Research paper

Microstructure Evolution and Mechanical Response of Ti-(43-45)Al-4Nb-1Mo-0.2B Alloys During the Hot-Pack Rolling

  • WEI Beibei ,
  • TANG Bin ,
  • CHEN Xiaofei ,
  • ZHANG Xiang ,
  • ZHU Lei ,
  • LIU Renci ,
  • LI Jinshan
Expand
  • 1 State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China
    2 Chongqing Innovation Center, Northwestern Polytechnical University, Chongqing 401135, China
    3 Shaanxi Key Laboratory of Electrical Materials and Infiltration Technology, School of Materials Science and Engineering, Xi'an University of Technology, Xi'an 710048, China
    4 Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
WEI Beibei, Tel: 18734890249, E-mail: wbb@mail.nwpu.edu.cn

Received date: 2024-03-12

  Revised date: 2024-04-22

  Online published: 2024-07-19

Supported by

National Key Research and Development Program of China(2021YFB3702603);Innovation Foundation for Doctor Dissertation of Northwestern Polytechnical University(CX2023045)

Abstract

Slight variations in the Al content can considerably affect the solidification path of TiAl alloys. Consequently, these variations influence the location of phase regions during the hot deformation process of TiAl alloys. In this study, Ti-(43-45)Al-4Nb-1Mo-0.2B (TNM, atomic fraction, %) ingots were synthesized via arc melting and labeled as 43Al, 44Al, or 45Al depending on their Al contents. Subsequently, TNM sheets were fabricated via hot-pack rolling, and the influence of Al content on the microstructure evolution and mechanical properties of these sheets during the rolling process was systematically investigated.Results indicate that TNM alloys with different Al contents are located in different phase regions when deformed at 1250 oC. After preheating for 1 h, the 43Al alloy is mainly composed of equiaxed α/α2 grains. In contrast, the 44Al alloy exhibits a unique core-shell-like structure with α2/γ lamellar colonies in the core and α/α2 grains surrounding it. Compared with the 44Al alloy, the 45Al alloy demonstrates a lamellar structure with larger α2/γ lamellar colonies. Furthermore, the initial structure remarkably influences the microstructure evolution of TNM sheets during the rolling process and determines the final microstructure composition of these sheets. With increasing Al content, the microstructure of TNM sheets transitions from nearly lamellar to duplex, eventually tending toward a near-γ structure. Additionally, two types of α2/γ lamellar colonies—newly formed and initially present—are observed in the 43Al and 45Al sheets, respectively. Owing to its unique core-shell-like structure, the 44Al sheet simultaneously contains both types of α2/γ lamellar colonies. Furthermore, the mechanical properties of TNM sheets with different Al contents were tested at room temperature. Results show a gradual decrease in the tensile strength of TNM sheets with increasing Al content. The 43Al sheet exhibits the best performance, which is attributed to the presence of newly formed lamellar structures. Meanwhile, the 44Al and 45Al sheets develop fractures rapidly because of the increased, clustered, and abnormal growth of equiaxed γ grains or presence of residual α2/γ lamellar colonies.

Cite this article

WEI Beibei , TANG Bin , CHEN Xiaofei , ZHANG Xiang , ZHU Lei , LIU Renci , LI Jinshan . Microstructure Evolution and Mechanical Response of Ti-(43-45)Al-4Nb-1Mo-0.2B Alloys During the Hot-Pack Rolling[J]. Acta Metall Sin, 2025 , 61(11) : 1603 -1614 . DOI: 10.11900/0412.1961.2024.00076

References

[1] Appel F, Brossmann U, Christoph U, et al. Recent progress in the development of gamma titanium aluminide alloys [J]. Adv. Eng. Mater., 2000, 2: 699
[2] Lin J P, Zhang L Q, Song X P, et al. Status of research and development of light-weight γ-TiAl intermetallic based compounds [J]. Mater. China, 2010, 29(2): 1
  林均品, 张来启, 宋西平 等. 轻质γ-TiAl金属间化合物的研究进展 [J]. 中国材料进展, 2010, 29(2): 1
[3] Das G, Kestler H, Clemens H, et al. Sheet gamma TiAl: Status and opportunities [J]. JOM, 2004, 56: 42
[4] Clemens H, Mayer S. Design, processing, microstructure, properties, and applications of advanced intermetallic TiAl alloys [J]. Adv. Eng. Mater., 2013, 15: 191
[5] Clemens H, Kestler H. Processing and applications of intermetallic γ-TiAl-based alloys [J]. Adv. Eng. Mater., 2000, 2: 551
[6] Lasalmonie A. Intermetallics: Why is it so difficult to introduce them in gas turbine engines? [J]. Intermetallics, 2006, 14: 1123
[7] Liang Y F, Lin J P. Fabrication and properties of γ-TiAl sheet materials: A review [J]. JOM, 2017, 69: 2571
[8] Chen Y Y, Ye Y, Sun J F. Present status for rolling TiAl alloy sheet [J]. Acta Metall. Sin., 2022, 58: 965
  陈玉勇, 叶 园, 孙剑飞. TiAl合金板材轧制研究现状 [J]. 金属学报, 2022, 58: 965
[9] Clemens H, Wallgram W, Kremmer S, et al. Design of novel β- solidifying TiAl alloys with adjustable β/B2-phase fraction and excellent hot-workability [J]. Adv. Eng. Mater., 2008, 10: 707
[10] Ren W, Yang X X, Li Y Z, et al. Research status on refinement of TiAl alloys via transformation of metastable microstructure [J]. Foundry Technol., 2022, 43: 484
  任 威, 杨肖肖, 李誉之 等. 亚稳组织转变细化TiAl合金显微组织研究现状 [J]. 铸造技术, 2022, 43: 484
[11] Raji S A, Popoola A P I, Pityana S L, et al. Characteristic effects of alloying elements on β solidifying titanium aluminides: A review [J]. Heliyon, 2020, 6: e04463
[12] Yang J R. Research progress on evolution behavior and control of β/B2 phase in β-solidified TiAl alloy [J]. Foundry Technol., 2022, 43: 237
  杨劼人. β凝固TiAl合金β/B2相演变行为及控制研究进展 [J]. 铸造技术, 2022, 43: 237
[13] Stark A, Oehring M, Pyczak F, et al. In situ observation of various phase transformation paths in Nb-rich TiAl alloys during quenching with different rates [J]. Adv. Eng. Mater., 2011, 13: 700
[14] Schmoelzer T, Liss K D, Zickler G A, et al. Phase fractions, transition and ordering temperatures in TiAl-Nb-Mo alloys: An in- and ex-situ study [J]. Intermetallics, 2010, 18: 1544
[15] Erdely P, Staron P, Maawad E, et al. Effect of hot rolling and primary annealing on the microstructure and texture of a β-stabilised γ-TiAl based alloy [J]. Acta Mater., 2017, 126: 145
[16] Zeng S W, Zhao A M, Luo L, et al. Development of β-solidifying γ-TiAl alloys sheet [J]. Mater. Lett., 2017, 198: 31
[17] Liu G H, Li T R, Wang X Q, et al. Effect of alloying additions on work hardening, dynamic recrystallization, and mechanical properties of Ti-44Al-5Nb-1Mo alloys during direct hot-pack rolling [J]. Mater. Sci. Eng., 2020, A773: 138838
[18] Jiang H T, Zeng S W, Zhao A M, et al. Hot deformation behavior of β phase containing γ-TiAl alloy [J]. Mater. Sci. Eng., 2016, A661: 160
[19] Li T R, Liu G H, Xu M, et al. High temperature deformation and control of homogeneous microstructure during hot pack rolling of Ti-44Al-5Nb-(Mo, V, B) alloys: The impact on mechanical properties [J]. Mater. Sci. Eng., 2019, A751: 1
[20] Yang G, Xu X J, Liang Y F, et al. Effects of Al and Mo on microstructure and hardness of as-cast TNM TiAl alloys [J]. Metals, 2021, 11: 1849
[21] Schwaighofer E, Clemens H, Mayer S, et al. Microstructural design and mechanical properties of a cast and heat-treated intermetallic multi-phase γ-TiAl based alloy [J]. Intermetallics, 2014, 44: 128
[22] Wei B B, Tang B, Chu Y D, et al. The microstructure evolution and tensile properties of Ti-43Al-4Nb-1Mo-0.2B alloy during hot rolling [J]. Mater. Sci. Eng., 2022, A861: 144347
[23] Wei B B, Tang B, Huang X Y, et al. Microstructure evolution and recrystallization of Ti-44.5Al-3.8Nb-1Mo-0.2B alloy with different initial microstructure during hot pack rolling [J]. Mater. Des., 2022, 223: 111138
[24] Xu W C, Huang K, Wu S F, et al. Influence of Mo content on microstructure and mechanical properties of β-containing TiAl alloy [J]. Trans. Nonferrous Met. Soc. China, 2017, 27: 820
[25] Xu X J, Hu R, Lin J P, et al. Evolution of microstructure and microsegregation of Ti-45Al-8Nb alloy during directional solidification [J]. Adv. Mater. Sci. Eng., 2018, 2018: 1713835
[26] Yu Y H, Kou H C, Wang Y C, et al. Formation of core-shell-like structure in β-solidified TiAl alloy and its effect on hot workability [J]. Acta Mater., 2023, 255: 119036
[27] Zhou H T, Kong F T, Wang X P, et al. High strength in high Nb containing TiAl alloy sheet with fine duplex microstructure produced by hot pack rolling [J]. J. Alloys Compd., 2017, 695: 3495
[28] Zghal S, Thomas M, Naka S, et al. Phase transformations in TiAl based alloys [J]. Acta Mater., 2005, 53: 2653
[29] Brokmeier H G, Oehring M, Lorenz U, et al. Neutron diffraction study of texture development during hot working of different gamma-titanium aluminide alloys [J]. Metall. Mater. Trans., 2004, A35: 3563
[30] Inui H, Oh M H, Nakamura A, et al. Room-temperature tensile deformation of polysynthetically twinned (PST) crystals of TiAl [J]. Acta Metall. Mater., 1992, 40: 3095
[31] Ding R G, Li H Y, Hu D W, et al. Features of fracture surface in a fully lamellar TiAl-base alloy [J]. Intermetallics, 2015, 58: 36
[32] Zhang S Z, Zhang C J, Du Z X, et al. Deformation behavior of high Nb containing TiAl based alloy in α + γ two phase field region [J]. Mater. Des., 2016, 90: 225
[33] Tian S W, He A R, Liu J H, et al. Investigation on the microstructure evolution and dynamic recrystallization mechanisms of TiAl alloy at elevated temperature [J]. J. Mater. Res. Technol., 2021, 14: 968
[34] Li T R, Liu G H, Xu M, et al. Flow stress prediction and hot deformation mechanisms in Ti-44Al-5Nb-(Mo, V, B) alloy [J]. Materials (Basel), 2018, 11: 2044
[35] Liu Y, Li J S, Tang B, et al. Decomposition and phase transformation mechanisms of α2 lamellae in β-solidified γ-TiAl alloys [J]. Acta Mater., 2023, 242: 118492
[36] Cui N, Kong F T, Wang X P, et al. Hot deformation behavior and dynamic recrystallization of a β-solidifying TiAl alloy [J]. Mater. Sci. Eng., 2016, A652: 231
[37] Yu Y H, Kou H C, Zhang Z L, et al. Deformation behavior of core-shell-like structure in β-solidified TiAl alloy during isothermal compression [J]. Mater. Lett., 2024, 357: 135637
Outlines

/