Phase Field Simulation of γ' Phase Rafting in Single Crystal Superalloys Under Applied Stress
Received date: 2024-04-25
Revised date: 2024-09-10
Online published: 2024-09-24
Supported by
National Key Research and Development Program of China(2021YFA1600601)
Nickel-based single crystal superalloys are critical materials for manufacturing advanced aircraft engine blades. During operation, microstructural changes in alloys under the applied stress significantly influence their fatigue and creep performances. However, relying solely on experimental methods poses challenges in capturing the dynamic processes by which the applied stress affects the alloy microstructure. Utilizing computational simulations to study the impact of the applied stress on the rafted γ' phase in single crystal superalloys offers distinct advantages. In this study, specific slip systems activated within the γ matrix are identified based on the type of the applied stress and their intrinsic plastic strain is calculated. The simulation models the formation of rafting under the applied stress and investigates the evolution of the microstructure during the rafting process in nickel-based single crystal superalloys. This study focuses on the effect of plastic strain within γ channels on the formation of the rafting morphology during the early stages of creep formation. Plastic strain generated under externally applied tensile stress promotes the preferential growth of γ′ precipitates along specific directions, which is the primary cause of γ′ phase rafting. Moreover, the lattice misfit directly determines the type of rafting (N-type or P-type). The spacing of dislocations at the γ′/γ interfaces, such as along {001} planes, significantly affects the morphology (aspect ratio) of γ′ precipitates but does not influence the growth kinetics or volume of γ′ precipitates at a given time step. In contrast to tensile stress, shear stress induces rafting microstructure coarsening at angles of approximately 30° or 60° relative to the horizontal direction, closely associated with activated slip systems. Additionally, different combinations of slip systems can result in the distortion of γ channels.
Key words: applied stress; superalloy; rafting; phase field method; elastoplasticity
ZHANG Jinhu , XU Haisheng , GUO Hui , LI Xuexiong , XU Dongsheng , YANG Rui . Phase Field Simulation of γ' Phase Rafting in Single Crystal Superalloys Under Applied Stress[J]. Acta Metall Sin, 2025 , 61(12) : 1911 -1924 . DOI: 10.11900/0412.1961.2024.00121
| [1] | Feng Q, Lu S, Li W D, et al. Recent progress in alloy design and creep mechanism of γ'-strengthened Co-based superalloys [J]. Acta Metall. Sin., 2023, 59: 1125 |
| 冯 强, 路 松, 李文道 等. γ'相强化钴基高温合金成分设计与蠕变机理研究进展 [J]. 金属学报, 2023, 59: 1125 | |
| [2] | Zhang J, Wang L, Xie G, et al. Recent progress in research and development of nickel-based single crystal superalloys [J]. Acta Metall. Sin., 2023, 59: 1109 |
| 张 健, 王 莉, 谢 光 等. 镍基单晶高温合金的研发进展 [J]. 金属学报, 2023, 59: 1109 | |
| [3] | Zhao Y H. Stability of phase boundary between L12-Ni3Al phases: A phase field study [J]. Intermetallics, 2022, 144: 107528 |
| [4] | Zhou N, Shen C, Mills M J, et al. Phase field modeling of channel dislocation activity and γ' rafting in single crystal Ni-Al [J]. Acta Mater., 2007, 55: 5369 |
| [5] | Fredholm A, Strudel J L. On the creep resistance of some nickel base single crystals [A]. Proceedings of the Superalloys [C]. Warrendale, Pennsylvania, USA: TMS, 1984: 211 |
| [6] | Wang X G, Liu J L, Jin T, et al. Effects of temperature and stress on microstructural evolution during creep deformation of Ru-free and Ru-containing single crystal superalloys [J]. Adv. Eng. Mater., 2015, 17: 1034 |
| [7] | Yang M, Zhang J, Wei H, et al. Influence of cooling rate on the formation of bimodal microstructures in nickel-base superalloys during continuous two-step aging [J]. Comput. Mater. Sci., 2018, 149: 14 |
| [8] | Liu X J, Chen Y C, Lu Y, et al. Present research situation and prospect of multi-scale design in novel Co-based superalloys: A review [J]. Acta Metall. Sin., 2020, 56: 1 |
| 刘兴军, 陈悦超, 卢 勇 等. 新型钴基高温合金多尺度设计的研究现状与展望 [J]. 金属学报, 2020, 56: 1 | |
| [9] | Zhao Y H. Understanding and design of metallic alloys guided by phase-field simulations [J]. npj Comput. Mater., 2023, 9: 94 |
| [10] | Wang D, Li Y S, Shi S J, et al. Crystal plasticity phase-field simulation of creep property of Co-base single crystal superalloy with pre-rafting [J]. Comput. Mater. Sci., 2021, 199: 110763 |
| [11] | Yang M, Zhang J, Wei H, et al. A phase-field model for creep behavior in nickel-base single-crystal superalloy: Coupled with creep damage [J]. Scr. Mater., 2018, 147: 16 |
| [12] | Ali M A, Amin W, Shchyglo O, et al. 45-degree rafting in Ni-based superalloys: A combined phase-field and strain gradient crystal plasticity study [J]. Int. J. Plast., 2020, 128: 102659 |
| [13] | Gaubert A, Le Bouar Y, Finel A. Coupling phase field and viscoplasticity to study rafting in Ni-based superalloys [J]. Philos. Mag., 2010, 90: 375 |
| [14] | Zhang J H, Guo H, Xu H S, et al. Phase-field study on the formation of α variant clusters induced by elastoplastic stress field around the void in titanium alloys [J]. Comput. Mater. Sci., 2022, 215: 111781 |
| [15] | Zhou N, Shen C, Mills M, et al. Large-scale three-dimensional phase field simulation of γ'-rafting and creep deformation [J]. Philos. Mag., 2010, 90: 405 |
| [16] | Kim S G, Kim W T, Suzuki T. Phase-field model for binary alloys [J]. Phys. Rev., 1999, 60E: 7186 |
| [17] | Chen L Q, Zhao Y H. From classical thermodynamics to phase-field method [J]. Prog. Mater. Sci., 2022, 124: 100868 |
| [18] | Wang Y U, Jin Y M, Khachaturyan A G. Phase field microelasticity theory and modeling of elastically and structurally inhomogeneous solid [J]. J. Appl. Phys., 2002, 92: 1351 |
| [19] | Khachaturyan A G. Theory of Structural Transformations in Solids [M]. New York: John Wiley & Sons, 1983: 201 |
| [20] | Zhang J H, Xu D S, Wang Y Z, et al. Influences of dislocations on nucleation and micro-texture formation of α phase in Ti-6Al-4V alloy [J]. Acta Metall. Sin., 2016, 52: 905 |
| 张金虎, 徐东生, 王云志 等. 位错对Ti-6Al-4V合金α相形核及微织构形成的影响 [J]. 金属学报, 2016, 52: 905 | |
| [21] | Zhou N, Shen C, Sarosi P M, et al. γ' rafting in single crystal blade alloys: A simulation study [J]. Mater. Sci. Technol., 2009, 25: 205 |
| [22] | Buffiere J Y, Ignat M. A dislocation based criterion for the raft formation in nickel-based superalloys single crystals [J]. Acta Metall. Mater., 1995, 43: 1791 |
| [23] | Wang D, Li Y S, Shi S J, et al. Phase-field simulation of γ' precipitates rafting and creep property of Co-base superalloys [J]. Mater. Des., 2020, 196: 109077 |
| [24] | Wang Y Z, Li J. Phase field modeling of defects and deformation [J]. Acta Mater., 2010, 58: 1212 |
| [25] | Shen C, Wang Y. Incorporation of γ-surface to phase field model of dislocations: Simulating dislocation dissociation in fcc crystals [J]. Acta Mater., 2004, 52: 683 |
| [26] | Zhao Y, Zhang H Y, Wei H, et al. Progress of phase-field investigations of γ' rafting in nickel-base single-crystal superalloys [J]. Chin. Sci. Bull., 2014, 59: 1684 |
| [27] | Shen C, Mills M J, Wang Y Z. Modeling dislocation dissociation and cutting of γ' precipitates in Ni-based superalloys by the phase field method [J]. MRS Online Proc. Library, 2002, 753: 521 |
| [28] | Shi S J, Li Y S, Yan Z W, et al. Crystal plasticity phase-field simulation of slip system anisotropy during creep of Co-Al-V monocrystal alloy under multidirectional strain [J]. Int. J. Mech. Sci., 2022, 227: 107436 |
/
| 〈 |
|
〉 |