Research paper

Effect of Stacking Fault Energy on the Dynamic Mechanical Properties and Deformation Mechanisms of CrMnFeCoNi High-Entropy Alloys

  • YIN Shipan ,
  • MENG Zeyu ,
  • HE Jingyao ,
  • LI Zezhou ,
  • ZHANG Fan ,
  • CHENG Xingwang
Expand
  • 1 School of Materials Science and Engineering, Beijing Institute of Technology, Beijing 100081, China
    2 National Key Laboratory of Science and Technology on Materials Under Shock and Impact, Beijing Institute of Technology, Beijing 100081, China
    3 Tangshan Research Institute, Beijing Institute of Technology, Tangshan 063000, China
ZHANG Fan, professor, Tel: 13581586228, E-mail: fanzhang@bit.edu.cn; CHENG Xingwang, professor, Tel: (010)68913951, E-mail: chengxw@bit.edu.cn

Received date: 2024-05-07

  Revised date: 2024-06-03

  Online published: 2024-08-15

Supported by

National Natural Science Foundation of China(52271141);National Key Laboratory Foundation of Science and Technology on Materials Under Shock and Impact(DZC2022-1)

Abstract

CrMnFeCoNi high-entropy alloys (HEAs) have attracted considerable attention because of their excellent mechanical properties. Furthermore, these alloys exhibit high energy absorption characteristics under high-strain rate deformation for various deformation modes. The stacking fault energy (SFE) plays a crucial role in improving the deformation modes and mechanical properties. Only few studies have investigated the effect of SFE on the dynamic mechanical properties and deformation mode of CrMnFeCoNi series HEAs. In this work, the effect of SFE on the dynamic mechanical properties and deformation mechanism of CrMnFeCoNi HEAs were investigated through quasi-static and dynamic mechanical tests and microstructural analysis using CrMnFeCoNi (SFE of 35 mJ/m2) and Cr26Mn20Fe20Co20Ni14 (SFE of 23 mJ/m2) HEAs. Results indicate that CrMnFeCoNi and Cr26Mn20Fe20Co20Ni14 HEAs exhibit a strain-rate hardening effect under dynamic deformation. Furthermore, the flow stress, energy absorption ability, and work hardening index increase under static and dynamic conditions with the decrease in SFE. Under quasi-static compression, deformation occurs via dislocation gliding in CrMnFeCoNi, whereas deformation twinning is profound in Cr26Mn20Fe20Co20Ni14 HEA with low SFE; therefore, deformation is dominated by dislocation slip and twinning. The contribution of deformation twinning to the deformation strain increases with the increase in strain rates. In particular, deformation occurs via dislocation gliding and twinning in CrMnFeCoNi HEA. Apart from dislocation slip and twinning, the interaction of twins and the transition from fcc to hcp structures provide additional deformation modes to accommodate the plastic deformation of Cr26Mn20Fe20Co20Ni14 HEA and improve the mechanical properties and energy absorption of these alloys. This work demonstrates that the change in SFE will lead to different deformation modes for accommodating plastic strain, thereby improving the mechanical properties of HEAs.

Cite this article

YIN Shipan , MENG Zeyu , HE Jingyao , LI Zezhou , ZHANG Fan , CHENG Xingwang . Effect of Stacking Fault Energy on the Dynamic Mechanical Properties and Deformation Mechanisms of CrMnFeCoNi High-Entropy Alloys[J]. Acta Metall Sin, 2025 , 61(12) : 1817 -1828 . DOI: 10.11900/0412.1961.2024.00133

References

[1] Yeh J W, Chen S K, Lin S J, et al. Nanostructured high-entropy alloys with multiple principal elements: Novel alloy design concepts and outcomes [J]. Adv. Eng. Mater., 2004, 6: 299
[2] Cantor B, Chang I T H, Knight P, et al. Microstructural development in equiatomic multicomponent alloys [J]. Mater. Sci. Eng., 2004, A375-377: 213
[3] Geant? V, Voiculescu I, Stef?noiu R, et al. Dynamic impact behaviour of high entropy alloys used in the military domain [J]. IOP Conf. Ser.: Mater. Sci. Eng., 2018, 374: 012041
[4] Zhao S T, Yin S, Liang X, et al. Deformation and failure of the CrCoNi medium-entropy alloy subjected to extreme shock loading [J]. Sci. Adv., 2023, 9: eadf8602
[5] Li Z Z, Zhao S T, Alotaibi S M, et al. Adiabatic shear localization in the CrMnFeCoNi high-entropy alloy [J]. Acta Mater., 2018, 151: 424
[6] Gludovatz B, Hohenwarter A, Catoor D, et al. A fracture-resistant high-entropy alloy for cryogenic applications [J]. Science, 2014, 345: 1153
[7] Liu D, Yu Q, Kabra S, et al. Exceptional fracture toughness of CrCoNi-based medium- and high-entropy alloys at 20 Kelvin [J]. Science, 2022, 378: 978
[8] Fan Z D, Li L, Chen Z H, et al. Temperature-dependent yield stress of single crystals of non-equiatomic Cr-Mn-Fe-Co-Ni high-entropy alloys in the temperature range 10-1173 K [J]. Acta Mater., 2023, 246: 118712
[9] Naeem M, He H Y, Harjo S, et al. Temperature-dependent hardening contributions in CrFeCoNi high-entropy alloy [J]. Acta Mater., 2021, 221: 117371
[10] Qiao Y, Chen Y, Cao F H, et al. Dynamic behavior of CrMnFeCoNi high-entropy alloy in impact tension [J]. Int. J. Impact Eng., 2021, 158: 104008
[11] He J Y, Wang Q, Zhang H S, et al. Dynamic deformation behavior of a face-centered cubic FeCoNiCrMn high-entropy alloy [J]. Sci. Bull., 2018, 63: 362
[12] An Z B, Mao S C, Liu Y N, et al. Inherent and multiple strain hardening imparting synergistic ultrahigh strength and ductility in a low stacking faulted heterogeneous high-entropy alloy [J]. Acta Mater., 2023, 243: 118516
[13] Gludovatz B, Hohenwarter A, Thurston K V S, et al. Exceptional damage-tolerance of a medium-entropy alloy CrCoNi at cryogenic temperatures [J]. Nat. Commun., 2016, 7: 10602
[14] Zhang F, Ren Y, Pei Z R, et al. Cooperative dislocations for pressure-dependent sequential deformation of multi-principal element alloys under shock loading [J]. Acta Mater., 2024, 276: 120150
[15] Otto F, Dlouhy A, Somsen C, et al. The influences of temperature and microstructure on the tensile properties of a CoCrFeMnNi high-entropy alloy [J]. Acta Mater., 2013, 61: 5743
[16] Laplanche G, Kostka A, Reinhart C, et al. Reasons for the superior mechanical properties of medium-entropy CrCoNi compared to high-entropy CrMnFeCoNi [J]. Acta Mater., 2017, 128: 292
[17] Li Z M. Interstitial equiatomic CoCrFeMnNi high-entropy alloys: Carbon content, microstructure, and compositional homogeneity effects on deformation behavior [J]. Acta Mater., 2019, 164: 400
[18] Deng Y, Tasan C C, Pradeep K G, et al. Design of a twinning-induced plasticity high entropy alloy [J]. Acta Mater., 2015, 94: 124
[19] Zhang Z J, Sheng H W, Wang Z J, et al. Dislocation mechanisms and 3D twin architectures generate exceptional strength-ductility-toughness combination in CrCoNi medium-entropy alloy [J]. Nat. Commun., 2017, 8: 14390
[20] Miao J, Slone C E, Smith T M, et al. The evolution of the deformation substructure in a Ni-Co-Cr equiatomic solid solution alloy [J]. Acta Mater., 2017, 132: 35
[21] Christian J W, Mahajan S. Deformation twinning [J]. Prog. Mater. Sci., 1995, 39: 1
[22] Wagner C, Laplanche G. Effects of stacking fault energy and temperature on grain boundary strengthening, intrinsic lattice strength and deformation mechanisms in CrMnFeCoNi high-entropy alloys with different Cr/Ni ratios [J]. Acta Mater., 2023, 244: 118541
[23] Moon J, Qi Y S, Tabachnikova E, et al. Microstructure and mechanical properties of high-entropy alloy Co20Cr26Fe20Mn20Ni14 processed by high-pressure torsion at 77 K and 300 K [J]. Sci. Rep., 2018, 8: 11074
[24] Moon J, Qi Y S, Tabachnikova E, et al. Deformation-induced phase transformation of Co20Cr26Fe20Mn20Ni14 high-entropy alloy during high-pressure torsion at 77 K [J]. Mater. Lett., 2017, 202: 86
[25] Gao X Z, Lu Y P, Liu J Z, et al. Extraordinary ductility and strain hardening of Cr26Mn20Fe20Co20Ni14 TWIP high-entropy alloy by cooperative planar slipping and twinning [J]. Materialia, 2019, 8: 100485
[26] Galindo-Nava E I, Rivera-Díaz-del-Castillo P E J. Understanding martensite and twin formation in austenitic steels: A model describing TRIP and TWIP effects [J]. Acta Mater., 2017, 128: 120
[27] Slone C E, Chakraborty S, Miao J, et al. Influence of deformation induced nanoscale twinning and FCC-HCP transformation on hardening and texture development in medium-entropy CrCoNi alloy [J]. Acta Mater., 2018, 158: 38
[28] Zhang T W, Ma S G, Zhao D, et al. Simultaneous enhancement of strength and ductility in a NiCoCrFe high-entropy alloy upon dynamic tension: Micromechanism and constitutive modeling [J]. Int. J. Plast., 2020, 124: 226
[29] Wang K, Jin X, Jiao Z M, et al. Mechanical behaviors and deformation constitutive equations of CrFeNi medium-entropy alloys under tensile conditions from 77 K to 1073 K [J]. Acta Metall. Sin., 2023, 59: 277
  王 凯, 晋 玺, 焦志明 等. CrFeNi中熵合金在宽温域拉伸条件下的力学行为与变形本构方程 [J]. 金属学报, 2023, 59: 277
[30] Wu X L, Yang M X, Jiang P, et al. Deformation nanotwins suppress shear banding during impact test of CrCoNi medium-entropy alloy [J]. Scr. Mater., 2020, 178: 452
[31] Chen J J, Ding Y T, Ma Y J, et al. Molecular dynamics simulation of tensile deformation behavior of monocrystalline Ni and its alloys with different stacking fault energies [J]. Rare Met. Mater. Eng., 2023, 52: 3186
  陈建军, 丁雨田, 马元俊 等. 分子动力学模拟不同层错能单晶Ni及其合金拉伸变形行为 [J]. 稀有金属材料与工程, 2023, 52: 3186
[32] An X H, Wu S D, Zhang Z F. Influnece of stacking fault energy on the microstructures, tensile and fatigue properties of nanostructured Cu-Al alloys [J]. Acta Metall. Sin., 2014, 50: 191
  安祥海, 吴世丁, 张哲峰. 层错能对纳米晶Cu-Al合金微观结构、拉伸及疲劳性能的影响 [J]. 金属学报, 2014, 50: 191
[33] Tian C G, Tao X P, Xu L, et al. Effects of stacking fault energy and temperature on creep performance of Ni-based alloy with different Co contents [J]. Rare Met. Mater. Eng., 2021, 50: 3532
  田成刚, 陶稀鹏, 徐 玲 等. 层错能和温度对不同Co含量的镍基高温合金蠕变性能的影响 [J]. 稀有金属材料与工程, 2021, 50: 3532
[34] Zhang Z F, Li K Q, Cai T, et al. Effects of stacking fault energy on the deformation mechanisms and mechanical properties of face-centered cubic metals [J]. Acta Metall. Sin., 2023, 59: 467
  张哲峰, 李克强, 蔡 拓 等. 层错能对面心立方金属形变机制与力学性能的影响 [J]. 金属学报, 2023, 59: 467
[35] Wagner C, Ferrari A, Schreuer J, et al. Effects of Cr/Ni ratio on physical properties of Cr-Mn-Fe-Co-Ni high-entropy alloys [J]. Acta Mater., 2022, 227: 117693
[36] Meyers M A. Dynamic Behavior of Materials [M]. New York: John Wiley & Sons, 1994: 189
[37] Hollomon J H. Tensile Deformation [J]. Trans. Metall. Soc. AIME, 1945, 162: 268
[38] Zackay V F. High-Strength Materials [M]. New York: John Wiley & Sons. Inc., 1965: 436
[39] Xiao J W, Wu N, Ojo O, et al. Stacking fault and transformation-induced plasticity in nanocrystalline high-entropy alloys [J]. J. Mater. Res., 2021, 36: 2705
[40] Liu L X, Pan J, Zhang C, et al. Achieving high strength and ductility in a 3D-printed high entropy alloy by cooperative planar slipping and stacking fault [J]. Mater. Sci. Eng., 2022, A843: 143106
[41] Liu S F, Wu Y, Wang H T, et al. Stacking fault energy of face-centered-cubic high entropy alloys [J]. Intermetallics, 2018, 93: 269
[42] Gutierrez-Urrutia I, Raabe D. Dislocation and twin substructure evolution during strain hardening of an Fe-22 wt.% Mn-0.6 wt.% C TWIP steel observed by electron channeling contrast imaging [J]. Acta Mater., 2011, 59: 6449
[43] Beladi H, Timokhina I B, Estrin Y, et al. Orientation dependence of twinning and strain hardening behaviour of a high manganese twinning induced plasticity steel with polycrystalline structure [J]. Acta Mater., 2011, 59: 7787
[44] Williams J C, Baggerly R G, Paton N E. Deformation behavior of HCP Ti-Al alloy single crystals [J]. Metall. Mater. Trans., 2002, 33A: 837
[45] Huang D, Zhuang Y X, Wang C H. Advanced mechanical properties obtained via accurately tailoring stacking fault energy in Co-rich and Ni-depleted Co x Cr33Ni67 - x medium-entropy alloys [J]. Scr. Mater., 2022, 207: 114269
[46] Jiang W, Gao X Z, Guo Y Z, et al. Dynamic impact behavior and deformation mechanisms of Cr26Mn20Fe20Co20Ni14 high-entropy alloy [J]. Mater. Sci. Eng., 2021, A824: 141858
[47] De Cooman B C, Estrin Y, Kim S K. Twinning-induced plasticity (TWIP) steels [J]. Acta Mater., 2018, 142: 283
[48] Choi J H, Jo M C, Lee H, et al. Cu addition effects on TRIP to TWIP transition and tensile property improvement of ultra-high-strength austenitic high-Mn steels [J]. Acta Mater., 2019, 166: 246
[49] Liu G Y, Gu J, Ni S, et al. Microstructural evolution of Cu-Al alloys subjected to multi-axial compression [J]. Mater. Charact., 2015, 103: 107
[50] Xiao G H, Tao N R, Lu K. Microstructures and mechanical properties of a Cu-Zn alloy subjected to cryogenic dynamic plastic deformation [J]. Mater. Sci. Eng., 2009, A513-514: 13
[51] Xu Y J, Du K, Cui C Y, et al. Deformation twinning with zero macroscopic strain in a coarse-grained Ni-Co-based superalloy [J]. Scr. Mater., 2014, 77: 71
Outlines

/