Effects of Solution Post-Treatment on Precipitation Evolution During Aging of GH4706 Alloy and Its Mechanical Properties
Received date: 2024-03-24
Revised date: 2024-08-04
Online published: 2024-09-26
Supported by
National Key Research and Development Program of China(2022YFB3705102)
GH4706 alloy is used for industrial gas turbine disks owing to its excellent properties, including high creep resistance, tensile strength, toughness, and microstructural stability up to approximately 650 oC. However, the increasing weight and size of large turbine disks have limited the cooling rate following the solution treatment, which hinders the control of the microstructure and mechanical properties of large GH4706 alloy disks. Herein, four solution post-treatments were conducted on a 1500-mm-diameter disk manufactured from GH4706 alloy after being treated at 980 oC for 4 h: air cooling + air cooling (AA), furnace cooling to 825 oC and stabilization treatment followed by air cooling (FSA), furnace cooling to 825 oC followed by air cooling (FA), and furnace cooling to 825 oC followed by asbestos cooling (FAs). The evolution of precipitates during aging (including for γ'/γ" coprecipitation and η phase) and their effects on mechanical properties were analyzed. Results indicated that reducing the cooling rate from 980 oC to 825 oC promoted the precipitation and growth of the η phase, leading to Ni and Ti consumptions. This inhibited γ'/γ" coprecipitation around the large η phase, thereby favoring the formation of a cellular microstructure. Further reduction in cooling rate from 825 oC to 600 oC substantially accelerated the growth of γ'/γ" coprecipitates into cubic forms. The volume fractions of the cellular microstructure in the FSA, FA, and FAs treatments were 4.1%, 1.0%, and 1.8%, respectively. The AA and FA treatments had negligible effects on the tensile properties of GH4706 alloy at room temperature; meanwhile, the FSA treatment slightly decreased tensile ductility. The FAs treatment led to a notable reduction in yield strength at room temperature. In impact testing at room temperature, the cellular microstructure accelerated crack initiation and propagation, resulting in a 64% lower impact toughness of GH4706 alloy for the FSA treatment compared to that for the AA treatment. However, during stress rupture testing at 650 oC, the cellular microstructure effectively hindered crack propagation and the growth and aggregation of micropores, thereby extending the rupture life. However, the FAs treatment reduced the rupture life due to strength loss caused by the large γ'/γ" coprecipitates. The FA treatment fostered an optimal level of cellular microstructure, thereby increasing the rupture life while maintaining excellent tensile and impact properties at room temperature, demonstrating remarkable overall mechanical properties.
WANG Chong , WANG Lei , DUAN Ran , TIAN Qiang , HUANG Shuo , ZHAO Guangpu . Effects of Solution Post-Treatment on Precipitation Evolution During Aging of GH4706 Alloy and Its Mechanical Properties[J]. Acta Metall Sin, 2025 , 61(11) : 1638 -1652 . DOI: 10.11900/0412.1961.2024.00090
| [1] | Mukherji D, Gilles R, Barbier B, et al. Lattice misfit measurement in Inconel 706 containing coherent γ′ and γ″ precipitates [J]. Scr. Mater., 2003, 48: 333 |
| [2] | Wanderka N, Naundorf V, Banhart J, et al. Microstructural characterization of Inconel 706 alloy [J]. Surf. Interface Anal., 2004, 36: 546 |
| [3] | Schilke P W, Schwant R C. Alloy 706 use, process optimization, and future directions for GE gas turbine rotor materials [A]. Superalloys 718, 625, 706 and Various Derivatives [C]. Warrendale: TMS, 2001: 25 |
| [4] | Fesland J P, Petit P. Manufacturing Alloy 706 forgings [A]. Superalloys 718, 625, 706 and Various Derivatives [C]. Warrendale: TMS, 1994: 229 |
| [5] | Petit P, Fesland J P. Manufacturing of large In 706 and In 718 forging parts [A]. Superalloys 718, 625, 706 and Various Derivatives [C]. Warrendale: TMS, 1997: 153 |
| [6] | Kim C, Park J, Hong H U, et al. Role of stabilization heat treatment inducing γ′-γ″ co-precipitates and grain boundary η phase on tensile and creep behaviors of Inconel 706 [J]. J. Alloys Compd., 2022, 900: 163479 |
| [7] | Zhang S, Zeng L R, Zhao D Q, et al. Comparison study of microstructure and mechanical properties of standard and direct-aging heat treated superalloy Inconel 706 [J]. Mater. Sci. Eng., 2022, A839: 142836 |
| [8] | Oh H, Kim S, Kim J G, et al. Low cycle fatigue behavior of Inconel 706 at 650 oC [J]. J. Mater. Res. Technol., 2022, 17: 2624 |
| [9] | Del Genovese D, Strunz P, Mukherji D, et al. Microstructural characterization of a modified 706-type Ni-Fe superalloy by small-angle neutron scattering and electron microscopy [J]. Metall. Mater. Trans., 2005, 36A: 3439 |
| [10] | Shibata T, Takahashi T, Shudo Y, et al. Effect of cooling rate from solution treatment on precipitation behavior and mechanical properties of Alloy 706 [A]. Superalloys 718, 625, 706 and Various Derivatives [C]. Warrendale: TMS, 1997: 379 |
| [11] | Geng L, Na Y S, Park N K. Continuous cooling transformation behavior of Alloy 718 [J]. Mater. Lett., 1997, 30: 401 |
| [12] | Huang S, Wang L, Zhang B J, et al. Effect of stabilization time on precipitation behavior and mechanical properties of GH4706 alloy [J]. Rare Met. Mater. Eng., 2015, 44: 219 |
| 黄 烁, 王 磊, 张北江 等. 稳化处理时间对GH4706合金显微组织演化及力学性能的影响[J]. 稀有金属材料与工程, 2015, 44: 219 | |
| [13] | Kim H, Oh H, Bae H J, et al. Effect of heat treatment conditions on the plastic deformation behavior of the Inconel 706 alloy [J]. J. Mater. Res. Technol., 2022, 21: 2145 |
| [14] | Shibata T, Shudo Y, Takahashi T, et al. Effect of stabilizing treatment on precipitation behavior of Alloy 706 [A]. Superalloys 1996 [C]. Warrendale: TMS, 1996: 627 |
| [15] | Zhang S, Zhang A W, Chang L T, et al. Effect of phosphorus on the stress rupture properties of IN706 superalloy [J]. Mater. Sci. Eng., 2019, A761: 137981 |
| [16] | Mukherji D, Strunz P, Del Genovese D, et al. Investigation of microstructural changes in Inconel 706 at high temperatures by in-situ small-angle neutron scattering [J]. Metall. Mater. Trans., 2003, 34A: 2781 |
| [17] | Heck K A. The time-temperature-transformation behavior of Alloy 706 [A]. Superalloys 718, 625, 706 and Various Derivatives [C]. Warrendale: TMS, 1994: 393 |
| [18] | Shibata T, Shudo Y, Yoshino Y. Effects of aluminum, titanium and NioBium on the time-temperature-precipitation behavior of Alloy 706 [A]. Superalloys 1996 [C]. Warrendale: TMS, 1996: 153 |
| [19] | Pickering E J, Mathur H, Bhowmik A, et al. Grain-boundary precipitation in Allvac 718Plus [J]. Acta Mater., 2012, 60: 2757 |
| [20] | Asgari S, Sharghi-Moshtaghin R, SadeghAhmadi M, et al. On phase transformations in a Ni-based superalloy [J]. Philos. Mag., 2013, 93: 1351 |
| [21] | Yang Y H, Yu J J, Sun X F, et al. Investigation of impact toughness of a Ni-based superalloy at elevated temperature [J]. Mater. Des., 2012, 36: 699 |
| [22] | Schilke P W, Pepe J J, Schwant R C. Alloy 706 metallurgy and turbine wheel application [A]. Superalloys 718, 625, 706 and Various Derivatives [C]. Warrendale: TMS, 1994: 1 |
| [23] | Zhao J C, Ravikumar V, Beltran A M. Phase precipitation and phase stability in nimonic 263 [J]. Metall. Mater. Trans., 2001, 32A: 1271 |
| [24] | Hou K L, Ou M Q, Wang M, et al. Precipitation of η phase and its effects on stress rupture properties of K4750 alloy [J]. Mater. Sci. Eng., 2019, A763: 138137 |
| [25] | Theska F, Stanojevic A, Oberwinkler B, et al. Microstructure-property relationships in directly aged Alloy 718 turbine disks [J]. Mater. Sci. Eng., 2020, A776: 138967 |
| [26] | Devaux A, Nazé L, Molins R, et al. Gamma double prime precipitation kinetic in Alloy 718 [J]. Mater. Sci. Eng., 2008, A486: 117 |
| [27] | Zhao Y A, Guan K, Yang Z W, et al. The effect of subsequent heat treatment on the evolution behavior of second phase particles and mechanical properties of the Inconel 718 superalloy manufactured by selective laser melting [J]. Mater. Sci. Eng., 2020, A794: 139931 |
| [28] | Liu F, Sun W R, Yang S L, et al. Effects of Al content on microstructure and stability of GH4169 nickel base alloy [J]. Acta Metall. Sin., 2008, 44: 791 |
| 刘 芳, 孙文儒, 杨树林 等. Al含量对GH4169镍基合金组织及其稳定性的影响 [J]. 金属学报, 2008, 44: 791 | |
| [29] | ?zgün ?, Y?lmaz R, Gülsoy H ?, et al. The effect of aging treatment on the fracture toughness and impact strength of injection molded Ni-625 superalloy parts [J]. Mater. Charact., 2015, 108: 8 |
| [30] | Taheri M, Jam J E, Beni M H, et al. The effect of service temperature on the impact strength and fracture toughness of GTD-111 superalloy [J]. Eng. Fail. Anal., 2021, 127: 105507 |
| [31] | Wang L. Mechanical Properties of Materials [M]. 4th Ed., Beijing: Chemical Industry Press, 2022: 4 |
| (王 磊, 材料的力学性能 [M]. 第4版. 北京: 化学工业出版社, 2022: 4) | |
| [32] | Tanguy B, Besson J, Piques R, et al. Ductile to brittle transition of an A508 steel characterized by Charpy impact test: Part II: Modeling of the Charpy transition curve [J]. Eng. Fract. Mech., 2005, 72: 413 |
| [33] | H?rkeg?rd G, Balbach W, St?rk K, et al. The influence of heat treatment on the mechanical behavior of IN706 [A]. Superalloys 718, 625, 706 and Various Derivatives [C]. Warrendale: TMS, 1997: 425 |
| [34] | Gao M, Dwyer D J, Wei R P. Chemical and microstructural aspects of creep crack growth in Inconel 718 alloy [A]. Superalloys 718, 625, 706 and Various Derivatives [C]. Warrendale: TMS, 1994: 581 |
| [35] | Peng B, Wang H, Zhou M, et al. Ultrastrong metallic materials via minimal lattice misfit and strong ordering effect [J]. Sci. China Mater., 2023, 66: 4182 |
/
| 〈 |
|
〉 |