Overview

Key Factors Affecting Cold Spray Particle Deposition: A Review of Powder Surface Oxidation

  • LI Wenya ,
  • YANG Jingwen ,
  • LUO Xiaotao ,
  • YIN Shuo ,
  • XU Yaxin
Expand
  • 1 Shaanxi Provincial Key Laboratory of Friction Welding Engineering Technology, State Key Laboratory of Solidification Technology, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi'an 710072, China
    2 School of Materials Science and Engineering, Xi'an Jiaotong University, Xi'an 710049, China
    3 School of Mechanical Manufacturing and Biomedical Engineering, Trinity University Dublin, D02PN40, Ireland

Received date: 2025-03-27

  Revised date: 2025-06-17

  Online published: 2025-07-18

Supported by

National Natural Science Foundation of China(52061135101);Project of Key Areas of Innovation Team in Shaanxi Province(2024RS-CXTD-20)

Abstract

Cold spraying (CS), recognized for its solid-state deposition characteristics, holds significant potential for the fabrication of high-performance coatings, the repair of damaged components, and the additive manufacturing of metals and metal matrix composites. However, oxide films present on the surfaces of powder particles exert a profound impact on particle deformation during CS, as well as on the interfacial microstructure, bonding quality, and mechanical properties of the resulting coatings or deposits. The presence of oxide films increases the critical deposition velocity, reduces the plastic deformation capacity of particles, and promotes the formation of unbonded regions or brittle inclusions at interfaces, thereby compromising deposition efficiency and mechanical integrity. Nevertheless, under specific conditions, the oxide film on the powder surface can be fractured by particle collisions, and the resulting discontinuous oxide film may become evenly distributed, potentially contributing to the dispersion strengthening and enhancing the hardness of the coating. This study presents a comprehensive review of the deformation behavior of oxide films during the CS process and their influence on coating microstructure and properties, with particular focus on the mechanism where how oxide film influences interfacial bonding, coating microstructure and performance. Furthermore, the study discusses the importance of minimizing oxygen content in feedstock powders to achieve high-strength and high-ductility deposits, providing theoretical guidance for optimizing coating performance. Finally, the role of oxide films in CS-based additive manufacturing is explored, and prospective research directions are outlined.

Cite this article

LI Wenya , YANG Jingwen , LUO Xiaotao , YIN Shuo , XU Yaxin . Key Factors Affecting Cold Spray Particle Deposition: A Review of Powder Surface Oxidation[J]. Acta Metall Sin, 2026 , 62(1) : 17 -28 . DOI: 10.11900/0412.1961.2025.00087

References

[1] Li W Y, Cao C C, Yin S. Solid-state cold spraying of Ti and its alloys: A literature review [J]. Prog. Mater. Sci., 2020, 110: 100633
[2] Yin S, Cavaliere P, Aldwell B, et al. Cold spray additive manufacturing and repair: Fundamentals and applications [J]. Addit. Manuf., 2018, 21: 628
[3] Assadi H, Kreye H, G?rtner F, et al. Cold spraying—A materials perspective [J]. Acta Mater., 2016, 116: 382
[4] Li W Y, Zhang Z Z, Xu Y X, et al. Research progress of cold sprayed Ni and Ni-based composite coatings: A review [J]. Acta Metall. Sin., 2022, 58: 1
  李文亚, 张正茂, 徐雅欣 等. 冷喷涂Ni及镍基复合涂层研究进展 [J]. 金属学报, 2022, 58: 1
[5] Li C J, Wang H T, Zhang Q, et al. Influence of spray materials and their surface oxidation on the critical velocity in cold spraying [J]. J. Therm. Spray Technol., 2010, 19: 95
[6] Wu J W, Fang H Y, Yoon S, et al. The rebound phenomenon in kinetic spraying deposition [J]. Scr. Mater., 2006, 54: 665
[7] Li W Y, Liao H L, Li C J, et al. On high velocity impact of micro-sized metallic particles in cold spraying [J]. Appl. Surf. Sci., 2006, 253: 2852
[8] Lienhard J, Crook C, Azar M Z, et al. Surface oxide and hydroxide effects on aluminum microparticle impact bonding [J]. Acta Mater., 2020, 197: 28
[9] Hassani-Gangaraj M, Veysset D, Nelson K A, et al. Impact-bonding with aluminum, silver, and gold microparticles: Toward understanding the role of native oxide layer [J]. Appl. Surf. Sci., 2019, 476: 528
[10] Ko K H, Choi J O, Lee H, et al. Influence of oxide chemistry of feedstock on cold sprayed Cu coatings [J]. Powder Technol., 2012, 218: 119
[11] Hasani S, Panjepour M, Shamanian M. The oxidation mechanism of pure aluminum powder particles [J]. Oxid. Met., 2012, 78: 179
[12] Alkhimov A P, Kosarev V F, Papyrin A N. A method of “cold” gas-dynamic deposition [J]. Soviet Phys. Doklady, 1990, 35: 1047
[13] Li C J, Li W Y, Luo X T, et al. Advanced Solid-State Cold Spray Deposition Technology for Metals: Theory and Application. [M]. Beijing: Science Press, 2023: 2
  李长久, 李文亚, 雒晓涛 等. 先进冷喷涂金属固态沉积技术: 理论与应用 [M]. 北京, 科学出版社, 2023: 2
[14] Li W Y, Zhang D D, Huang C J, et al. State of the art of cold spraying additive manufacturing and remanufacturing [J]. Weld. Joining, 2016, (4): 2
  李文亚, 张冬冬, 黄春杰 等. 冷喷涂技术在增材制造和修复再制造领域的应用研究现状 [J]. 焊接, 2016, (4): 2
[15] Li W Y, Cao C C, Wang G Q, et al. ‘Cold spray +’ as a new hybrid additive manufacturing technology: A literature review [J]. Sci. Technol. Weld. Joining, 2019, 24: 420
[16] Gilmore D L, Dykhuizen R C, Neiser R A, et al. Particle velocity and deposition efficiency in the cold spray process [J]. J. Therm. Spray Technol., 1999, 8: 576
[17] Dykhuizen R C, Smith M F, Gilmore D L, et al. Impact of high velocity cold spray particles [J]. J. Therm. Spray Technol., 1999, 8: 559
[18] Van Steenkiste T H, Smith J R, Teets R E, et al. Kinetic spray coatings [J]. Surf. Coat. Technol., 1999, 111: 62
[19] Van Steenkiste T H, Smith J R, Teets R E. Aluminum coatings via kinetic spray with relatively large powder particles [J]. Surf. Coat. Technol., 2002, 154: 237
[20] Li C J, Li W Y, Liao H L. Examination of the critical velocity for deposition of particles in cold spraying [J]. J. Therm. Spray Technol., 2006, 15: 212
[21] Li W Y. Study on the effect of particle parameters on deposition behavior, microstructure evolution and properties in cold spraying [D]. Xian: Xi'an Jiaotong University, 2005
  李文亚. 粒子参量对冷喷涂层沉积行为、组织演变与性能影响的研究 [D]. 西安: 西安交通大学, 2005
[22] Tao Q Y, Ding W W, Chen G, et al. Towards an atomic-scale understanding of oxide film in the Ti powder surface [J]. Scr. Mater., 2022, 210: 114471
[23] Luo X T, Ge Y, Xie Y C, et al. Dynamic evolution of oxide scale on the surfaces of feed stock particles from cracking and segmenting to peel-off while cold spraying copper powder having a high oxygen content [J]. J. Mater. Sci. Technol., 2021, 67: 105
[24] Vaquila I, Vergara L I, Passeggi M C G, et al. Chemical reactions at surfaces: Titanium oxidation [J]. Surf. Coat. Technol., 1999, 122: 67
[25] Xia Y, Zhao J L, Tian Q H, et al. Review of the effect of oxygen on titanium and deoxygenation technologies for recycling of titanium metal [J]. JOM, 2019, 71: 3209
[26] Yu M, Li W Y, Guo X P, et al. Impacting behavior of large oxidized copper particles in cold spraying [J]. J. Therm. Spray Technol., 2013, 22: 433
[27] Li W Y, Li C J, Liao H L. Significant influence of particle surface oxidation on deposition efficiency, interface microstructure and adhesive strength of cold-sprayed copper coatings [J]. Appl. Surf. Sci., 2010, 256: 4953
[28] Chen C Y, Xie Y C, Huang R Z, et al. On the role of oxide film's cleaning effect into the metallurgical bonding during cold spray [J]. Mater. Lett., 2018, 210: 199
[29] Bu H Y, Lu C. Review of critical velocity in cold spraying and its factors [J]. Mater. Protec., 2011, 44(4): 46
  卜恒勇, 卢 晨. 冷喷涂临界速度及其影响因素 [J]. 材料保护, 2011, 44(4): 46
[30] Kang K, Yoon S, Ji Y, et al. Oxidation dependency of critical velocity for aluminum feedstock deposition in kinetic spraying process [J]. Mater. Sci. Eng., 2008, A486: 300
[31] Li W Y, Zhang C, Wang H T, et al. Significant influences of metal reactivity and oxide films at particle surfaces on coating microstructure in cold spraying [J]. Appl. Surf. Sci., 2007, 253: 3557
[32] Navabi A, Vandadi M, Bond T, et al. Deformation and cracking phenomena in cold sprayed 6061 Al alloy powders with nanoscale aluminum oxide films [J]. Mater. Sci. Eng., 2022, A841: 143036
[33] Rahmati S, Veiga R G A, Zú?iga A, et al. A numerical approach to study the oxide layer effect on adhesion in cold spray [J]. J. Therm. Spray Technol., 2021, 30: 1777
[34] Tiamiyu A A, Schuh C A. Particle flattening during cold spray: Mechanistic regimes revealed by single particle impact tests [J]. Surf. Coat. Technol., 2020, 403: 126386
[35] Tang Q, Veysset D, Assadi H, et al. Strength gradient in impact-induced metallic bonding [J]. Nat. Commun., 2024, 15: 9630
[36] Zhang Z M, Li W Y, Yang J W, et al. Effect of powder oxidation on microstructures and mechanical properties of cold-sprayed nickel coatings and improvement by post-spray heat treatment [J]. J. Therm. Spray Technol., 2024, 33: 1968
[37] Li Y J, Luo X T, Li C J. Improving deposition efficiency and inter-particle bonding of cold sprayed Cu through removing the surficial oxide scale of the feedstock powder [J]. Surf. Coat. Technol., 2021, 407: 126709
[38] Li W Y, Yang J W, Zhang Z M, et al. High ductility induced by twin-assisted grain rotation and merging in solid-state cold spray additive manufactured Cu [J]. J. Mater. Sci. Technol., 2025, 214: 11
[39] Chen C Y, Xie Y C, Yin S, et al. Ductile and high strength Cu fabricated by solid-state cold spray additive manufacturing [J]. J. Mater. Sci. Technol., 2023, 134: 234
[40] Huang C J, Chen T, Fu B L, et al. Ductility and fracture behavior of cold spray additive manufactured zinc [J]. Addit. Manuf., 2024, 89: 104310
[41] Singh R, Kondás J, Bauer C, et al. Bulk-like ductility of cold spray additively manufactured copper in the as-sprayed state [J]. Addit. Manuf. Lett., 2022, 3: 100052
[42] List A, Huang C, Wiehler L, et al. Influence of ductility on fracture in tensile testing of cold gas sprayed deposits [J]. J. Therm. Spray Technol., 2023, 32: 1780
Outlines

/