Effect of Rare Earth Element Ce on the Bulk Texture and Mechanical Anisotropy of As-Extruded Mg-0.3Al- 0.2Ca-0.5Mn Alloy Sheets
Received date: 2024-02-04
Revised date: 2024-04-16
Online published: 2024-04-29
Supported by
National Key Research and Development Program of China(2023YFA1608801)
Because deformed magnesium alloys with low density and desirable mechanical properties can save energy and reduce emissions, they are in considerable demand in industrial applications. However, due to their hcp crystal structure, magnesium alloys have a limited number of slip systems that can be activated at room temperature. At present, many deformed magnesium alloys still face the problems of insufficient formability and poor mechanical anisotropy at room temperature, which limit the development of secondary forming processes. Meanwhile, many reports have proven that regulating the texture of deformed magnesium alloys is an effective strategy to improve their formability. Therefore, this study primarily employs the neutron diffraction technology, combined with microscopic characterization methods such as SEM and EBSD, to systematically study the effects of the minor rare earth element Ce on the microstructure, bulk texture, and mechanical anisotropy of extruded Mg-0.3Al-0.2Ca-0.5Mn magnesium alloy sheet. The results show that as the Ce content increases, second-phase particles in the extruded magnesium alloy sheet gradually transform from Al8Mn5 to Ce-containing Al8Mn4Ce and Al11Ce3 particles and the number density of second-phase particles increases remarkably. The addition of 0.05%Ce (mass fraction) did not considerably improve the basal texture of the sheet. However, after the addition of 0.5%Ce, fiber texture components distributed along the transverse direction (TD) are substantially reduced while the texture of (0002) pole figure of the alloy changed from a bimodal basal texture to a bimodal nonbasal texture along the extrusion direction (ED). This nonbasal texture formation is mainly caused by larger Ce-containing second-phase particles (> 1 μm) promoting the particle-stimulated nucleation effect and preferential growth of nonbasal-oriented recrystallized grains. Therefore, when 0.5%Ce is added, the basal texture of the alloy is remarkably optimized, so that the ratio of the tensile yield strength along TD to that along ED is close to 1, implying that the anisotropy of the extruded Mg-0.3Al-0.2Ca-0.5Mn alloy has been substantially reduced by the minor addition of Ce element.
ZHU Guijie , WANG Siqing , ZHA Min , LI Meijuan , SUN Kai , CHEN Dongfeng . Effect of Rare Earth Element Ce on the Bulk Texture and Mechanical Anisotropy of As-Extruded Mg-0.3Al- 0.2Ca-0.5Mn Alloy Sheets[J]. Acta Metall Sin, 2024 , 60(8) : 1079 -1090 . DOI: 10.11900/0412.1961.2024.00044
| 1 | Kurzynowski T, Pawlak A, Smolina I. The potential of SLM technology for processing magnesium alloys in aerospace industry [J]. Arch. Civ. Mech. Eng., 2020, 20: 23 |
| 2 | Song J F, She J, Chen D L, et al. Latest research advances on magnesium and magnesium alloys worldwide [J]. J. Magnes. Alloy., 2020, 8: 1 |
| 3 | Bommala V K, Krishna M G, Rao C T. Magnesium matrix composites for biomedical applications: A review [J]. J. Magnes. Alloy., 2019, 7: 72 |
| 4 | Kulekci M K. Magnesium and its alloys applications in automotive industry [J]. Int. J. Adv. Manuf. Technol., 2008, 39: 851 |
| 5 | Ding H L, Shi X B, Wang Y Q, et al. Texture weakening and ductility variation of Mg-2Zn alloy with Ca or RE addition [J]. Mater. Sci. Eng., 2015, A645: 196 |
| 6 | You S H, Huang Y D, Kainer K U, et al. Recent research and developments on wrought magnesium alloys [J]. J. Magnes. Alloy., 2017, 5: 239 |
| 7 | Wang Q H, Jiang B, Chen D L, et al. Strategies for enhancing the room-temperature stretch formability of magnesium alloy sheets: A review [J]. J. Mater. Sci., 2021, 56: 12965 |
| 8 | Huang X S, Suzuki K, Chino Y, et al. Texture and stretch formability of AZ61 and AM60 magnesium alloy sheets processed by high-temperature rolling [J]. J. Alloys Compd., 2015, 632: 94 |
| 9 | Miller V M, Berman T D, Beyerlein I J, et al. Prediction of the plastic anisotropy of magnesium alloys with synthetic textures and implications for the effect of texture on formability [J]. Mater. Sci. Eng., 2016, A675: 345 |
| 10 | Bohlen J, Nürnberg M R, Senn J W, et al. The texture and anisotropy of magnesium-zinc-rare earth alloy sheets [J]. Acta Mater., 2007, 55: 2101 |
| 11 | Shi B D, Yang C, Peng Y, et al. Anisotropy of wrought magnesium alloys: A focused overview [J]. J. Magnes. Alloy., 2022, 10: 1476 |
| 12 | Hantzsche K, Bohlen J, Wendt J, et al. Effect of rare earth additions on microstructure and texture development of magnesium alloy sheets [J]. Scr. Mater., 2010, 63: 725 |
| 13 | Imandoust A, Barrett C D, Al-Samman T, et al. A review on the effect of rare-earth elements on texture evolution during processing of magnesium alloys [J]. J. Mater. Sci., 2017, 52: 1 |
| 14 | Li J S, Li M X, Hua Z M, et al. Effect of micro-alloyed Ce on the microstructure evolution and mechanical properties of rolled Mg-0.6Al-0.5Mn-0.2Ca alloy sheets [J]. J. Mater. Res. Technol., 2022, 19: 3088 |
| 15 | Zhao J, Jiang B, Wang Q H, et al. Influence of Ce content on the microstructures and tensile properties of Mg-1Gd-0.5Zn alloys [J]. Mater. Sci. Eng., 2021, A823: 141675 |
| 16 | Zuo J, Nakata T, Xu C, et al. Effect of annealing on microstructure evolution and age-hardening behavior of dilute Mg-Al-Ca-Mn alloy [J]. J. Mater. Res. Technol., 2022, 18: 1754 |
| 17 | Nakata T, Xu C, Ajima R, et al. Strong and ductile age-hardening Mg-Al-Ca-Mn alloy that can be extruded as fast as aluminum alloys [J]. Acta Mater., 2017, 130: 261 |
| 18 | Zhu G J, Li M J, Liu X L, et al. The latest progress on neutron texture diffractometer at China Advanced Research Reactor [J]. Nucl. Instrum. Methods Phys. Res. Sect., 2023, 1047A: 167729 |
| 19 | Li M X, Wang C, Li Y J, et al. Tailoring the microstructure and enhancing the corrosion resistance of extruded dilute Mg-0.6Al-0.5Mn-0.25Ca alloy by adding trace Ce [J]. Corros. Sci., 2022, 207: 110605 |
| 20 | Wang X, Guan D K. The evolution of coarse grains and its effects on weakened basal texture during annealing of a cold-rolled magnesium AZ31B alloy [J]. J. Magnes. Alloy., 2022, 10: 1235 |
| 21 | Basu I, Al-Samman T, Gottstein G. Shear band-related recrystallization and grain growth in two rolled magnesium-rare earth alloys [J]. Mater. Sci. Eng., 2013, A579: 50 |
| 22 | Chai Y F, Jiang B, Song J F, et al. Improvement of mechanical properties and reduction of yield asymmetry of extruded Mg-Sn-Zn alloy through Ca addition [J]. J. Alloys Compd., 2019, 782: 1076 |
| 23 | Chai Y F, He C, Jiang B, et al. Influence of minor Ce additions on the microstructure and mechanical properties of Mg-1.0Sn-0.6Ca alloy [J]. J. Mater. Sci. Technol., 2020, 37: 26 |
| 24 | Yang J D, Wang W X, Zhang M, et al. Effects of Gd/Nd ratio on the microstructures and tensile creep behavior of Mg-8Al-Gd-Nd alloys crept at 423 K [J]. J. Mater. Res. Technol., 2021, 14: 2522 |
| 25 | Masoumi M, Hoseini M, Pekguleryuz M. The influence of Ce on the microstructure and rolling texture of Mg-1%Mn alloy [J]. Mater. Sci. Eng., 2011, A528: 3122 |
| 26 | Peng P, Zhang K M, She J, et al. Role of second phases and grain boundaries on dynamic recrystallization behavior in ZK60 magnesium alloy [J]. J. Alloys Compd., 2021, 861: 157958 |
| 27 | Peng P, Zhang L P, Zhao J Y, et al. Simultaneous improvement of strength and ductility in ZK60 magnesium alloy by constructing the bimodal grain structure [J]. J. Mater. Res. Technol., 2023, 22: 1026 |
| 28 | Zhao J, Jiang B, Yuan Y, et al. Influence of Ca and Zn synergistic alloying on the microstructure, tensile properties and strain hardening of Mg-1Gd alloy [J]. Mater. Sci. Eng., 2020, A785: 139344 |
| 29 | Chen W Z, Ma J F, Cui C, et al. Texture role in the mechanical property improvement contributed by grain refinement for Mg-2.6Nd-0.55Zn-0.5Zr alloy subjected to extrusion process [J]. Mater. Sci. Eng., 2022, A831: 142185 |
| 30 | Sabbaghian M, Fakhar N, Nagy P, et al. Investigation of shear and tensile mechanical properties of ZK60 Mg alloy sheet processed by rolling and sheet extrusion [J]. Mater. Sci. Eng., 2021, A828: 142098 |
| 31 | Guan K, Meng F Z, Qin P F, et al. Effects of samarium content on microstructure and mechanical properties of Mg-0.5Zn-0.5Zr alloy [J]. J. Mater. Sci. Technol., 2019, 35: 1368 |
| 32 | Wu J L, Jin L, Dong J, et al. The texture and its optimization in magnesium alloy [J]. J. Mater. Sci. Technol., 2020, 42: 175 |
| 33 | Lu J W, Yin D D, Huang G H, et al. Plastic anisotropy and deformation behavior of extruded Mg-Y sheets at elevated temperatures [J]. Mater. Sci. Eng., 2017, A700: 598 |
| 34 | Yin D D, Boehlert C J, Long L J, et al. Tension-compression asymmetry and the underlying slip/twinning activity in extruded Mg-Y sheets [J]. Int. J. Plast., 2021, 136: 102878 |
/
| 〈 |
|
〉 |