The manufacture of metallic components involves alloy design, raw material preparation, melting, ingot/slab casting, hot forging or rolling, heat treatment, and precision cold processing etc. Consequently, research on the entire life cycle of metal production and application is imperative. Only by integrating the complete life cycle of the technological chain can the properties of metals be fully and appropriately utilized. Previous research has primarily focused on breakthroughs at individual “points”, often neglecting the “chain”. This has led to a “chain break” phenomenon in the processing of metal materials and components, resulting in high-end components that are unqualified, unstable, unreliable, or heavily dependent on imports. To address these issues, this study takes the research on the 8-meter-diameter main bearing of a shield tunneling machine as an example. It adopts novel V, B, and rare earth co-alloying in bearing steel for bearing rings, leveraging high-purity and high-homogeneity bearing steel production, as well as precision machining of high-performance bearing components. The study elucidates key technologies and their correlations throughout the bearing manufacturing process, with a particular focus on heat treatment technology that linking bearing materials to components and precision machining technology for large rollers. Through the development of whole-chain technologies, the main bearing for the shield tunneling machine was successfully manufactured. Building upon this research, a new concept of metal chain creation is proposed. This concept begins with alloy design and connects the entire chain of raw material preparation, melting, ingot/slab casting, hot forging or rolling, heat treatment, and precision cold processing, assembly manufacturing, evaluation, and application test. By identifying and manipulating critical data at each stage of the process, iterative optimization is achieved. This approach integrates the technological chain, fosters an innovation chain, connects the industrial chain, and realizes controllable manufacturing of metal materials and high-end components.
Key words: metal chain; alloy design; hot working; cold working; creation
LI Dianzhong , HU Xiaoqiang , WANG Pei . Metal Chain Creation[J]. Acta Metall Sin, 2025 , 61(2) : 203 -210 . DOI: 10.11900/0412.1961.2024.00412
| 1 | Wang F, Song M, Elkot M N, et al. Shearing brittle intermetallics enhances cryogenic strength and ductility of steels [J]. Science, 2024, 384: 1017 |
| 2 | Qu Z, Zhang Z J, Liu R, et al. High fatigue resistance in a titanium alloy via near-void-free 3D printing [J]. Nature, 2024, 626: 999 |
| 3 | Zhang S J, To S, Wang S J, et al. A review of surface roughness generation in ultra-precision machining [J]. Int. J. Mach. Tools Manuf., 2015, 91:76 |
| 4 | Zhu W L, Beaucamp A. Compliant grinding and polishing: A review [J]. Int. J. Mach. Tools Manuf., 2020, 158: 103634 |
| 5 | Xing J N. Influence of heat treatment process on microstructure and properties of large-scale ring components [D]. Shenyang: Shenyang Jianzhu University, 2023 |
| 邢嘉妮. 热处理工艺对大型环状构件组织与性能的影响 [D]. 沈阳: 沈阳建筑大学, 2023 | |
| 6 | Liang Y X, Cai X, Zheng L G, et al. Effect of secondary tempering on microstructure and properties of 42CrMo4M steel [J]. Trans. Mater. Heat Treat. 2023, 44(8): 106 |
| 梁雅鑫, 蔡 欣, 郑雷刚 等. 二次回火对42CrMo4M组织性能的影响 [J]. 材料热处理学报. 2023, 44(8): 106 | |
| 7 | Liang Y X. Development and application of secondary tempering process for large toroidal components in 42CrMo4M [D]. Shenyang: University of Science and Technology of China, 2023 |
| 梁雅鑫. 大型环形构件用42CrMo4M钢二次回火工艺开发与应用 [D]. 沈阳: 中国科学技术大学, 2023 | |
| 8 | Hu X Q, Feng S B, Gao Y. “ Research and development of main bearings for super large diameter shield machines” Technology report of Strategic Priority Research Program of the Chinese Academy of Sciences [R]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2023 |
| 胡小强, 封少波, 高 洋. “超大直径盾构机用主轴承研制”中国科学院战略性先导科技专项科技报告 [R]. 沈阳: 中国科学院金属研究所, 2023 | |
| 9 | Hu X Q, Li D Z. Research and application of 42CrMo4M steel for main bearing large ring of shield machine [R]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2024 |
| 胡小强, 李殿中. 盾构机主轴承大型套圈用42CrMo4M钢研发与应用 [R]. 沈阳: 中国科学院金属研究所, 2024 | |
| 10 | Li D Z, Chen X Q, Fu P X, et al. Inclusion fotation-driven channel segregation in solidifying steels [J]. Nat. Commun., 2014, 5: 5572 |
| 11 | Cao Y F, Chen Y, Li D Z. Formation mechanism of channel segregation in carbon steels by inclusion flotation: X-ray microtomography characterization and multi-phase flow modeling [J]. Acta. Mater., 2016, 107: 325 |
| 12 | Li D Z, Wang P, Chen X Q, et al. Low-oxygen rare earth steels [J]. Nat. Mater., 2022, 21: 1137 |
| 13 | Li Y H, Jiang Z H, Wang P, et al. Effect of a modified quenching on impact toughness of 52100 bearing steels [J]. J. Mater. Sci. Technol., 2023, 160: 96 |
| 14 | Liu T Y, Xia Y F, Li R H, et al. The combined effects of carbides and martensite blocks heterogeneity on the fatigue life scatter in bearing steel [J]. Mater. Sci. Eng., 2024, A915: 147277 |
| 15 | Li Y H, Jiang Z H, Li L L, et al. Wear behavior and damage characterization for AISI 52100 bearing steels: Effect of hardness and spherical carbides [J]. J. Mater. Res. Technol., 2024, 30: 8359 |
| 16 | Li Y H, Jiang Z H, Wang P, et al. Effect of austenitizing temperature on isothermal quenching microstructure and mechanical properties of 52100 bearing steel [J]. Mater. Sci. Eng., 2024, A892: 146051 |
| 17 | Li Z, Fu Z H, Yang C Y, et al. Improving the microstructure and impact toughness of bainite/martensite bearing steel by rare earth treatment [J]. Metall. Mater. Trans., 2024, 55: 4965 |
| 18 | Li D Z, Wang P. Tailoring microstructures of metals [J]. Acta. Metall. Sin., 2023, 59: 447 |
| 李殿中, 王 培. 金属材料的组织定制 [J]. 金属学报, 2023, 59: 447 | |
| 19 | Xing J N, Cai X, Zheng L G, et al. Effect of quenching and tempering temperature on microstructure and mechanical properties of a new medium carbon alloy steel 42CrMo4M [J]. Trans. Mater. Heat Treat., 2022, 43(5): 124 |
| 邢嘉倪, 蔡 欣, 郑雷刚 等. 淬火及回火温度对新型中碳合金钢42CrMo4M组织性能的影响 [J]. 材料热处理学报 2022, 43(5):124 | |
| 20 | Wei S T, Wu C J, Zheng L G, et al. Effect of surface quenching process on hardened layer of 42CrMo steel for large bearing ring [J]. Heat Treat. Met., 2022, 47(10): 218 |
| 魏世同, 吴长江, 郑雷刚 等. 表面淬火工艺对大型轴承套圈用42CrMo钢淬硬层的影响 [J]. 金属热处理, 2022, 47(10): 218 | |
| 21 | Wu C J. Study on surface quenching technology and properties of thick and large section 42CrMo steel [D]. Shenyang: Shenyang University of Technology, 2023 |
| 吴长江. 厚大断面42CrMo钢表淬工艺与性能研究 [D]. 沈阳: 沈阳工业大学, 2023 | |
| 22 | Feng S B, Wu C J, Yuan L, et al. Research and application of surface quenching process for rings of main slewing bearing used in shield tunneling machines [J]. Bearing, 2024, 11: 121 |
| 封少波, 吴长江, 袁 麟 等. 盾构机主轴承套圈表面淬火工艺研究及应用 [J]. 轴承, 2024, 11: 121 | |
| 23 | Hu X Q, Feng S B, Gao Y, et al. Review materials of the main bearing with a diameter of 8.01 m for super large shield [R]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2023 |
| 胡小强, 封少波, 高 洋 等. 超大直径盾构机用Ф8.01米主轴承评审材料 [R]. 沈阳: 中国科学院金属研究所, 2023 | |
| 24 | Hu X Q. Final research project report on bearing steels with medium carbon content and their heat-treatment processes supported by the Strategic Priority Research Program of the Chinese Academy of Sciences [R]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2024 |
| 胡小强. 中碳轴承钢材料与热处理先导专项课题实施绩效报告 [R]. 沈阳: 中国科学院金属研究所, 2024 | |
| 25 | Liu S, Yan Y, Wang B, et al. Effect of heat treatment on strengthening and toughening mechanism of 42CrMoVRE steel [J]. Trans. Mater. Heat Treat., 2023, 44(6): 90 |
| 刘 帅, 颜 莹, 王 斌 等. 热处理对42CrMoVRE钢强韧化机制的影响 [J]. 材料热处理学报, 2023, 44(6): 90 | |
| 26 | Qian Q H, Hu X Q, Li S C, et al. Recent advances in key technologies of shield tunnel engineering in China [J]. Tunnel Construction, 2024, 44(5): 897 |
| 钱七虎, 胡小强, 李树忱 等. 中国盾构隧道工程关键技术的新进展综述 [J]. 隧道建设(中英文), 2024, 44(5): 897 | |
| 27 | Hu X Q. Logarithmic convexity design and machining of large rollers [R]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2021 |
| 胡小强. 大型滚子对数凸度设计与加工 [R]. 沈阳: 中国科学院金属研究所, 2021 |
/
| 〈 |
|
〉 |