Effects of Powder Molding Process on the Microstructure and Mechanical Properties of As-Sintered Ultrafine- Grained WC-12Co Cemented Carbides
Received date: 2024-01-17
Revised date: 2024-07-21
Online published: 2024-09-06
Supported by
National Key Research and Development Program of China(2022YFB3708800);National Natural Science Foundation of China(52171061);National Natural Science Foundation of China(92163107);National Natural Science Foundation of China(52101032)
The quality of the green body is crucial for achieving excellent mechanical properties in sintered cemented carbides via the powder metallurgy process, making it necessary to explore and optimize the powder molding process. In this study, the effects of the content and solution concentration of the pressing binder, as well as the green density during the powder molding process, on the geometries, microstructures, and mechanical properties of sintered WC-12Co cemented carbides were investigated. These materials were produced using in situ synthesized ultrafine WC-Co composite powder as the raw material. The results indicated that increasing the polyethylene glycol (PEG) content as the pressing binder within a certain range led to a linear increase in the magnetic Co content of the sintered cemented carbides. The concentration of the PEG solution primarily influenced its dispersion in the powder and feedstock particle size. Both of which considerably influenced the phase constitution, density, and mechanical properties of the prepared cemented carbides. During the pressing process, as the green density increased within a certain range, the shrinkage rate of the sintered alloys exhibited a good linear relationship with it. Additionally, the density of the cemented carbides initially increased notably and then stabilized, whereas the fracture strength initially increased and then decreased. By optimizing the conditions to 1.5% PEG content, 4.1% PEG concentration, and a green density of 7.7 g/cm3, the sintered cemented carbide achieved an exceptional average transverse rupture strength of 4571 MPa with minimal fluctuations in the measured values. The formation of numerous Co-rich nanophases within the WC grains, which hinder dislocation movement, is the primary reason for the enhanced strength of the cemented carbide.
WANG Chao , WANG Haibin , XUAN Shilei , LIU Xuan , LIU Xuemei , SONG Xiaoyan . Effects of Powder Molding Process on the Microstructure and Mechanical Properties of As-Sintered Ultrafine- Grained WC-12Co Cemented Carbides[J]. Acta Metall Sin, 2025 , 61(10) : 1579 -1592 . DOI: 10.11900/0412.1961.2024.00013
| [1] | Wang K W, Zhao K, Liu J L, et al. Interplay of microstructure and mechanical properties of WC-6Co cemented carbides by hot oscillating pressing method [J]. Ceram. Int., 2021, 47: 20731 |
| [2] | Ke Z, Zheng Y, Zhang G T, et al. Microstructure and mechanical properties of dual-grain structured WC-Co cemented carbides [J]. Ceram. Int., 2019, 45: 21528 |
| [3] | Li M, Gong M F, Zhang C Y, et al. Research progress of sintering technique of ultrafine and Nano WC-Co cemented carbides [J]. Mater. Rep., 2020, 34: 15138 |
| 李 萌, 弓满锋, 张程煜 等. 超细、纳米晶WC-Co硬质合金烧结技术的研究现状 [J]. 材料导报, 2020, 34: 15138 | |
| [4] | Yang J, Roa J J, Odén M, et al. 3D FIB/FESEM tomography of grinding-induced damage in WC-Co cemented carbides [J]. Procedia CIRP, 2020, 87: 385 |
| [5] | Saai A, Bj?rge R, Dahl F, et al. Adaptation of laboratory tests for the assessment of wear resistance of drill-bit inserts for rotary-percussive drilling of hard rocks [J]. Wear, 2020, 456-457: 203366 |
| [6] | Ding Q J, Zheng Y, Ke Z, et al. Effects of fine WC particle size on the microstructure and mechanical properties of WC-8Co cemented carbides with dual-scale and dual-morphology WC grains [J]. Int. J. Refract. Met. Hard Mater., 2020, 87: 105166 |
| [7] | Ortner H M, Ettmayer P, Kolaska H, et al. The history of the technological progress of hardmetals [J]. Int. J. Refract. Met. Hard Mater., 2015, 49: 3 |
| [8] | Martins V, Rodrigues W C, Ferrandini P L, et al. Comparative studies of WC-Co and WC-Co-Ni composites obtained by conventional powder metallurgy [J]. Mater. Res., 2011, 14: 274 |
| [9] | Stanciu V I, Erauw J P, Boilet L, et al. WC-Co composite made with doped binder: The effect of binder proportion on microstructure and mechanical properties [J]. Int. J. Refract. Met. Hard Mater., 2023, 112: 106161 |
| [10] | Guo X H. The latest study on extrusion molding binder and production technology of cemented carbide [J]. Rare Met. Cem. Carbides, 2014, 42(6): 46 |
| 郭幸华. 硬质合金挤压成形剂及生产技术研究进展 [J]. 稀有金属与硬质合金, 2014, 42(6): 46 | |
| [11] | Du W C, Ren X R, Pei Z J, et al. Ceramic binder jetting additive manufacturing: A literature review on density [J]. J. Manuf. Sci. Eng., 2020, 142: 040801 |
| [12] | Chen C Y. Research of effects of paraffin as pressing binder on properties of cemented carbide [J]. Fujian Metall., 2016, (5): 42 |
| 陈成艺. 石蜡成形剂改性对硬质合金影响的研究 [J]. 福建冶金, 2016, (5): 42 | |
| [13] | Chen S L, Fu K, Zhou J H, et al. Study on improvement of paraffin as the molding agent of cemented carbide [J]. Rare Met. Cem. Carbides, 2014, 42(3): 58 |
| 陈双琳, 付 坤, 周建华 等. 硬质合金成形剂石蜡的改进研究 [J]. 稀有金属与硬质合金, 2014, 42(3): 58 | |
| [14] | Liu J, Liu A H, Liu Y X, et al. Effect of 56# paraffin wax and PEG4000 on formability of cemented carbide inserts [J]. Cem. Carbides, 2023, 40: 134 |
| 刘 娟, 刘安虎, 刘雅璇 等. 56#石蜡和PEG 4000对硬质合金数控刀片成型性能的影响 [J]. 硬质合金, 2023, 40: 134 | |
| [15] | Qu X H, Gao J X, Qin M L, et al. Application of a wax-based binder in PIM of WC-TiC-Co cemented carbides [J]. Int. J. Refract. Met. Hard Mater., 2005, 23: 273 |
| [16] | Eso O, Wang X, Wolf S, et al. Property correlations of WC-Co with modified binders [J]. Int. J. Refract. Met. Hard Mater., 2024, 118: 106482. |
| [17] | Meng X W. Research on performance of new pressing binder in hardmetal [J]. Adv. Mater. Res., 2010, 148-149: 1730 |
| [18] | Sun D, Li G S, Lin C F, et al. Research on pre-debinding process of binders for ultrafine cemented carbide bar extrusion molding [J]. Powder Metall. Technol., 2010, 28: 262 |
| 孙 丹, 李广生, 林春芳 等. 超细硬质合金棒料挤压成形剂预脱除工艺研究 [J]. 粉末冶金技术, 2010, 28: 262 | |
| [19] | Hong H X, Sun A K, Wang D Z. Application of a new pressing binder composed of stearic acid and alcohol-soluble polyurethane resin [J]. Cem. Carbide, 2023, 40: 347 |
| 洪海侠, 孙翱魁, 王德志. 硬脂酸-醇溶性聚氨酯树脂新型成型剂的应用研究 [J]. 硬质合金, 2023, 40: 347 | |
| [20] | Zwiren A D, Murphy T F. Comparison of SS-316L PM material processed via binder jetting with SS-316L powder processed by pressing and sintering [J]. Int. J. Powder Metall., 2018, 54: 39 |
| [21] | Zhang W F. Study on preparation of ultrafine hardmetal rods [D]. Wuhan: Wuhan University of Technology, 2004 |
| 张卫丰. 超细硬质合金棒材的制备研究 [D]. 武汉: 武汉理工大学, 2004 | |
| [22] | Zhao L L, Zhang Y, Feng W, et al. Effect of shrinkage coefficient on compaction and physical property of cemented carbide die forming [J]. Tool Eng., 2019, 53(9): 62 |
| 赵丽丽, 张 严, 冯 文 等. 硬质合金模压成型收缩系数对压制性能与物理性能的影响 [J]. 工具技术, 2019, 53(9): 62 | |
| [23] | Liu W B, Song X Y, Zhang J X, et al. Preparation of ultrafine WC-Co composite powder by in situ reduction and carbonization reactions [J]. Int. J. Refract. Met. Hard Mater., 2009, 27: 115 |
| [24] | Liu X W, Song X Y, Wang H B, et al. Complexions in WC-Co cemented carbides [J]. Acta Mater., 2018, 149: 164 |
| [25] | Meng X W, Xu T. Application research on a new pressing binder for cemented carbide [J]. Cem. Carbide, 2011, 28: 158 |
| 孟小卫, 徐 涛. 新型硬质合金成型剂应用研究 [J]. 硬质合金, 2011, 28: 158 | |
| [26] | Zhu E T. Study on the preparation and properties of Nano WC-Co composite powder by in-situ synthesis and high performance cemented carbide [D]. Hefei: Hefei University of Technology, 2021 |
| 朱二涛. 原位合成纳米WC-Co复合粉末及高性能硬质合金制备和性能研究 [D]. 合肥: 合肥工业大学, 2021 | |
| [27] | Zhao C, Lu H, Wang H B, et al. Seeding ductile nanophase in ceramic grains [J]. Mater. Horiz., 2024, 11: 1908 |
/
| 〈 |
|
〉 |