Formation of In Situ Particle Composite Solidification Microstructure of Gd-Co-Ti Alloy Under Microgravity Conditions
Received date: 2024-05-20
Revised date: 2024-08-26
Online published: 2025-04-30
Supported by
Space Utilization System of China Manned Space Engineering(KJZ-YY-NCL-1-06);National Key Research and Development Program of China(2021YFA0716303);National Natural Science Foundation of China(52174380);Natural Science Foundation of Liaoning Province(2023-MS-023)
Gd and its alloys are good magnetic materials, and the addition of the transition metal Co to Gd-Ti alloy can facilitate the formation of thermally stable magnetic compounds. The Gd-Co-Ti alloy exhibits significant potential for the development of magnetic in situ composite materials. However, because of the large positive mixing enthalpy between Gd and Ti, the Gd-Co-Ti alloy is a typical monotectic alloy, exhibiting a miscibility gap in the liquid state. Under the ground gravity conditions, the alloy tends to form a phase-segregated solidification microstructure resulting from liquid-liquid phase transformation. Strong convection in the melt during solidification aggravates this process, rendering it difficult for various influencing factors to interact. However, research on solidification theory for these alloys is limited. Microgravity environments can effectively weaken or even eliminate natural convection in alloy melts, which is beneficial for studying the solidification process and microstructure formation in monotectic alloys. Previous studies have focused on the phase structures, material properties, and thermodynamic behavior of Gd-Co-Ti ternary monotectic alloys. However, research on their solidification process is sparse. In this study, rapid and sub-rapid solidification experiments under drop-tube microgravity conditions were performed using Gd-Co-Ti ternary monotectic alloys. The effects of cooling rates on the solidification microstructure of the alloy were investigated. The resulting samples exhibited a composite microstructure comprising homogeneously dispersed subspherical TiCo-rich particles in the Gd matrix. These particles include: (i) TiCo-rich phase particles formed via liquid-liquid phase transformation, and (ii) TiCo-rich nanoparticles formed through desolventizing precipitation during the cooling process after solidification. To elucidate the microstructure evolution in Gd-Co-Ti alloys solidified under drop-tube conditions, a population dynamics model was established. The model comprehensively considers the thermal and mass transfer characteristics during solidification, as well as the nucleation, growth, and spatial motions of TiCo-rich phase droplets. The algorithm for solving the controlling equations in this model was developed based on the finite volume method. The microstructure formation was simulated, and the results were consistent with the experimental data, thus validating the accuracy of the model. The numerical results demonstrated that the nucleation of the TiCo-rich phase droplets occurred during the liquid-liquid phase transformation under drop-tube microgravity conditions. The number density of these TiCo-rich phase droplets remained unchanged after nucleation, indicating that the Ostwald coarsening of the TiCo-rich droplets was weak during the cooling of the alloy melt. Thus, nucleation and diffusion growth were the primary factors influencing the size of TiCo-rich phase droplets formed during the liquid-liquid phase transformation. With the increase in the sample sizes, the cooling rate of the alloy melt and the number density of the TiCo-rich particles decreased; thus, the average radius of the TiCo-rich particles in the solidification microstructure increased. Furthermore, the maximum nucleation rate (IDMax) and the number density (ND) of the TiCo-rich phase droplets/particles exhibited an exponential dependence on the cooling rate (
SUN Hao , JIANG Hongxiang , ZHAO Jiuzhou , ZHANG Lili , HE Jie . Formation of In Situ Particle Composite Solidification Microstructure of Gd-Co-Ti Alloy Under Microgravity Conditions[J]. Acta Metall Sin, 2025 , 61(12) : 1933 -1944 . DOI: 10.11900/0412.1961.2024.00174
| [1] | Sinha V K, Cheng S F, Wallace W E, et al. Magnetic behavior of heavy rare earth RTiFe11 - x Co x alloys [J]. J. Magn. Magn. Mater., 1989, 81: 227 |
| [2] | Gjoka M, Sarafidis C, Niarchos D, et al. Structure and magnetic properties of Gd4(Co, Ti)41 alloys [J]. J. Alloys Compd., 2006, 423: 59 |
| [3] | Takeuchi A, Inoue A. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element [J]. Mater. Trans., 2005, 46: 2817 |
| [4] | Dong B W, Jie J C, Dong Z Z, et al. Novel insight into mechanism of secondary phase's morphology evolution in hypomonotectic Cu-Pb-Sn alloy during solidification [J]. J. Mol. Liq., 2019, 292: 111336 |
| [5] | Lu W Q, Zhang S G, Li J G. Segregation driven by collision and coagulation of minor droplets in Al-Bi immiscible alloys under aerodynamic levitation condition [J]. Mater. Lett., 2013, 107: 340 |
| [6] | Zhao J Z, Jiang H X. Progress in the solidification of monotectic alloys [J]. Acta Metall. Sin., 2018, 54: 682 |
| 赵九洲, 江鸿翔. 偏晶合金凝固过程研究进展 [J]. 金属学报, 2018, 54: 682 | |
| [7] | Ahlborn H, Loehberg K. Aluminium-indium-experiment SOLUOG—A sounding rocket experiment on immiscible alloys [A]. Proceedings of the 17th Aerospace Sciences Meeting [C]. New Orleans: AIAA, 1979: 172 |
| [8] | Carlberg T, Fredriksson H. The influence of microgravity on the solidification of Zn-Bi immiscible alloys [J]. Metall. Trans., 1980, 11A: 1665 |
| [9] | Feuerbacher B, Hamacher H, Naumann R J. Binary systems with miscibility gap in the liquid state [A]. Materials Sciences in Space: A Contribution to the Scientific Basis of Space Processing [M]. Berlin, Heidelberg: Springer, 1986: 343 |
| [10] | Zhao J Z, Sun H, Zhang L L, et al. In-situ composite microstructure formation of immiscible alloy solidified in space [J]. Natl. Sci. Rev., 2023, 10: nwac261 |
| [11] | Zhang Y, Wu Y, Tang Y, et al. In situ study on the oscillation of mobile droplets and force analysis during the directional solidification of Al-Bi alloy [J]. J. Mater. Sci. Technol., 2024, 177: 1 |
| [12] | Sun H, Jiang H X, Li Y Q, et al. Control of competitive phase selection by in-situ nanoparticles [J]. J. Alloys Compd., 2023, 962: 171202 |
| [13] | Mullis A M, Jegede O E, Bigg T D, et al. Dynamics of core-shell particle formation in drop-tube processed metastable monotectic alloys [J]. Acta Mater., 2020, 188: 591 |
| [14] | Zhang L L, Yang L J, Zhao J Z, et al. Selection of a micro-alloying interface active component to stabilize the interface between droplets and liquid matrix in monotectic alloys [J]. Acta Mater., 2023, 250: 118823 |
| [15] | Li Y Q, Zhao J Z, Jiang H X, et al. Microstructure formation in directionally solidified Pb-Al alloy [J]. Acta Metall. Sin., 2022, 58: 1072 |
| 李彦强, 赵九洲, 江鸿翔 等. Pb-Al合金定向凝固组织形成过程 [J]. 金属学报, 2022, 58: 1072 | |
| [16] | Yang L J, Zhang L L, Zhao J Z, et al. A simple criterion for the selection of interfacial active element to control liquid-liquid decomposition of immiscible alloys [J]. Scr. Mater., 2024, 238: 115753 |
| [17] | Sun Q, Jiang H X, Zhao J Z. Effect of micro-alloying element Bi on solidification and microstructure of Al-Pb alloy [J]. Acta Metall. Sin., 2016, 52: 497 |
| 孙 倩, 江鸿翔, 赵九洲. 微量元素Bi对Al-Pb合金凝固过程及显微组织的影响 [J]. 金属学报, 2016, 52: 497 | |
| [18] | Zhou B F, Lin W H, Shen Z, et al. Growth dynamics of the segregated phase in Zn-6wt%Bi immiscible alloy superheated in super high static magnetic field [J]. J. Alloys Compd., 2021, 879: 160410 |
| [19] | Li W, Jiang H X, Zhang L L, et al. Solidification of Al-Bi-Sn immiscible alloy under microgravity conditions of space [J]. Scr. Mater., 2019, 162: 426 |
| [20] | Wei C, Wang J, He Y X, et al. Influence of high magnetic field on the liquid-liquid phase separation behavior of an undercooled Cu-Co immiscible alloy [J]. J. Alloys Compd., 2020, 842: 155502 |
| [21] | Liu Y, Li Y X, Guo J J, et al. Numerical simulation of macro-segregation formation during solidification process of immiscible alloys [J]. Acta Metall. Sin., 2003, 39: 679 |
| 刘 源, 李言祥, 郭景杰 等. 难混溶合金凝固过程中宏观偏析形成的数值模拟 [J]. 金属学报, 2003, 39: 679 | |
| [22] | Zhao J Z, Ratke L. A model describing the microstructure evolution during a cooling of immiscible alloys in the miscibility gap [J]. Scr. Mater., 2004, 50: 543 |
| [23] | Deng C K, Jiang H X, Zhao J Z, et al. Study on the solidification of Ag-Ni monotectic alloy [J]. Acta Metall. Sin., 2020, 56: 212 |
| 邓聪坤, 江鸿翔, 赵九洲 等. Ag-Ni偏晶合金凝固过程研究 [J]. 金属学报, 2020, 56: 212 | |
| [24] | Wu Y H, Zhu B R, Su J W, et al. A comparative study of metastable phase separation for undercooled liquid Fe35Cu65 alloy under natural and forced cooling conditions [J]. J. Alloys Compd., 2022, 927: 167079 |
| [25] | Li Y Q, Jiang H X, Sun H, et al. Microstructure evolution of immiscible alloy solidified under the effect of composite electric and magnetic fields [J]. J. Mater. Sci. Technol., 2023, 162: 247 |
| [26] | Wu W H, Wang J Y, Zhai W, et al. A computational and experimental study of ultrasonicated phase separation process for liquid Al-Bi immiscible alloy [J]. Metall. Mater. Trans., 2023, 54B: 1845 |
| [27] | Wu Y H, Wang W L, Chang J, et al. Evolution kinetics of microgravity facilitated spherical macrosegregation within immiscible alloys [J]. J. Alloys Compd., 2018, 763: 808 |
| [28] | Wu Y H, Wang W L, Wei B B. Experimental investigation and numerical simulation on liquid phase separation of ternary Fe-Sn-Si/Ge monotectic alloy [J]. Acta Phys. Sin., 2016, 65: 106402 |
| 吴宇昊, 王伟丽, 魏炳波. 液态三元Fe-Sn-Si/Ge偏晶合金相分离过程的实验和模拟研究 [J]. 物理学报, 2016, 65: 106402 | |
| [29] | Liu S C, Jie J C, Zhang J J, et al. A surface energy driven dissolution model for immiscible Cu-Fe alloy [J]. J. Mol. Liq., 2018, 261: 232 |
| [30] | Li W, Sun Q, Jiang H X, et al. Solidification of Al-Bi alloy and influence of microalloying element Sn [J]. Acta Metall. Sin., 2019, 55: 831 |
| 黎 旺, 孙 倩, 江鸿翔 等. Al-Bi合金凝固过程及微合金化元素Sn的影响 [J]. 金属学报, 2019, 55: 831 | |
| [31] | Zhao J Z, Jiang H X, Sun Q, et al. Progress of research on solidification process and microstructure control of immiscible alloys [J]. Mater. China, 2017, 36(4): 12 |
| 赵九洲, 江鸿翔, 孙 倩 等. 偏晶合金凝固过程及凝固组织控制方法研究进展 [J]. 中国材料进展, 2017, 36(4): 12 | |
| [32] | Mattern N, Zinkevich M, Han J H, et al. Experimental and thermodynamic assessment of the Co-Gd-Ti system [J]. Calphad, 2016, 54: 144 |
| [33] | Sun H. Rapid/sub-rapid solidification microstructure formation and control of liquid-liquid phase separation alloy under ground/space conditions [D]. Hefei: University of Science and Technology of China, 2024 |
| 孙 昊. 地面/空间液-液相分离合金快速/亚快速凝固组织形成及调控 [D]. 合肥: 中国科学技术大学, 2024 | |
| [34] | Zhao J Z. The kinetics of the liquid-liquid decomposition under the rapid solidification conditions of gas atomization [J]. Mater. Sci. Eng., 2007, A454-455: 637 |
| [35] | Zhao J Z, Kolbe M, Li H L, et al. Formation of the microstructure in a rapidly solidified Cu-Co alloy [J]. Metall. Mater. Trans., 2007, 38A: 1162 |
| [36] | Zhao J Z, Gao L L, He J, et al. Liquid-liquid phase transformation kinetics of an atomized Al-Pb alloy drop [J]. Acta Metall. Sin., 2006, 42: 113 |
| 赵九洲, 高玲玲, 何 杰 等. Al-Pb合金雾化液滴的液-液相变动力学 [J]. 金属学报, 2006, 42: 113 | |
| [37] | Ratke L, Diefenbach S. Liquid immiscible alloys [J]. Mater. Sci. Eng., 1995, R15: 263 |
| [38] | Zhao J, Ratke L. Repeated nucleation of minority phase droplets induced by drop motion [J]. Scr. Mater., 1998, 39: 181 |
| [39] | Wu M H, Ludwig A, Ratke L. Modeling of marangoni-induced droplet motion and melt convection during solidification of hypermonotectic alloys [J]. Metall. Mater. Trans., 2003, 34A: 3009 |
| [40] | Ishikawa T, Okada J T, Paradis P F, et al. Thermophysical property measurements of liquid gadolinium by containerless methods [J]. Int. J. Thermophys., 2010, 31: 388 |
| [41] | Iida T, Guthrie R I L, translated by Xian A P, Wang L W. The Physical Properties of Liquid Metals [M]. Beijing: Science Press, 2006: 256 |
| 饭田孝道, Guthrie R I L著 . 冼爱平, 王连文 译. 液态金属的物理性能 [M]. 北京: 科学出版社, 2006: 256 | |
| [42] | Kaptay G. A Calphad-compatible method to calculate liquid/liquid interfacial energies in immiscible metallic systems [J]. Calphad, 2008, 32: 338 |
| [43] | Gale W F, Totemeier T C. Smithells Metals Reference Book [M]. 8th Ed., Oxford: Elsevier, 2004: 1127 |
/
| 〈 |
|
〉 |