Microstructure Evolution and Mechanical Properties of 6061 Aluminum Alloy Fabricated by Friction Stir Additive Manufacturing
Received date: 2023-05-12
Revised date: 2023-11-24
Online published: 2024-05-27
Supported by
National Natural Science Foundation of China(11775017);National Natural Science Foundation of China(51971021)
Friction stir additive manufacturing (FSAM) is an advanced solid-phase forming technology based on the principle of friction stir. As no heat source is required, the FSAM process can avoid metallurgical defects during melting and solidification of the material. The FSAM also conserves energy and protects the environment. To replace the traditional forming technology with a heat source, current research aims to optimize the forming process parameters of aluminum and magnesium alloys. Similarly to the friction stir welding process, increasing the temperature in the FSAM process will dissolve part of the strengthening phase, coarsening the particles and softening the welding core area. In addition, during layer-by-layer stacking in FSAM, the stir tool will re-stir the previously formed area, introducing a new thermal cycle during the stirring process. Because the changes in the temperature and stress field are more complex in the FSAM process than in the friction stir welding process, the influence of microstructure evolution on the mechanical properties of materials in the FSAM process is worthy of investigation. In this study, a multilayer defect-free FSAM material was fabricated from 2-mm-thick 6061 aluminum alloy sheets. The microstructural evolution along the building direction was observed during the FSAM process to investigate its effect on the microhardness and tensile properties. Dynamic crystallization formed fine equiaxed grains in the stir zone, which were further refined after re-stirring in the overlapping interface regions. The tensile strength and elongation of the FSAM material were 47.7%-55.2% and 144.6%-148.8% those of the base material, respectively. Multiple thermal cycling weakens the performance of the overlapping interface regions. The spherical α-Al(MnCrFe)Si phase plays a strengthening role in the matrix. Extensive dissolution of the strengthening phase during the FSAM process is mainly responsible for the performance deterioration of the FSAM material. After heat treatment at 520 oC for 1 h and at 165 oC for 18 h of aging, the properties of the FSAM material were largely improved: the hardness slightly increased from that of the base material and the tensile strength reached 87.2%-91.9% that of the base material.
YANG Fan , PEI Shichao , LUO Xinrui , CHEN Yuxiang , LI Ningyu , CHANG Yongqin . Microstructure Evolution and Mechanical Properties of 6061 Aluminum Alloy Fabricated by Friction Stir Additive Manufacturing[J]. Acta Metall Sin, 2025 , 61(8) : 1129 -1140 . DOI: 10.11900/0412.1961.2023.00220
| [1] | Alt?parmak S C, Yardley V A, Shi Z S, et al. Challenges in additive manufacturing of high-strength aluminium alloys and current developments in hybrid additive manufacturing [J]. Int. J. Lightweight Mater. Manuf., 2021, 4: 246 |
| [2] | Mishra A, Agarwal R, Kumar N, et al. A critical review on the additive manufacturing of aluminium alloys [J]. Mater. Today: Proc., 2021, 47: 4074 |
| [3] | Kim S, Moon S K. A part consolidation design method for additive manufacturing based on product disassembly complexity [J]. Appl. Sci. (Basel), 2020, 10: 1100 |
| [4] | Karayel E, Bozkurt Y. Additive manufacturing method and different welding applications [J]. J. Mater. Res. Technol., 2020, 9: 11424 |
| [5] | He P F, Wei Z Y, Wang Y C, et al. A novel droplet + arc additive manufacturing for aluminum alloy: Method, microstructure and mechanical properties [J]. Addit. Manuf., 2023, 61: 103356 |
| [6] | Xiao Y C, Li Y, Shi L, et al. Experimental and numerical analysis of friction stir additive manufacturing of 2024 aluminium alloy [J]. Mater. Today Commun., 2023, 35: 105639 |
| [7] | Carroll B E, Otis R A, Borgonia J P, et al. Functionally graded material of 304L stainless steel and Inconel 625 fabricated by directed energy deposition: Characterization and thermodynamic modeling [J]. Acta Mater., 2016, 108: 46 |
| [8] | Khodabakhshi F, Gerlich A P. Potentials and strategies of solid-state additive friction-stir manufacturing technology: A critical review [J]. J. Manuf. Process., 2018, 36: 77 |
| [9] | Rometsch P A, Zhu Y M, Wu X H, et al. Review of high-strength aluminium alloys for additive manufacturing by laser powder bed fusion [J]. Mater. Des., 2022, 219: 110779 |
| [10] | Hauser T, Reisch R T, Breese P P, et al. Porosity in wire arc additive manufacturing of aluminium alloys [J]. Addit. Manuf., 2021, 41: 101993 |
| [11] | Ahmad Z. Aluminium Alloys—New Trends in Fabrication and Applications [M]. Rijeka Croatia: IntechOpen, 2012: 159 |
| [12] | Li H Z, Wang C M, Zhang H, et al. Research progress of friction stir additive manufacturing technology [J]. Acta Metall. Sin., 2023, 59: 106 |
| 李会朝, 王彩妹, 张 华 等. 搅拌摩擦增材制造技术研究进展 [J]. 金属学报, 2023, 59: 106 | |
| [13] | Mao Y Q, Ke L M, Huang C P, et al. Formation characteristic, microstructure, and mechanical performances of aluminum-based components by friction stir additive manufacturing [J]. Int. J. Adv. Manuf. Technol., 2016, 83: 1637 |
| [14] | Palanivel S, Nelaturu P, Glass B, et al. Friction stir additive manufacturing for high structural performance through microstructural control in an Mg based WE43 alloy [J]. Mater. Des., 2015, 65: 934 |
| [15] | Li Y, He C S, Wei J X, et al. Correlation of local microstructures and mechanical properties of Al-Zn-Mg-Cu alloy build fabricated via underwater friction stir additive manufacturing [J]. Mater. Sci. Eng., 2021, A805: 140590 |
| [16] | Liu F J, Fu L, Chen H Y. Microstructures and mechanical properties of thin plate aluminium alloy joint prepared by high rotational speed friction stir welding [J]. Acta Metall. Sin., 2017, 53: 1651 |
| 刘奋军, 傅 莉, 陈海燕. 铝合金薄板高转速搅拌摩擦焊接头组织与力学性能 [J]. 金属学报, 2017, 53: 1651 | |
| [17] | Gussev M N, Sridharan N, Norfolk M, et al. Effect of post weld heat treatment on the 6061 aluminum alloy produced by ultrasonic additive manufacturing [J]. Mater. Sci. Eng., 2017, A684: 606 |
| [18] | Nie F H, Dong H G, Chen S, et al. Microstructure and mechanical properties of pulse MIG welded 6061/A356 aluminum alloy dissimilar butt joints [J]. J. Mater. Sci. Technol., 2018, 34: 551 |
| [19] | Zhang Z, Tan Z J, Li J Y, et al. Experimental and numerical studies of re-stirring and re-heating effects on mechanical properties in friction stir additive manufacturing [J]. Int. J. Adv. Manuf. Technol., 2019, 104: 767 |
| [20] | Malopheyev S, Vysotskiy I, Kulitskiy V, et al. Optimization of processing-microstructure-properties relationship in friction-stir welded 6061-T6 aluminum alloy [J]. Mater. Sci. Eng., 2016, A662: 136 |
| [21] | Li J Y, Kong S N, Liu C K, et al. Chemical composition effect on microstructures and mechanical properties in friction stir additive manufacturing [J]. Acta. Metall. Sin. (Engl. Lett.), 2022, 35: 1494 |
| [22] | Zhao Z J, Yang X Q, Li S L, et al. Interfacial bonding features of friction stir additive manufactured build for 2195-T8 aluminum-lithium alloy [J]. J. Manuf. Process., 2019, 38: 396 |
| [23] | Yin Y H, Sun N, North T H, et al. Hook formation and mechanical properties in AZ31 friction stir spot welds [J]. J. Mater. Process. Technol., 2010, 210: 2062 |
| [24] | Zhang C C, Chang B H, Tao J, et al. Microstructure evolution during friction stir welding of 2024 aluminum alloy [J]. Trans. China Weld. Inst., 2013, 34(3): 57 |
| 张成聪, 常保华, 陶 军 等. 2024铝合金搅拌摩擦焊过程组织演化分析 [J]. 焊接学报, 2013, 34(3): 57 | |
| [25] | He P D, Webster R F, Yakubov V, et al. Fatigue and dynamic aging behavior of a high strength Al-5024 alloy fabricated by laser powder bed fusion additive manufacturing [J]. Acta Mater., 2021, 220: 117312 |
| [26] | Lodgaard L, Ryum N. Precipitation of dispersoids containing Mn and/or Cr in Al-Mg-Si alloys [J]. Mater. Sci. Eng., 2000, A283: 144 |
| [27] | Kalinenko A, Vysotskii I, Malopheyev S, et al. Relationship between welding conditions, abnormal grain growth and mechanical performance in friction-stir welded 6061-T6 aluminum alloy [J]. Mater. Sci. Eng., 2021, A817: 141409 |
| [28] | Zhang L, Jiao W L, Wei H J, et al. Influence of manganese and pre-heat treatment on microstructure and mechanical properties of Al-Si alloy [J]. Chin. J. Nonferrous Met., 2005, 15: 368 |
| 张 磊, 焦万丽, 尉海军 等. 锰结合预先热处理对铝硅合金中富铁相组织和力学性能的影响 [J]. 中国有色金属学报, 2005, 15: 368 |
/
| 〈 |
|
〉 |