Research paper

Industrial Trial and Numerical Simulation of Inclusion Removal During Ladle Holding Period

  • DUAN Haojian ,
  • XIE Zhongyan ,
  • LI Zhankui ,
  • XU Xuejun ,
  • HUANG Caide ,
  • WEN Han ,
  • ZHANG Lifeng
Expand
  • 1 School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China
    2 Steelmaking Department, Shougang Jingtang United Iron and Steel Co. Ltd., Tangshan 063200, China
    3 School of Mechanical and Materials Engineering, North China University of Technology, Beijing 100144, China
ZHANG Lifeng, professor, Tel: (010)88801689, E-mail: zhanglifeng@ncut.edu.cn

Received date: 2024-09-03

  Revised date: 2024-10-15

  Online published: 2025-03-18

Supported by

National Key Research and Development Program of China(2023YFB3709900);National Nature Science Foundation of China(U22A20171);National Nature Science Foundation of China(52474341)

Abstract

In high-quality steel production, the final stage of secondary refining typically involves a ladle holding period to facilitate the flotation and removal of inclusions. This improves the cleanliness of the molten steel. This study investigated the evolution of inclusion number density and area fraction during the ladle holding period by conducting industrial trial on composition adjustment via the sealed argon bubbling refining process of steel plate hot rolled commercial (SPHC) low-carbon steel. The results indicated that inclusions would be removed by floating during the ladle holding period. The inclusion number density and area fraction decreased from 52.8 mm-2 and 279 × 10-6 at the start of the holding period to 22.1 mm-2 and 148 × 10-6 after 15 min, respectively. To clarify the movement and removal of inclusions, a numerical model was developed based on a discrete phase model, incorporating multiphase flow and heat transfer during the ladle holding period. The calculations revealed the following conclusions: (1) inclusions smaller than 10 μm primarily followed the molten steel's fluid flow, with removal rates of 51.6% and 66.7% after 900 and 1800 s, respectively; (2) inclusions with a diameter of 100 μm were influenced by the molten steel's fluid flow and their buoyancy, achieving removal rates of 70.2% and 89.2% after 900 and 1800 s, respectively; (3) inclusions with a diameter of 1000 μm primarily underwent self-floating, reaching an approximately 100% removal rate after 120 s.

Cite this article

DUAN Haojian , XIE Zhongyan , LI Zhankui , XU Xuejun , HUANG Caide , WEN Han , ZHANG Lifeng . Industrial Trial and Numerical Simulation of Inclusion Removal During Ladle Holding Period[J]. Acta Metall Sin, 2026 , 62(7) : 1288 -1296 . DOI: 10.11900/0412.1961.2024.00304

References

[1] Zhang L F, Thomas B G. State of the art in evaluation and control of steel cleanliness [J]. ISIJ Int., 2003, 43: 271
[2] Zhang L F. Nucleation, growth, transport, and entrapment of inclusions during steel casting [J]. JOM, 2013, 65: 1138
[3] Zhang L F, Ren Q, Duan H J, et al. Modelling of non-metallic inclusions in steel [J]. Min. Proc. Ext. Metall., 2020, 129: 184
[4] Zhang L F. Non-Metallic Inclusions in Steel: Fundmentals [M]. Beijing: Metallurgical Industry Press, 2019: 1
  张立峰. 钢中非金属夹杂物 [M]. 北京: 冶金工业出版社, 2019: 1
[5] Zhang L F. Non-Metallic Inclusions in Steel: Industrial Practice [M]. Beijing: Metallurgical Industry Press, 2019: 1
  张立峰. 钢中非金属夹杂物: 工业实践 [M]. 北京: 冶金工业出版社, 2019: 1
[6] Ilegbusi O J, Szekely J. Melt stratification in ladles [J]. ISIJ Int., 1987, 27: 563
[7] Austin P R, Camplin J M, Herbertson J, et al. Mathematical modelling of thermal stratification and drainage of steel ladles [J]. ISIJ Int., 1992, 32: 196
[8] Chakraborty S, Sahai Y. Effect of holding time and surface cover in ladles on liquid steel flow in continuous casting tundishes [J]. Metall. Trans., 1992, 23B: 153
[9] Chakraborty S, Sahai Y. Effect of slag cover on heat loss and liquid steel flow in ladles before and during teeming to a continuous casting tundish [J]. Metall. Trans., 1992, 23B: 135
[10] Olika B, Pan Y H, Bj?rkman B, et al. Numerical simulation and industrial investigation on the melt stratification phenomena in ladles holding molten steel [J]. Scand. J. of Metall., 1996, 25(1): 18
[11] Grip C E, Jonsson L, J?nsson P, et al. Numerical prediction and experimental verification of thermal stratification during holding in pilot plant and production ladles [J]. ISIJ Int., 1999, 39: 715
[12] Xia J L, Ahokainen T. Transient flow and heat transfer in a steelmaking ladle during the holding period [J]. Metall. Mater. Trans., 2001, 32B: 733
[13] Xia J L, Ahokainen T. Thermal stratification in a steel ladle [J]. Can. Metall. Quart., 2001, 40: 479
[14] Pan Y H, Bj?rkman B. Numerical analysis on the similarity between steel ladles and hot-water models regarding natural convection phenomena [J]. ISIJ Int., 2002, 42: 53
[15] Pan Y H, Bj?rkman B. Physical and mathematical modelling of thermal stratification phenomena in steel ladles [J]. ISIJ Int., 2002, 42: 614
[16] Pan Y H, Grip C E, Bj?rkman B. Numerical studies on the parameters influencing steel ladle heat loss rate, thermal stratification during holding and steel stream temperature during teeming [J]. Scand. J. Metall., 2003, 32: 71
[17] Zhang C J, Wang A, Li Q X, et al. Analysis of temperture drop during 80 t ladle standing [J]. Henan Metall., 2013, 21: 20
  张彩军, 王 昂, 李庆效 等. 80 t钢包静置过程温降分析 [J]. 河南冶金, 2013, 21: 20
[18] Lu B Y, Meng X N, Zhu M Y. Numerical analysis for the heat transfer behavior of steel ladle as the thermoelectric waste-heat source [J]. Catal. Today, 2018, 318: 180
[19] Duan H J, Ren Y, Zhang L F. Fluid flow, thermal stratification, and inclusion motion during holding period in steel ladles [J]. Metall. Mater. Trans., 2019, 50B: 1476
[20] Gopala Krishna E D, Shamshoddin S, Ande R. Numerical simulation of fluid flow and heat transfer in a ductile iron ladle during holding and teeming [J]. J. Thermal. Sci. Eng. Appl., 2019, 11: 011007
[21] Yan H, Conejo A N, Zhang H, et al. Numerical simulation of heat transfer during ladle holding period [J]. Cont. Cast., 2022, (1): 31
  颜 晗, Conejo A N, 张 晗 等. 钢包静置过程中传热现象的数值模拟 [J]. 连铸, 2022, (1): 31
[22] Huang C D, Duan H J, Zhang L F. Modeling of motion of inclusions in argon-stirred steel ladles [J]. Steel Res. Int., 2024, 95: 2300537
[23] Morsi S A, Alexander A J. An investigation of particle trajectories in two-phase flow systems [J]. J. Fluid Mech., 1972, 55: 193
[24] Pearson K. The problem of the random walk [J]. Nature, 1905, 72: 294
[25] Duan H J, Huang C D, Zhang L F. Numerical simulation of transient flow and heat transfer in a steel ladle during holding period [J]. Metall. Mater. Trans., 2024, 55B: 2273
[26] Duan H J, Ren Y, Zhang L F. Effects of interphase forces on fluid flow in gas-stirred steel ladles using the Eulerian-Lagrangian multiphase approach [J]. JOM, 2018, 70: 2128
[27] Duan H J, Zhang L F, Thomas B G, et al. Fluid flow, dissolution, and mixing phenomena in argon-stirred steel ladles [J]. Metall. Mater. Trans., 2018, 49B: 2722
Outlines

/