Deposition Mechanism and Defect Control of CrN/NbN Coatings with Excellent Tribocorrosion Performance
Received date: 2024-06-03
Revised date: 2024-09-24
Online published: 2024-12-27
Supported by
National Natural Science Foundation of China(52101063);Natural Science Foundation of Anhui Province(2108085QE187);Natural Science Foundation of the Higher Education Institutions of Anhui Province(KJ2021A0392)
The rapid exploitation of marine resources in China has heightened the need for advanced marine engineering equipment and imposed more stringent requirements on the surface performance of its key components. CrN/NbN coatings, with their excellent corrosion and wear resistances, demonstrate potential for applications in marine service environments. In this study, CrN/NbN coatings were deposited on 45# steel substrates using arc ion plating technology. A multilayer/nanolayer design and ion etching process were implemented to reduce coating defect densities, thereby enhancing overall coating performance. SEM analysis revealed that S2-S6 coatings exhibited fine columnar structures, with well-defined and cohesive sublayer interfaces in S2 and S3 multilayer coatings. XRD and TEM analyses confirmed that the primary phases of the coatings were CrN and NbN. HRTEM analyses demonstrated that S6 coating present nanolayer structure with a modulation period of 8.9 nm, where CrN and NbN sublayer thicknesses were approximately 2.7 and 6.2 nm, respectively. A coherent interface was observed in the S6 coating, accompanied by the interdiffusion of Nb and Cr elements between the CrN and NbN sublayers. The fast Fourier transform (FFT) image displayed streak-like features characteristic of stacking faults, as well as two sets of diffraction patterns indicative of coherent sublayer interfaces. Nanoindentation tests revealed that among the fabricated coatings, the S1 monolayer coating exhibited the lowest hardness of (21.8 ± 0.7) GPa, while the S4 coating demonstrated the highest hardness of (30.1 ± 1.4) GPa, attributed to its coherent interfaces and stacking faults. Ion etching had minimal impact on coating phases and mechanical properties. However, ion bombardment effectively interrupted the continuous growth of large particles, resulting in smoother surfaces and interfaces and thereby reducing surface defect proportions. The defect percentages for S3 and S5 coatings were (2.7 ± 0.19)% and (2.43 ± 0.49)%, respectively. These lower defect densities contributed to higher pore resistance (Rpo) and charge transfer resistance (Rct). As sublayer thickness decreased, the electrochemical and tribocorrosion performance of CrN/NbN coatings improved progressively, with the S6 sample achieving the lowest corrosive wear rate of 2.42 × 10-6 mm3/(N·m). The tribocorrosion failure mechanism was preliminarily explored, identifying layer-by-layer peeling as the dominant failure mode. Compared to NbN monolayer coatings, CrN/NbN multilayer/nanolayer coatings exhibited superior mechanical properties and corrosion resistance due to interface blocking and reinforcing effects. Furthermore, the application of ion etching to CrN/NbN multilayer/nanolayer coatings enhanced their electrochemical corrosion and tribocorrosion properties by disrupting the growth of large defects.
Key words: CrN/NbN; multilayer/nanomultilayer coating; ion etching; tribocorrosion
LIU Yongkang , LU Yuanyuan , YANG Ying , LIU Xingguang , ZHENG Jun , ZHANG Shihong . Deposition Mechanism and Defect Control of CrN/NbN Coatings with Excellent Tribocorrosion Performance[J]. Acta Metall Sin, 2026 , 62(4) : 649 -668 . DOI: 10.11900/0412.1961.2024.00185
| [1] | Ghorbani A, Elmkhah H, Imantalab O, et al. The impact of mechanical post-treatment on the tribological and corrosion behavior of CrN/CrAlN coatings applied using the CAE-PVD technique [J]. Appl. Surf. Sci. Adv., 2023, 18: 100477 |
| [2] | Vengesa Y, Fattah-Alhosseini A, Elmkhah H, et al. Investigation of corrosion and tribological characteristics of annealed CrN/CrAlN coatings deposited by CAE-PVD [J]. Ceram. Int., 2023, 49: 3016 |
| [3] | Zhou S G, Qin B D, Wang S C, et al. Multilayer interfaces to achieve excellent corrosion and tribological performances for CrAlCN nanocomposite coating in the seawater [J]. Mater. Chem. Phys., 2023, 301: 127689 |
| [4] | Kumar S, Maity S R, Patnaik L. Effect of tribological process parameters on the wear and frictional behaviour of Cr-(CrN/TiN) composite coating: An experimental and analytical study [J]. Ceram. Int., 2021, 47: 16018 |
| [5] | Yu H Y, Liang W P, Miao Q, et al. Effect of shot peening pretreatment on the high-temperature tribological behaviours of a TaN coating prepared via double-cathode glow plasma alloying [J]. Surf. Coat. Technol., 2021, 427: 127825 |
| [6] | Liu Z X, Li Y, Xie X H, et al. The tribo-corrosion behavior of monolayer VN and multilayer VN/C hard coatings under simulated seawater [J]. Ceram. Int., 2021, 47: 25655 |
| [7] | González-Carmona J M, Trivi?o J D, Gómez-Ovalle á, et al. Wear mechanisms identification using Kelvin probe force microscopy in TiN, ZrN and TiN/ZrN hard ceramic multilayers coatings [J]. Ceram. Int., 2020, 46: 24592 |
| [8] | Er D, Azar G T P, Kazmanl? K, et al. The corrosion protection ability of TiAlN coatings produced with CA-PVD under superimposed pulse bias [J]. Surf. Coat. Technol., 2018, 346: 1 |
| [9] | Panjan P, Drnov?ek A, Gselman P, et al. Review of growth defects in thin films prepared by PVD techniques [J]. Coatings, 2020, 10: 447 |
| [10] | Liu Y R, Li S Y, Zhou X H, et al. Enhanced anti-tribocorrosion property of a-C film under high hydrostatic pressure by high power pulsed magnetron sputter (HiPIMS) [J]. J. Mater. Res. Technol., 2024, 28: 3052 |
| [11] | Creus J, Mazille H, Idrissi H. Porosity evaluation of protective coatings onto steel, through electrochemical techniques [J]. Surf. Coat. Technol., 2000, 130: 224 |
| [12] | Kong J Z, Zhai Q W, Shen J J, et al. Role of atomic layer deposited TiO x N y interlayer in tribological and corrosion properties of CrN coating [J]. Surf. Coat. Technol., 2022, 429: 127981 |
| [13] | Staszuk M, Reimann ?, Paku?a D, et al. Investigations of TiO2/nano TiO2 bimodal coatings obtained by a hybrid PVD/ALD method on Al-Si-Cu alloy substrate [J]. Coatings, 2022, 12: 338 |
| [14] | Liu Y R, Li S Y, Li H, et al. Controllable defect engineering to enhance the corrosion resistance of Cr/GLC multilayered coating for deep-sea applications [J]. Corros. Sci., 2022, 199: 110175 |
| [15] | Wang D S, Hu M, Jiang D, et al. The improved corrosion resistance of sputtered CrN thin films with Cr-ion bombardment layer by layer [J]. Vacuum, 2017, 143: 329 |
| [16] | Wan Z X, Zhang T F, Lee H B R, et al. Improved corrosion resistance and mechanical properties of CrN hard coatings with an atomic layer deposited Al2O3 interlayer [J]. ACS Appl. Mater. Interfaces, 2015, 7: 26716 |
| [17] | Lin K F, Chang Y C, Chang S H, et al. Improving the corrosion and wear resistance of CoCrNiSi0.3 medium-entropy alloy by magnetron sputtered (CrN/Cr) x multilayer films [J]. Surf. Coat. Technol., 2024, 478: 130407 |
| [18] | Shi X W, Zhao Y M, Gao X, et al. Anti-corrosive yet color-tunable AlN/Si multilayer hard coatings on 304 stainless steel by magnetron sputtering [J]. Ceram. Int., 2024, 50: 1166 |
| [19] | Noori M, Atapour M, Ashrafizadeh F, et al. Nanostructured multilayer CAE-PVD coatings based on transition metal nitrides on Ti6Al4V alloy for biomedical applications [J]. Ceram. Int., 2023, 49: 23367 |
| [20] | Guo H X, Sun Q S, Zhou D P, et al. Erosion behavior of CrN, CrAlN and CrAlN/CrN multilayer coatings deposited on Ti6Al4V [J]. Surf. Coat. Technol., 2022, 437: 128284 |
| [21] | Ma F L, Li J L, Zeng Z X, et al. Structural, mechanical and tribocorrosion behaviour in artificial seawater of CrN/AlN nano-multilayer coatings on F690 steel substrates [J]. Appl. Surf. Sci., 2018, 428: 404 |
| [22] | Wang T, Zhang G J, Jiang B L. Comparison in mechanical and tribological properties of CrTiAlMoN and CrTiAlN nano-multilayer coatings deposited by magnetron sputtering [J]. Appl. Surf. Sci., 2016, 363: 217 |
| [23] | Cai F, Zhou Q, Chen J K, et al. Effect of inserting the Zr layers on the tribo-corrosion behavior of Zr/ZrN multilayer coatings on titanium alloys [J]. Corros. Sci., 2023, 213: 111002 |
| [24] | Ortíz C H, Hernandez-Renjifo E, Caicedo J C. Study of corrosion protection through the implementation of TiC/TiSiCN multilayer coatings [J]. Mater. Chem. Phys., 2024, 315: 128821 |
| [25] | Chen Y M. Study on microstructure regulation and strengthening mechanism of nano-multilayer ceramic coatings [D]. Beijing: University of Science and Technology Beijing, 2023 |
| 陈彦梦. 纳米多层陶瓷涂层的微观结构调控及强化机制研究 [D]. 北京: 北京科技大学, 2023 | |
| [26] | Wang D, Lin S S, Yang Z, et al. Failure mechanisms of CrN and CrAlN coatings for solid particle erosion resistance [J]. Vacuum, 2022, 204: 111313 |
| [27] | Ji C C, Guo Q Q, Li J P, et al. Microstructure and properties of CrN coating via multi-arc ion plating on the valve seat material surface [J]. J. Alloys Compd., 2022, 891: 161966 |
| [28] | Ding J C, Zhang T F, Wang Q M, et al. Microstructure and mechanical properties of the Cr-Mo-Si-N nanocomposite coatings prepared by a hybrid system of AIP and HiPIMS technologies [J]. J. Alloys Compd., 2018, 740: 774 |
| [29] | Guan X Y, Wang Y X, Zhang G G, et al. Microstructures and properties of Zr/CrN multilayer coatings fabricated by multi-arc ion plating [J]. Tribol. Int., 2017, 106: 78 |
| [30] | Panjan P, ?ekada M, Panjan M, et al. Growth defects in PVD hard coatings [J]. Vacuum, 2009, 84: 209 |
| [31] | Jasempoor F, Elmkhah H, Imantalab O, et al. Improving the mechanical, tribological, and electrochemical behavior of AISI 304 stainless steel by applying CrN single layer and Cr/CrN multilayer coatings [J]. Wear, 2022, 504-505: 204425 |
| [32] | Guan X Y, Wang Y X, Xue Q J, et al. Toward high load bearing capacity and corrosion resistance Cr/Cr2N nano-multilayer coatings against seawater attack [J]. Surf. Coat. Technol., 2015, 282: 78 |
| [33] | Abusuilik S B, Inoue K. Effects of intermediate surface treatments on corrosion resistance of cathodic arc PVD hard coatings [J]. Surf. Coat. Technol., 2013, 237: 421 |
| [34] | Guan X Y, Wang Y X, Zhang G G, et al. Effects of intermediate Ar plasma treatments on CrN coating microstructures and property evolutions [J]. Surf. Interface. Anal., 2017, 49: 323 |
| [35] | Purandare Y P, Robinson G L, Ehiasarian A P, et al. Investigation of high power impulse magnetron sputtering deposited nanoscale CrN/NbN multilayer coating for tribocorrosion resistance [J]. Wear, 2020, 452-453: 203312 |
| [36] | Biswas B, Purandare Y, Khan I, et al. Effect of substrate bias voltage on defect generation and their influence on corrosion and tribological properties of HIPIMS deposited CrN/NbN coatings [J]. Surf. Coat. Technol., 2018, 344: 383 |
| [37] | Hovsepian P E, Ehiasarian A P, Purandare Y P, et al. Novel HIPIMS deposited nanostructured CrN/NbN coatings for environmental protection of steam turbine components [J]. J. Alloys Compd., 2018, 746: 583 |
| [38] | Ramadoss R, Kumar N, Dash S, et al. Wear mechanism of CrN/NbN superlattice coating sliding against various counterbodies [J]. Int. J. Refract. Met. Hard Mater., 2013, 41: 547 |
| [39] | Huang W, Zalnezhad E, Musharavati F, et al. Investigation of the tribological and biomechanical properties of CrAlTiN and CrN/NbN coatings on SST 304 [J]. Ceram. Int., 2017, 43: 7992 |
| [40] | Chen M H, Ding J C, Kwon S H, et al. Corrosion resistance and conductivity of NbN-coated 316L stainless steel bipolar plates for proton exchange membrane fuel cells [J]. Corros. Sci., 2022, 196: 110042 |
| [41] | Lao J J, Kong M, Zhang H J, et al. Growth structure and mechanical properties of TiN/SiC nano-multilayers [J]. Acta Phys. Sin., 2004, 53: 1961 |
| 劳技军, 孔 明, 张惠娟 等. TiN/SiC纳米多层膜的生长结构与力学性能 [J]. 物理学报, 2004, 53: 1961 | |
| [42] | Chen Y M, Guo T, Pang X L, et al. Formation of high-density stacking faults in ceramic films induced by Ti transition layer [J]. Scr. Mater., 2022, 211: 114496 |
| [43] | Zhang H, He Y Z, Pan Y, et al. Thermally stable laser cladded CoCrCuFeNi high-entropy alloy coating with low stacking fault energy [J]. J. Alloys Compd., 2014, 600: 210 |
| [44] | Shin C S, Kim Y W, Hellgren N, et al. Epitaxial growth of metastable δ-TaN layers on MgO(001) using low-energy, high-flux ion irradiation during ultrahigh vacuum reactive magnetron sputtering [J]. J. Vac. Sci. Technol., 2002, 20A: 2007 |
| [45] | Huang Y, Chen Z, Wagner A, et al. High density of stacking faults strengthened TaN/TiN multilayer [J]. Acta Mater., 2023, 255: 119027 |
| [46] | Yu H, Bahadori M, Thompson G B, et al. Understanding dislocation slip in stoichiometric rocksalt transition metal carbides and nitrides [J]. J. Mater. Sci., 2017, 52: 6235 |
| [47] | Araujo J A, Giorj?o R A R, Bettini J, et al. Modeling intrinsic residual stresses built-up during growth of nanostructured multilayer NbN/CrN coatings [J]. Surf. Coat. Technol., 2016, 308: 264 |
| [48] | Fang W, Chen J K, Cai F, et al. Surface stress release in AlCrN coatings determined by synchrotron radiation multi-reflection grazing-incidence X-ray diffraction [J]. Thin Solid Films, 2023, 787: 140142 |
| [49] | Cede?o-Vente M L, Manríquez J, Mondragón-Rodríguez G C, et al. Application of a transmission line model to evaluate the influence of structural defects on the corrosion behavior of arc-PVD CrN coatings [J]. Ceram. Int., 2021, 47: 20885 |
| [50] | Yang Y, Wang F, Wu Y D, et al. The corrosive wear behavior of Cr/NiCrN multilayer coatings with various cycle periods [J]. Surf. Technol., 2021, 50: 301 |
| 杨 英, 王 芳, 巫业栋 等. 不同循环周期Cr/NiCrN多层涂层腐蚀磨损行为 [J]. 表面技术, 2021, 50: 301 | |
| [51] | Chu X, Wong M S, Sproul W D, et al. Deposition, structure, and hardness of polycrystalline transition-metal nitride superlattice films [J]. J. Mater. Res., 1999, 14: 2500 |
| [52] | Kao C M, Lee J W, Chen H W, et al. Microstructures and mechanical properties evaluation of TiAlN/CrSiN multilayered thin films with different bilayer periods [J]. Surf. Coat. Technol., 2010, 205: 1438 |
| [53] | Zhang S, Sun D E, Fu Y Q, et al. Toughening of hard nanostructural thin films: A critical review [J]. Surf. Coat. Technol., 2005, 198: 2 |
| [54] | Kong W C, Yu Z, Hu J. Electrochemical performance and corrosion mechanism of Cr-DLC coating on nitrided Ti6Al4V alloy by magnetron sputtering [J]. Diam. Relat. Mater., 2021, 116: 108398 |
| [55] | Park H S, Kappl H, Lee K H, et al. Structure modification of magnetron-sputtered CrN coatings by intermediate plasma etching steps [J]. Surf. Coat. Technol., 2000, 133-134: 176 |
| [56] | Liu Y K, Yang Y, Liu X G, et al. Tribocorrosion of CrN coatings on different steel substrates [J]. Surf. Coat. Technol., 2024, 484: 130829 |
| [57] | Liu L M, Zheng H, Dong M P, et al. Effect of bias voltage on the tribocorrosion performance of TiAlSiN coatings on FH790 steel by arc ion plating [J]. Surf. Coat. Technol., 2023, 454: 129177 |
/
| 〈 |
|
〉 |