CuNi alloys under sliding [J]. ACS Appl. Mater. Interfaces, 2020, 12: 32197
[31] Wang J Y, Shi J Q, Lu Y, et al. Deformation evolution of Cu/Ta nanoscale multilayer during nanoindentation by a molecular dynamics study [J]. Surf. Coat. Technol., 2022, 441: 128562
[32] Shi J Q, Wang J Y, Yi X B, et al. Nanoscratching-induced plastic deformation mechanism and tribology behavior of Cu/Ta bilayer and multilayer by a molecular dynamics study [J]. Appl. Surf. Sci., 2022, 586: 152775
[33] Wang T, Jin L, Shi T L, et al. Effect of Al and W atom doping on the deformation mechanism and tribological properties of Cu95 X5/Ta nanobilayer by molecular dynamics simulation [J]. Tribol. Int., 2025, 210: 110818
[34] Faken D, Jónsson H. Systematic analysis of local atomic structure combined with 3D computer graphics [J]. Comput. Mater. Sci., 1994, 2: 279
[35] Stukowski A, Bulatov V V, Arsenlis A. Automated identification and indexing of dislocations in crystal interfaces [J]. Modell. Simul. Mater. Sci. Eng., 2012, 20: 085007
[36] Fu E G, Li N, Misra A, et al. Mechanical properties of sputtered Cu/V and Al/Nb multilayer films [J]. Mater. Sci. Eng., 2008, A493: 283
[37] Bain E C. Factors affecting the inherent hardenability of steel [J]. J. Heat Treat., 1979, 1: 57
[38] Burgers W G. On the process of transition of the cubic-body-centered modification into the hexagonal-close-packed modification of zirconium [J]. Physica, 1934, 1: 561
[39] Bertin N, Carson R, Bulatov V V, et al. Crystal plasticity model of BCC metals from large-scale MD simulations [J]. Acta Mater., 2023, 260: 119336
Outlines

/