Solidification of Undercooled (Fe1 -x Co x)79.3B20.7 Alloys
Received date: 2024-08-20
Revised date: 2024-10-29
Online published: 2024-11-08
Supported by
National Natural Science Foundation of China(52231002);National Natural Science Foundation of China(51821001)
M-B (M = Fe, Co, Ni) alloys have garnered significant attention in the automotive, petrochemical, and power electronics industries owing to their excellent corrosion resistance, wear resistance, and high-temperature strength. The service performances of the M-B alloys are closely related to that of borides. Among them, M23B6 generally exists as a metastable phase. However, the understanding of its formation is limited compared to that of other borides. To reveal the effect of Fe/Co content ratio on the solidification behavior of the Fe-Co-B alloys, particularly the formation of M23B6 phase, alloys with nominal composition of (Fe1 - x Co x)79.3B20.7 (x = 0-1) were undercooled using the melt fluxing technique. Consequently, the solidification behaviors were systematically investigated. With the increase in the Co content, the stable eutectic reaction changed from L→α-M + M2B for x <0.4 to L→α-M + M3B for x >0.4. Consequently, the two eutectic reactions occurred at the same temperature at x =0.4, and a peritectic reaction L + M2B→M3B was observed at x > 0.4. With the increase in the undercooling, the primary phase changes from M2B and M23B6 to α-M/M3B in the alloys with x ≤0.6, and from M3B, M2B, and M23B6 to α-M/M3B in the alloys with x >0.6. The increase in Co content reduced the critical undercooling for the M23B6 phase to precipitate primarily and improved its stability, that is, the primary M23B6 phase decomposed into α-M/M2B in the following cooling process when the Co content is not excessively high. However, it could sometimes be reserved to room temperature in case of a very large Co content.
YANG Lin , MA Changsong , LIU Lianjie , LI Jinfu . Solidification of Undercooled (Fe1 -x Co x)79.3B20.7 Alloys[J]. Acta Metall Sin, 2025 , 61(1) : 99 -108 . DOI: 10.11900/0412.1961.2024.00291
| 1 | Zhang J J, Liu J C, Liao H M, et al. A review on relationship between morphology of boride of Fe-B alloys and the wear/corrosion resistant properties and mechanisms[J]. J. Mater. Res. Technol., 2019, 8: 6308 |
| 2 | Liu Z W, Zhou B, Liao X F, et al. Research status and future development of (Ce, La, Y)-F-B permanent magnets based on full high-abundance rare earth elements[J]. Acta Metall. Sin., 2024, 60: 585 |
| 刘仲武, 周 帮, 廖雪峰 等. 全高丰度稀土(Ce, La, Y)-Fe-B永磁的研究现状和未来发展[J]. 金属学报, 2024, 60: 585 | |
| 3 | ünal E, Ya?ar A, Karahan ? H. A review of electrodeposited composite coatings with Ni-B alloy matrix[J]. Mater. Res. Express, 2019, 6: 092004 |
| 4 | Liu Z W, He J Y. Several issues on the development of grain boundary diffusion process for Nd-Fe-B permanent magnets[J]. Acta Metall. Sin., 2021, 57: 1155 |
| 刘仲武, 何家毅. 钕铁硼永磁晶界扩散技术和理论发展的几个问题[J]. 金属学报, 2021, 57: 1155 | |
| 5 | Barati Q, Hadavi S M M. Electroless Ni-B and composite coatings: A critical review on formation mechanism, properties, applications and future trends[J]. Surf. Interfaces, 2020, 21: 100702 |
| 6 | Xu X L, Hao Y C, Wu Q, et al. Microstructure refinement mechanisms in undercooled solidification of binary and ternary nickel based alloys[J]. J. Mater. Res. Technol., 2023, 24: 737 |
| 7 | Madah F, Amadeh A A, Dehghanian C. Investigation on the phase transformation of electroless Ni-B coating after dry sliding against alumina ball[J]. J. Alloys Compd., 2016, 658: 272 |
| 8 | Pal S, Jayaram V. Effect of microstructure on the hardness and dry sliding behavior of electroless Ni-B coating[J]. Materialia, 2018, 4: 47 |
| 9 | Safavi M S, Tanhaei M, Ahmadipour M F, et al. Electrodeposited Ni-Co alloy-particle composite coatings: A comprehensive review[J]. Surf. Coat. Technol., 2020, 382: 125153 |
| 10 | Li J F, Zhou Y H. Remelting of primary solid in rapid solidification of deeply undercooled alloy melts[J]. Acta Metall. Sin., 2018, 54: 627 |
| 李金富, 周尧和. 液态金属深过冷快速凝固过程中初生固相的重熔[J]. 金属学报, 2018, 54: 627 | |
| 11 | Liang L, Xu X L, Zhao Y H, et al. Solidification microstructure evolution and grain refinement mechanism under high undercooling of undercooled Ni90Cu10 alloys[J]. Mater. Res. Express, 2019, 6(12): 1265k5 |
| 12 | Li J F, Lü Y L, Yang G C, et al. Secondary arm spacing of undercooled Ni50Cu50 alloy[J]. Acta Metall. Sin., 1998, 34: 586 |
| 李金富, 吕衣礼, 杨根仓 等. 过冷Ni50Cu50合金的二次枝晶间距[J]. 金属学报, 1998, 34: 586 | |
| 13 | Quirinale D G, Rustan G E, Kreyssig A, et al. Synergistic stabilization of metastable Fe23B6 and γ-Fe in undercooled Fe83B17 [J]. Appl. Phys. Lett., 2015, 106: 241906 |
| 14 | Liu L J, Yang L, Li J F. Solidification pathways in highly undercooled Co79.3B20.7 alloy[J]. Metall. Mater. Trans., 2021, 52A: 4324 |
| 15 | Wei X X, Xu W, Kang J L, et al. Metastable Co23B6 phase solidified from deeply undercooled Co79.3B20.7 alloy melt[J]. J. Mater. Sci., 2016, 51: 6436 |
| 16 | Xu J F, Liu F, Dang B. Phase selection in undercooled Ni-3.3 wt pct B alloy melt[J]. Metall. Mater. Trans., 2013, 44A: 1401 |
| 17 | Liu F, Xu J F, Zhang D, et al. Solidification of highly undercooled hypereutectic Ni-Ni3B alloy melt[J]. Metall. Mater. Trans., 2014, 45A: 4810 |
| 18 | Battezzati L, Antonione C, Baricco M. Undercooling of Ni-B and Fe-B alloys and their metastable phase diagrams[J]. J. Alloys Compd., 1997, 247: 164 |
| 19 | Ohodnicki Jr P R, Cates N C, Laughlin D E, et al. Ab initio theoretical study of magnetization and phase stability of the (Fe, Co, Ni)23B6 and (Fe, Co, Ni)23Zr6 structures of Cr23C6 and Mn23Th6 prototypes[J]. Phys. Rev., 2008, 78B: 144414 |
| 20 | Li J F, Li W. Structure and glass-forming ability of Al-based amorphous alloys[J]. Acta Metall. Sin., 2022, 58: 457 |
| 李金富, 李 伟. 铝基非晶合金的结构与非晶形成能力[J]. 金属学报, 2022, 58: 457 | |
| 21 | Yang G, Liu W G, Han X B, et al. Effects of alloying substitutions on the anti-disproportionation behavior of ZrCo alloy[J]. Int. J. Hydrogen Energy, 2017, 42: 15782 |
| 22 | Zhang Q S, Zhang W, Louzguine-Luzgin D V, et al. Effect of substituting elements on glass-forming ability of the new Zr48Cu36Al8Ag8 bulk metallic glass-forming alloy[J]. J. Alloys Compd., 2010, 504: S18 |
| 23 | Wu M D, Wang J C, Li P L, et al. Research progress on the anti-disproportionation of the ZrCo alloy by element substitution[J]. Materials, 2020, 13: 3977 |
| 24 | Xu T, Li R, Xiao R J, et al. Tuning glass formation and brittle behaviors by similar solvent element substitution in (Mn, Fe)-based bulk metallic glasses[J]. Mater. Sci. Eng., 2015, A626: 16 |
| 25 | Mitrica D, Badea I C, Serban B A, et al. Complex concentrated alloys for substitution of critical raw materials in applications for extreme conditions[J]. Materials, 2021, 14: 1197 |
| 26 | Yang T, Yuan Z M, Bu W G, et al. Effect of elemental substitution on the structure and hydrogen storage properties of LaMgNi4 alloy[J]. Mater. Des., 2016, 93: 46 |
| 27 | Palumbo M, Cacciamani G, Bosco E, et al. Driving forces for crystal nucleation in Fe-B liquid and amorphous alloys[J]. Intermetallics, 2003, 11: 1293 |
| 28 | Okamoto H. B-Fe (Boron-Iron)[J]. J. Phase Equilib. Diffus., 2004, 25: 297 |
| 29 | Massalski T B, Okamoto H, Subramanian P R, et al. Binary Alloy Phase Diagrams[M]. 2nd Ed., Materials Park: ASM International, 1990: 482 |
| 30 | Raghavan V. B-Co-Fe (Boron-Cobalt-Iron)[J]. J. Phase Equilib. Diffus., 2012, 33: 392 |
| 31 | Liu Y Q, Zhao X S, Yang J, et al. Thermodynamic optimization of the boron-cobalt-iron system[J]. J. Alloys Compd., 2011, 509: 4805 |
| 32 | Jackson K A, Uhlmann D R, Hunt J D. On the nature of crystal growth from the melt[J]. J. Cryst. Growth, 1967, 1: 1 |
| 33 | Li M J, Kuribayashi K. Nucleation-controlled microstructures and anomalous eutectic formation in undercooled Co-Sn and Ni-Si eutectic melts[J]. Metall. Mater. Trans., 2003, 34A: 2999 |
| 34 | Herlach D M. Non-equilibrium solidification of undercooled metallic metals[J]. Mater. Sci. Eng., 1994, R12: 177 |
| 35 | Li M J, Ozawa S, Kuribayashi K. On determining the phase-selection principle in solidification from undercooled melts-competitive nucleation or competitive growth?[J]. Philos. Mag. Lett., 2004, 84: 483 |
| 36 | Turnbull D. Kinetics of solidification of supercooled liquid mercury droplets[J]. J. Chem. Phys., 1952, 20: 411 |
| 37 | Turnbull D. Formation of crystal nuclei in liquid metals[J]. J. Appl. Phys., 1950, 21: 1022 |
| 38 | Wei X X, Xu W, Kang J L, et al. Phase selection in solidification of undercooled Co-B alloys[J]. J. Mater. Sci. Technol., 2017, 33: 352 |
/
| 〈 |
|
〉 |