Evolution of Short-to-Medium Range Orders During the Liquid-Liquid Phase Transition of a Pd-Si Metallic Glass
Received date: 2024-02-29
Revised date: 2024-05-09
Online published: 2024-05-23
Supported by
National Key Research and Development Program of China(2021YFB3802800);National Natural Science Foundation of China(52222104);National Natural Science Foundation of China(52201190);National Natural Science Foundation of China/Research Grants Council of Hong Kong Special Administrative Region Joint Research Scheme, Project(N_CityU173/22);National Natural Science Foundation International (Regional) Cooperation and Exchange Project(12261160364);Open Research Fund of Songshan Lake Materials Laboratory(2022SLABFN19);Guangdong-Hong Kong-Macao Joint Laboratory for Neutron Scattering Science and Technology
Liquid-liquid phase transition (LLPT) is a universal phenomenon that occurs in different types of liquids. Understanding its mechanism can help solve the long-standing mystery of liquid and amorphous structures. In metallic liquids, LLPT has been widely reported to be observed in the supercooled liquid region in multicomponent alloy systems. However, few observations of LLPT were reported in binary metallic systems, mainly due to the poor thermal stability of these systems in the supercooled liquid region. Herein, the phase transition of Pd82Si18 metallic glass in its supercooled liquid region was studied by in situ synchrotron X-ray scattering and transmission electron microscopy (TEM). The in situ synchrotron diffraction data revealed the precipitation of fcc crystals after 200 s of annealing at 638 K. Before 200 s, the position of the first broad diffraction peak, Q1, shifted toward lower momentum transfer (Q) values and the peak broadened, indicating the occurrence of LLPT at the initial stage of annealing. The structural changes occurring during LLPT were analyzed based on the pair distribution function; the changes were characterized by a transition from short- to medium-range orders as per the reduced atomic pair distribution function curve G(r). The intensity of peaks up to the fourth nearest neighbor shell in the G(r)curve exhibited different variations trends during LLPT. The peaks were classified into two groups: those indicating an fcc structure and those indicating a six-membered tricapped trigonal prism (6M-TTP; a typical medium-range order observed recently in Pd-based metallic glasses) structure. The number of peaks associated with the 6M-TTP structure gradually decreased during annealing. In contrast, the number of peaks associated with the fcc structure gradually increased at medium-range scale and decreased at short-range scale before 200 s. An analysis of the G(r) peaks indicated that LLPT is characterized by a transition from the 6M-TTP-type atomic cluster to a new type of cluster. This new type of cluster shows an atomic correlation similar to that observed in the fcc structure in the medium-range scale; however, its short-range order deteriorates. Further, high-angle annular dark field scanning TEM images revealed nanoscale structural heterogeneities during LLPT. The SAED and HRTEM results confirmed that the sample annealed for a short duration (i.e., before 200 s) with a nanoscale heterogeneous structure is amorphous, thus demonstrating the coexistence of two liquid phases. Notably, one of the two liquid phases is prone to crystallization under ion milling, thereby forming a crystal-amorphous network structure. The crystals formed due to ion milling exhibit the fcc structure and have the same crystal orientation. This research provides new evidence to unravel the LLPT mechanism in supercooled metallic liquids. Further, it presents a new model for explaining the complex structure and phase transition in metallic liquids.
DONG Weixia , YAO Zhongzheng , LIU Sinan , CHEN Guoxing , WANG Xun-Li , WU Zhenduo , LAN Si . Evolution of Short-to-Medium Range Orders During the Liquid-Liquid Phase Transition of a Pd-Si Metallic Glass[J]. Acta Metall Sin, 2024 , 60(8) : 1119 -1129 . DOI: 10.11900/0412.1961.2024.00057
| 1 | Tanaka H. General view of a liquid-liquid phase transition [J]. Phys. Rev., 2000, 62E: 6968 |
| 2 | Harrington S, Zhang R, Poole P H, et al. Liquid-liquid phase transition: Evidence from simulations [J]. Phys. Rev. Lett., 1997, 78: 2409 |
| 3 | Kurita R, Tanaka H. On the abundance and general nature of the liquid-liquid phase transition in molecular systems [J]. J. Phys. Condens. Matter, 2005, 17: L293 |
| 4 | Zalden P, Quirin F, Schumacher M, et al. Femtosecond X-ray diffraction reveals a liquid-liquid phase transition in phase-change materials [J]. Science, 2019, 364: 1062 |
| 5 | Lan S, Wu Z D, Wei X Y, et al. Structure origin of a transition of classic-to-avalanche nucleation in Zr-Cu-Al bulk metallic glasses [J]. Acta Mater., 2018, 149: 108 |
| 6 | Gallo P, Bachler J, Bove L E, et al. Advances in the study of supercooled water [J]. Eur. Phys. J., 2021, 44E: 143 |
| 7 | Wilding M C, Wilson M, McMillan P F. Structural studies and polymorphism in amorphous solids and liquids at high pressure [J]. Chem. Soc. Rev., 2006, 35: 964 |
| 8 | Boates B, Bonev S A. First-order liquid-liquid phase transition in compressed nitrogen [J]. Phys. Rev. Lett., 2009, 102: 015701 |
| 9 | Mukherjee G D, Boehler R. High-pressure melting curve of nitrogen and the liquid-liquid phase transition [J]. Phys. Rev. Lett., 2007, 99: 225701 |
| 10 | Mishima O, Calvert L D, Whalley E. An apparently first-order transition between two amorphous phases of ice induced by pressure [J]. Nature, 1985, 314: 76 |
| 11 | Mishima O, Takemura K, Aoki K. Visual observations of the amorphous-amorphous transition in H2O under pressure [J]. Science, 1991, 254: 406 |
| 12 | Brazhkin V V, Popova S V, Voloshin R N. High-pressure transformations in simple melts [J]. High Pressure Res., 1997, 15: 267 |
| 13 | Tamblyn I, Bonev S A. Structure and phase boundaries of compressed liquid hydrogen [J]. Phys. Rev. Lett., 2010, 104: 065702 |
| 14 | Kim K H, Amann-Winkel K, Giovambattista N, et al. Experimental observation of the liquid-liquid transition in bulk supercooled water under pressure [J]. Science, 2020, 370: 978 |
| 15 | Henry L, Mezouar M, Garbarino G, et al. Liquid-liquid transition and critical point in sulfur [J]. Nature, 2020, 584: 382 |
| 16 | Yang Z Q, Xu J X, Zhao G, et al. Ab initio investigation of the first-order liquid-liquid phase transition in molten sulfur [J]. Phys. Rev., 2024, 109B: 014209 |
| 17 | Yao B, Paluch M, Wojnarowska Z. Effect of bulky anions on the liquid-liquid phase transition in phosphonium ionic liquids: Ambient and high-pressure dielectric studies [J]. Sci. Rep., 2023, 13: 3040 |
| 18 | Yao B B, Paluch M, Dulski M, et al. Tailoring phosphonium ionic liquids for a liquid-liquid phase transition [J]. J. Phys. Chem. Lett., 2023, 14: 2958 |
| 19 | Zhou C, Hu L N, Sun Q J, et al. Indication of liquid-liquid phase transition in CuZr-based melts [J]. Appl. Phys. Lett., 2013, 103: 171904 |
| 20 | Ge J C, He H Y, Zhou J, et al. In-situ scattering study of a liquid-liquid phase transition in Fe-B-Nb-Y supercooled liquids and its correlation with glass-forming ability [J]. J. Alloys Compd., 2019, 787: 831 |
| 21 | Dong W X, Wu Z D, Ge J C, et al. In situ neutron scattering studies of a liquid-liquid phase transition in the supercooled liquid of a Zr-Cu-Al-Ag glass-forming alloy [J]. Appl. Phys. Lett., 2021, 118: 191901 |
| 22 | Dong W X, Ge J C, Ke Y B, et al. In-situ observation of an unusual phase transformation pathway with Guinier-Preston zone-like precipitates in Zr-based bulk metallic glasses [J]. J. Alloys Compd., 2020, 819: 153049 |
| 23 | Lan S, Ren Y, Wei X Y, et al. Hidden amorphous phase and reentrant supercooled liquid in Pd-Ni-P metallic glasses [J]. Nat. Commun., 2017, 8: 14679 |
| 24 | Lan S, Blodgett M, Kelton K F, et al. Structural crossover in a supercooled metallic liquid and the link to a liquid-to-liquid phase transition [J]. Appl. Phys. Lett., 2016, 108: 211907 |
| 25 | Küchemann S, Samwer K. Ultrafast heating of metallic glasses reveals disordering of the amorphous structure [J]. Acta Mater., 2016, 104: 119 |
| 26 | Hammersley A P. FIT2D: A multi-purpose data reduction, analysis and visualization program [J]. J. Appl. Cryst., 2016, 49: 646 |
| 27 | Qiu X, Thompson J W, Billinge S J L. PDFgetX2: A GUI-driven program to obtain the pair distribution function from X-ray powder diffraction data [J]. J. Appl. Cryst., 2004, 37: 678 |
| 28 | Koza M M, Schober H, Fischer H E, et al. Kinetics of the high- to low-density amorphous water transition [J]. J. Phys. Condens. Matter 2003, 15: 321 |
| 29 | Price D L, Moss S C, Reijers R, et al. Intermediate-range order in glasses and liquids [J]. J. Phys. Condens. Matter 1989, 1: 1005 |
| 30 | Sampath S, Benmore C J, Lantzky K M, et al. Intermediate-range order in permanently densified GeO2 glass [J]. Phys. Rev. Lett., 2003, 90: 115502 |
| 31 | Ge J C, Luo P, Wu Z D, et al. Correlations of multiscale structural evolution and homogeneous flows in metallic glass ribbons [J]. Mater. Res. Lett., 2023, 11: 547 |
| 32 | Egami T, Billinge S J L. Underneath the Bragg Peaks: Structural Analysis of Complex Materials [M]. 2nd Ed., San Diego, the USA: Pergamon, 2012: 1 |
| 33 | Klug H P, Alexander L E. X-Ray Diffraction Procedures: For Polycrystalline and Amorphous Materials [M]. 2nd Ed., Hoboken: Wiley, 1974: 1 |
| 34 | Gaskell P H. Local and medium range structures in amorphous alloys [J]. J. Non-Cryst. Solids, 1985, 75: 329 |
| 35 | Lan S, Zhu L, Wu Z D, et al. A medium-range structure motif linking amorphous and crystalline states [J]. Nat. Mater., 2021, 20: 1347 |
| 36 | Masumoto T, Maddin R. The mechanical properties of palladium 20 a/o silicon alloy quenched from the liquid state [J]. Acta Metall., 1971, 19: 725 |
| 37 | Ma D, Stoica A D, Yang L, et al. Nearest-neighbor coordination and chemical ordering in multicomponent bulk metallic glasses [J]. Appl. Phys. Lett., 2007, 90: 211908 |
| 38 | Ding J, Ma E, Asta M, et al. Second-nearest-neighbor correlations from connection of atomic packing motifs in metallic glasses and liquids [J]. Sci. Rep., 2015, 5: 17429 |
| 39 | Ohkubo T, Hirotsu Y. Electron diffraction and high-resolution electron microscopy study of an amorphous Pd82Si18 alloy with nanoscale phase separation [J]. Phys. Rev., 2003, 67B: 094201 |
| 40 | Bussey J M, Weber M H, Smith-Gray N J, et al. Examining phase separation and crystallization in glasses with X-ray nano-computed tomography [J]. J. Non-Cryst. Solids, 2023, 600: 121987 |
| 41 | Stoica M, Sarac B, Spieckermann F, et al. X-ray diffraction computed nanotomography applied to solve the structure of hierarchically phase-separated metallic glass [J]. ACS Nano, 2021, 15: 2386 |
| 42 | Zhou Q, Han W C, Luo D W, et al. Mechanical and tribological properties of Zr-Cu-Ni-Al bulk metallic glasses with dual-phase structure [J]. Wear, 2021, 474-475: 203880 |
| 43 | Kumar G, Nagahama D, Ohnuma M, et al. Structural evolution in the supercooled liquid of Zr36Ti24Be40 metallic glass [J]. Scr. Mater., 2006, 54: 801 |
| 44 | Zheng H J, Lv Y M, Sun Q J, et al. Thermodynamic evidence for cluster ordering in Cu46Zr42Al7Y5 ribbons during glass transition [J]. Sci. Bull., 2016, 61: 706 |
| 45 | Marcus M A. Phase separation and crystallization in amorphous Pd-Si-Sb [J]. J. Non-Cryst. Solids, 1979, 30: 317 |
| 46 | Liu S N, Wang L F, Ge J C, et al. Deformation-enhanced hierarchical multiscale structure heterogeneity in a Pd-Si bulk metallic glass [J]. Acta Mater., 2020, 200: 42 |
| 47 | Kim D H, Kim W T, Park E S, et al. Phase separation in metallic glasses [J]. Prog. Mater. Sci., 2013, 58: 1103 |
/
| 〈 |
|
〉 |