Research paper

Effect of Prewelding Pretreatment on Welding Residual Stress of Titanium Alloy Thick Plate

  • ZHOU Mu ,
  • WANG Qian ,
  • WANG Yanxu ,
  • ZHAI Zirong ,
  • HE Lunhua ,
  • LI Bing ,
  • MA Yingjie ,
  • LEI Jiafeng ,
  • YANG Rui
Expand
  • 1 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
    2 Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    3 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    4 Center for Adaptive System Engineering, ShanghaiTech University, Shanghai 201210, China
    5 Spallation Neutron Source Science Center, Dongguan 523803, China
    6 Beijing National Laboratory for Condensed Matter Physics, Institute of Physics, Chinese Academy of Sciences, Beijing 100190, China
MA Yingjie, professor, Tel: 13840026329, E-mail: yjma@imr.ac.cnWANG Yanxu, professor, Tel: 18525069032, E-mail: yxwang@imr.ac.cn

Received date: 2024-02-28

  Revised date: 2024-05-02

  Online published: 2024-05-27

Supported by

National Key Research and Development Program of China(2021YFC2801801);CSNS Consortium on High-Performance Materials of Chinese Academy of Sciences(JZHKYPT-2021-01)

Abstract

Welding is an essential means of joining structural components to form a new structure. Welding residual stress mainly results from materials expanding or contracting due to temperature variations, which can reduce the life of titanium alloys. Therefore, to reduce undesired residual stress, the welding process and microstructure of the materials involved should be optimized. Titanium alloys play a crucial role in marine and aviation fields due to their excellent corrosion resistance and high specific strength. This work investigates the influence mechanism of the prewelding pretreatment process on the structure, mechanical properties, and residual stress of the electron beam welding joint of a titanium alloy thick plate. The macrostructure and microstructure of titanium alloy welding joints prepared using different pretreatment processes are characterized. Results showed that preheating before welding substantially widens the fusion zone (FZ) and heat-affected zone (HAZ) of the welding joint, coarsening α lamellae in both zones. Thus, the hardness of the FZ and HAZ of the preheated welding joint is reduced to close to that of the base metal. Simultaneously, the strength and toughness of the welding joint is considerably improved such that it is similar to the base metal. The neutron diffraction, deep-hole drilling, and Rostenthal-Norton contour methods are used to measure the residual stress of the electron beam welding joint. The neutron diffraction method exhibits high detection accuracy and can achieve stress monitoring in different zones of the weld seam. Deep-hole drilling is a mechanical strain relief technique for measuring transverse and longitudinal residual stress through component thickness. The Rostenthal-Norton contour method can obtain a three-dimensional stress on the welding joint. A combination of these three measurement techniques can complement and be used to verify each other, providing reasonable data for the residual stress evaluation. The detection results of unpreheated welding joints are compared and analyzed, and the residual stress distribution in the FZ and HAZ zones along different directions is obtained. The FZ is subjected to tensile residual stress along all three directions. Alternatively, the HAZ is subjected to compressive stress along the transverse and longitudinal directions and tensile stress along the normal direction. The residual stress at base metal is small. Additionally, the residual stress results obtained by the deep-hole drilling method for the welding joints using two preheating processes are compared. The results showed that preheating before welding can considerably reduce residual stress at the weld. The reason is discussed in depth. Numerical simulation is used to calculate the changes in the temperature and stress fields under different preheating temperatures. The dynamic change rules of thermal stress under different preheating temperatures are obtained. Results showed that increasing the preheating temperature reduces thermal stress and the thermal expansion mismatch in different areas of the welded joint. Moreover, the microstructure, element distribution, and grain orientation of the FZ and HAZ of joints welded using two pretreatment processes are analyzed. Preheating coarsens the α lamellae and promotes the redistribution of alloy elements, thereby reducing the stress concentration between α and β phases. Besides, variant selection of the HAZ is induced by the preheating process. The number and differences in the orientation of α variants are decreased, thereby reducing the stress concentration between variants.

Cite this article

ZHOU Mu , WANG Qian , WANG Yanxu , ZHAI Zirong , HE Lunhua , LI Bing , MA Yingjie , LEI Jiafeng , YANG Rui . Effect of Prewelding Pretreatment on Welding Residual Stress of Titanium Alloy Thick Plate[J]. Acta Metall Sin, 2024 , 60(8) : 1064 -1078 . DOI: 10.11900/0412.1961.2024.00054

References

1 Aba-Perea P E, Pirling T, Preuss M. In-situ residual stress analysis during annealing treatments using neutron diffraction in combination with a novel furnace design [J]. Mater. Des., 2016, 110: 925
2 Lim S H, Zhang Z, Seng D H L, et al. In-situ warm shot peening on Ti-6Al-4V alloy: Effects of temperature on fatigue life, residual stress, microstructure and mechanical properties [J]. J. Alloys Compd., 2021, 882: 160701
3 Sun G A, Chen B. The technology and application of residual stress analysis by neutron diffraction [J]. Nucl. Tech., 2007, 30(4):286
  孙光爱, 陈 波. 中子衍射残余应力分析技术及其应用 [J]. 核技术, 2007, 30(4): 286
4 Woo W, Em V, Hubbard C R, et al. Residual stress determination in a dissimilar weld overlay pipe by neutron diffraction [J]. Mater. Sci. Eng., 2011, A528: 8021
5 Ren Y, Paradowska A, Wang B, et al. Residual stress state of X65 pipeline girth welds before and after local and furnace post weld heat treatment [J]. J. Pressure Vessel Technol., 2017, 139: 041401
6 Liu T, Bunn J R, Fancher C M, et al. Neutron diffraction analysis of residual strain in high-pressure die cast A383 engine blocks [J]. J. Mater. Eng. Perform., 2020, 29: 5428
7 Burca G, James J A, Kockelmann W, et al. A new bridge technique for neutron tomography and diffraction measurements [J]. Nucl. Instrum. Methods Phys. Res., 2011, 651A: 229
8 Li S L, Li Y, Wang Y K, et al. Multiscale residual stress evaluation of engineering materials/components based on neutron and synchrotron radiation technology [J]. Acta Metall. Sin., 2023, 59: 1001
  李时磊, 李 阳, 王友康 等. 基于中子与同步辐射技术的工程材料/部件多尺度残余应力评价 [J]. 金属学报, 2023, 59: 1001
9 Zhang Z W, Feng Y F, Tan Q, et al. Residual stress distribution in Ni-based superalloy turbine discs during fabrication evaluated by neutron/X-ray diffraction measurement and thermomechanical simulation [J]. Mater. Des., 2019, 166: 107603
10 Song S P, Paradowska A M, Dong P S. Investigation of residual stresses distribution in titanium weldments [J]. Mater. Sci. Forum, 2014, 777: 171
11 Lin Y C, Lee K H. Effect of preheating on the residual stress in type 304 stainless steel weldment [J]. J. Mater. Process. Technol., 1997, 63: 797
12 Asadi P, Alimohammadi S, Kohantorabi O, et al. Effects of material type, preheating and weld pass number on residual stress of welded steel pipes by multi-pass TIG welding (C-Mn, SUS304, SUS316) [J]. Therm. Sci. Eng. Prog., 2020, 16: 100462
13 Maly M, H?ller C, Skalon M, et al. Effect of process parameters and high-temperature preheating on residual stress and relative density of Ti6Al4V processed by selective laser melting [J]. Materials, 2019, 12: 930
14 Chen B, Skouras A, Wang Y Q, et al. In situ neutron diffraction measurement of residual stress relaxation in a welded steel pipe during heat treatment [J]. Mater. Sci. Eng., 2014, A590: 374
15 Yan G X, Crivoi A, Sun Y J, et al. An Arrhenius equation-based model to predict the residual stress relief of post weld heat treatment of Ti-6Al-4V plate [J]. J. Manuf. Process., 2018, 32: 763
16 Lombardi A, Sediako D, Machin A, et al. Effect of solution heat treatment on residual stress in Al alloy engine blocks using neutron diffraction [J]. Mater. Sci. Eng., 2017, A697: 238
17 Wang B, Zhou L, Cao Y S, et al. Analysis of residual stress relief for Ti62A alloy welded joints by post weld heat treatment considering creep effect [J]. J. Mater. Res. Technol., 2023, 24: 7462
18 Wei H. Effect of texture on properties and residual stress in Cu-Ni-Si alloys and its mechanism [D]. Beijing: University of Science and Technology Beijing, 2021
  韦 贺. 铜镍硅系合金中织构对性能和残余应力的影响及作用机制 [D]. 北京: 北京科技大学, 2021
19 Zhu W X. Study on residual stress reduction process of GH4169 alloy rings [D]. Guizhou: Guizhou University, 2021
  朱文祥. GH4169合金环件残余应力消减工艺研究 [D]. 贵州: 贵州大学, 2021
20 Zhang K Y, Dong W C, Zhao D, et al. Effect of solid-state phase transformation on stress and distortion for Fe-Co-Ni ultra-high strength steel components during welding and vacuum gas quenching processes [J]. Acta Metall. Sin., 2023, 59: 1633
  张开元, 董文超, 赵 栋 等. 固态相变对Fe-Co-Ni超高强度钢长臂梁构件焊接-淬火过程应力和变形的影响 [J]. 金属学报, 2023, 59: 1633
21 Etesami S A, Fotovvati B, Asadi E. Heat treatment of Ti-6Al-4V alloy manufactured by laser-based powder-bed fusion: Process, microstructures, and mechanical properties correlations [J]. J. Alloys Compd., 2022, 895: 162618
22 Lou Y H, Lin G X, Liu Y P, et al. Effect of post-weld heat treatment on microstructure and mechanical properties of electron beam welded TC4 joints [J]. Hot Work. Technol., 2013, 42(19): 179
  娄宇航, 蔺广学, 刘俞平 等. TC4真空电子束焊后热处理对接头组织性能的影响 [J]. 热加工工艺, 2013, 42(19): 179
23 Brinson H F, Brinson L C. Stress and strain analysis and measurement [A]. Polymer Engineering Science and Viscoelasticity: An Introduction [M]. New York: Springer, 2015: 15
24 Chen J, Jiang Y L, Chen H N. Three-dimensional residual stress determination in Q345 weldment before and after PWHT by deep-hole drilling method [J]. Weld. J., 2022, (12): 25
  陈 静, 姜云禄, 陈怀宁. 深孔法测试Q345焊接试板热处理前后三维残余应力的可行性 [J]. 焊接, 2022, (12): 25
25 Pederson R, Niklasson F, Skystedt F, et al. Microstructure and mechanical properties of friction- and electron-beam welded Ti-6Al-4V and Ti-6Al-2Sn-4Zr-6Mo [J]. Mater. Sci. Eng., 2012, A552: 555
26 Zhang S L, Ma Y J, Huang S S, et al. Temperature-gradient induced microstructure evolution in heat-affected zone of electron beam welded Ti-6Al-4V titanium alloy [J]. J. Mater. Sci. Technol., 2019, 35: 1681
27 Attallah M M, Preuss M, Boonchareon C, et al. Microstructural and residual stress development due to inertia friction welding in Ti-6246 [J]. Metall. Mater. Trans., 2012, 43A: 3149
28 Hall E O. The deformation and ageing of mild steel: III Discussion of results [J]. Proc. Phys. Soc., 1951, 64B: 747
29 Owen C, Jeffs S, Perkins K, et al. The evolution of Ti-6Al-4V following extreme thermo-mechanical processing [A]. Proceedings of the 13th World Conference on Titanium [C]. Hoboken: John Wiley & Sons, Inc., 2016: 456
30 Rae W, Lomas Z, Jackson M, et al. Measurements of residual stress and microstructural evolution in electron beam welded Ti-6Al-4V using multiple techniques [J]. Mater. Charact., 2017, 132: 10
31 Xu W W, Shang S L, Zhou B C, et al. A first-principles study of the diffusion coefficients of alloying elements in dilute α-Ti alloys [J]. Phys. Chem. Chem. Phys., 2016, 18: 16870
Outlines

/