Research paper

Mesomechanical Modeling and Experimental Study of Effective Elastic Tensors in Additively Manufactured Titanium Alloys

  • TAN Ruohan ,
  • SONG Yongfeng ,
  • CHEN Chao ,
  • LI Dan ,
  • CHENG Shu ,
  • LI Xiongbing
Expand
  • 1 School of Traffic & Transportation Engineering, Central South University, Changsha 410075, China
    2 State Key Laboratory of Precision Electronic Manufacturing Technology and Equipment, Guangdong University of Technology, Guangzhou 510006, China
    3 Powder Metallurgy Research Institute, Central South University, Changsha 410083, China
LI Xiongbing, professor, Tel: 15084761518, E-mail: lixb213@csu.edu.cn

Received date: 2023-11-14

  Revised date: 2024-06-04

  Online published: 2024-07-17

Supported by

Hunan Provincial Science and Technology Innovation Leading Talent Project(2023RC1015);Natural Science Foundation of Hunan Province(2023JJ60159)

Abstract

Additively manufactured (AM) Ti-6Al-4V alloys are known for their lightweight and superior mechanical properties and are increasingly being favored in the aerospace, energy, and biomedical industries. Among the available AM technologies, selective laser melting (SLM) stands out for its ability to fabricate complex-shaped Ti-6Al-4V efficiently and economically through near-net-shape manufacturing. Despite their advantages, SLM-produced parts often suffer from mechanical anisotropy and contain microdefects such as pores, cracks, and residual stresses, restricting their wider application. Addressing these issues requires a thorough understanding of the effects of texture and porosity on the mechanical properties of AM materials, which is necessary for developing components that comply with strict industry standards. Previous research has predominantly focused on studying the impact of texture or porosity on material properties, overlooking the interplay between these two critical factors. This work introduces an advanced modified Mori-Tanaka (MMT) model that simultaneously considers both texture and porosity in dual-phase AM Ti-6Al-4V alloys. This model enhances the traditional Mori-Tanaka approach by integrating it with the differential method, facilitating a nuanced analysis of how texture and porosity jointly influence the mechanical behavior of polycrystals. For model development, phase transitions and grain orientations are characterized using EBSD, whereas the 3D Gaussian distribution function describes the texture distribution within the polycrystal. Micro/nano computed tomography (CT) plays a pivotal role in determining the volume fraction and morphology of pores, providing crucial data for the model. These parameters were incorporated into the mesomechanical model to analyze the effective elastic stiffness tensor and Young's modulus, quantifying their collective impact on the alloy's mechanical properties. To validate the model, tensile and ultrasonic tests are conducted for two samples with different porosities and textures and compared their outcomes to evaluate the material's mechanical behavior, which exhibits characteristics of transverse isotropy. The comparison highlights the MMT model's superior precision, especially at higher porosity levels, with mean absolute percentage errors (MAPE) between Young's modulus obtained from the MMT model and the tensile test for two samples were 0.87% and 2.51%, respectively. Similarly, the MAPE between the effective elastic stiffness tensor derived from the MMT model and the ultrasonic test were 9.47% and 4.45%, respectively. These findings underscore the model's effectiveness in predicting material properties and its potential as a robust tool for exploring the interactions between microstructural elements and macroscopic mechanical properties of AM polycrystalline materials.

Cite this article

TAN Ruohan , SONG Yongfeng , CHEN Chao , LI Dan , CHENG Shu , LI Xiongbing . Mesomechanical Modeling and Experimental Study of Effective Elastic Tensors in Additively Manufactured Titanium Alloys[J]. Acta Metall Sin, 2025 , 61(9) : 1438 -1448 . DOI: 10.11900/0412.1961.2023.00451

References

[1] Tshephe T S, Akinwamide S O, Olevsky E, et al. Additive manufacturing of titanium-based alloys—A review of methods, properties, challenges, and prospects [J]. Heliyon, 2022, 8(3): e09041
[2] Li S J, Hou W T, Hao Y L, et al. Research progress on the mechanical properties of the biomedical titanium alloy porous structures fabricated by 3D printing technique [J]. Acta Metall. Sin., 2023, 59: 478
  李述军, 侯文韬, 郝玉琳 等. 3D打印医用钛合金多孔材料力学性能研究进展 [J]. 金属学报, 2023, 59: 478
[3] Song B, Zhang J L, Zhang Y J, et al. Research progress of materials design for metal laser additive manufacturing [J]. Acta Metall. Sin., 2023, 59: 15
  宋 波, 张金良, 章媛洁 等. 金属激光增材制造材料设计研究进展 [J]. 金属学报, 2023, 59: 15
[4] Vilaro T, Colin C, Bartout J D. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting [J]. Metall. Mater. Trans., 2011, 42A: 3190
[5] Liu W C, Huang J, Liu J W, et al. Experimental and crystal plasticity modelling study on the crack initiation in micro-texture regions of Ti-6Al-4V during high cycle fatigue tests [J]. Int. J. Fatigue, 2021, 148: 106203
[6] Ren Y M, Lin X, Huang W D. Research progress of microstructure and fatigue behavior in additive manufacturing Ti-6Al-4V alloy [J]. Rare Met. Mater. Eng., 2017, 46: 3160
  任永明, 林 鑫, 黄卫东. 增材制造Ti-6Al-4V合金组织及疲劳性能研究进展 [J]. 稀有金属材料与工程, 2017, 46: 3160
[7] Cheng M, Lu Z G, Wu J, et al. Effect of thermal induced porosity on high-cycle fatigue and very high-cycle fatigue behaviors of hot isostatic-pressed Ti-6Al-4V powder components [J]. J. Mater. Sci. Technol., 2022, 98: 177
[8] Zhao T F, Zhang L, Huang M J. Effective elasticity tensors of fiber-reinforced composite materials with 2D or 3D fiber distribution coefficients [J]. Acta Mech., 2019, 230: 4175
[9] Man C S, Zhao D. Remarks on texture coefficients of polycrystals with improper crystallite symmetry [J]. J. Elast., 2020, 138: 111
[10] Sha G F. Explicit backscattering coefficient for ultrasonic wave propagating in hexagonal polycrystals with fiber texture [J]. J. Nondestr. Eval., 2018, 37: 51
[11] Li J, Rokhlin S I. Elastic wave scattering in random anisotropic solids [J]. Int. J. Solids Struct., 2016, 78-79: 110
[12] Park I, Moon J, Bae S, et al. Application of micro-CT to Mori-Tanaka method for non-randomly oriented pores in air-entrained cement pastes [J]. Constr. Build. Mater., 2020, 255: 119342
[13] Giraud A, Huynh Q V, Hoxha D, et al. Effective poroelastic properties of transversely isotropic rock-like composites with arbitrarily oriented ellipsoidal inclusions [J]. Mech. Mater., 2007, 39: 1006
[14] Yan H B. Determination of the effective modulus of the syntactic foam containing hollow spheres by differential scheme and Mori-Tanaka method [J]. J. Beijing Univ. Aeronaut. Astronaut., 2000, 26: 688
  严寒冰. 用微分法及Mori-Tanaka法求解复合泡沫塑料的有效模量 [J]. 北京航空航天大学学报, 2000, 26: 688
[15] Gui J C, Ma T S, Chen P, et al. Anisotropic damage to hard brittle shale with stress and hydration coupling [J]. Energies, 2018, 11: 926
[16] Zhang Q G, Fan X Y, Chen P, et al. Geomechanical behaviors of shale after water absorption considering the combined effect of anisotropy and hydration [J]. Eng. Geol., 2020, 269: 105547
[17] Asef M R, Farrokhrouz M. A semi-empirical relation between static and dynamic elastic modulus [J]. J. Petrol. Sci. Eng., 2017, 157: 359
[18] Tan R H, Song Y F, Li X B, et al. Effective elastic stiffness tensor and ultrasonic velocities for 3D printed polycrystals with pores and texture [J]. Res. Nondestr. Eval., 2022, 33: 196
[19] Warwick J L W, Coakley J, Raghunathan S L, et al. Effect of texture on load partitioning in Ti-6Al-4V [J]. Acta Mater., 2012, 60: 4117
[20] Cho J H, Rollett A D, Oh K H. Determination of volume fractions of texture components with standard distributions in Euler space [J]. Metall. Mater. Trans., 2004A, 35: 1075
[21] Gong S, Li Z, Zhao Y Y. An extended Mori-Tanaka model for the elastic moduli of porous materials of finite size [J]. Acta Mater., 2011, 59: 6820
[22] Simonelli M, Tse Y Y, Tuck C. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti-6Al-4V [J]. Mater. Sci. Eng., 2014, A616: 1
[23] Bozzolo N, Gerspach F, Sawina G, et al. Accuracy of orientation distribution function determination based on EBSD data—A case study of a recrystallized low alloyed Zr sheet [J]. J. Microsc., 2007, 227: 275
[24] Simonelli M, Tse Y Y, Tuck C. On the texture formation of selective laser melted Ti-6Al-4V [J]. Metall. Mater. Trans., 2014, 45A: 2863
[25] Huang S S, Ma Y J, Zhang S L, et al. Influence of alloying elements partitioning behaviors on the microstructure and mechanical properties in α + β titanium alloy [J]. Acta Metall. Sin., 2019, 55: 741
  黄森森, 马英杰, 张仕林 等. α + β两相钛合金元素再分配行为及其对显微组织和力学性能的影响 [J]. 金属学报, 2019, 55: 741
[26] Kasperovich G, Haubrich J, Gussone J, et al. Correlation between porosity and processing parameters in TiAl6V4 produced by selective laser melting [J]. Mater. Des., 2016, 105: 160
[27] Ge J G, Yan X C, Lei Y P, et al. A detailed analysis on the microstructure and compressive properties of selective laser melted Ti6Al4V lattice structures [J]. Mater. Des., 2021, 198: 109292
[28] Liu Z, Liu J R, Zhao Z B, et al. Microstructure and tensile property of TC4 alloy produced via electron beam rapid manufacturing [J]. Acta Metall. Sin., 2019, 55: 692
  刘 征, 刘建荣, 赵子博 等. 电子束快速成形制备TC4合金的组织和拉伸性能分析 [J]. 金属学报, 2019, 55: 692
[29] Banerjee D, Williams J C. Perspectives on titanium science and technology [J]. Acta Mater., 2013, 61: 844
[30] Yuan M D, Dai A B, Ma J T, et al. Nondestructive measurement of anisotropic elastic constants of selective laser melted 316L based on a tri-mode ultrasonic method [J]. Meas. Sci. Technol., 2023, 34: 045101
[31] Dai A B, Yuan M D, Wu J W, et al. Nondestructive characterization of elastic constants for 316L parts by selective laser melting based on dual-mode ultrasonic transducer [J]. Chin. J. Sci. Instrum., 2021, 42(6): 95
  戴安帮, 袁懋诞, 吴俊伟 等. 基于双模式超声换能器的选择性激光熔化316L制件弹性常数无损表征研究 [J]. 仪器仪表学报, 2021, 42(6): 95
[32] Prioul R, Bakulin A, Bakulin V. Nonlinear rock physics model for estimation of 3D subsurface stress in anisotropic formations: Theory and laboratory verification [J]. Geophysics, 2004, 69: 415
[33] Mishra N, Das K. A Mori-Tanaka based micromechanical model for predicting the effective electroelastic properties of orthotropic piezoelectric composites with spherical inclusions [J]. SN Appl. Sci., 2020, 2: 1206
[34] Wu J. Thermal expansion coefficient prediction of asphalt mixture with the Eshelby equivalent inclusion theory [J]. Appl. Mech. Mater., 2014, 584-586: 1071
[35] Zhang Y, Han L. Foundation of Mesomechanics [M]. Beijing: Science Press, 2014: 91
  张 研, 韩 林. 细观力学基础 [M]. 北京: 科学出版社, 2014: 91
[36] Yang J J, Yu H C, Wang Z M, et al. Effect of crystallographic orientation on mechanical anisotropy of selective laser melted Ti-6Al-4V alloy [J]. Mater. Charact., 2017, 127: 137
[37] Yang L, Zhao F, Jiang L, et al. Development of composition and heat treatment process of 2000 MPa grade spring steels assisted by machine learning [J]. Acta Metall. Sin., 2023, 59: 1499
  杨 累, 赵 帆, 姜 磊 等. 机器学习辅助2000 MPa级弹簧钢成分和热处理工艺开发 [J]. 金属学报, 2023, 59: 1499
[38] Zhang S Y, Lin X, Chen J, et al. Influence of processing parameter on the microstructure and forming characterizations of Ti-6Al-4V titanium alloy after laser rapid forming processing [J]. Rare Met. Mater. Eng., 2007, 36: 1839
  张霜银, 林 鑫, 陈 静 等. 工艺参数对激光快速成形TC4钛合金组织及成形质量的影响 [J]. 稀有金属材料与工程, 2007, 36: 1839
Outlines

/