Research paper

Atomic-Scale Interaction Mechanism of Hydrogen Trapping at Grain Boundaries in High-Strength Aluminum Alloys

  • LUO Liewen ,
  • WANG Mingyang ,
  • GAO Zhiming ,
  • XIA Dahai ,
  • DENG Yida ,
  • HU Wenbin
Expand
  • 1 School of Materials Science and Engineering, Tianjin University, Tianjin 300350, China
    2 State Key Laboratory of Tropic Ocean Engineering Materials and Materials Evaluation, School of Materials Science and Engineering, Hainan University, Haikou 570228, China
XIA Dahai, associate professor, Tel: (022)27407338, E-mail: dahaixia@tju.edu.cn

Received date: 2025-06-11

  Revised date: 2025-07-22

  Online published: 2025-08-21

Supported by

National Natural Science Foundation of China(52171077);National Natural Science Foundation of China(52031007)

Abstract

High-strength aluminum alloys, such as Al-Cu-Li and Al-Zn-Mg, are essential structural materials in aerospace, manufacturing, transportation, and mobile communication owing to their excellent strength-to-weight ratio. However, their use in critical applications is significantly limited by hydrogen embrittlement (HE), a phenomenon in which H atoms interact with microstructural features such as grain boundaries (GBs), leading to irreversible degradation of mechanical properties and potentially catastrophic failures. Despite extensive research, the atomic-scale mechanisms of H trapping at GBs and their detrimental effects on GB cohesion remain unclear, impeding the development of effective anti-embrittlement strategies. This study utilizes first-principles calculations to investigate these issues, aiming to provide a theoretical foundation for anti-embrittlement engineering. The results indicate that H atoms are most stably adsorbed at the short-bridge site on the Al (001) surface, with an adsorption energy of -3.051 eV, and tend to occupy tetrahedral interstitial sites (TIS) in the matrix. The diffusion path of H atoms into the matrix follows the TIS-OIS-TIS mechanism (where OIS denotes the octahedral interstitial site), with significant migration barriers of 0.32-0.56 eV, suggesting a challenge for H penetration into the matrix. Notably, Mg and Zr atoms spontaneously segregate to Site 1 of the Al Σ3(111)[110] GB; however, their effects are different: Mg weakens GB cohesion through charge depletion, whereas Zr significantly strengthens GBs by inducing high charge density, strong electronic localization, and d-p orbital hybridization. In addition, Zr segregation not only traps H atoms with a minimum trapping energy of -0.459 eV but also effectively suppresses H-induced damage to adjacent Al-Al metallic bonds, preserving GB strength. By contrast, Zn segregation has limited strengthening effects on GBs and may even facilitate H trapping. This study clarifies, at the atomic scale, that Zr enhances HE resistance through dual mechanisms: reinforcing GB cohesion and inhibiting H-induced degradation.

Cite this article

LUO Liewen , WANG Mingyang , GAO Zhiming , XIA Dahai , DENG Yida , HU Wenbin . Atomic-Scale Interaction Mechanism of Hydrogen Trapping at Grain Boundaries in High-Strength Aluminum Alloys[J]. Acta Metall Sin, 2025 , 61(11) : 1747 -1757 . DOI: 10.11900/0412.1961.2025.00165

References

[1] Campari A, Ustolin F, Alvaro A, et al. A review on hydrogen embrittlement and risk-based inspection of hydrogen technologies [J]. Int. J. Hydrogen Energy, 2023, 48: 35316
[2] Yang Z X, Zhang X T, Yu S Q, et al. Effect of microstructure on hydrogen trapping behavior and hydrogen embrittlement sensitivity of medium manganese steel [J]. Anti-Corros. Methods Mater., 2025, 72: 364
[3] Wang Q Y, Jing X J, Zhang X S, et al. Effect of hydrogen charging current density on hydrogen damage sensitivity of laser-peened 316L stainless steel [J]. Anti-Corros. Methods Mater., 2025, 72: 615
[4] Ye W H, Lu N, Zhang Z X, et al. Unveiling the mechanisms of hydrogen permeation in defective spinel γ-Al2O3: A first-principles study [J]. Int. J. Hydrogen Energy, 2025, 97: 1014
[5] Yang B, Chen X L, Shi X B, et al. Softening mechanism and hydrogen permeability of rare earth Y-doped V-Cr alloys [J]. Acta Metall. Sin., 2025, 61: 887
  杨 波, 陈小亮, 史晓斌 等. 稀土Y掺杂V-Cr合金增塑机理及透氢性能 [J]. 金属学报, 2025, 61: 887
[6] Han G, Chen X F, Zhao T X, et al. Effect of alloying element doping on hydrogen adsorption and corrosion behavior of Fe2O3 (001) via high throughput method [J]. Anti-Corros. Methods Mater., 2025, 72: 490
[7] Li X F, Ma X F, Zhang J, et al. Review of hydrogen embrittlement in metals: Hydrogen diffusion, hydrogen characterization, hydrogen embrittlement mechanism and prevention [J]. Acta Metall. Sin. (Engl. Lett.), 2020, 33: 759
[8] Han G, Zhao T X, Chen X F, et al. Effect of hydrogen on surface structure of Fe2O3 (001) containing point defects [J]. Anti-Corros. Methods Mater., 2025, 75: 664
[9] Campestrini P, Van Westing E P M, Van Rooijen H W, et al. Relation between microstructural aspects of AA2024 and its corrosion behaviour investigated using AFM scanning potential technique [J]. Corros. Sci., 2000, 42: 1853
[10] Sun W W, Zhu Y M, Marceau R, et al. Precipitation strengthening of aluminum alloys by room-temperature cyclic plasticity [J]. Science, 2019, 363: 972
[11] Young G A, Scully J R. The effects of test temperature, temper, and alloyed copper on the hydrogen-controlled crack growth rate of an Al-Zn-Mg-(Cu) alloy [J]. Metall. Mater. Trans., 2002, 33A: 1167
[12] Bond G M, Robertson I M, Birnbaum H K. The influence of hydrogen on deformation and fracture processes in high-strength aluminum alloys [J]. Acta Metall., 1987, 35: 2289
[13] Song R G, Dietzel W, Zhang B J, et al. Stress corrosion cracking and hydrogen embrittlement of an Al-Zn-Mg-Cu alloy [J]. Acta Mater., 2004, 52: 4727
[14] Zhao H, Chakraborty P, Ponge D, et al. Hydrogen trapping and embrittlement in high-strength Al alloys [J]. Nature, 2022, 602: 437
[15] Young Jr G A, Scully J R. The diffusion and trapping of hydrogen in high purity aluminum [J]. Acta Mater., 1998, 46: 6337
[16] Wang M Y, Xia D H. Research progress on hydrogen embrittlement mechanism of high strength Al-alloy [J]. J. Chin. Soc. Corros., 2025, 45: 261
  王明洋, 夏大海. 高强铝合金氢脆机理研究进展 [J]. 中国腐蚀与防护学报, 2025, 45: 261
[17] Davis J R. Corrosion of Aluminum and Aluminum Alloys [M]. Materials Park: ASM International, 1999: 36
[18] Garner A, Euesden R, Yao Y C, et al. Multiscale analysis of grain boundary microstructure in high strength 7xxx Al alloys [J]. Acta Mater., 2021, 202: 190
[19] Christodoulou L, Flower H M. Hydrogen embrittlement and trapping in Al6% Zn-3% Mg [J]. Acta Metall., 1980, 28: 481
[20] Zhao H, De Geuser F, da Silva A K, et al. Segregation assisted grain boundary precipitation in a model Al-Zn-Mg-Cu alloy [J]. Acta Mater., 2018, 156: 318
[21] Wu X B, You Y W, Kong X S, et al. First-principles determination of grain boundary strengthening in tungsten: Dependence on grain boundary structure and metallic radius of solute [J]. Acta Mater., 2016, 120: 315
[22] Lozovoi A Y, Paxton A T, Finnis M W. Structural and chemical embrittlement of grain boundaries by impurities: A general theory and first-principles calculations for copper [J]. Phys. Rev. B, 2006, 74: 155416
[23] Huang Z F, Nie J F. Interaction between hydrogen and solute atoms in {10 1 ˉ 2} twin boundary and its impact on boundary cohesion in magnesium [J]. Acta Mater., 2021, 214: 117009
[24] Bhattacharya S K, Kohyama M, Tanaka S, et al. Si segregation at Fe grain boundaries analyzed by ab initio local energy and local stress [J]. J. Phys.: Condens. Mater., 2014, 26: 355005
[25] Wu X B, Kong X S, You Y W, et al. Effect of transition metal impurities on the strength of grain boundaries in vanadium [J]. J. Appl. Phys., 2016, 120: 095901
[26] Li H, Zhao Y X, Zhang X Y, et al. Co-segregation behavior and weakening effect of the major elements in Al-Zn-Mg-Cu series alloys on Al Σ3(111)[110] symmetrical tilt grain boundary: A first-principles study [J]. J. Mater. Res. Technol., 2022, 18: 3158
[27] Ji Y C, Dong C F, Chen L, et al. High-throughput computing for screening the potential alloying elements of a 7xxx aluminum alloy for increasing the alloy resistance to stress corrosion cracking [J]. Corros. Sci., 2021, 183: 109304
[28] Ji Y Y, Wang M Y, Qin W M, et al. Near-atomic-scale study of the oxide films on the grain boundaries of Al-Mg alloys at the initial stage of corrosion: Experimental investigations and DFT calculations [J]. Corros. Sci., 2025, 244: 112640
[29] Khanzadeh M, Alipour H, Alahyarizadeh G. Understanding hydrogen behavior on aluminum: DFT investigations on adsorption and diffusion mechanisms [J]. Int. J. Hydrogen Energy, 2024, 73: 632
[30] Zhao D D, Li Y J. Carbon segregation at Σ3 {112} grain boundaries in silicon [J]. Comput. Mater. Sci., 2018, 143: 80
Outlines

/