Research paper

Homogenization of Nuclei in Al-Nb-B Inoculant and Its Effect on Microstructure and Mechanical Properties of Cast Al Alloy

  • WAN Jie ,
  • LI Haotian ,
  • LIU Shuji ,
  • LU Hongzhou ,
  • WANG Lisheng ,
  • ZHANG Zhendong ,
  • LIU Chunhai ,
  • JIA Jianlei ,
  • LIU Haifeng ,
  • CHEN Yuzeng
Expand
  • 1 State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China
    2 China International Trust and Investment Corporation Dicastal Co. Ltd., Qinhuangdao 066011, China
    3 China International Trust and Investment Corporation Metal Co. Ltd., Beijing 100004, China
CHEN Yuzeng, professor, Tel: 13572260961, E-mail: yzchen@nwpu.edu.cn

Received date: 2024-05-09

  Revised date: 2024-10-07

  Online published: 2024-11-04

Supported by

National Natural Science Foundation of China(52071262);National Natural Science Foundation of China(52301197);National Natural Science Foundation of China(52234009);Fundamental Research Funds for the Central Universities(D5000240144);Qinchuangyuan “Scientist + Engineer” Team Development Program of Shaanxi Province(2022KXJ-020);Natural Science Basic Research Program of Shaanxi Province(2023-JC-QN-0421)

Abstract

Silicon (Si)-containing aluminum (Al) alloys are highly valued in the fabrication of large-scale components with thin walls and complex geometries, such as automobile engine housings, gas turbine blades, and electrical equipment housings. These alloys are favored owing to their high fluidity, excellent filling ability, low risk of hot cracking, and excellent weldability. However, the broad solidification range of these alloys can lead to the formation of coarse primary Al dendrites and casting defects such as shrinkage porosity. To improve casting quality, inoculation is commonly carried out in practice. Numerous inoculants, such as Al-Ti, Al-B, Al-Ti-B, Al-Ti-C, and Al-Ti-B-C, have so far been developed. Among these, Al-Ti-B is widely adopted in industry owing to its high grain refinement efficiency. However, its efficiency decreases significantly when the Si content in Al alloys exceeds 5% (mass fraction), a phenomenon known as “Si poisoning”. To this end, an Al-Nb-B inoculant was developed to replace Al-Ti-B. Al-Nb-B demonstrates excellent grain refinement effect and effective resistance to Si poisoning, making it ideal for cast Al alloys with high Si contents. Typically, Al-Nb-B is fabricated using conventional casting methods with Al-Nb and Al-B intermetallic alloys as feedstocks. However, because these feedstocks have higher melting points than Al alloys, the reaction time required for the fabrication of Al-Nb-B is lengthy. This leads to the coarsening and sedimentation of nuclei in the molten Al, resulting in a non-uniform distribution in the as-cast inoculant, limiting its industrial application. To overcome this challenge, a fabrication method utilizing molten salt reactions has been proposed to homogenize the distribution of nuclei in Al-Nb-B inoculants. This approach not only improves the homogeneity of the nuclei but also reduces their average particle size from 10 μm to 1 μm. This is attributed to the relatively fast reaction rate between the molten salt and the liquid Al. As a result, the grain refinement efficiency improved significantly from 34% to 79%. Furthermore, plastic deformation aids in further homogenizing nucleus distribution. Hot extrusion is more effective than cold-rolling in this regard, showing the best results for enhancing grain refinement and antidegradation performance of the molten salt-based inoculant. The performance of this newly developed molten salt-based inoculant was verified during the fabrication of cast Al alloys ZL104 and ZL114A, which not only refines grain size by 79.2% and 78.5%, respectively but also significantly reduces casting defects. Consequently, the ductility and impact toughness of both ZL104 and ZL114A alloys improved simultaneously. This study provides a new approach to fabricating high-performance Al-Nb-B inoculants for cast Al alloys.

Cite this article

WAN Jie , LI Haotian , LIU Shuji , LU Hongzhou , WANG Lisheng , ZHANG Zhendong , LIU Chunhai , JIA Jianlei , LIU Haifeng , CHEN Yuzeng . Homogenization of Nuclei in Al-Nb-B Inoculant and Its Effect on Microstructure and Mechanical Properties of Cast Al Alloy[J]. Acta Metall Sin, 2025 , 61(1) : 117 -128 . DOI: 10.11900/0412.1961.2024.00152

References

1 Guan R G, Lou H F, Huang H, et al. Development of aluminum alloy materials: Current status, trend, and prospects[J]. Strat. Study CAE, 2020, 22: 68
  管仁国, 娄花芬, 黄 晖 等. 铝合金材料发展现状、趋势及展望[J]. 中国工程科学, 2020, 22: 68
2 Li Y, Li H X, Katgerman L, et al. Recent advances in hot tearing during casting of aluminium alloys[J]. Prog. Mater. Sci., 2021, 117: 100741
3 Yang J, Zhao Y, Yan K K, et al. Heat treatment of high pressure die cast AlSi7MgMn alloy[J]. Foundry Technol., 2022, 43: 506
  杨 洁, 赵 越, 闫康康 等. 高压铸造AlSi7MgMn合金热处理工艺研究[J]. 铸造技术, 2022, 43: 506
4 Wan J, Geng H R, Chen B, et al. Assessing the thermal stability of laser powder bed fused AlSi10Mg by short-period thermal exposure[J]. Virtual Phys. Prototyp., 2023, 18: e2165122
5 Feng Z, Tan H, Fang Y B, et al. Selective laser melting of TiB2/AlSi10Mg composite: Processability, microstructure and fracture behavior[J]. J. Mater. Process. Technol., 2022, 299: 117386
6 Eborall M D. Grain refinement of aluminium and its alloys by small additions of other elements[J]. J. Inst. Met., 1949, 76: 295
7 Cibula A. The grain refinement of aluminium alloy castings by additions of titanium and boron[J]. J. Inst. Met., 1951, 80: 1
8 Han Y F, Zhang H L, Xu J, et al. Development of grain refining mechanism of Al alloys by Al-Ti-B master alloys[J]. Mater. China, 2018, 37: 632
  韩延峰, 张瀚龙, 徐 钧 等. 基于Al-Ti-B细化剂的铝合金异质形核机制研究进展[J]. 中国材料进展, 2018, 37: 632
9 Li Y, Jiang Y, Liu B, et al. Understanding grain refining and anti Si-poisoning effect in Al-10Si/Al-5Nb-B system[J]. J. Mater. Sci. Technol., 2021, 65: 190
10 Qiu D, Taylor J A, Zhang M X, et al. A mechanism for the poisoning effect of silicon on the grain refinement of Al-Si alloys[J]. Acta Mater., 2007, 55: 1447
11 Li Y, Hu B, Liu B, et al. Insight into Si poisoning on grain refinement of Al-Si/Al-5Ti-B system[J]. Acta Mater., 2020, 187: 51
12 Nowak M, Bolzoni L, Babu N H. Grain refinement of Al-Si alloys by Nb-B inoculation. Part I: Concept development and effect on binary alloys[J]. Mater. Des., 2015, 66: 366
13 Witusiewicz V T, Bondar A A, Hecht U, et al. The Al-B-Nb-Ti system: IV. Experimental study and thermodynamic re-evaluation of the binary Al-Nb and ternary Al-Nb-Ti systems[J]. J. Alloys Compd., 2009, 472: 133
14 Xu J, Li Y, Hu B, et al. Development of Al-Nb-B master alloy with high Nb/B ratio for grain refinement of hypoeutectic Al-Si cast alloys[J]. J. Mater. Sci., 2019, 54: 14561
15 Birol Y. Effect of the salt addition practice on the grain refining efficiency of Al-Ti-B master alloys[J]. J. Alloys Compd., 2006, 420: 207
16 Li D X, Yan X R, Fan Y, et al. An anti Si/Zr-poisoning strategy of Al grain refinement by the evolving effect of doped complex[J]. Acta Mater., 2023, 249: 118812
17 Zhu Z G, Hu Z H, Seet H L, et al. Recent progress on the additive manufacturing of aluminum alloys and aluminum matrix composites: Microstructure, properties, and applications[J]. Int. J. Mach. Tools Manuf., 2023, 190: 104047
18 Birol Y. An improved practice to manufacture Al-Ti-B master alloys by reacting halide salts with molten aluminium[J]. J. Alloys Compd., 2006, 420: 71
19 Yamagata H, Kasprzak W, Aniolek M, et al. The effect of average cooling rates on the microstructure of the Al-20%Si high pressure die casting alloy used for monolithic cylinder blocks[J]. J. Mater. Process. Technol., 2008, 203: 333
20 Brandes E A, Brook G B. Smithells Metals Reference Book[M]. 7th Ed., Amsterdam: Elsevier, 2013: 14
21 Bolzoni L, Nowak M, Hari Babu N. Assessment of the influence of Al-2Nb-2B master alloy on the grain refinement and properties of LM6 (A413) alloy[J]. Mater. Sci. Eng., 2015, A628: 230
22 Venkateswarlu K, Chakraborty M, Murty B S. Influence of thermo-mechanical processing of Al-5Ti-1B master alloy on its grain refining efficiency[J]. Mater. Sci. Eng., 2004, A364: 75
23 Venkateswarlu K, Murty B S, Chakraborty M. Effect of hot rolling and heat treatment of Al-5Ti-1B master alloy on the grain refining efficiency of aluminium[J]. Mater. Sci. Eng., 2001, A301: 180
24 Schaffer P L, Dahle A K. Settling behaviour of different grain refiners in aluminium[J]. Mater. Sci. Eng., 2005, A413-414: 373
25 Schaffer P L, Arnberg L, Dahle A K. Segregation of particles and its influence on the morphology of the eutectic silicon phase in Al-7wt.% Si alloys[J]. Scr. Mater., 2006, 54: 677
26 Xu J, Li R X, Li Q. Effect of agglomeration on nucleation potency of inoculant particles in the Al-Nb-B master alloy: Modeling and experiments[J]. Metall. Mater. Trans., 2021, 52A: 1077
27 Si J M, Ren Z Y, Zhang G W. Effect of electric field solidification parameters on microstructure and properties of ZL114A alloy[J]. Foundry Technol., 2014, 35: 749
  司金梅, 任智勇, 张国伟. 电场凝固参数对ZL114A铝合金组织与性能的影响[J]. 铸造技术, 2014, 35: 749
28 Tian S K, Jin Y P, Wang P, et al. Effect of aging treatment on mechanical properties and microstructure of low pressure cast ZL114A alloy[J]. Heat Treat. Met., 2024, 49(1): 179
  田少鲲, 金圆平, 王 萍 等. 时效处理对低压铸造ZL114A合金力学性能及显微组织的影响[J]. 金属热处理, 2024, 49(1): 179
29 Chen Y S, Lu G, Yan Q S, et al. Mechanical properties and creep mechanism of yttrium and cerium modified ZL114A alloy via vacuum counter-pressure casting[J]. J. Mech. Eng., 2023, 59(18): 186
  陈义斯, 芦 刚, 严青松 等. 稀土钇、铈变质真空差压铸造ZL114A合金的力学性能及蠕变机制[J]. 机械工程学报, 2023, 59(18): 186
30 Chai G C, B?ckerud L, R?lland T, et al. Dendrite coherency during equiaxed solidification in binary aluminum alloys[J]. Metall. Mater. Trans., 1995, 26A: 965
31 Goulart P R, Spinelli J E, Osório W R, et al. Mechanical properties as a function of microstructure and solidification thermal variables of Al-Si castings[J]. Mater. Sci. Eng., 2006, A421: 245
32 Elsebaie O, Samuel A M, Samuel F H. Effects of Sr-modification, iron-based intermetallics and aging treatment on the impact toughness of 356 Al-Si-Mg alloy[J]. J. Mater. Sci., 2011, 46: 3027
33 Bolzoni L, Nowak M, Hari Babu N. Grain refinement of Al-Si alloys by Nb-B inoculation. Part II: Application to commercial alloys[J]. Mater. Des., 2015, 66: 376
34 Li Y, Bai Q L, Liu J C, et al. The influences of grain size and morphology on the hot tearing susceptibility, contraction, and load behaviors of AA7050 alloy inoculated with Al-5Ti-1B master alloy[J]. Metall. Mater. Trans., 2016, 47A: 4024
35 Wan J, Yang J L, Zhou X Y, et al. Superior tensile properties of graphene/Al composites assisted by in-situ alumina nanoparticles[J]. Carbon, 2023, 204: 447
36 Wang B B, Xie G M, Wu L H, et al. Grain size effect on tensile deformation behaviors of pure aluminum[J]. Mater. Sci. Eng., 2021, A820: 141504
37 Basavakumar K G, Mukunda P G, Chakraborty M. Influence of grain refinement and modification on microstructure and mechanical properties of Al-7Si and Al-7Si-2.5Cu cast alloys[J]. Mater. Charact., 2008, 59: 283
Outlines

/