Research paper

Effect of Cr and Sc on High-Temperature Stability of Grain Structure in W-Based Alloys

  • DU Wenli ,
  • HOU Chao ,
  • LI Yurong ,
  • HAN Tielong ,
  • SONG Xiaoyan
Expand
  • Key Laboratory of Advanced Functional Materials, Ministry of Education, College of Materials Science and Engineering, Beijing University of Technology, Beijing 100124, China

Received date: 2024-02-28

  Revised date: 2024-06-05

  Online published: 2024-07-09

Supported by

National Natural Science Foundation of China(92163107);National Natural Science Foundation of China(52371128)

Abstract

W-based alloys play an indispensable role in various fields, such as aerospace and nuclear industries. However, their thermal stability decreases with grain structure refinement, limiting their high-temperature applications. Although certain solute elements can enhance thermal stability through phase separation or grain boundary segregation, a systematic research on the extent of grain structure stabilization and the mechanisms of multicomponent addition is lacking. Herein, ultrafine-grained W-10Cr and W-5Cr-5Sc alloys with uniform grain structures and similar average grain sizes were prepared. The thermal stabilities of these W-based alloys were systematically investigated to elucidate their stabilization mechanisms. Results indicate that sudden grain growth occurs at approximately 1300 oC in W-10Cr and W-5Cr-5Sc alloys, representing an increase of approximately 200 oC compared with pure W. Kinetic analysis shows that the grain growth index and activation energy for grain growth are minimized at temperatures corresponding to thermal destabilization. Moreover, the grain growth indices of W-10Cr and W-5Cr-5Sc alloys exceed those of pure W during thermal instability. Furthermore, beyond the thermal destabilization threshold, the grain growth rate of the W-5Cr-5Sc alloy was lower than that of the W-10Cr alloy. The addition of Sc modifies the Cr distribution in the alloy. In the W-10Cr alloy, the high-temperature stabilization mechanism of the grain structure was attributed to the precipitation of Cr-rich phases and the segregation of Cr at the grain boundaries. By contrast, the stabilization mechanism in the W-5Cr-5Sc alloy shifts toward the precipitation of Sc-rich phases along with the simultaneous segregation of Cr and Sc at the grain boundaries.

Cite this article

DU Wenli , HOU Chao , LI Yurong , HAN Tielong , SONG Xiaoyan . Effect of Cr and Sc on High-Temperature Stability of Grain Structure in W-Based Alloys[J]. Acta Metall Sin, 2025 , 61(11) : 1664 -1672 . DOI: 10.11900/0412.1961.2024.00052

References

[1] Zhang T, Deng H W, Xie Z M, et al. Recent progresses on designing and manufacturing of bulk refractory alloys with high performances based on controlling interfaces [J]. J. Mater. Sci. Technol., 2020, 52: 29
[2] Li X Y, Zhang L, Dong Y H, et al. Towards pressureless sintering of nanocrystalline tungsten [J]. Acta Mater., 2021, 220: 117344
[3] Cao L J, Hou C, Tang F W, et al. Thermal stability and high-temperature mechanical performance of nanostructured W-Cu-Cr-ZrC composite [J]. Composites, 2021, 208B: 108600
[4] Zhang T, Deng H W, Xie Z M, et al. Solute segregation and nanoparticle dispersion induced super high stability in a bulk nanocrystalline W-based alloy [J]. J. Mater. Res. Technol., 2023, 26: 2242
[5] Xue H X, Cai X C, Sun B R, et al. Bulk nanocrystalline W-Ti alloys with exceptional mechanical properties and thermal stability [J]. J. Mater. Sci. Technol., 2022, 114: 16
[6] Wu Z M, He L, Ye L S, et al. Ultrafine-grained W-based alloys prepared by HIP with ultrahigh hardness and excellent thermal stability [J]. Int. J. Refract. Met. Hard Mater., 2023, 115: 106318
[7] Lang S T, Yan Q Z, Wang Y J, et al. Preparation and microstructure characterization of W-0.1wt.%TiC alloy via chemical method [J]. Int. J. Refract. Met. Hard Mater., 2016, 55: 33
[8] Seo M, Wang K, Echols J R, et al. Microstructure deformation and near-pore environment of resolidified tungsten in high heat flux conditions [J]. J. Nucl. Mater., 2022, 565: 153725
[9] Zhou Q, Zhao J, Xie J Y, et al. Grain size dependent strain rate sensitivity in nanocrystalline body-centered cubic metal thin films [J]. Mater. Sci. Eng., 2014, A608: 184
[10] Grimes R W, Konings R J M, Edwards L. Greater tolerance for nuclear materials [J]. Nat. Mater., 2008, 7: 683
[11] Meyers M A, Mishra A, Benson D J. Mechanical properties of nanocrystalline materials [J]. Prog. Mater Sci., 2006, 51: 427
[12] Zhao Y H, Topping T, Bingert J F, et al. High tensile ductility and strength in bulk nanostructured nickel [J]. Adv. Mater., 2008, 20: 3028
[13] Han W Z, Demkowicz M J, Fu E G, et al. Effect of grain boundary character on sink efficiency [J]. Acta Mater., 2012, 60: 6341
[14] Bai X M, Voter A F, Hoagland R G, et al. Efficient annealing of radiation damage near grain boundaries via interstitial emission [J]. Science, 2010, 327: 1631
[15] Cheng G M, Xu W Z, Wang Y Q, et al. Grain size effect on radiation tolerance of nanocrystalline Mo [J]. Scr. Mater., 2016, 123: 90
[16] El-Atwani O, Suslova A, Novakowski T J, et al. In-situ TEM/heavy ion irradiation on ultrafine-and nanocrystalline-grained tungsten: Effect of 3 MeV Si, Cu and W ions [J]. Mater. Charact., 2015, 99: 68
[17] Zhang L, Li X Y, Qu X H, et al. Powder metallurgy route to ultrafine‐grained refractory metals [J]. Adv. Mater., 2023, 35: 2205807
[18] Sun S, Gao P, Sun G X, et al. Nanostructuring as a route to achieve ultra-strong high- and medium-entropy alloys with high creep resistance [J]. J. Alloys Compd., 2020, 830: 154656
[19] Millett P C, Selvam R P, Bansal S, et al. Atomistic simulation of grain boundary energetics-effects of dopants [J]. Acta Mater., 2005, 53: 3671
[20] Kalidindi A R, Schuh C A. Stability criteria for nanocrystalline alloys [J]. Acta Mater., 2017, 132: 128
[21] Peng H R, Gong M M, Chen Y Z, et al. Thermal stability of nanocrystalline materials: Thermodynamics and kinetics [J]. Int. Mater. Rev., 2017, 62: 303
[22] Bachmaier A, Motz C. On the remarkable thermal stability of nanocrystalline cobalt via alloying [J]. Mater. Sci. Eng., 2015, A624: 41
[23] Shi X H, Chen Y Z, Ma X Y, et al. Microstructural evolution of nanocrystalline Fe-Zr alloys upon annealing treatment [J]. Mater. Charact., 2015, 103: 58
[24] Koch C C, Scattergood R O, Darling K A, et al. Stabilization of nanocrystalline grain sizes by solute additions [J]. J. Mater. Sci., 2008, 43: 7264
[25] Chookajorn T, Park M, Schuh C A. Duplex nanocrystalline alloys: Entropic nanostructure stabilization and a case study on W-Cr [J]. J. Mater. Res., 2015, 30: 151
[26] Park M, Schuh C A. Accelerated sintering in phase-separating nanostructured alloys [J]. Nat. Commun., 2015, 6: 6858
[27] Tang F W, Liu X M, Wang H B, et al. Solute segregation and thermal stability of nanocrystalline solid solution systems [J]. Nanoscale, 2019, 11: 1813
[28] Michels A, Krill C E, Ehrhardt H, et al. Modelling the influence of grain-size-dependent solute drag on the kinetics of grain growth in nanocrystalline materials [J]. Acta Mater., 1999, 47: 2143
[29] Zhang W, Chen L, Xu C G, et al. Grain growth kinetics and densification mechanism of (TiZrHfVNbTa)C high-entropy ceramic under pressureless sintering [J]. J. Mater. Sci. Technol., 2022, 110: 57
[30] Humphreys F J, Hatherly M. Recrystallization and Related Annealing Phenomena [M]. Amsterdam: Elsevier, 1995: 284
Outlines

/