Research paper

Texture Evolution and Deformation Modes for Zr-4 Alloy During Stamping: Experiments and Modeling

  • DENG Siying ,
  • DONG Jiaxuan ,
  • CHEN Shuaifeng ,
  • SONG Hongwu ,
  • ZHANG Shihong
Expand
  • 1 Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2 College of Materials Science and Engineering, Shenyang Ligong University, Shenyang 110159, China
SONG Hongwu, associate professor, Tel: (024)83970203, E-mail: hwsong@imr.ac.cn

Received date: 2024-06-25

  Revised date: 2024-08-16

  Online published: 2024-11-15

Supported by

National Natural Science Foundation of China(52105413);National Natural Science Foundation of China(52105412)

Abstract

Zirconium alloy sheets exhibit limited formability at room temperature, often leading to cracking during the fabrication of spacer grids in nuclear reactors. This study presents stamping experiments conducted on Zr-4 sheets, with microstructure and texture characteristics measured at various positions along the longitudinal section using EBSD. The in-grain misorientation axes method was employed to analyze deformation mode selection. Supported by finite element method simulations, a visco-plastic self-consistent model was applied to quantify the activation of deformation modes and elucidate the relationship between texture evolution and slip/twin activity. In addition, the effects of strain paths on crack formation mechanisms were investigated. The results indicate that cracking primarily occurred around the punch radius. Positions near the punch radius followed a plane strain path, whereas regions along the slope wall and die radius exhibited a uniaxial tension path. Prismatic <a> slip was found to dominate deformation across all loading strain paths. Near the die radius, pyramidal <c + a> slip and tensile twinning were activated to accommodate stamping deformation, resulting in the formation of new texture components aligned along the rolling direction. The increase in basal texture strength around the punch radius was attributed to basal <a> slip, serving as a secondary dominant slip system. Furthermore, prismatic slip, in coordination with basal slip, facilitated the texture transition from a double-peak structure to a basal texture.

Cite this article

DENG Siying , DONG Jiaxuan , CHEN Shuaifeng , SONG Hongwu , ZHANG Shihong . Texture Evolution and Deformation Modes for Zr-4 Alloy During Stamping: Experiments and Modeling[J]. Acta Metall Sin, 2026 , 62(8) : 1417 -1426 . DOI: 10.11900/0412.1961.2024.00214

References

[1] Han E H. Research trends on micro and nano-scale materials degradation in nuclear power plant [J]. Acta Metall. Sin., 2011, 47: 769
  韩恩厚. 核电站关键材料在微纳米尺度上的环境损伤行为研究——进展与趋势 [J]. 金属学报, 2011, 47: 769
[2] Murty K L, Charit I. Texture development and anisotropic deformation of zircaloys [J]. Prog. Nucl. Energy, 2006, 48: 325
[3] Ren Q Y, Chen J, Zhao R R, et al. Mechanical performance of newly developed supporting structure of spacer grid [J]. At. Energy Sci. Technol., 2020, 54: 2411
  任全耀, 陈 杰, 赵瑞瑞 等. 新型定位格架夹持结构的力学特性研究 [J]. 原子能科学技术, 2020, 54: 2411
[4] Akhtar A, Teghtsoonian A. Plastic deformation of zirconium single crystals [J]. Acta Metall., 1971, 19: 655
[5] McCabe R J, Cerreta E K, Misra A, et al. Effects of texture, temperature and strain on the deformation modes of zirconium [J]. Philos. Mag., 2006, 86A: 3595
[6] Akhtar A. Prismatic slip in zirconium single crystals at elevated temperatures [J]. Metall. Trans., 1975, 6A: 1217
[7] Li Y, Po G, Cui Y N, et al. Prismatic-to-basal plastic slip transition in zirconium [J]. Acta Mater., 2023, 242: 118451
[8] Knezevic M, Zecevic M, Beyerlein I J, et al. Strain rate and temperature effects on the selection of primary and secondary slip and twinning systems in HCP Zr [J]. Acta Mater., 2015, 88: 55
[9] McCabe R J, Proust G, Cerreta E K, et al. Quantitative analysis of deformation twinning in zirconium [J]. Int. J. Plast., 2009, 25: 454
[10] Lei C Y, Mao J Z, Zhou D W, et al. Effects of annealing treatments on forming performance of zirconium alloys [J]. Trans. Nonferrous Met. Soc. China, 2022, 32: 2908
[11] Deng Z P, Zhou D W, Jiang P S, et al. Optimization on stamping process parameters for zirconium alloy sheet strip based on orthogonal experiment [J]. Forg. Stamping Technol., 2019, 44(9): 12
  邓振鹏, 周惦武, 蒋朋松 等. 基于正交试验的锆合金薄板带材冲压工艺参数优化 [J]. 锻压技术, 2019, 44(9): 12
[12] Lei C Y, Mao J Z, Zhang X M, et al. A comparison study of the yield surface exponent of the Barlat yield function on the forming limit curve prediction of zirconium alloys with M-K method [J]. Int. J. Mater. Form., 2021, 14: 467
[13] Kim M, Bang S, Lee H, et al. Enhancement of dimple formability in sheet metals by 2-step forming [J]. Mater. Des. (1980-2015), 2014, 54: 121
[14] Marimuthu K P, Choi W, Kim N, et al. Numerical investigations on the effect of pit on two-step dimple forming of atomic fuel spacer grid [J]. Int. J. Adv. Manuf. Technol., 2018, 94: 293
[15] Deng S Y, Song H W, Liu H, et al. Effect of uniaxial loading direction on mechanical responses and texture evolution in cold pilgered Zircaloy-4 tube: Experiments and modeling [J]. Int. J. Solids Struct., 2021, 213: 63
[16] Liu H, Deng S Y, Chen S F, et al. Correlation of the anisotropic hardening behavior and texture features of cold rolled Zr-4 sheet under uniaxial tension [J]. J. Mater. Sci. Technol., 2022, 119: 111
[17] Luan B F, Gao S S, Chai L J, et al. Compression deformation behavior of Zr-1Sn-0.3Nb alloy with different initial orientations at 650 oC [J]. Mater. Des. (1980-2015), 2013, 52: 1065
[18] Chen J W, Luan B F, Chai L J, et al. Heterogeneous microstructure and texture evolution during fabrication of Zr-Sn-Nb zirconium alloy sheets [J]. Acta Metall. Sin., 2012, 48: 393
  陈建伟, 栾佰峰, 柴林江 等. Zr-Sn-Nb新型锆合金板材加工过程中不均匀组织与织构演变 [J]. 金属学报, 2012, 48: 393
[19] Knezevic M, Beyerlein I J, Nizolek T, et al. Anomalous basal slip activity in zirconium under high-strain deformation [J]. Mater. Res. Lett., 2013, 1: 133
[20] Cao Y C, Chen D, Xia L, et al. Effects of primary α grains on rolling reductions and deformation modes in Zr alloys: Experiments and modeling [J]. Mech. Mater., 2024, 19: 104957
[21] Kearns J J. On the relationship among ‘f ’ texture factors for the principal planes of zirconium, hafnium and titanium alloys [J]. J. Nucl. Mater., 2001, 299: 171
[22] Su R, Liu J Y, Qiao X Y, et al. Advances in scanning white light interferometry for surface topography measurement [J]. Laser Optoelectron. Prog., 2023, 60: 0312005
  苏 榕, 刘嘉宇, 乔潇悦 等. 用于表面形貌测量的扫描白光干涉技术进展 [J]. 激光与光电子学进展, 2023, 60: 0312005
[23] Akhtar A. Compression of zirconium single crystals parallel to the c-axis [J]. J. Nucl. Mater., 1973, 47: 79
[24] Akhtar A. Basal slip in zirconium [J]. Acta Metall., 1973, 21: 1
[25] Chun Y B, Battaini M, Davies C H J, et al. Distribution characteristics of in-grain misorientation axes in cold-rolled commercially pure titanium and their correlation with active slip modes [J]. Metall. Mater. Trans., 2010, 41A: 3473
Outlines

/