Research paper

Microstructure Models Adaptability and Its Application in Ring Rolling Process of GH4169 Superalloy

  • WEI Zhen ,
  • LI Xin ,
  • JIANG He ,
  • WANG Chuan ,
  • DONG Jianxin
Expand
  • School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China
JIANG He, professor, Tel: 13811910685, E-mail: jianghe@ustb.edu.cn

Received date: 2024-03-01

  Revised date: 2024-07-19

  Online published: 2024-10-22

Supported by

National Natural Science Foundation of China(92160201);Wuxi Industry Foreseeing and Key Technology Research and Development Projects(G20191004)

Abstract

Superalloy ring forgings are a class of prototypical rotary components extensively used in casings, combustion chambers, sealing rings, and support rings in the aviation, aerospace, and nuclear energy fields. These components are often subjected to severe conditions, such as high temperatures, pressures, and rotational speeds as well as the combined effects of high- and low-frequency vibrations. As a result, these ring forgings exhibit excellent mechanical properties and thermal endurance. The microstructure determines the overall mechanical properties of the ring forgings. Their production is complex and involves multiple cycles of thermal deformation. During the thermal deformation phase, the alloy's microstructure undergoes a series of alterations due to the synergistic effects of thermal and mechanical forces. If recrystallization in the preceding stage is incomplete, the resulting microstructure may become heterogeneous and can be carried over to later stages, potentially leading to the formation of mixed crystals. This phenomenon can considerably affect the mechanical performance of ring forgings. Currently, the preparation and formation of ring forgings in China largely rely on traditional “experience-based optimization” approach, which is time-consuming and costly. Therefore, it is essential to establish an accurate microstructural evolution model and predict microstructural changes during thermal processing using numerical simulations. These improvements will enable better control of the alloy microstructure and the optimization of the manufacturing process. To better understand the complex microstructural evolution during the superalloy ring forging formation process, the adaptability of the existing GH4169 alloy microstructure model to the ring rolling process was investigated. Due to the highly nonlinear relationships between the recrystallization kinetics equations and factors such as the strain rate, temperature, and duration of ring rolling, the existing microstructure model was modified. Both the existing and modified models were programmed in FORTRAN language and implemented in Simufact software to simulate microstructural evolution during ring rolling. A numerical simulation method that captures the microstructure inheritance over multiple processing steps was established. The modified model's accuracy and simulation method's feasibility were verified through experiments. A comparative analysis of typical mixed-crystal regions in ring forgings using EBSD and the established numerical simulation, showed that the recrystallized structure of ring forgings combines dynamic and meta-dynamic recrystallization structures. Finally, the established simulation method was employed to analyze the effect of pass deformation on the microstructure during two-pass ring rolling. The results showed that increasing the final rolling deformation improved the uniformity of the ring forgings' microstructure.

Cite this article

WEI Zhen , LI Xin , JIANG He , WANG Chuan , DONG Jianxin . Microstructure Models Adaptability and Its Application in Ring Rolling Process of GH4169 Superalloy[J]. Acta Metall Sin, 2026 , 62(3) : 497 -508 . DOI: 10.11900/0412.1961.2024.00064

References

[1] Xie D, Wang Y, Ouyang Q Y, et al. Analytical calculation model for radial-axial coordinated feed strategy in large-scale flat ring rolling based on ultimate bending moment [J]. J. Mater. Process. Technol., 2023, 319: 118072
[2] Lin Y C, Qian S S, Chen X M, et al. Staggered spinning of thin-walled Hastelloy C-276 cylindrical parts: Numerical simulation and experimental investigation [J]. Thin-Walled Struct., 2019, 140: 466
[3] Lv N, Liu D, Yang Y H, et al. Studying the residual stress homogenization and relief in aerospace rolling ring of GH4169 alloy using ageing treatment [J]. Int. J. Adv. Manuf. Technol., 2021, 112: 3415
[4] Hu Y, Liu D, Yang Y H, et al. Multi-objective optimization of cavity design for GH4738 superalloy profile ring rolling process based on FEM and RSM [J]. Int. J. Adv. Manuf. Technol., 2022, 123: 2929
[5] Jiang H, He F Y, Xu L, et al. Research progress on ring rolling technology of superalloy ring forging [J]. Rare Met. Mater. Eng., 2021, 50: 1860
  江 河, 何方有, 许 亮 等. 高温合金环形件环轧工艺研究进展 [J]. 稀有金属材料与工程, 2021, 50: 1860
[6] Chen M C, Zhu C D, Yu Z Q, et al. A novel process for manufacturing large-diameter thin-walled metal ring: Double-roll pendulum hot rotary forging technology [J]. J. Manuf. Process., 2022, 76: 379
[7] Xiao G F, Xia Q X, Zhang Y L, et al. Manufacturing of Ni-based superalloy thin-walled components by complex strain-path spinning combined with solution heat treatment [J]. Int. J. Adv. Manuf. Technol., 2021, 117: 199
[8] Chen M S, Wang G Q, Li H B, et al. Annealing treatment methods and mechanisms for refining mixed and coarse grains in a solution treatment nickel-based superalloy [J]. Adv. Eng. Mater., 2019, 21: 9
[9] Chen M S, Zou Z H, Lin Y C, et al. Microstructural evolution and grain refinement mechanisms of a Ni-based superalloy during a two-stage annealing treatment [J]. Mater. Charact., 2019, 151: 445
[10] Yuan S J, Fan X B. Developments and perspectives on the precision forming processes for ultra-large size integrated components [J]. Int. J. Extrem. Manuf., 2019, 1: 022002
[11] Qi H P, Li Y T. Research status and developing trends on the ring rolling process of profile ring parts [A]. International Conference on the Technology of Plasticity [C]. Cambridge: Elsevier, 2017: 1260
[12] Zhang B Y, Wang Z T, Yu H, et al. Microstructural origin and control mechanism of the mixed grain structure in Ni-based superalloys [J]. J. Alloys Compd., 2022, 900: 163515
[13] Hu Y, Liu D, Zhu X L, et al. Effect of rolling passes on thermal parameters and microstructure evolution via ring-rolling process of GH4738 superalloy [J]. Int. J. Adv. Manuf. Technol., 2018, 96: 1165
[14] Sun Z C, Yang H, Ou X Z. Effects of process parameters on microstructural evolution during hot ring rolling of AISI 5140 steel [J]. Comput. Mater. Sci., 2010, 49: 134
[15] Zhu X L, Liu D, Xing L J, et al. Microstructure evolution of inconel 718 alloy during ring rolling process [J]. Int. J. Precis. Eng. Manuf., 2016, 17: 775
[16] Li L H, Dong J X, Zhang M C, et al. Integrated simulation of the forging process for GH4738 alloy turbine disk and its application [J]. Acta Metall. Sin., 2014, 50: 821
  李林翰, 董建新, 张麦仓 等. GH4738合金涡轮盘锻造过程的集成式模拟及应用 [J]. 金属学报, 2014, 50: 821
[17] Li X J, Cui Z S, Feng C, et al. Multi-scale simulation on the whole integrated forming process for nuclear pressure vessel head and over cone [J]. J. Plast. Eng., 2016, 23: 1
  李馨家, 崔振山, 冯 超 等. 核电封头-过渡锥体一体化成形全工艺过程多尺度模拟 [J]. 塑性工程学报, 2016, 23: 1
[18] Na Y S, Yeom J T, Park N K, et al. Simulation of microstructures for alloy 718 blade forging using 3D FEM simulator [J]. J. Mater. Process. Technol., 2003, 141: 337
[19] Yeom J T, Lee C S, Kim J H, et al. Finite-element analysis of microstructure evolution in the cogging of an alloy 718 ingot [J]. Mater. Sci. Eng., 2007, A449-451: 722
[20] Cui Z S, Liu C. Numerical prediction and experimental research of microstructure development during hot rolling [J]. J. Mech. Eng. 2000, 36(7): 92
  崔振山, 刘 才. 热轧过程微观组织演变的数值预报与试验研究 [J]. 机械工程学报, 2000, 36(7): 92
[21] Yao Z H. Microstructure evolution model and its application during hot deformation for GH864 superalloy [D]. Beijing: University of Science and Technology Beijing, 2011
  姚志浩. GH864合金热变形过程组织演化模型及其应用 [D]. 北京: 北京科技大学, 2011
[22] Jiang S C, Zhang J, He Y H, et al. Microstructure evolution and processing maps of GH4169 during deformation [J]. Iron Steel Vanadium Titanium, 2021, 42(2): 161
  蒋世川, 张 健, 何云华 等. GH4169合金高温变形显微组织演变及热加工图 [J]. 钢铁钒钛, 2021, 42(2): 161
[23] Liu X Z. Research on high temperature ring rolling forming process of ring workpiece of GH4738 alloy [D]. Harbin: Harbin Institute of Technology, 2017
  刘信祖. GH4738合金环形件高温环轧成形工艺研究 [D]. 哈尔滨: 哈尔滨工业大学, 2017
[24] Tang X F, Wang B Y, Zhang H, et al. Study on the microstructure evolution during radial-axial ring rolling of IN718 using a unified internal state variable material model [J]. Int. J. Mech. Sci., 2017, 128-129: 235
[25] Li Y L, Zeng M T, Tan Y B, et al. Microstructure evolution of Inconel 718 superalloy with fine-grains at different strain during hot deformation [J]. Chin. J. Rare Met., 2023, 47: 807
  李应隆, 曾梦婷, 谭元标 等. 应变量对细晶Inconel 718高温合金热变形组织演变的影响 [J]. 稀有金属, 2023, 47: 807
[26] Nicola? A, Franchet J M, Cormier J, et al. Discrimination of dynamically and post-dynamically recrystallized grains based on EBSD data: Application to Inconel 718 [J]. J. Microsc., 2019, 273: 135
[27] Nicola? A, Fiorucci G, Franchet J M, et al. Influence of strain rate on subsolvus dynamic and post-dynamic recrystallization kinetics of Inconel 718 [J]. Acta Mater., 2019, 174: 406
[28] Lin Y C, Wu X Y, Chen X M, et al. EBSD study of a hot deformed nickel-based superalloy [J]. J. Alloys Compd., 2015, 640: 101
[29] Chen X M, Lin Y C, Chen M S, et al. Microstructural evolution of a nickel-based superalloy during hot deformation [J]. Mater. Des., 2015, 77: 41
Outlines

/