Microstructural Control and Tribological Behavior of High-Nitrogen 316LN Austenitic Stainless Steel
Received date: 2025-02-17
Revised date: 2025-03-26
Online published: 2025-06-19
Supported by
National Key Research and Development Program of China(2022YFB3705300);National Natural Science Foundation of China(52374403);National Natural Science Foundation of China(U23A20613);National Natural Science Foundation of China(52004224);Research Fund of Analytical & Testing Center(2023-T-009);State Key Laboratory of Solidification Processing of Northwestern Polytechnical University(2021-TS-10)
Traditional austenitic stainless steel (ASS) faces challenges in operating safely under low-temperature sliding wear conditions because of its relatively low strength and hardness. To address this issue, this study focused on high-nitrogen 316LN ASSs. Through controlled rolling and annealing, three microstructures were designed: non-recrystallized, heterogeneous, and fully recrystallized microstructures (marked by NG, HS, and CG structures, respectively). The influence of environmental temperature and microstructure on the tribological behavior and wear mechanisms of high-nitrogen 316LN ASSs was investigated. The results demonstrate that the HS structure exhibits the lowest friction coefficient because the reduced number of abrasive particles limits the direct contact between the worn surface and the counterpart, outperforming the NG and CG structures. As the environmental temperature decreases, the wear rates of all the structures decrease, with the lowest wear rate observed at -120 oC. At this temperature, the CG structure exhibits the lowest wear rate—surpassing the NG and HS structures—attributed to its low stacking-fault energy, inducing martensitic transformation and forming a nano/submicron crystalline hardened layer. This layer effectively prevents crack propagation and enhances wear resistance. Although martensitic transformation and surface hardening also occur in the HS structure, the wear debris generated during sliding acts as a third-body abrasive, accelerating wear and degrading wear resistance. In contrast, the CG structure, which exhibits excellent low-temperature plastic deformation ability, shows only mild abrasion during the wear process.
Key words: high-nitrogen steel; low-temperature friction; wear mechanism
ZHAO Liyuan , LI Xiaolin , DING Ran , DENG Xiangtao , FENG Hao , LI Huabing , WANG Haifeng . Microstructural Control and Tribological Behavior of High-Nitrogen 316LN Austenitic Stainless Steel[J]. Acta Metall Sin, 2026 , 62(4) : 561 -571 . DOI: 10.11900/0412.1961.2025.00044
| [1] | Gupta R K, Birbilis N. The influence of nanocrystalline structure and processing route on corrosion of stainless steel: A review [J]. Corros. Sci., 2015, 92: 1 |
| [2] | Rashidi S, Choi J P, Stevenson J W, et al. Effect of aluminizing on the high-temperature oxidation behavior of an alumina-forming austenitic stainless steel [J]. JOM, 2019, 71: 109 |
| [3] | Sun G Q, Huang J Q, Peng J, et al. Effect of strain hardening on wear and corrosion resistance of 316L austenitic stainless steel [J]. J. Mater. Eng. Perform., 2024, 33: 8108 |
| [4] | Parry V, Col A, Pascal C. Beneficial effect of cold-working on high temperature oxidation resistance of austenitic stainless steel [J]. Corros. Sci., 2019, 160: 108149 |
| [5] | Zhao L Y, Yang J W, Tian L, et al. The influence of tempering parameters on the microstructure, mechanical property, and the corresponding strengthening mechanism of metastable 301 austenitic stainless steel [J]. Steel Res. Int., 2024, 95: 2300674 |
| [6] | Li J C, Chen Y J, Zhao Y M, et al. Super-hard (MoSiTiVZr)N x high-entropy nitride coatings [J]. J. Alloys Compd., 2022, 926: 166807 |
| [7] | Li X R, Xiong J, Liu J B, et al. Microstructure evolution and wear resistance of nitrogen-strengthened γ-Fe based alloy fabricated by N2 pressure sintering [J]. J. Mater. Res. Technol., 2023, 23: 6262 |
| [8] | Zhao J T, Sun L F, He Z F, et al. Mechanical behavior of cryogenic rolling processed high nitrogen-austenitic stainless steel with high strength and good toughness [J]. Acta Metall. Sin., 2025, 62: 1884 |
| 赵今涛, 孙利芳, 何竹风 等. 基于深冷轧制备的高强韧高氮奥氏体不锈钢力学行为 [J]. 金属学报, 2025, 62: 1884 | |
| [9] | Lu S J, Zhao X B, Li Z, et al. Enhanced performances of deep nitriding austenitic stainless steel by a novel complex treatment [J]. Mater. Res. Express, 2019, 6: 016507 |
| [10] | Cheng Z, Li C X, Dong H, et al. Low temperature plasma nitrocarburising of AISI 316 austenitic stainless steel [J]. Surf. Coat. Technol., 2005, 191: 195 |
| [11] | Mills D J, Knutsen R D. An investigation of the tribological behaviour of a high-nitrogen Cr-Mn austenitic stainless steel [J]. Wear, 1998, 215: 83 |
| [12] | He Z F, Sun L F, Guo Y X, et al. Strengthening high-nitrogen austenitic stainless steel via constructing multi-scaled heterostructure [J]. J. Mater. Res. Technol., 2024, 32: 2076 |
| [13] | Li Z N, Jiang Y, La P, et al. Strength-ductility synergy in 316L austenitic stainless steel with a heterogeneous structure [J]. Mater. Sci. Eng., 2022, A861: 144385 |
| [14] | Niu G, Zurob H S, Misra R D K, et al. Strength-ductility synergy in a 1.4 GPa austenitic steel with a heterogeneous lamellar microstructure [J]. J. Mater. Sci. Technol., 2022, 106: 133 |
| [15] | Liu J, Deng X T, Huang L, et al. Friction and wear behavior of nano/ultrafine-grained and heterogeneous ultrafine-grained 18Cr-8Ni austenitic stainless steels [J]. Tribol. Int., 2020, 152: 106520 |
| [16] | Qin W B, Kang J J, Li J S, et al. Tribological behavior of the 316L stainless steel with heterogeneous lamella structure [J]. Materials, 2018, 11: 1839 |
| [17] | Gao Y R, Li H X, Zhao D Y, et al. Cryogenic friction behavior of aluminum alloys sheets under dry contact condition [J]. Tribol. Int., 2023, 180: 108227 |
| [18] | El-Tayeb N S M, Yap T C, Brevern P V. On the tribo-cryogenic characteristics of titanium alloys [J]. Proc. Inst. Mech. Eng., 2010, 224: 395 |
| [19] | Ren Y, Zhou Q, Hua D P, et al. Wear-resistant CoCrNi multi-principal element alloy at cryogenic temperature [J]. Sci. Bull., 2024, 69: 227 |
| [20] | Kennedy F E, Ye Y X, Baker I, et al. Development of a new cryogenic tribotester and its application to the study of cryogenic wear of AISI 316 stainless steel [J]. Wear, 2022, 496-497: 204309 |
| [21] | Hübner W. Phase transformations in austenitic stainless steels during low temperature tribological stressing [J]. Tribol. Int., 2001, 34: 231 |
| [22] | Pang M H, Zhai S J, Hu Y K, et al. Tribological properties of 304 stainless steel with rainwater corrosion [J]. Mater. Chem. Phys., 2023, 297: 127329 |
| [23] | Chaudhari R, Ingle A, Kalita K. Tribological investigation of effect of grain size in 304 austenitic stainless steel [J]. Trans. Indian Inst. Met., 2017, 70: 2399 |
| [24] | Shen J C, Wu C H, Zhang L C. Effects of sliding speed and lubrication on the tribological behaviour of stainless steel [J]. Int. J. Adv. Manuf. Technol., 2018, 94: 341 |
| [25] | Zhao L Y, Li X L, Ren Y J, et al. Cryogenic tribological behavior of coarse, ultrafine grained and heterogeneous Fe-18Cr-8Ni austenitic stainless steel [J]. Mater. Charact., 2024, 217: 114406 |
| [26] | Aktas B, Tekin H. Effects of Co3O4 addition on friction and dry sliding wear characteristics of 8 mol% yttria-stabilized cubic zirconia [J]. J. Mater. Eng. Perform., 2019, 28: 549 |
| [27] | Zambrano O A, Iglesias-Guerrero B, Rodríguez S A, et al. Running-in period during sliding wear of austenitic steels [J]. Tribol. Lett., 2024, 72: 70 |
| [28] | ?elebi M, Güler O, Karabacak A H, et al. Investigation of microstructural, hardness, and wear properties of AlCrCuFeNi high entropy alloys produced by hot-pressing with the enhancement of manufacturability through electroless Ag incorporation [J]. Tribol. Int., 2025, 201: 110277 |
| [29] | Wang H M, Du Y, Pei X H, et al. Tribological property and wear mechanism of NbMoZrVSi x refractory high-entropy alloy strengthened by eutectic structure [J]. Acta Metall. Sin., 2024, 60: 937 |
| 王瀚铭, 杜 银, 裴旭辉 等. 共晶组织强化NbMoZrVSi x 难熔高熵合金的摩擦磨损性能及磨损机理 [J]. 金属学报, 2024, 60: 937 | |
| [30] | Zhao L Y, Tian L, Li Q, et al. An investigation on the wear resistance and mechanism of Fe60 - x Co20Mo x Ni20 (x = 10, 15, 20) high-entropy alloy reinforced by μ-phase [J]. Wear, 2024, 554-555: 205463 |
| [31] | Shen M X, Zheng J P, Meng X K, et al. Influence of Al2O3 particles on the friction and wear behaviors of nitrile rubber against 316L stainless steel [J]. J. Zhejiang Univ., 2015, 16A: 151 |
| [32] | Lian X K, Li Y, Xiong Y, et al. Effect of annealing time on microstructure and mechanical properties of cryorolled AISI 310S stainless steel [J]. J. Iron Steel Res. Int., 2023, 30: 548 |
| [33] | Xu D M, Li G Q, Wan X L, et al. The effect of annealing on the microstructural evolution and mechanical properties in phase reversed 316LN austenitic stainless steel [J]. Mater. Sci. Eng., 2018, A720: 36 |
| [34] | Bisht A, Kumar L, Subburaj J, et al. Effect of stacking fault energy on the evolution of microstructure and texture during blast assisted deformation of FCC materials [J]. J. Mater. Process. Technol., 2019, 271: 568 |
| [35] | Li W, Li J Y, Gong Q D, et al. Annealing parameters effect on microstructure evolution, tensile properties and deformation behaviors of direct-cold-rolled UNS S32101 duplex stainless steel with heterogeneous layered structure [J]. Mater. Sci. Eng., 2023, A883: 145439 |
| [36] | Wei X C, Hua M, Xue Z Y, et al. Evolution of friction-induced microstructure of SUS 304 meta-stable austenitic stainless steel and its influence on wear behavior [J]. Wear, 2009, 267: 1386 |
/
| 〈 |
|
〉 |