Neural Network Molecular Dynamics Study of Ultrafast Laser-Induced Melting of Copper Nanofilms
Received date: 2024-05-07
Revised date: 2024-07-25
Online published: 2024-08-14
Supported by
National Natural Science Foundation of China(12104507);Science and Technology Innovation Program of Hunan Province(2021RC4026);Postgraduate Technology Innovation Program of Hunan Province(CX20220070)
Exploring ultrafast structural transitions in materials triggered by femtosecond laser pulses—from their condensed states to high-temperature, high-pressure conditions, and potentially to ideal plasmas—is a crucial scientific endeavor with profound implications for fields such as inertial confinement fusion, metal additive manufacturing, and laser processing. These extreme conditions, which are challenging to replicate and directly observe in experiments due to temporal and spatial resolution limitations, require theoretical models and simulations to decode the underlying microscopic mechanisms. Molecular dynamics (MD) simulations, especially when paired with advanced potential energy surfaces, are effective tools for addressing these challenges. However, maintaining a balance between computational efficiency and physical accuracy, particularly when simulating excited states induced by laser interactions, remains a formidable task. In this context, neural network potential energy surfaces (NNPES) have demonstrated exceptional capability for capturing the complex interactions and properties of materials under extreme conditions, providing vital links between quantum mechanics and macroscale phenomena. Using Cu as a prototypical example, the ability of NNPES to accurately depict lattice vibrations, thermophysical properties, and complex dynamics during laser-matter interactions has been demonstrated. By seamlessly integrating NNPES with a two-temperature MD model, this study directly simulates the atomic-scale dynamics of Cu thin films subjected to intense pulsed laser irradiation. This innovative approach, which combines quantum-level accuracy with large-scale thermodynamics and detailed microstructural evolution, provides unprecedented insights into the fundamental mechanisms of laser-induced melting. Our findings reveal two distinct melting behaviors in Cu, dependent on laser fluence. At fluences near the melting threshold, a heterogeneous melting process initiated at the film surface because of the lower free energy barrier was observed. The solid-liquid interface then moves inward at velocities of tens of meters per second, requiring hundreds of picoseconds for melting to complete. Conversely, at fluences well above the threshold, Cu films experience rapid and homogeneous melting, markedly different from conventional heating-induced melting. Here, the lattice temperature almost instantaneously exceeds the thermal stability limit, leading to uniform liquid nucleation and rapid growth throughout the film, culminating in complete melting within just tens of picoseconds. This study not only illuminates the atomic-scale dynamics of laser-induced melting but also underscores the transition from heterogeneous to homogeneous melting mechanisms as a function of laser fluence. This study serves as an invaluable research tool for enhancing our understanding of laser-matter interactions and their potential applications in optimizing laser-based manufacturing processes and predicting material behavior under extreme conditions. Moreover, the reliability and versatility of NNPES set the stage for extending the research to more complex systems, including alloys and amorphous materials. This expansion fosters robust connections between microscopic theories and macroscale applications, deepening our understanding of material responses to intense laser irradiation. Future studies employing this framework could explore complex physical phenomena such as explosive boiling and material disintegration during laser ablation, offering unique atomic-scale insights that could pave the way for groundbreaking discoveries and technological advancements.
GAO Tianyu , ZENG Qiyu , CHEN Bo , KANG Dongdong , DAI Jiayu . Neural Network Molecular Dynamics Study of Ultrafast Laser-Induced Melting of Copper Nanofilms[J]. Acta Metall Sin, 2024 , 60(10) : 1439 -1450 . DOI: 10.11900/0412.1961.2024.00143
| 1 | Abu-Shawareb H, Acree R, Adams P, et al. Lawson criterion for ignition exceeded in an inertial fusion experiment [J]. Phys. Rev. Lett., 2022, 129: 075001 |
| 2 | Shugaev M V, Wu C P, Armbruster O, et al. Fundamentals of ultrafast laser-material interaction [J]. MRS Bull., 2016, 41: 960 |
| 3 | Roy N K, Dibua O G, Jou W, et al. A comprehensive study of the sintering of copper nanoparticles using femtosecond, nanosecond, and continuous wave lasers [J]. J. Micro Nano-Manuf., 2018, 6: 010903 |
| 4 | Cheng C W, Chang C L, Chen J K, et al. Femtosecond laser melting of silver nanoparticles: Comparison of model simulations and experimental results [J]. Appl. Phys., 2018, 124A: 371 |
| 5 | Zhang H, Li C, Bevillon E, et al. Ultrafast destructuring of laser-irradiated tungsten: Thermal or nonthermal process [J]. Phys. Rev., 2016, 94B: 224103 |
| 6 | Chen Z, Mo M, Soulard L, et al. Interatomic potential in the nonequilibrium warm dense matter regime [J]. Phys. Rev. Lett., 2018, 121: 075002 |
| 7 | Ernstorfer R, Harb M, Hebeisen C T, et al. The formation of warm dense matter: Experimental evidence for electronic bond hardening in gold [J]. Science, 2009, 323: 1033 |
| 8 | Mo M Z, Chen Z, Li R K, et al. Heterogeneous to homogeneous melting transition visualized with ultrafast electron diffraction [J]. Science, 2018, 360: 1451 |
| 9 | Mo M Z, Murphy S, Chen Z J, et al. Visualization of ultrafast melting initiated from radiation-driven defects in solids [J]. Sci. Adv., 2019, 5: eaaw0392 |
| 10 | Wu J, Tang M X, Zhao L R, et al. Ultrafast atomic view of laser-induced melting and breathing motion of metallic liquid clusters with MeV ultrafast electron diffraction [J]. Proc. Natl. Acad. Sci. USA, 2022, 119: e2111949119 |
| 11 | Mahieu B, Jourdain N, Ta Phuoc K, et al. Probing warm dense matter using femtosecond X-ray absorption spectroscopy with a laser-produced betatron source [J]. Nat. Commun., 2018, 9: 3276 |
| 12 | Jourdain N, Lecherbourg L, Recoules V, et al. Ultrafast thermal melting in nonequilibrium warm dense copper [J]. Phys. Rev. Lett., 2021, 126: 065001 |
| 13 | Chen Z, Curry C B, Zhang R, et al. Ultrafast multi-cycle terahertz measurements of the electrical conductivity in strongly excited solids [J]. Nat. Commun., 2021, 12: 1638 |
| 14 | Hohlfeld J, Wellershoff S S, Gu?dde J, et al. Electron and lattice dynamics following optical excitation of metals [J]. Chem. Phys., 2000, 251: 237 |
| 15 | Lin Z B, Zhigilei L V. Thermal excitation of d band electrons in Au: Implications for laser-induced phase transformations [A]. Proceedings of SPIE 6261, High-Power Laser Ablation VI [C]. Taos: SPIE, 2006: 62610U |
| 16 | Lin Z B, Zhigilei L V, Celli V. Electron-phonon coupling and electron heat capacity of metals under conditions of strong electron-phonon nonequilibrium [J]. Phys. Rev., 2008, 77B: 075133 |
| 17 | Lee J W, Kim M, Kang G, et al. Investigation of nonequilibrium electronic dynamics of warm dense copper with femtosecond X-ray absorption spectroscopy [J]. Phys. Rev. Lett., 2021, 127: 175003 |
| 18 | Grolleau A, Dorchies F, Jourdain N, et al. Femtosecond resolution of the nonballistic electron energy transport in warm dense copper [J]. Phys. Rev. Lett., 2021, 127: 275901 |
| 19 | Lin Z B, Zhigilei L V. Time-resolved diffraction profiles and atomic dynamics in short-pulse laser-induced structural transformations: Molecular dynamics study [J]. Phys. Rev., 2006, 73B: 184113 |
| 20 | Molina J M, White T G. A molecular dynamics study of laser-excited gold [J]. Matter Radiat. Extremes, 2022, 7: 036901 |
| 21 | Ivanov D S, Zhigilei L V. Effect of pressure relaxation on the mechanisms of short-pulse laser melting [J]. Phys. Rev. Lett., 2003, 91: 105701 |
| 22 | Daraszewicz S L, Giret Y, Naruse N, et al. Structural dynamics of laser-irradiated gold nanofilms [J]. Phys. Rev., 2013, 88B: 184101 |
| 23 | Murphy S T, Daraszewicz S L, Giret Y, et al. Dynamical simulations of an electronically induced solid-solid phase transformation in tungsten [J]. Phys. Rev., 2015, 92B: 134110 |
| 24 | Murphy S T, Giret Y, Daraszewicz S L, et al. Contribution of electronic excitation to the structural evolution of ultrafast laser-irradiated tungsten nanofilms [J]. Phys. Rev., 2016, 93B: 104105 |
| 25 | Arefev M I, Shugaev M V, Zhigilei L V. Kinetics of laser-induced melting of thin gold film: How slow can it get? [J]. Sci. Adv., 2022, 8: eabo2621 |
| 26 | Behler J, Parrinello M. Generalized neural-network representation of high-dimensional potential-energy surfaces [J]. Phys. Rev. Lett., 2007, 98: 146401 |
| 27 | Zhang L F, Han J Q, Wang H, et al. Deep potential molecular dynamics: A scalable model with the accuracy of quantum mechanics [J]. Phys. Rev. Lett., 2018, 120: 143001 |
| 28 | Zeng Q Y, Chen B, Yu X X, et al. Towards large-scale and spatiotemporally resolved diagnosis of electronic density of states by deep learning [J]. Phys. Rev., 2022, 105B: 174109 |
| 29 | Zeng Q Y, Yu X X, Yao Y P, et al. Ab initio validation on the connection between atomistic and hydrodynamic description to unravel the ion dynamics of warm dense matter [J]. Phys. Rev. Res., 2021, 3: 033116 |
| 30 | Yang F H, Zeng Q Y, Chen B, et al. Lattice thermal conductivity of MgSiO3 perovskite and post-perovskite under lower mantle conditions calculated by deep potential molecular dynamics [J]. Chin. Phys. Lett., 2022, 39: 116301 |
| 31 | Niu H Y, Bonati L, Piaggi P M, et al. Ab initio phase diagram and nucleation of gallium [J]. Nat. Commun., 2020, 11: 2654 |
| 32 | Santos-Florez P A, Yanxon H, Kang B, et al. Size-dependent nucleation in crystal phase transition from machine learning metadynamics [J]. Phys. Rev. Lett., 2022, 129: 185701 |
| 33 | Chen B, Zeng Q Y, Yu X X, et al. Three-step formation of diamonds in shock-compressed hydrocarbons: Decomposition, species separation, and nucleation [J]. arXiv: 2208. 01830, 2022 |
| 34 | Chen B, Zeng Q Y, Wang H, et al. Atomistic mechanism of phase transition in shock compressed gold revealed by deep potential [J]. arXiv: 2006. 13136, 2021 |
| 35 | Qiu R, Zeng Q Y, Wang H, et al. Anomalous thermal transport across the superionic transition in ice [J]. Chin. Phys. Lett., 2023, 40: 116301 |
| 36 | Zeng Q Y, Chen B, Zhang S, et al. Full-scale ab initio simulations of laser-driven atomistic dynamics [J]. npj Comput. Mater., 2023, 9: 213 |
| 37 | Wang H, Zhang L F, Han J Q, et al. DeePMD-kit: A deep learning package for many-body potential energy representation and molecular dynamics [J]. Comput. Phys. Commun., 2018, 228: 178 |
| 38 | Zhang L F, Lin D Y, Wang H, et al. Active learning of uniformly accurate interatomic potentials for materials simulation [J]. Phys. Rev. Mater., 2019, 3: 023804 |
| 39 | Zhang Y Z, Gao C, Liu Q R, et al. Warm dense matter simulation via electron temperature dependent deep potential molecular dynamics [J]. Phys. Plasmas, 2020, 27: 122704 |
| 40 | Zeng Q Y, Dai J Y. Structural transition dynamics of the formation of warm dense gold: From an atomic scale view [J]. Sci. China Phys. Mech. Astron., 2020, 63: 263011 |
| 41 | Dai J Y, Hou Y, Yuan J M. Unified first principles description from warm dense matter to ideal ionized gas plasma: Electron-ion collisions induced friction [J]. Phys. Rev. Lett., 2010, 104: 245001 |
| 42 | Dai J Y, Kang D D, Zhao Z X, et al. Dynamic ionic clusters with flowing electron bubbles from warm to hot dense iron along the hugoniot curve [J]. Phys. Rev. Lett., 2012, 109: 175701 |
| 43 | Kresse G, Furthmüller J. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set [J]. Phys. Rev., 1996, 54B: 11169 |
| 44 | Perdew J P, Burke K, Ernzerhof M. Generalized gradient approximation made simple [J]. Phys. Rev. Lett., 1996, 77: 3865 |
| 45 | Bl?chl P E. Projector augmented-wave method [J]. Phys. Rev., 1994, 50B: 17953 |
| 46 | Ivanov D S, Zhigilei L V. Combined atomistic-continuum modeling of short-pulse laser melting and disintegration of metal films [J]. Phys. Rev., 2003, 68B: 064114 |
| 47 | Plimpton S. Fast parallel algorithms for short-range molecular dynamics [J]. J. Comput. Phys., 1995, 117: 1 |
| 48 | Kittel C. Kittel's Introduction to Solid State Physic [M]. Beijing: Machine Press, 2020: 86 |
| 49 | Tadano T, Gohda Y, Tsuneyuki S. Anharmonic force constants extracted from first-principles molecular dynamics: Applications to heat transfer simulations [J]. J. Phys.: Condens. Matter., 2014, 26: 225402 |
| 50 | Nilsson G, Rolandson S. Lattice dynamics of copper at 80 K [J]. Phys. Rev., 1973, 7B: 2393 |
| 51 | Japel S, Schwager B, Boehler R, et al. Melting of copper and nickel at high pressure: The role of d electrons [J]. Phys. Rev. Lett., 2005, 95: 167801 |
| 52 | Simon F, Glatzel G. Bemerkungen zur schmelzdruckkurve [J]. Z. Anorg. Allg. Chem., 1929, 178: 309 |
| 53 | Cagran C, Wilthan B, Pottlacher G. Enthalpy heat of fusion and specific electrical resistivity of pure silver, pure copper and the binary Ag-28Cu alloy [J]. Thermochim. Acta, 2006, 445: 104 |
| 54 | Nizomov Z, Saidov R H, Gulov B N, et al. Temperature dependence of the heat capacity of aluminium, copper, silicon, magnesium, zinc and comparison with Debye theory [J]. Interconf, 2021, 55: 307 |
| 55 | Smirnov N A. Copper, gold, and platinum under femtosecond irradiation: Results of first-principles calculations [J]. Phys. Rev., 2020, 101B: 094103 |
| 56 | Cho B I, Ogitsu T, Engelhorn K, et al. Measurement of electron-ion relaxation in warm dense copper [J]. Sci. Rep., 2016, 6: 18843 |
| 57 | Hohlfeld J, Müller J G, Wellershoff S S, et al. Time-resolved thermoreflectivity of thin gold films and its dependence on film thickness [J]. Appl. Phys., 1997, 64B: 387 |
| 58 | Zhang Y W, Chen J K. Ultrafast melting and resolidification of gold particle irradiated by pico- to femtosecond lasers [J]. J. Appl. Phys., 2008, 104: 054910 |
/
| 〈 |
|
〉 |