Effect of Ultrasonic Power on the Microstructure and Mechanical Property of W90/Sn/Mg Joint
Received date: 2024-05-13
Revised date: 2025-01-07
Online published: 2025-03-17
Supported by
National Natural Science Foundation of China(52105330);National Natural Science Foundation of China(52175307);Natural Science Foundation of Shandong Province(ZR2023JQ021)
Tungsten alloy, known for its high hardness, thermal stability, and excellent nuclear radiation shielding performance, is a critical material for radiation shielding applications. It is widely used in aerospace, national defense, and medical fields. However, tungsten alloy has drawbacks such as high density and processing difficulty, which limit its applicability in high-efficiency, miniaturized, and lightweight designs, particularly in nuclear medical treatment and nuclear-powered flight devices. A double-layered W/Mg structure is expected to serve as a next-generation nuclear radiation shielding material. Due to the significant differences in melting temperatures and coefficients of thermal expansion between W and Mg, conventional soldering methods are ineffective for joining them. In this study, a W90 tungsten heavy alloy and AZ31B magnesium alloy were successfully bonded using an ultrasonic-assisted soldering method with pure Sn. The bonding temperature was 250 oC, and the ultrasonic duration was 4 s. The interfacial microstructure of the W90/Sn/Mg joint under varying ultrasonic power levels was analyzed using SEM and EDS. Additionally, the shear strength of the joint was tested to assess the impact of ultrasonic power on interfacial bonding and mechanical performance. The results indicated that effective bonding formed at the W90/Sn interface, with Ni3Sn4 compounds appearing between the (Ni, Fe) matrix and Sn. The seam consisted of a β-Sn matrix phase and Mg2Sn compounds, with an Mg2Sn layer forming on Mg/Sn interface. As ultrasonic power increased, joint width decreased while the Mg2Sn layer thickness increased. The shear strength of the joint initially increased with ultrasonic power but later decreased. At ultrasonic power levels of 100 and 150 W, the joint strength reached a maximum of 10.5 MPa, with failure occurring at the W90/Sn interface. When ultrasonic power increased to 200 W, joint strength declined, and fracture occurred at the Mg2Sn layer. The acoustic pressure distribution of liquid Sn during the ultrasonic-assisted soldering process was simulated. During a single ultrasonic cycle, the acoustic pressure of liquid Sn oscillated periodically from negative to positive and back to negative values. The maximum acoustic pressure was observed at the center of the liquid Sn, gradually decreasing toward the edges. The cavitation effect, driven by collapsing bubbles, generated high temperatures, high pressures, micro-jets, and shock waves, as explained through theoretical calculations. Based on the Keller-Miksis equation, as ultrasonic power increased, the ratio of the cavitation bubble radius to its initial radius increased from 16.3 to 47.7, with collapse velocities ranging from 3262 m/s to 6985 m/s. According to the Noltingk-Neppiras theory, as acoustic pressure increased, cavitation-induced temperatures rose from 14614 K to 24989 K, while pressure increased from 1.08 × 105 MPa to 9.45 × 105 MPa. The generated temperature and pressure were sufficient to break the Mg alloy’s oxide film and promote interfacial reactions.
ZHANG Xudong , FU Wei , SONG Xiaoguo , SONG Na , SUN Hao , HU Shengpeng . Effect of Ultrasonic Power on the Microstructure and Mechanical Property of W90/Sn/Mg Joint[J]. Acta Metall Sin, 2026 , 62(8) : 1376 -1384 . DOI: 10.11900/0412.1961.2024.00158
| [1] | Huangfu H, Wang Z L, Liu Y L, et al. A first principles investigation of W1 - x Ir x alloys: Structural, electronic, mechanical, and thermal properties [J]. Acta Metall. Sin., 2022, 58: 231 |
| 皇甫顥, 王子龙, 刘永利 等. W1 - x Ir x 固溶合金几何结构、电子结构、力学和热力学性能的第一性原理计算 [J]. 金属学报, 2022, 58: 231 | |
| [2] | Xu Z W, Bai J X, Qian L M. Surface microstructural alterations and grain refinement mechanisms of tungsten heavy alloys by thermo-mechanical coupling: A laser-assisted milling case [J]. J. Manuf. Process., 2023, 108: 359 |
| [3] | Li J R, Xie D S, Zhang D D, et al. Microstructure evolution mechanism of new low-alloyed high-strength Mg-0.2Ce-0.2Ca alloy during extrusion [J]. Acta Metall. Sin., 2023, 59: 1087 |
| 李景仁, 谢东升, 张栋栋 等. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理 [J]. 金属学报, 2023, 59: 1087 | |
| [4] | Fu W, Song X G, Long L, et al. Interfacial microstructure and mechanical properties of indirect brazed graphite/copper joint [J]. Acta Metall. Sin., 2016, 52: 734 |
| 付 伟, 宋晓国, 龙 隆 等. 石墨/紫铜间接钎焊接头的界面组织及力学性能 [J]. 金属学报, 2016, 52: 734 | |
| [5] | Song X G, Li J X, Fu W, et al. Microstructure and properties of brazed W-W joints by Ti-35Ni alloy [J]. J. Mater. Eng. Perform., 2022, 31: 6827 |
| [6] | Xia C Z, Sun W W, Zhou Y, et al. Effect of Ni-Ti filler on brazed W-Cu/18-8 joints [J]. J. Mater. Process. Technol., 2018, 259: 15 |
| [7] | Xu Y X, Qiu X M, Wang S Y, et al. Brazing of tungsten based alloy/superalloy GH907 with lean Cu-Ag based fillers: Wetting, interfaces and performance evaluation [J]. Mater. Lett., 2021, 284: 128982 |
| [8] | Shang J L, Yan J Z, Li N. Brazing W and Fe-Ni-Co alloy using Ag-28Cu and Ag-27Cu-3.5Ti fillers [J]. J. Alloys Compd., 2014, 611: 91 |
| [9] | Wang Z, Qu W Q, Zhuang H S. Development of a Mg-Al filler metal for brazing magnesium alloy AZ31B [J]. Mater. Lett., 2016, 182: 75 |
| [10] | Ma L, Qiao P X, Long W M, et al. Interface characteristics and mechanical properties of the induction brazed joint of magnesium alloy AZ31B with an Al-based filler metal [J]. Mater. Des., 2012, 37: 465 |
| [11] | Ma L, He D Y, Li X Y, et al. Microstructure and mechanical properties of magnesium alloy AZ31B brazed joint using a Zn-Mg-Al filler metal [J]. J. Mater. Sci. Technol., 2010, 26: 743 |
| [12] | Xu Z W, Li Z W, Li J Q, et al. Control Al/Mg intermetallic compound formation during ultrasonic-assisted soldering Mg to Al [J]. Ultrason. Sonochem., 2018, 46: 79 |
| [13] | Wang Z, Wang H Y, Liu L M. Study on low temperature brazing of magnesium alloy to aluminum alloy using Sn-xZn solders [J]. Mater. Des., 2012, 39: 14 |
| [14] | Dai X Y, Zhang H T, Wang B, et al. Improving weld strength of arc-assisted ultrasonic seam welded Mg/Al joint with Sn interlayer [J]. Mater. Des., 2016, 98: 262 |
| [15] | Jiang G L, Zhou X. Molecular dynamics simulation on the interfacial behavior of Mg-Zn-Al/Mg brazing with ultrasonic assistance [J]. Acta Metall. Sin., 2026, 62: 372 |
| 江国龙, 周 霞. 超声辅助下Mg-Zn-Al/Mg钎焊界面行为的分子动力学模拟 [J]. 金属学报, 2026, 62: 372 | |
| [16] | Dong H J, Wei S J, Li Z L, et al. In-situ formation of amorphous Al2O3 interphase during ultrasonic-assisted soldering process of ZrO2 ceramic and 1060Al using Sn filler at low temperature [J]. Surf. Interfaces, 2023, 36: 102491 |
| [17] | Dong H J, Wei S J, Li Z L, et al. Room-temperature direct bonding of ZrO2 ceramic and SiCP/Al composite using ultrasonic waves [J]. Ceram. Int., 2023, 49: 431 |
| [18] | Zhang C G, Ji H J, Xu H B, et al. Interfacial microstructure and mechanical properties of ultrasonic-assisted brazing joints between Ti-6Al-4V and ZrO2 [J]. Ceram. Int., 2020, 46: 7733 |
| [19] | Ma X J, Huang B, Zhao X, et al. Comparisons of spark-charge bubble dynamics near the elastic and rigid boundaries [J]. Ultrason. Sonochem., 2018, 43: 80 |
| [20] | Shen Y, Yasui K, Sun Z C, et al. Study on the spatial distribution of the liquid temperature near a cavitation bubble wall [J]. Ultrason. Sonochem., 2016, 29: 394 |
| [21] | Brujan E A. Shock wave emission and cavitation bubble dynamics by femtosecond optical breakdown in polymer solutions [J]. Ultrason. Sonochem., 2019, 58: 104694 |
| [22] | Kim K S, Kwon S H. Comfort and quality of life of cancer patients [J]. Asian Nurs. Res., 2007, 1: 125 |
| [23] | Suslick K S, Hammerton D A, Cline R E. Sonochemical hot spot [J]. J. Am. Chem. Soc., 1986, 108: 5641 |
| [24] | Li Z W. Cavitation dynamics and its application during ultrasonic-assisted soldering [D]. Harbin: Harbin Institute of Technology, 2021 |
| 李政玮. 超声波钎焊过程中声空化动力学及其应用研究 [D]. 哈尔滨: 哈尔滨工业大学, 2021 | |
| [25] | Li Z W, Xu Z W, He P, et al. Dependence of wetting on cavitation during the spreading of a filler droplet on the ultrasonically agitated Al substrate [J]. Ultrason. Sonochem., 2022, 82: 105893 |
| [26] | Li G K, Zhao Y, Li J Q, et al. Evolution behavior of cavitation bubble in pure Sn liquid medium with narrow gap under low-amplitude ultrasound [J]. Ultrason. Sonochem., 2023, 99: 106567 |
| [27] | Wu B Z. Research on interfacial bonding mechanism and process of ultrasonic assisted active soldering SiC ceramic [D]. Harbin: Harbin Institute of Technology, 2019 |
| 吴炳智. SiC陶瓷超声辅助活性软钎焊界面结合机理及工艺研究 [D]. 哈尔滨: 哈尔滨工业大学, 2019 | |
| [28] | Brujan E A, Ikeda T, Matsumoto Y. On the pressure of cavitation bubbles [J]. Exp. Therm. Fluid Sci., 2008, 32: 1188 |
| [29] | Priyadarshi A, Khavari M, Subroto T, et al. On the governing fragmentation mechanism of primary intermetallics by induced cavitation [J]. Ultrason. Sonochem., 2021, 70: 105260 |
/
| 〈 |
|
〉 |