Effect of Solidification Conditions on Microstructure Evolution in DD6 Single-Crystal Superalloy
Received date: 2025-02-24
Revised date: 2025-04-25
Online published: 2025-07-28
Single-crystal superalloys are widely used in aircraft engines owing to their excellent high-temperature performance. As key factors in controlling the formation of microstructures, solidification conditions directly influence the comprehensive properties of alloys. Therefore, it is of great significance to understand the mechanisms of alloy microstructure evolution under different solidification conditions and to optimize the solidification process to improve the performance of advanced aircraft engine hot-section components. To investigate the effects of the solidification conditions on the evolution of as-cast and heat-treated microstructures in the second-generation single-crystal superalloy DD6, single-crystal bars oriented along the [001] direction were prepared using high-rate solidification (HRS) and liquid metal cooling (LMC) processes. The results showed that in the as-cast state, the γ′ phases in the dendritic core of the HRS alloy exhibited a relatively regular cubic shape, whereas those in the LMC alloy were irregularly cubic; the γ′ phases in the interdendritic regions of the HRS and LMC alloys were irregularly cubic and larger in size than those in the dendritic core. As the pouring temperature increased, the size of γ′ phases in the HRS alloy first increased and then decreased, reaching a maximum at 1560 oC. At the same pouring temperature of 1590 oC, the size of the γ′ phases in the LMC alloy was smaller. After the heat treatment, the volume fraction of the γ + γ′ eutectic under all conditions decreased significantly. A trend was observed where the smaller the size of the γ + γ′ eutectic in the as-cast alloy, the greater the reduction in its content, regardless of the initial γ + γ′ eutectic content in the as-cast state. In the heat-treated HRS and LMC alloys, the γ′ phases in the dendritic core and interdendritic regions were uniformly distributed and regularly arranged, and they demonstrated good cubicity. Furthermore, the size uniformity of the γ′ particles in the LMC alloy was superior to that in the HRS alloy. The differences in the microstructures of the as-cast alloys were primarily caused by differences in the temperature gradient during directional solidification. Therefore, increasing the pouring temperature or employing LMC to enhance the temperature gradient helped to refine the dendritic structure of the alloy, reduce microsegregation, and this can simplify the alloy's heat treatment process.
XIE Hongji , LI Jiarong , LUO Yushi , ZHENG Sujie , LUO Kailun . Effect of Solidification Conditions on Microstructure Evolution in DD6 Single-Crystal Superalloy[J]. Acta Metall Sin, 2026 , 62(4) : 550 -560 . DOI: 10.11900/0412.1961.2025.00049
| [1] | Seo S M, Kim I S, Lee J H, et al. Eta phase and boride formation in directionally solidified Ni-base superalloy IN792+Hf [J]. Metall. Mater. Trans., 2007, 38A: 883 |
| [2] | Whitesell H S, Overfelt R A. Influence of solidification variables on the microstructure, macrosegregation, and porosity of directionally solidified Mar-M247 [J]. Mater. Sci. Eng., 2001, A318: 264 |
| [3] | Karunaratne M S A, Rae C M F, Reed R C. On the microstructural instability of an experimental nickel-based single-crystal superalloy [J]. Metall. Mater. Trans., 2001, 32A: 2409 |
| [4] | Versnyder F I, Shank M E. The development of columnar grain and single crystal high temperature materials through directional solidification [J]. Mater. Sci. Eng., 1970, 6: 213 |
| [5] | Li J R, Xiong J C, Tang D Z. Advanced High Temperature Structural Materials and Technology [M]. Beijing: National Defense Industry Press, 2012: 128 |
| 李嘉荣, 熊继春, 唐定中. 先进高温结构材料与技术 [M]. 北京: 国防工业出版社, 2012: 128 | |
| [6] | Giamei A F, Tschinkel J G. Liquid metal cooling: A new solidification technique [J]. Metall. Trans., 1976, 7A: 1427 |
| [7] | Gro?mann J, Preuhs J, E?er W, et al. Investment casting of high performance turbine blades by liquid metal cooling—A step forward towards industrial scale manufacturing [A]. Proceedings of International Symposium on Liquid Metal Processing and Castings [C]. New York: AVS, 1999: 31 |
| [8] | Liu L, Huang T W, Zhang J, et al. Microstructure and stress rupture properties of single crystal superalloy CMSX-2 under high thermal gradient directional solidification [J]. Mater. Lett., 2007, 61: 227 |
| [9] | Lohmüller A, E?er W, Gro?mann J, et al. Improved quality and economics of investment castings by liquid metal cooling—The selection of cooling media [A]. Superalloys 2000 [C]. Warrendale, PA: TMS, 2000: 181 |
| [10] | Elliot A J, Karney G B, Gigliotti M F X, et al. Issues in processing by the liquid-Sn assisted directional solidification technique [A]. Superalloys 2004 [C]. Warrendale, PA: TMS, 2004: 421 |
| [11] | Brundidge C L, van Drasek D, Wang B, et al. Structure refinement by a liquid metal cooling solidification process for single-crystal nickel-base superalloys [J]. Metall. Mater. Trans., 2012, 43A, 965 |
| [12] | Fan Z D, Wang D, Liu C, et al. Low-cycle fatigue properties of nickel-based superalloys processed by high-gradient directional solidification [J]. Acta Metall. Sin. (Engl. Lett.), 2017, 39: 878 |
| [13] | Zhao K, Ma Y H, Lou L H. Improvement of creep rupture strength of a liquid metal cooling directionally solidified nickel-base superalloy by carbides [J]. J. Alloys Compd., 2009, 475: 648 |
| [14] | Li J R, Zhao J Q, Liu S Z, et al. Effects of low angle boundaries on the mechanical properties of single crystal superalloy DD6 [A]. Superalloys 2008 [C]. Warrendale, PA: TMS, 2008: 443 |
| [15] | Xu Q Y, Yang C, Yan X W, et al. Development of numerical simulation in nickel-based superalloy turbine blade directional solidification [J]. Acta Metall. Sin., 2019, 55: 1175 |
| 许庆彦, 杨 聪, 闫学伟 等. 高温合金涡轮叶片定向凝固过程数值模拟研究进展 [J]. 金属学报, 2019, 55: 1175 | |
| [16] | Liu G, Liu L, Zhao X B, et al. Microstructure and microsegregation in a Ni-based single crystal superalloy directionally solidified under high thermal gradient [J]. Acta Metall. Sin., 2010, 46: 77 |
| 刘 刚, 刘 林, 赵新宝 等. 一种镍基单晶高温合金的高温度梯度定向凝固组织及枝晶偏析 [J]. 金属学报, 2010, 46: 77 | |
| [17] | Sun F L, Li J R, Liu S Z, et al. Microstructure and mechanical property of single crystal superalloy DD6 with different states [J]. J. Iron Steel Res., 2003, 15: 269 |
| 孙凤礼, 李嘉荣, 刘世忠 等. 单晶高温合金DD6不同状态下的显微组织和力学性能 [J]. 钢铁研究学报, 2003, 15: 269 | |
| [18] | Zhang X Y, Liu L, Huang T W, et al. Effect of solidification parameters on the segregation and γ/γ' eutectic evolution in Ni-based single crystal superalloy DD6 [J]. Rare Met. Mater. Eng., 2013, 42: 2547 |
| 张晓越, 刘 林, 黄太文 等. 凝固参数对DD6偏析和γ/γ'共晶组织演化的影响 [J]. 稀有金属材料与工程, 2013, 42: 2547 | |
| [19] | Wang Y M, Li S M, Zhong H, et al. Evaluation of the uniform distribution of dendritic microstructure in directionally solidified single-crystal DD6 superalloy [J]. Acta Metall. Sin., 2015, 51: 1038 |
| 王玉敏, 李双明, 钟 宏 等. 定向凝固DD6单晶高温合金枝晶组织均匀性研究 [J]. 金属学报, 2015, 51: 1038 | |
| [20] | Zhang S H, Lu Y Z, Zheng W, et al. Effect of primary dendrite arm spacing on the anisotropic stress rupture properties in a nickel-base single crystal superalloy DD26 [J]. Mater. Rep., 2016, 30(14): 6 |
| 张少华, 卢玉章, 郑 伟 等. 一次枝晶间距对DD26单晶高温合金持久各向异性的影响 [J]. 材料导报, 2016, 30(14): 6 | |
| [21] | Shi Z X, Liu S Z, Zhao J Q. Effect of C content on microstructures and stress rupture properties of a single crystal superalloy [J]. Nonferrous Met. Mater. Eng., 2018, 39(5): 1 |
| 史振学, 刘世忠, 赵金乾. C含量对一种单晶高温合金组织和持久性能的影响 [J]. 有色金属材料与工程, 2018, 39(5): 1 | |
| [22] | Yang C B, Liu L, Zhao X B, et al. Dendrite arm spacings and microsegregations in <001> and <011> orientated single crystal superalloys DD407 [J]. Acta Metall. Sin., 2011, 47: 1246 |
| 杨初斌, 刘 林, 赵新宝 等. <001>和<011>取向DD407单晶高温合金枝晶间距和微观偏析 [J]. 金属学报, 2011, 47: 1246 | |
| [23] | Wagner A, Shollock B A, McLean M. Grain structure development in directional solidification of nickel-base superalloys [J]. Mater. Sci. Eng., 2004, A374: 270 |
| [24] | Kurz W, Fisher D J. Dendrite growth at the limit of stability: Tip radius and spacing [J]. Acta Metall., 1981, 29: 11 |
| [25] | Yang L, Li J R, Jin H P, et al. Numerical simulation on directional solidification process of DD6 single crystal superalloy thin-walled specimen [J]. J. Mater. Eng., 2014, (11): 15 |
| 杨 亮, 李嘉荣, 金海鹏 等. DD6单晶精铸薄壁试样定向凝固过程数值模拟 [J]. 材料工程, 2014, (11): 15 | |
| [26] | Luo Y S, Zhao Y S, Liu Z Y, et al. Effects of heat treatment on microstrucutures and stress rupture properties of a second generation Ni-based single crystal DD11 [J]. J. Chongqing Univ., 2016, 39(3): 43 |
| 骆宇时, 赵云松, 刘志远 等. 热处理对第二代镍基单晶合金DD11显微组织及持久性能的影响 [J]. 重庆大学学报, 2016, 39(3): 43 | |
| [27] | Xiong J C, Li J R, Han M, et al. Effects of pouring temperature on the solidification microstructure of single crystal superalloy DD6 [J]. J. Mater. Eng., 2009, (2): 43 |
| 熊继春, 李嘉荣, 韩 梅 等. 浇注温度对DD6单晶高温合金凝固组织的影响 [J]. 材料工程, 2009, (2): 43 | |
| [28] | Liu L, Sun D J, Huang T W, et al. Directional solidification under high thermal gradient and its application in superalloys processing [J]. Acta Metall. Sin., 2018, 54: 615 |
| 刘 林, 孙德建, 黄太文 等. 高梯度定向凝固技术及其在高温合金制备中的应用 [J]. 金属学报, 2018, 54: 615 | |
| [29] | Cao L M, Li X H, Chen J Y, et al. Influence of solution heat treatment temperature on the microstructure of the third generation Ni-based single crystal superalloy DD10 [J]. J. Mater. Eng., 2011, (10): 23 |
| 曹腊梅, 李相辉, 陈晶阳 等. 固溶温度对第三代镍基单晶高温合金DD10组织的影响 [J]. 材料工程, 2011, (10): 23 | |
| [30] | Zeng Q, Chen X H, Wu B P, et al. Effect of solution and aging heat treatment on microstructures and stress rupture properties of Fourth generation Ni-based single crystal superalloy [J]. Rare Met. Mater. Eng., 2022, 51: 3394 |
| 曾 强, 陈旭辉, 吴保平 等. 固溶时效处理工艺对一种四代镍基单晶高温合金组织及性能的影响 [J]. 稀有金属材料与工程, 2022, 51: 3394 | |
| [31] | Zhang W G, Liu L, Huang T W, et al. Effect of cooling rate on γ' precipitate of DZ4125 alloy under high thermal gradient directional solidification [J]. Acta Metall. Sin., 2009, 45: 592 |
| 张卫国, 刘 林, 黄太文 等. 高温度梯度定向凝固冷却速率对DZ4125合金γ'相的影响 [J]. 金属学报, 2009, 45: 592 | |
| [32] | Liang Y J, Li J, Li A, et al. Solidification path of single-crystal nickel-base superalloys with minor carbon additions under laser rapid directional solidification conditions [J]. Scr. Mater., 2017, 127: 58 |
| [33] | Xie H J, Li J R, Han M, et al. Effect of over-temperature on microstructure and high cycle fatigue properties of DD6 single crystal superalloy [J]. Rare Met. Mater. Eng., 2018, 47: 2483 |
| 谢洪吉, 李嘉荣, 韩 梅 等. 超温对DD6单晶高温合金组织及高周疲劳性能影响 [J]. 稀有金属材料与工程, 2018, 47: 2483 | |
| [34] | Xue Y P, Yang L, Yu J, et al. Evolution of γ' phase in DD6 single crystal turbine blade [J]. J. Aeronaut. Mater., 2020, 40(6): 8 |
| 薛燕鹏, 杨 亮, 喻健 等. DD6单晶叶片的γ'相演化 [J]. 航空材料学报, 2020, 40(6): 8 | |
| [35] | Li X. Effect of transverse magnetic field on the microstructure in directionally solidified single crystal Ni-based superalloy CMSX-6 [D]. Shanghai: Shanghai Jiao Tong University, 2015 |
| 李 旭. 横向静磁场作用下单晶高温合金CMSX-6定向凝固组织生长行为的研究 [D]. 上海: 上海交通大学, 2015 |
/
| 〈 |
|
〉 |