Numerical Simulation of the Dynamic Contraction of Dendrite Solidification in the Al-4.7%Cu Alloy
Received date: 2024-11-28
Revised date: 2024-12-26
Online published: 2025-04-29
Supported by
National Natural Science Foundation of China(51975182)
The dynamic formation process of microshrinkage pole in alloy castings is directly related to the dendrite solidification process. To simulate dendrite shrinkage in the Al-4.7%Cu (mass fraction) alloy during solidification, we proposed a coupling model combining cellular automata (CA) and the lattice Boltzmann method (LBM), referred to as the CA-LBM model. In this model, CA was used to simulate the formation of shrinkage pores during dendrite growth, whereas LBM was applied to study the diffusion process of shrinkage pores in the liquid phase (fully liquid conditions). First, the accuracy of the proposed CA-LBM numerical model was verified through the numerical simulation of the diffusion homogenization of a vacuum cavity in liquid. Then, the solidification process of a single dendrite—with and without dendrite shrinkage were compared, followed by the calculations of the multi-dendrite solidification contraction process with and without dendrite shrinkage. Simulations of the single-dendrite solidification process indicated that no internal pores were formed in the single dendrites when shrinkage was not considered. However, when shrinkage was considered, uniform microshrinkage pores appeared in the single dendrites. Moreover, the presence of shrinkage pores notably influenced dendrite morphology by promoting secondary branching. The results of the multidendrite contraction simulation also showed that micro-shrinkage pores tended to form at the junctions of the last solidified dendrites. A comparison between the calculated number of shrinkage poles and the theoretical value showed a small error, indicating the effectiveness and reliability of the proposed numerical model.
Key words: Al-Cu alloy; solidification; dendrite shrinkage; CA-LBM numerical model
ZHU Baofeng , LI Chenyu , ZHANG Shijie , LI Ri . Numerical Simulation of the Dynamic Contraction of Dendrite Solidification in the Al-4.7%Cu Alloy[J]. Acta Metall Sin, 2026 , 62(3) : 509 -522 . DOI: 10.11900/0412.1961.2024.00406
| [1] | Zhu J D, Cockcroft S L, Maijer D M. Modeling of microporosity formation in A356 aluminum alloy casting [J]. Metall. Mater. Trans., 2006, 37A: 1075 |
| [2] | Lee P D, Chirazi A, See D. Modeling microporosity in aluminum-silicon alloys: A review [J]. J. Light Met., 2001, 1: 15 |
| [3] | Dong S Y, Zhuang Z, Xu Q Y, et al. Preliminary study on simulation of microporosity evolution and fatigue life of aluminum alloy casting [J]. Int. J. Cast Met. Res., 2003, 15: 309 |
| [4] | Nabavizadeh S A, Eshraghi M, Felicelli S D. A comparative study of multiphase lattice Boltzmann methods for bubble-dendrite interaction during solidification of alloys [J]. Appl. Sci., 2019, 9: 57 |
| [5] | Khalajzadeh V, Beckermann C. Simulation of shrinkage porosity formation during alloy solidification [J]. Metall. Mater. Trans., 2020, 51A: 2239 |
| [6] | Kannan P, Balasubramanian K, Rajeswari N. Process optimization for pore defect in casting—A review [J]. Appl. Mech. Mater., 2015, 813-814: 581 |
| [7] | Lee P D, Hunt J D. Hydrogen porosity in directional solidified aluminium-copper alloys: In situ observation [J]. Acta Mater., 1997, 45: 4155 |
| [8] | Lee P D, Hunt J D. Measuring the nucleation of hydrogen porosity during the solidification of aluminium-copper alloys [J]. Scr. Mater., 1997, 36: 399 |
| [9] | Atwood R C, Sridhar S, Lee P D. Equations for nucleation of hydrogen gas pores during solidification of aluminium seven weight percent silicon alloy [J]. Scr. Mater., 1999, 41: 1255 |
| [10] | Atwood R C, Sridhar S, Zhang W, et al. Diffusion-controlled growth of hydrogen pores in aluminium-silicon castings: In situ observation and modelling [J]. Acta Mater., 2000, 48: 405 |
| [11] | See D, Atwood R C, Lee P D. A comparison of three modeling approaches for the prediction of microporosity in aluminum-silicon alloys [J]. J. Mater. Sci., 2001, 36: 3423 |
| [12] | Atwood R C, Lee P D. A three-phase model of hydrogen pore formation during the equiaxed dendritic solidification of aluminum-silicon alloys [J]. Metall. Mater. Trans., 2002, 33B: 209 |
| [13] | Lee P D, Atwood R C, Dashwood R J, et al. Modeling of porosity formation in direct chill cast aluminum-magnesium alloys [J]. Mater. Sci. Eng., 2002, A328: 213 |
| [14] | Hamilton R W, See D, Butler S, et al. Multiscale modeling for the prediction of casting defects in investment cast aluminum alloys [J]. Mater. Sci. Eng., 2003, A343: 290 |
| [15] | Atwood R C, Lee P D. Simulation of the three-dimensional morphology of solidification porosity in an aluminium-silicon alloy [J]. Acta Mater., 2003, 51: 5447 |
| [16] | Chaijaruwanich A, Lee P D, Dashwood R J, et al. Evolution of pore morphology and distribution during the homogenization of direct chill cast Al-Mg alloys [J]. Acta Mater., 2007, 55: 285 |
| [17] | Kareh K M, Lee P D, Atwood R C, et al. Pore behaviour during semi-solid alloy compression: Insights into defect creation under pressure [J]. Scr. Mater., 2014, 89: 73 |
| [18] | Puncreobutr C, Lee P D, Kareh K M, et al. Influence of Fe-rich intermetallics on solidification defects in Al-Si-Cu alloys [J]. Acta Mater., 2014, 68: 42 |
| [19] | Pequet C, Rappaz M, Gremaud M. Modeling of microporosity, macroporosity, and pipe-shrinkage formation during the solidification of alloys using a mushy-zone refinement method: Applications to aluminum alloys [J]. Metall. Mater. Trans., 2002, 33A: 2095 |
| [20] | Stefanescu D M. Computer simulation of shrinkage related defects in metal castings—A review [J]. Int. J. Cast Met. Res., 2005, 18: 129 |
| [21] | Carlson K D, Lin Z P, Beckermann C. Modeling the effect of finite-rate hydrogen diffusion on porosity formation in aluminum alloys [J]. Metall. Mater. Trans., 2007, 38B: 541 |
| [22] | Yao L, Cockcroft S, Zhu J D, et al. Modeling of microporosity size distribution in aluminum alloy A356 [J]. Metall. Mater. Trans., 2011, 42A: 4137 |
| [23] | Wu W, Sun D K, Dai T, et al. Modeling of dendritic growth and bubble formation [J]. Acta Phys. Sin., 2012, 61(15): 39 |
| 吴 伟, 孙东科, 戴 挺 等. 枝晶生长和气泡形成的数值模拟 [J]. 物理学报, 2012, 61(15): 39 | |
| [24] | Zhu M F, Li Z Y, An D, et al. Cellular automaton modeling of microporosity formation during solidification of aluminum alloys [J]. ISIJ Int., 2014, 54: 384 |
| [25] | Niyama E, Uchida T, Morikawa M, et al. A method of shrinkage prediction and its application to steel casting practice [J]. J. Jpn. Foundry. Soc., 1982, 54: 507 |
| [26] | Polyakov S, Korotchenko A, Bast J. Use of the Niyama criterion to predict porosity of the mushy zone with deformation [J]. Arch. Foundry Eng., 2011, 11: 131 |
| [27] | Liu C C, He J S. Numerical prediction of shrinkage defect in aluminum alloy electron beam weld based on Niyama criterion program [J]. Adv. Mater. Res., 2014, 1030-1032: 130 |
| [28] | Ignaszak Z. Discussion on usability of the Niyama criterion for porosity predicting in cast iron castings [J]. Arch. Foundry Eng., 2017, 17: 196 |
| [29] | Ivanina E S, Monastyrskiy V P, Ershov M Y. Quantitative estimation of formation of shrinkage porosity by the niyama criterion [J]. Inorg. Mater. Appl. Res., 2022, 13: 100 |
| [30] | Carlson K D, Beckermann C. Prediction of shrinkage pore volume fraction using a dimensionless Niyama criterion [J]. Metall. Mater. Trans., 2009, 40A: 163 |
| [31] | Monroe C, Beckermann C. Prediction of hot tearing using a dimensionless Niyama criterion [J]. JOM, 2014, 66: 1439 |
| [32] | Guo J, Beckermann C, Carlson K, et al. Microporosity prediction and validation for Ni-based superalloy castings [J]. IOP Conf. Ser., 2015, 84: 012003 |
| [33] | Khalajzadeh V, Carlson K D, Backman D G, et al. A pore-centric model for combined shrinkage and gas porosity in alloy solidification [J]. Metall. Mater. Trans., 2017, 48A: 1797 |
| [34] | Zhang A, Guo Z P, Jiang B, et al. Phase-field modeling of microstructure and gas porosity evolution during solidification of alloys: A review [J]. Chin. J. Nonferrous Met., 2021, 31: 2976 |
| 张 昂, 郭志鹏, 蒋 斌 等. 合金凝固组织和气孔演变相场模拟研究进展 [J]. 中国有色金属学报, 2021, 31: 2976 | |
| [35] | Backer G, Wang Q G. Microporosity simulation in aluminum castings using an integrated pore growth and interdendritic flow model [J]. Metall. Mater. Trans., 2007, 38B: 533 |
| [36] | Liu Y Q. Investigation on solidification process of aluminum alloys and casting technologies of complicated structural components [D]. Xi'an: Northwestern Polytechnical University, 2015 |
| 刘永勤. 铝合金凝固过程及其结构件的铸造工艺研究 [D]. 西安: 西北工业大学, 2015 | |
| [37] | Lee P D, Hunt J D. Hydrogen porosity in directionally solidified aluminium-copper alloys: A mathematical model [J]. Acta Mater., 2001, 49: 1383 |
| [38] | Huang J L, Conley J G, Mori T. Simulation of microporosity formation in modified and unmodified A356 alloy castings [J]. Metall. Mater. Trans., 1998, 29B: 1249 |
| [39] | Gui Z L, Dai T, Zhu M F. Present status of numerical simulation of micro-porosity in aluminum alloys [J]. Spec. Cast. Nonferrous Alloys, 2007, 10: 766 |
| 桂仲林, 戴 挺, 朱鸣芳. 铝合金显微疏松数值模拟的研究现状 [J]. 特种铸造及有色合金, 2007, 10: 766 | |
| [40] | Su M, Sun D K, Zhu M F. Application of lattice boltzmann method to dendrite growth simulation [J]. Mater Mec. Eng., 2007, 31(2): 75 |
| 苏 敏, 孙东科, 朱鸣芳. Lattice Boltzmann方法在枝晶生长模拟中的应用 [J]. 机械工程材料, 2007, 31(2): 75 | |
| [41] | Li Z Y, Zhu M F, Dai T. Modeling of microporosity formation in an Al-7%Si Alloy [J]. Acta Metall. Sin., 2013, 49: 1032 |
| 李正扬, 朱鸣芳, 戴 挺. Al-7%Si合金显微气孔形成的模拟研究 [J]. 金属学报, 2013, 49: 1032 | |
| [42] | Meidani H, Jacot A. Phase-field simulation of micropores constrained by the dendritic network during solidification [J]. Acta Mater., 2011, 59: 3032 |
| [43] | Zhang A, Guo Z P, Jiang B, et al. Multiphase and multiphysics modeling of dendrite growth and gas porosity evolution during solidification [J]. Acta Mater., 2021, 214: 117005 |
| [44] | Du L F, Wang L L, Zheng B, et al. Phase-field modeling of microstructure evolution during solidification in presence of gas bubble [J]. Comput. Mater. Sci., 2016, 114: 94 |
| [45] | Liu L, Pian S, Zhang Z, et al. A cellular automaton-lattice Boltzmann method for modeling growth and settlement of the dendrites for Al-4.7%Cu solidification [J]. Comput. Mater. Sci., 2018, 146: 9 |
| [46] | Wang L. Simulation of flow around cylinder with lattice Boltzmann method [J]. Acta Sci. Nat. Univ. Pekin., 2002, 38: 647 |
| 王 龙. 圆柱绕流的LBM模拟 [J]. 北京大学学报(自然科学版), 2002, 38: 647 | |
| [47] | Zhu M F, Stefanescu D M. Virtual front tracking model for the quantitative modeling of dendritic growth in solidification of alloys [J]. Acta Mater., 2007, 55: 1741 |
| [48] | Jelinek B, Eshraghi M, Felicelli S, et al. Large-scale parallel lattice Boltzmann-cellular automaton model of two-dimensional dendritic growth [J]. Comput. Phys. Commun., 2014, 185: 939 |
/
| 〈 |
|
〉 |