Thermal Deformation Behavior and Hot Rolling Process of X65/Inconel 625 Bimetal Composite Plate for Deep Sea Oil and Gas Field Transportation
Received date: 2024-08-28
Revised date: 2024-11-01
Online published: 2024-11-04
Supported by
National Natural Science Foundation of China(52201093);Special Project of Ministry of Industry and Information Technology(2240STCZB2346);Open Fund of State Key Laboratory of Marine Equipment(SKLMEA-K202205)
The service environment of deep-sea oil and gas pipelines is becoming increasingly harsh, making it difficult for traditional single-metal pipeline steels to meet the unique demands of such environments. Bimetal composite materials leverage the advantages of bimetal components to achieve properties that are not possible with single metal materials. Hot rolling, a solid-phase bonding process that joins pipeline steel substrates and stainless steel at high temperatures, is an efficient method for creating strong interfaces. This technique is particularly suitable for the large-scale industrial production of bimetal clad plates, necessitating the establishment of an industrial production line. To overcome the challenge posed by deformation inconsistencies that adversely affect the properties and interface bonding strength of heterogeneous bimetal clad materials during hot rolling, the precise control of the hot rolling process for X65/Inconel 625 bimetal composite plates intended for deep-sea oil and gas transportation was investigated. Thermal compression tests on the X65 pipeline steel and Inconel 625 corrosion-resistant alloy were carried out using a Gleeble-3800 thermal simulation testing machine. The flow stress, constitutive relationships, thermal working diagram, interface bending resistance, and microstructure characteristics of the bimetallic materials were examined. The results indicate that the peak stress difference in the bimetallic materials decreases as the deformation temperature increases and the strain rate decreases. At high temperatures (≥ 950 oC), the primary softening mechanism for X65 steel is dynamic recovery, whereas that for Inconel 625 is dynamic recrystallization. Our findings suggest that the optimal hot rolling process for the bimetal clad plate should involve a final rolling temperature of 1000 oC and a reduction of 70%, based on theoretical analysis and experimental data. The interface is straight and well-combined, and demonstrates strong bending deformation ability. The bimetal clad plate achieves a rolling direction yield strength of 469 MPa, tensile strength of 606 MPa, elongation of 30%, and shear strength of 442 MPa.
LIU Geng , SHAN Yiyin , YAN Wei , SU Rui , REN Yi , SHI Xianbo . Thermal Deformation Behavior and Hot Rolling Process of X65/Inconel 625 Bimetal Composite Plate for Deep Sea Oil and Gas Field Transportation[J]. Acta Metall Sin, 2026 , 62(4) : 572 -586 . DOI: 10.11900/0412.1961.2024.00303
| [1] | Li Z, Zhao J W, Jia F H, et al. Interfacial characteristics and mechanical properties of duplex stainless steel bimetal composite by heat treatment [J]. Mater. Sci. Eng., 2020, A787: 139513 |
| [2] | Hedayati O, Korei N, Adeli M, et al. Microstructural evolution and interfacial diffusion during heat treatment of Hastelloy/stainless steel bimetals [J]. J. Alloys Compd., 2017, 712: 172 |
| [3] | Li Z, Zhao J W, Jia F H, et al. Analysis of bending characteristics of bimetal steel composite [J]. Int. J. Mech. Sci., 2018, 148: 272 |
| [4] | Poberezhnyi L, Maruschak P, Prentkovskis O, et al. Fatigue and failure of steel of offshore gas pipeline after the laying operation [J]. Arch. Civ. Mech. Eng., 2016, 16: 524 |
| [5] | O’Grady R, Harte A. Localised assessment of pipeline integrity during ultra-deep S-lay installation [J]. Ocean Eng., 2013, 68: 27 |
| [6] | Su G X, Shi Y, Li G, et al. High-efficiency fabrication of Inconel 625 coating for AISI 1045 carbon steel through laser cladding with hot wire: Microstructure and wear resistance [J]. J. Manuf. Process., 2023, 102: 622 |
| [7] | Li H L, Liu S X, Sun F X, et al. Preliminary investigation on underwater wet welding of Inconel 625 alloy: Microstructure, mechanical properties and corrosion resistance [J]. J. Mater. Res. Technol., 2022, 20: 2394 |
| [8] | Acarer M, Gülen? B, Findik F. Investigation of explosive welding parameters and their effects on microhardness and shear strength [J]. Mater. Des., 2003, 24: 659 |
| [9] | Liu F J, Zheng J Y, Xu P, et al. Forming mechanism of double-layered tubes by internal hydraulic expansion [J]. Int. J. Press Vessels Pip., 2004, 81: 625 |
| [10] | Huang Q X, Yang X R, Ma L F, et al. Interface-correlated characteristics of stainless steel/carbon steel plate fabricated by AAWIV and hot rolling [J]. J. Iron Steel Res. Int., 2014, 21: 931 |
| [11] | Xie G M, Luo Z A, Wang G L, et al. Interface characteristic and properties of stainless steel/HSLA steel clad plate by vacuum rolling cladding [J]. Mater. Trans., 2011, 52: 1709 |
| [12] | Li L, Yin F X, Nagai K. Progress of laminated materials and clad steels production [J]. Mater. Sci. Forum, 2011, 675-677: 439 |
| [13] | Tachibana S, Kuronuma Y, Yokota T, et al. Effect of hot rolling and cooling conditions on intergranular corrosion behavior in Alloy625 clad steel [J]. Corros. Sci., 2015, 99: 125 |
| [14] | Chen C X, Guo Y, Liu B X, et al. Interfacial microstructure characteristics and mechanical properties of X65/IN625 composite plates with different interlayers [J]. Mater. Lett., 2024, 362: 136184 |
| [15] | Liu W H, Yue X M, Hu Q, et al. Effects of recrystallization and element diffusion behavior on interfacial bonding quality and mechanical properties of aluminum laminated composites [J]. J. Alloys Compd., 2024, 985: 174045 |
| [16] | Zhu Z C, He Y, Zhang X J, et al. Effect of interface oxides on shear properties of hot-rolled stainless steel clad plate [J]. Mater. Sci. Eng., 2016, A669: 344 |
| [17] | Liu B X, Yin F X, Dai X L, et al. The tensile behaviors and fracture characteristics of stainless steel clad plates with different interfacial status [J]. Mater. Sci. Eng., 2017, A679: 172 |
| [18] | Cao F R, Ding X, Xiang C, et al. Flow stress, microstructural evolution, and constitutive analysis during high-temperature deformation in Mg-4.4Li-2.5Zn-0.46Al-0.74Y alloy [J]. Acta Metall. Sin., 2021, 57: 860 |
| 曹富荣, 丁 鑫, 项 超 等. Mg-4.4Li-2.5Zn-0.46Al-0.74Y合金高温变形流动应力、组织演变与本构分析 [J]. 金属学报, 2021, 57: 860 | |
| [19] | Li F L, Fu R, Bai Y R, et al. Effects of initial grain size and strengthening phase on thermal deformation and recrystallization behavior of GH4096 superalloy [J]. Acta Metall. Sin., 2023, 59: 855 |
| 李福林, 付 锐, 白云瑞 等. 初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响 [J]. 金属学报, 2023, 59: 855 | |
| [20] | Zhou G, Wang C, Li J L, et al. Structure evolution mechanism and physical modeling of Ni60Ti40 during dynamic recrystallization [J]. Mater. Charact., 2022, 190: 112028 |
| [21] | Li N, Zhao C Z, Jiang Z H, et al. Flow behavior and processing maps of high-strength low-alloy steel during hot compression [J]. Mater. Charact., 2019, 153: 224 |
| [22] | Chen L, Zhang B, Yang Y, et al. Evolution of hot processing map and microstructure of as-forged nickel-based superalloy during hot deformation [J]. J. Mater. Res. Technol., 2023, 24: 7638 |
| [23] | Jonas J J, Sellars C M, Tegart W J M. Strength and structure under hot-working conditions [J]. Int. Mater. Rev., 1969, 14: 1 |
| [24] | Ma X, Zeng W D, Tian F, et al. Optimization of hot process parameters of Ti-6.7Al-2Sn-2.2Zr-2.1Mo-1W-0.2Si alloy with lamellar starting microstructure based on the processing map [J]. Mater. Sci. Eng., 2012, A545: 132 |
| [25] | Peng X N, Guo H Z, Shi Z F, et al. Constitutive equations for high temperature flow stress of TC4-DT alloy incorporating strain, strain rate and temperature [J]. Mater. Des., 2013, 50: 198 |
| [26] | Prasad Y V R K, Gegel H L, Doraivelu S M, et al. Modeling of dynamic material behavior in hot deformation: Forging of Ti-6242 [J]. Metall. Mater. Trans., 1984, 15A: 1883 |
| [27] | Hernandez C A, Medina S F, Ruiz J. Modelling austenite flow curves in low alloy and microalloyed steels [J]. Acta Mater., 1996, 44: 155 |
| [28] | Tan Y B, Ma Y H, Zhao F. Hot deformation behavior and constitutive modeling of fine grained Inconel 718 superalloy [J]. J. Alloys Compd., 2018, 741: 85 |
| [29] | Li J S, Cheng G J, Yen H W, et al. Microstrain and boundary misorientation evolution for recrystallized super DSS after deformation [J]. Mater. Chem. Phys., 2020, 246: 122815 |
| [30] | Lin Y C, He M, Zhou M, et al. New constitutive model for hot deformation behaviors of Ni-based superalloy considering the effects of initial δ phase [J]. J. Mater. Eng. Perform., 2015, 24: 3527 |
/
| 〈 |
|
〉 |