Research paper

Effect of Zr Content on Recrystallization Behavior and Mechanical Properties of Al-Mg-Si Cast-Rolled Sheet

  • SUN Yuchong ,
  • LIU Zhimin ,
  • XU Zhen ,
  • TIAN Shuangyong ,
  • TIAN Shuang
Expand
  • College of Materials and Metallurgy, University of Science and Technology Liaoning, Anshan 114051, China
XU Zhen, professor, Tel: 15904924772, E-mail: ustlxuzhen@ustl.edu.cn

Received date: 2024-04-08

  Revised date: 2024-11-15

  Online published: 2025-02-14

Supported by

National Natural Science Foundation of China(52104377)

Abstract

Twin roll casting is a short-process, high-energy-efficiency method for producing aluminum alloy sheets. During the forming process of cast-rolled aluminum alloy sheets, defects such as segregation, coarse secondary phases, and poor properties may occur owing to the quenching effect of the rolling mill rolls. Microalloying can effectively mitigate these defects and enhance the mechanical properties of aluminum alloy sheets produced by cast rolling. In the aluminum alloy twin roll casting process, regulating the recrystallization behavior and improving the microstructure by promoting or suppressing the particle-stimulated nucleation (PSN) effect is critical for producing high-quality cast-rolled sheets. This study prepared six Al-Mg-Si cast-rolled aluminum alloy sheets with varying Zr contents to investigate the evolution of their microstructure and properties, aiming to reveal the influence of Zr content on the recrystallization behavior and mechanical properties of Al-Mg-Si cast-rolled aluminum alloy sheets from the perspective of PSN. The results demonstrated that as the Zr content increased, the grain size initially increased, subsequently decreased, and then increased again. The Zr element was observed to combine with Al to form nano-sized Al3Zr precipitates with L12 structure. These precipitates effectively inhibited the recrystallization behavior associated with PSN in cast-rolled sheets and promoted grain fibrosis. Specifically, when the Zr content was 0.4% (mass fraction), the degree of grain fibrosis reached its maximum; however, with a Zr content of 0.6%, the inhibitory effect of Zr on grain recrystallization was reduced. At this concentration, the coarse D023-structured Al3Zr primary phase emerged, exacerbating the PSN effect and increasing the degree of recrystallization in the cast-rolled sheet. Furthermore, as the Zr content increased in the cast-rolled sheet, the size and volume fraction of the Fe-rich phase exhibited a trend of first increasing, then decreasing, and subsequently increasing again. Notably, when the Zr content was 0.3%, the comprehensive mechanical properties of the cast-rolled sheet were optimal. The tensile fracture surface exhibited ductile fracture characteristics, and the Fe-rich phase distribution in the sheet was dispersed. The tensile strength, yield strength, and elongation were measured to be 226.91 MPa, 104.81 MPa, and 15.05%, respectively.

Cite this article

SUN Yuchong , LIU Zhimin , XU Zhen , TIAN Shuangyong , TIAN Shuang . Effect of Zr Content on Recrystallization Behavior and Mechanical Properties of Al-Mg-Si Cast-Rolled Sheet[J]. Acta Metall Sin, 2026 , 62(3) : 421 -430 . DOI: 10.11900/0412.1961.2024.00102

References

[1] Arnoldt A, Semmelrock L, Soukup D, et al. Analysis of second phase particles in metals using deep learning: Segmentation of nanoscale dispersoids in 6xxx series aluminum alloys (Al-Mg-Si) [J]. Mater. Charact., 2022, 191: 112138
[2] Jin H M, Tie D, Guan R G. Precipitation behavior during re-aging of Al-Mg-Si-Cu alloy [J]. Mater. Des., 2022, 220: 110883
[3] Wang X F, Liu H, Tang X B, et al. Influence of asymmetric rolling on the microstructure, texture evolution and mechanical properties of Al-Mg-Si alloy [J]. Mater. Sci. Eng., 2022, A844: 143154
[4] Wu X, Guan Z P, Yang Z Z, et al. Effect of Cu content on central-segregation composition and mechanical properties of Al-Mg-Si alloys produced by twin-roll casting [J]. Mater. Sci. Eng., 2023, A869: 144782
[5] Zhang S Y, Wang X, Mo Y T, et al. Towards relieving center segregation in twin-roll cast Al-Mg-Si-Cu strips by controlling the thermal-mechanical process [J]. J. Mater. Sci. Technol., 2023, 148: 31
[6] Kuang J, Zhao X L, Zhang Y Q, et al. Impact of thermal exposure on the microstructure and mechanical properties of a twin-roll cast Al-Mn-Fe-Si strip [J]. J. Mater. Sci. Technol., 2022, 107: 183
[7] Liu X, Zhao Q L, Ji Z W, et al. Effectively mitigated macro-segregation and improved tensile properties of twin-roll casting Al-Cu strips via the addition of TiC nanoparticles [J]. J. Mater. Process. Technol., 2021, 296: 117200
[8] Cann J L, De Luca A, Dunand D C, et al. Sustainability through alloy design: Challenges and opportunities [J]. Prog. Mater. Sci., 2021, 117: 100722
[9] Sun Y C, Zhang B, Xu Z, et al. Microstructure evolution and recrystallization behavior of hot rolled AA6061 twin-roll casting plate with different manganese contents [J]. J. Alloys Compd., 2022, 918: 165618
[10] Wu H L, Chen Y Q, Lin L, et al. Research progress on effects of Sc and Zr microalloying on microstructure and properties of Al-Zn-Mg-(Cu) alloys [J]. Chin. J. Nonferrous Met., 2023, 33: 3689
  巫海亮, 陈宇强, 林 林 等. Sc和Zr微合金化对Al-Zn-Mg-(Cu)合金微观组织和性能影响的研究进展 [J]. 中国有色金属学报, 2023, 33: 3689
[11] Zhang Y X, Zhao H D, Liu F. Microstructure characteristics and mechanical properties improvement of gravity cast Al-7Si-0.4Mg alloys with Zr additions [J]. Mater. Charact. 2021, 176: 111117
[12] Pan S W, Qian F, Li C N, et al. Synergistic strengthening by nano-sized α-Al(Mn, Fe)Si and Al3Zr dispersoids in a heat-resistant Al-Mn-Fe-Si-Zr alloy [J]. Mater. Sci. Eng., 2021, A819: 141460
[13] Zhang M X, Wang C, Zhang S Y, et al. Enhanced aging precipitation behavior and mechanical properties of 6022 Al-Mg-Si alloy with Zr addition [J]. Mater. Sci. Eng., 2022, A840: 142957
[14] Wang Y T, Li J, Xia X Z, et al. A novel Al-Cr-Sc-Zr alloy additively manufactured via laser directed energy deposition: Microstructure, phase analysis and mechanical properties [J]. J. Mater. Process. Technol., 2023, 322: 118204
[15] Qian W, Kai X Z, Tao R, et al. Microstructure evolution and high-temperature performances of AA6111 alloy strengthened by Sc, Zr co-microalloying [J]. Mater. Sci. Eng., 2023, A887: 145788
[16] Wang Y F, Lin X, Zhao Y F, et al. Microstructure and strengthening mechanisms of Zr-modified Al-Cu-Mg alloy processed by selective laser melting [J]. Mater. Sci. Eng., 2023, A870: 144874
[17] Fang H C, Luo F H, Chen K H. Effect of intermetallic phases and recrystallization on the corrosion and fracture behavior of an Al-Zn-Mg-Cu-Zr-Yb-Cr alloy [J]. Mater. Sci. Eng., 2017, A684: 480
[18] Xia P, Wang S C, Huang H L, et al. Effect of Sc and Zr additions on recrystallization behavior and intergranular corrosion resistance of Al-Zn-Mg-Cu alloys [J]. Materials, 2021, 14: 5516
[19] Liu S D, Chen J C, Chai W R, et al. Effects of combined additions of Mn and Zr on dispersoid formation and recrystallization behavior in Al-Zn-Mg alloys [J]. Metall. Mater. Trans., 2019, 50A: 4877
[20] Moghanaki S K, Kazeminezhad M, Logé R. Heating rate effect on particle stimulated nucleation and grains structure during non-isothermal annealing of multi-directionally forged solution treated AA2024 [J]. Mater. Charact., 2017, 127: 317
[21] Ghayoumabadi M E, Mochugovskiy A G, Tabachkova N Y, et al. The influence of minor additions of Y, Sc, and Zr on the microstructural evolution, superplastic behavior, and mechanical properties of AA6013 alloy [J]. J. Alloys Compd., 2022, 900: 163477
[22] Pan S W. Precipitation behavior and dispersion-strengthening mechanism of nano-sized dispersoids in zirconium-containing aluminium alloys [D]. Beijing: University of Science and Technology Beijing, 2022
  潘士伟. 纳米弥散相在含锆铝合金中的析出行为与强化机制 [D]. 北京: 北京科技大学, 2022
[23] Pan S W, Chen X H, Zhou X L, et al. Micro-alloying effect of Er and Zr on microstructural evolution and yield strength of Al-3Cu (wt.%) binary alloys [J]. Mater. Sci. Eng., 2020, A790: 139391
[24] Wang Z P, Xiao H Y, Chen W, et al. New insight into precipitation of Al3Zr and correlative effect on recrystallization behavior in a rapidly-solidified Al-Zn-Mg-Cu-Zr alloy [J]. Mater. Charact., 2022, 191: 112142
[25] Yao Z W, Liu F Z, Ling J Q, et al. Effect of floating grains on the deformed microstructure of Mn- and Cr-containing Al-Mg-Si-Cu alloys [J]. Mater. Lett., 2023, 330: 133393
[26] Kolahdooz A, Dehkordi S A. Effects of important parameters in the production of Al-A356 alloy by semi-solid forming process [J]. J. Mater. Res. Technol., 2019, 8: 189
[27] Li L J, Li R G, Zhang J J, et al. Effects of cryorolling on properties and precipitation behavior of a high-strength and high-conductivity Cu-1Cr-0.2Zr-0.25Nb alloy [J]. Acta Metall Sin, 2024, 60: 405
  李龙健, 李仁庚, 张家郡 等. 低温轧制对高强高导Cu-1Cr-0.2Zr-0.25Nb合金性能及析出行为的影响 [J]. 金属学报, 2024, 60: 405
[28] Feng X M, Wang Z L, Jiang L, et al. Simultaneous enhancement in mechanical and corrosion properties of Al-Mg-Si alloys using machine learning [J]. J. Mater. Sci. Technol., 2023, 167: 1
[29] Wang Z W, Lu W J, Zhao H, et al. Ultrastrong lightweight compositionally complex steels via dual-nanoprecipitation [J]. Sci. Adv., 2020, 6: eaba9543
[30] Niu F J, Wu C L, Wu J, et al. Study on strengthening mechanism of Al-3.0Cu-1.8Mg-0.5Si alloy processed by thermo-mechanical treatment [J]. J. Hunan Univ. (Nat. Sci.), 2022, 49(6): 192
  牛凤姣, 伍翠兰, 武 静 等. 形变时效态Al-3.0Cu-1.8Mg-0.5Si合金的强化机制研究 [J]. 湖南大学学报(自然科学版), 2022, 49(6): 192