Research paper

Effect of Deformation Spheroidization Treatment on the Corrosion Behavior and Mechanical Properties of Pearlite Steel in Simulated Cargo Oil Tank Inner Substrate Environment

  • GUO Jiaming ,
  • CHEN Nan ,
  • HE Xiaoyan ,
  • WEI Jie ,
  • CHEN Huiqin ,
  • DONG Junhua ,
  • KE Wei
Expand
  • 1 School of Materials Science and Engineering, Taiyuan University of Science and Technology, Taiyuan 030024, China
    2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
WEI Jie, associate professor, Tel: 13478204310, E-mail: jwei@imr.ac.cn; CHEN Huiqin, professor, Tel: 18703417081, E-mail: chenhuiqin@tyust.edu.cn; DONG Junhua, professor, Tel: 13842056525, E-mail: jhdong@imr.ac.cn

Received date: 2024-05-08

  Revised date: 2024-07-30

  Online published: 2025-04-03

Supported by

National Natural Science Foundation of China(52373232)

Abstract

With the rapid growth of the international crude oil shipping industry, ensuring the safety of oil tanker transportation has become a critical concern. The cargo oil tank (COT), the primary structure for storing crude oil, is particularly susceptible to corrosion, with the inner bottom plate being a key site for failure and potential oil leakage. Low-alloy corrosion-resistant steel, mandated by the International Maritime Organization as an alternative to traditional anticorrosion coatings, faces challenges in China due to insufficient corrosion resistance, limiting its long-term applicability in COTs. Enhancing the intrinsic properties of ship plate steel while minimizing costs is therefore crucial for improving its corrosion resistance and mechanical performance. In the simulated acidic Cl- environment of a COT bottom plate, a micro-galvanic couple forms between ferrite and cementite in pearlite, with ferrite acting as the anodic phase and cementite as the cathodic phase. Over time, accumulated cementite thickens on the surface, increasing the anode/cathode area ratio and accelerating the corrosion rate due to intensified micro-galvanic effects. To mitigate this, a deformation spheroidization process was employed to refine the microstructure without additional alloying elements. By optimizing forging and heat treatment parameters, a tempered sorbitic microstructure was achieved in T8 steel. Microstructural evolution was characterized using SEM and EBSD, while mechanical properties were assessed through microhardness testing, tensile experiments, and fracture morphology analysis. Corrosion behavior before and after optimization was examined via mass loss tests, electrochemical analysis, and corrosion product characterization. The results indicate that spheroidization heat treatment enhances the strength, plasticity, and toughness of T8 steel through grain refinement, dislocation strengthening, and dispersion strengthening. The transformation of bulk layered cementite into fine-grained cementite effectively suppresses its accumulation on the surface during corrosion, mitigating the accelerating effect of micro-galvanic corrosion. Consequently, the corrosion resistance of T8 steel in the simulated COT environment was significantly improved. This study demonstrates a cost-effective approach to enhancing both the mechanical properties and corrosion resistance of ship plate steel through microstructural control, offering new insights for the development of corrosion-resistant materials for cargo oil tanks.

Cite this article

GUO Jiaming , CHEN Nan , HE Xiaoyan , WEI Jie , CHEN Huiqin , DONG Junhua , KE Wei . Effect of Deformation Spheroidization Treatment on the Corrosion Behavior and Mechanical Properties of Pearlite Steel in Simulated Cargo Oil Tank Inner Substrate Environment[J]. Acta Metall Sin, 2025 , 61(12) : 1858 -1872 . DOI: 10.11900/0412.1961.2024.00145

References

[1] Yi M S, Seo K C, Park J S. Study on the root causes and prevention of coating cracks in the cargo hold of a product carrier [J]. Metals, 2022, 12: 1688
[2] Sun F L, Cheng X Q, Li X G. Corrosion property of a new repair-free steel developed for bottom plate of cargo oil tanks [J]. Adv. Mater. Res., 2013, 690-693: 206
[3] Woloszyk K, Goerlandt F, Montewka J. A methodology for ultimate strength assessment of ship hull girder accounting for enhanced corrosion degradation modelling [J]. Mar. Struct., 2024, 93: 103530
[4] Yang J W, Han C L, Xu J, et al. Development of corrosion resistant steel for cargo oil tanks of crude oil tankers [J]. Corros. Sci. Prot. Technol., 2013, 25: 411
  杨建炜, 韩承良, 许 静 等. 原油油船货油舱耐腐蚀钢的开发 [J]. 腐蚀科学与防护技术, 2013, 25: 411
[5] Su H, Luo X B, Yang C F, et al. Effects of Cu on corrosion resistance of low alloyed steels in acid chloride media [J]. J. Iron Steel Res. Int., 2014, 21: 619
[6] Zhao Q H, Liu W, Zhao J, et al. Influence of chromium on the initial corrosion behavior of low alloy steels in the CO2-O2-H2S-SO2 wet-dry corrosion environment of cargo oil tankers [J]. Int. J. Min. Met. Mater., 2015, 22: 829
[7] Xu X Y, Tian L, Zhou Y, et al. Effect of Nb on corrosion behavior of inner bottom plate of cargo oil tankers [J]. J. Iron Steel Res. Int., 2019, 26: 611
[8] Ahmadi F, Ranji A R. Reliability assessment of ship hull girders considering pitting corrosion and crack [J]. Eng. Res. Express, 2024, 6: 015503
[9] Li H L, Chai F, Yang C F, et al. Corrosion behavior of low alloy steel for cargo oil tank under upper deck conditions [J]. J. Iron Steel Res. Int., 2018, 25: 120
[10] Zhou D. Effect of pH and NaCl concentration on corrosion behavior of steels for the inner bottom plate of cargo oil tank [D]. Ma'anshan: Anhui University of Technology, 2017
  周 鼎. pH值和NaCl浓度对货油舱内底板用钢腐蚀行为的影响 [D]. 马鞍山: 安徽工业大学, 2017
[11] Moslehyani A, Mobaraki M, Isloor A M, et al. Photoreactor-ultrafiltration hybrid system for oily bilge water photooxidation and separation from oil tanker [J]. React. Funct. Polym., 2016, 101: 28
[12] Guo L, Chen W L, Huang Q L, et al. An investigation into the factors and mechanisms underlying corrosion failure of B10 copper tubes in shipboard pipelines [J]. J. Phys.: Conf. Ser., 2023, 2639: 012049
[13] Wu H B, Liang J M, Tang D, et al. Influence of inclusion on corrosion behavior of E36 grade low-alloy steel in cargo oil tank bottom plate environment [J]. J. Iron Steel Res. Int., 2014, 21: 1016
[14] Hao X H, Dong J H, Mu X, et al. Influence of Sn and Mo on corrosion behavior of ferrite-pearlite steel in the simulated bottom plate environment of cargo oil tank [J]. J. Mater. Sci. Technol., 2019, 35: 799
[15] Wei J, Zhou Y T, Dong J H, et al. Effect of cementite spheroidization on improving corrosion resistance of pearlitic steel under simulated bottom plate environment of cargo oil tank [J]. Acta Mater., 2019, 6: 100316
[16] Liu H, Wei J, Dong J H, et al. Influence of cementite spheroidization on relieving the micro-galvanic effect of ferrite-pearlite steel in acidic chloride environment [J]. J. Mater. Sci. Technol., 2021, 61: 234
[17] ASTM. Standard test methods for tension testing of metallic materials [S]. West Conshohocken: ASTM International, 2008
[18] ISO. 8407:2009 Corrosion of metals and alloys—Removal of corrosion products from corrosion test specimens [S]. Switzerland: ISO, 2009
[19] Hao X H, Zhao X C, Chen H, et al. Comparative study on corrosion behaviors of ferrite-pearlite steel with dual-phase steel in the simulated bottom plate environment of cargo oil tanks [J]. J. Mater. Res. Technol., 2021, 12: 399
[20] Yuan Y, Wang J J, Wei J, et al. Cu alloying enables superior strength-ductility combination and high corrosion resistance of FeMnCoCr high entropy alloy [J]. J. Alloys Compd., 2024, 970: 172543
[21] Xue F, Wei X, Dong J H, et al. Effect of chloride ion on corrosion behavior of low carbon steel in 0.1 M NaHCO3 solution with different dissolved oxygen concentrations [J]. J. Mater. Sci. Technol., 2019, 35: 596
[22] Xue F, Wei X, Dong J H, et al. Effect of residual dissolved oxygen on the corrosion behavior of low carbon steel in 0.1 M NaHCO3 solution [J]. J. Mater. Sci. Technol., 2018, 34: 1349
[23] Lu H R, Shi H Y, Zhang H, et al. Enhanced yield strength by fine grain strengthening and TRIP/TWIP effect of metastable β-type Ti-4V-2Mo-2Fe alloy with high ductility [J]. Mater. Charact., 2024, 207: 113591
[24] Liu W J, Zhang C J, Guo P K, et al. Achieving enhanced mechanical properties in the Mg-Y-Zn-V alloy by refining grains and improving the morphology and distribution of LPSO via pre-forging and subsequent rolling [J]. J. Mater. Res. Technol., 2024, 29: 2493
[25] Ma C H, Ma X L, Pei X, et al. Effect of rolling reduction on the microstructure and mechanical properties of hot-rolled Mg-Li-Al-Ca alloys [J]. Mater. Today Commun., 2023, 37: 107469
[26] Kishore K, Sarkar K, Arora K S. Effect of alloying elements on microstructure, wear, and corrosion behavior of Fe-based hardfacing [J]. Weld. World, 2023, 67: 2463
[27] Cao C N. Principles of Electrochemistry of Corrosion [M]. 2nd Ed., Beijing: Chemical Industry Press, 2004: 34
  曹楚南. 腐蚀电化学原理 [M]. 第2版. 北京: 化学工业出版社, 2004: 34
Outlines

/