Research paper

Microstructures and Mechanical Properties of the Fe50Mn29Co10Cr10Cu1 High-Entropy Alloy Regulated by Rolling Temperature

  • WANG Jiajun ,
  • YUAN Ye ,
  • HE Zhufeng ,
  • ZHU Mingwei ,
  • JIA Nan
Expand
  • 1 Key Laboratory for Anisotropy and Texture of Materials, Ministry of Education, School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
    2 School of Materials Science and Engineering, Shenyang Aerospace University, Shenyang 110136, China

Received date: 2024-01-05

  Revised date: 2024-02-16

  Online published: 2024-05-20

Supported by

National Natural Science Foundation of China(52371097);National Natural Science Foundation of China(52301135);National Natural Science Foundation of China(51922026)

Abstract

Face-centered-cubic high-entropy alloys have attracted extensive attention due to their comprehensive mechanical and other properties. However, these alloys suffer from low yield strength, making it imperative to develop alloys with high yield and tensile strengths. This study systematically investigates the microstructural characteristics and tensile mechanical properties of the Fe50Mn29-Co10Cr10Cu1 high-entropy alloy processed by rolling at three temperatures (-196, 25, and 300 °C) followed by annealing. The aim is to elucidate the deformation mechanisms associated with different processing routes and their influences on strength and ductility. During uniaxial tensile deformation, deformation twins produced by liquid-nitrogen and room-temperature rolling along with lath-like reversed austenite impede dislocation slip, thereby improving the yield strength of the alloy. In contrast, the alloy processed by warm rolling and annealing shows few deformation twins, with dislocation slip and stacking faults dominating as the deformation mechanisms. The alloy processed by liquid-nitrogen rolling followed by 500 oC annealing exhibits high yield strength but poor plasticity. Conversely, alloys rolled at room temperature and 300 oC followed by 500 oC annealing demonstrate higher yield strengths and certain degree of work hardening capability, showing corresponding yield strengths of 752 and 604 MPa, tensile strengths of 917 and 784 MPa, and uniform elongations of 11.2% and 26.2%. The differing microstructures resulting from processing at varied temperatures and subsequent annealing lead to significant differences in mechanical behavior under tensile testing.

Cite this article

WANG Jiajun , YUAN Ye , HE Zhufeng , ZHU Mingwei , JIA Nan . Microstructures and Mechanical Properties of the Fe50Mn29Co10Cr10Cu1 High-Entropy Alloy Regulated by Rolling Temperature[J]. Acta Metall Sin, 2025 , 61(10) : 1502 -1514 . DOI: 10.11900/0412.1961.2024.00002

References

[1] Wei Y J, Li Y Q, Zhu L C, et al. Evading the strength-ductility trade-off dilemma in steel through gradient hierarchical nanotwins [J]. Nat. Commun., 2014, 5: 3580
[2] Yeh J W, Chen S K, Lin S J, et al. Nanostructured high-entropy alloys with multiple principal elements: Novel alloy design concepts and outcomes [J]. Adv. Eng. Mater., 2004, 6: 299
[3] Cantor B, Chang I T H, Knight P, et al. Microstructural development in equiatomic multicomponent alloys [J]. Mater. Sci. Eng., 2014, A375-377: 213
[4] Huang H L, Wu Y, He J Y, et al. Phase-transformation ductilization of brittle high-entropy alloys via metastability engineering [J]. Adv. Mater., 2017, 29: 1701678
[5] Yoshida S, Ikeuchi T, Bhattacharjee T, et al. Effect of elemental combination on friction stress and Hall-Petch relationship in face-centered cubic high/medium entropy alloys [J]. Acta Mater., 2019, 171: 201
[6] Otto F, Dlouhy A, Somsen C, et al. The influences of temperature and microstructure on the tensile properties of a CoCrFeMnNi high-entropy alloy [J]. Acta Mater., 2013, 61: 5743
[7] Kao Y F, Chen S K, Sheu J H, et al. Hydrogen storage properties of multi-principal-component CoFeMnTix Vy Zrz alloys [J]. Int. J. Hydrogen Energy, 2010, 35: 9046
[8] Xiao N, Guan X, Wang D, et al. Impact of W alloying on microstructure, mechanical property and corrosion resistance of face-centered cubic high entropy alloys: A review [J]. Int. J. Miner. Metall. Mater., 2023, 30: 1667
[9] Liu M H, Du C W, Liu Z Y, et al. A review on pitting corrosion and environmentally assisted cracking on duplex stainless steel [J]. Microstructures, 2023, 3: 2023020
[10] Tian Y Z, Sun S J, Lin H R, et al. Fatigue behavior of CoCrFeMnNi high-entropy alloy under fully reversed cyclic deformation [J]. J. Mater. Sci. Technol., 2019, 35: 334
[11] Xu N, Huang Y B, Gao Y X, et al. Novel casting CoCrNiAl eutectic high entropy alloys with high strength and good ductility [J]. Microstructures, 2023, 3(3): 2023015
[12] Gludovatz B, Hohenwarter A, Catoor D, et al. A fracture-resistant high-entropy alloy for cryogenic applications [J]. Science, 2014, 345: 1153
[13] Xu X N, Li H J, Sun B Z, et al. Enhanced strength-ductility-toughness synergy in an HSLA steel with multi-gradient ultrafine grained structure by adopting a two-stage rolling coupling inter-pass ultra-fast cooling process [J]. J. Mater. Process. Technol., 2023, 313: 117832
[14] Jiang W, Wang H, Li Z M, et al. Enhanced mechanical properties of a carbon and nitrogen Co-doped interstitial high-entropy alloy via tuning ultrafine-grained microstructures [J]. J. Mater. Sci. Technol., 2023, 144: 128
[15] Huang S, Li W, Lu S, et al. Temperature dependent stacking fault energy of FeCrCoNiMn high entropy alloy [J]. Scr. Mater., 2015, 108: 44
[16] Chandan A K, Murugaiyan P, Chowdhury S G. Temperature-dependent stacking fault energy, deformation behavior, and tensile properties of a new high-entropy alloy [J]. Mater. Sci. Eng., 2023, A883: 145522
[17] Oh H S, Ma D C, Leyson G P, et al. Lattice Distortions in the FeCoNiCrMn high entropy alloy studied by theory and experiment [J]. Entropy, 2016, 18: 321
[18] Laplanche G, Kostka A, Horst O M, et al. Microstructure evolution and critical stress for twinning in the CrMnFeCoNi high-entropy alloy [J]. Acta Mater., 2016, 118: 152
[19] Sun S J, Tian Y Z, Lin H R, et al. Modulating the prestrain history to optimize strength and ductility in CoCrFeMnNi high-entropy alloy [J]. Scr. Mater., 2019, 163: 111
[20] Sun S J, Tian Y Z, Lin H R, et al. Revisiting the role of prestrain history in the mechanical properties of ultrafine-grained CoCrFe-MnNi high-entropy alloy [J]. Mater. Sci. Eng., 2021, A801: 140398
[21] Moon J, Bouaziz O, Kim H S, et al. Twinning engineering of a CoCrFeMnNi high-entropy alloy [J]. Scr. Mater., 2021, 197: 113808
[22] Bouaziz O, Scott C P, Petitgand G. Nanostructured steel with high work-hardening by the exploitation of the thermal stability of mechanically induced twins [J]. Scr. Mater., 2009, 60: 714
[23] Bouaziz O, Allain S, Scott C. Effect of grain and twin boundaries on the hardening mechanisms of twinning-induced plasticity steels [J]. Scr. Mater., 2008, 58: 484
[24] Avrami M. Kinetics of phase change. I General theory [J]. J. Chem. Phys., 1939, 7: 1103
[25] He Z F. Microscopic deformation and strengthening-toughening of FeMnCoCr-based high-entropy alloys [D]. Shenyang: Northeastern University, 2021
  何竹风. FeMnCoCr系高熵合金的微观形变与强韧化研究 [D]. 沈阳: 东北大学, 2021
[26] Zhang H T, Wang C L, Shi S Y, et al. Tuning deformation mechanisms of face-centered-cubic high-entropy alloys via boron doping [J]. J. Alloys Compd., 2022, 911: 165103
[27] Li Z M, Tasan C C, Springer H, et al. Interstitial atoms enable joint twinning and transformation induced plasticity in strong and ductile high-entropy alloys [J]. Sci. Rep., 2017, 7: 40704
[28] He Z F, Jia N, Yan H L, et al. Multi-heterostructure and mechanical properties of N-doped FeMnCoCr high entropy alloy [J]. Int. J. Plast., 2021, 139: 102965
[29] He Z F, Guo Y X, Sun L F, et al. Interstitial-driven local chemical order enables ultrastrong face-centered cubic multicomponent alloys [J]. Acta Mater., 2023, 243: 118495
[30] Jiang S, Peng R L, Heged?s Z, et al. Micromechanical behavior of multilayered Ti/Nb composites processed by accumulative roll bonding: An in-situ synchrotron X-ray diffraction investigation [J]. Acta Mater., 2021, 205: 116546
[31] Su J, Raabe D, Li Z M. Hierarchical microstructure design to tune the mechanical behavior of an interstitial TRIP-TWIP high-entropy alloy [J]. Acta Mater., 2019, 163: 40
[32] Sun S J, Tian Y Z, An X H, et al. Ultrahigh cryogenic strength and exceptional ductility in ultra?ne-grained CoCrFeMnNi high-entropy alloy with fully recrystallized structure [J]. Mater. Today Nano, 2018, 4: 46
[33] Ungár T, Gubicza J, Ribárik G, et al. Crystallite size distribution and dislocation structure determined by diffraction profile analysis: Principles and practical application to cubic and hexagonal crystals [J]. J. Appl. Cryst., 2001, 34: 298
[34] Li X Q, Irving D L, Vitos L. First-principles investigation of the micromechanical properties of fcc-hcp polymorphic high-entropy alloys [J]. Sci. Rep., 2018, 8: 11196
[35] Ungár T, Dragomir I, Révész á, et al. The contrast factors of dislocations in cubic crystals: The dislocation model of strain anisotropy in practice [J]. J. Appl. Cryst., 1999, 32: 992
[36] Fullman R L. Measurement of particle sizes in opaque bodies [J]. JOM, 1953, 5: 447
[37] Mohammad-Ebrahimi M H, Zarei-Hanzaki A, Abedi H R, et al. The enhanced static recrystallization kinetics of a non-equiatomichigh entropy alloy through the reverse transformation of strain induced martensite [J]. J. Alloys Compd., 2019, 806: 1550
[38] Leem D S, Lee Y D, Jun J H, et al. Amount of retained austenite at room temperature after reverse transformation of martensite to austenite in an Fe-13%Cr-7%Ni-3%Si martensitic stainless steel [J]. Scr. Mater., 2001, 45: 767
[39] He B B, Wang M, Huang M X. Improving tensile properties of room-temperature quenching and partitioning steel by dislocation engineering [J]. Metall. Mater. Trans., 2019, 50A: 4021
[40] Toth L S, Gu C F, Beausir B, et al. Geometrically necessary dislocations favor the Taylor uniform deformation mode in ultra-fine-grained polycrystals [J]. Acta Mater., 2016, 117: 35
[41] Zhu C Y, Harrington T, Gray III G T, et al. Dislocation-type evolution in quasi-statically compressed polycrystalline nickel [J]. Acta Mater., 2018, 155: 104
[42] Yan B Y, Jiang S Y, Hu L, et al. Crystal plasticity finite element simulation of NiTi shape memory alloy under canning compression based on constitutive model containing dislocation density [J]. Mech. Mater., 2021, 157: 103830
[43] Zhi H H, Zhang C, Antonov S, et al. Investigations of dislocation-type evolution and strain hardening during mechanical twinning in Fe-22Mn-0.6C twinning-induced plasticity steel [J]. Acta Mater., 2020, 195: 371
[44] Brinckmann S, Siegmund T, Huang Y G. A dislocation density based strain gradient model [J]. Int. J. Plast., 2006, 22: 1784
[45] Muránsky O, Balogh L, Tran M, et al. On the measurement of dislocations and dislocation substructures using EBSD and HRSD techniques [J]. Acta Mater., 2019, 175: 297
[46] Liu Y, Cai S L. Gradients of strain to increase strength and ductility of magnesium alloys [J]. Metals, 2019, 9: 1028
[47] Huang M X, He B B. Alloy design by dislocation engineering [J]. J. Mater. Sci. Technol., 2018, 34: 417
[48] He B B, Hu B, Yen H W, et al. High dislocation density-induced large ductility in deformed and partitioned steels [J]. Science, 2017, 357: 1029
[49] Deng Y, Tasan C C, Pradeep K G, et al. Design of a twinning-induced plasticity high entropy alloy [J]. Acta Mater., 2015, 94: 124
[50] Li Z M, Pradeep K G, Deng Y, et al. Metastable high-entropy dual-phase alloys overcome the strength-ductility trade-off [J]. Nature, 2016, 534: 227
[51] Wang M M, Li Z M, Raabe D. In-situ SEM observation of phase transformation and twinning mechanisms in an interstitial high-entropy alloy [J]. Acta Mater., 2018, 147: 236
[52] Zhang H F, Yan H L, Fang F, et al. Molecular dynamic simulations of deformation mechanisms for FeMnCoCrNi high-entropy alloy bicrystal micropillars [J]. Acta Metall. Sin., 2023, 59: 1051
  张海峰, 闫海乐, 方 烽 等. FeMnCoCrNi高熵合金双晶微柱变形机制的分子动力学模拟 [J]. 金属学报, 2023, 59: 1051
[53] Liu Y X, Zhang H F, Yang Y L, et al. Chemical short-range order dependence of micromechanical behavior in CoCrNi medium-entropy alloy studied by atomic simulations [J]. J. Alloys Compd., 2023, 968: 172002
[54] Lu W J, Liebscher C H, Dehm G, et al. Bidirectional transformation enables hierarchical nanolaminate dual-phase HEAs [J]. Adv. Mater., 2018, 30: 1804727
[55] Yuan Y, Wang J J, Wei J, et al. Cu alloying enables superior strength-ductility combination and high corrosion resistance of FeMnCoCr high entropy alloy [J]. J. Alloys Compd., 2024, 970: 172543
[56] Zhu Y T, Liao X Z, Wu X L. Deformation twinning in nanocrystalline materials [J]. Prog. Mater. Sci., 2012, 57: 1
Outlines

/