Effects of Ambient and Cryogenic Rolling on {111}/{111} Near Singular Boundary Formation During Subsequent Recrystallization Annealing in Pure Aluminum
Received date: 2024-01-30
Revised date: 2024-03-13
Online published: 2024-04-25
Supported by
National Natural Science Foundation of China(51971063);Natural Science Foundation of Fujian Province(2021J011076)
Recent advancements in grain boundary engineering have revealed that the {111}/{111} near singular boundary (NSB) exhibits superior resistance to corrosion attacks than the random boundary in aluminum and its alloys. Thus, understanding the influential factors and formation mechanisms of the {111}/{111} NSB, as well as regulating such boundaries, is crucial for enhancing the resistance performance of aluminum and its alloys against intergranular corrosion attacks. To intrinsically comprehend the formation mechanism of the {111}/{111} NSB in aluminum alloys, this study used high purity aluminum (99.99%) as the experimental material. Initially, the starting samples were synthesized through multidirectional forging at room temperature (25 oC), followed by recrystallization annealing at 370 oC. The as-synthesized starting samples exhibited uniform microstructures with an average grain size of 20 μm and random grain orientations. Subsequently, two parallel starting samples were rolled at 25 oC and at the cryogenic temperature (-196 oC), respectively, with an 80% thickness reduction, followed by immediate recrystallization annealing at 370 oC for 30 min. Later, a quantitative grain boundary inter-connection characterization method based on EBSD and five parameter analysis was employed to statistically analyze the grain boundary character distributions within the samples. The results revealed that the cryo-rolled and recrystallized sample featured a higher proportion of the {111}/{111} NSB compared to the 25 oC-rolled and recrystallized sample. Specifically, the {111}/{111} NSB fraction in the former reached 6.0%, 2.22 times that in the latter. XRD analysis, hardness testing, and EBSD measurements revealed the development of a strong {011}<
LI Zhenxiang , WANG Weiguo , Rohrer Gregory S , HONG Lihua , CHEN Song , LIN Yan , ZHOU Bangxin . Effects of Ambient and Cryogenic Rolling on {111}/{111} Near Singular Boundary Formation During Subsequent Recrystallization Annealing in Pure Aluminum[J]. Acta Metall Sin, 2025 , 61(11) : 1673 -1688 . DOI: 10.11900/0412.1961.2024.00035
| [1] | Deng Y L, Zhang X M. Development of aluminium and aluminium alloy [J]. Chin. J. Nonferrous Met., 2019, 29: 2115 |
| 邓运来, 张新明. 铝及铝合金材料进展 [J]. 中国有色金属学报, 2019, 29: 2115 | |
| [2] | Hong T J, Dong F L, Ding F J, et al. Application of aluminum alloy in automotive lightweight [J]. Hot Work. Technol., 2020, 49(4): 1 |
| 洪腾蛟, 董福龙, 丁凤娟 等. 铝合金在汽车轻量化领域的应用研究 [J]. 热加工工艺, 2020, 49(4): 1 | |
| [3] | Liang G, Zhu S, Wang W Y, et al. Research status and development trend of aluminum alloy anticorrosion technology [J]. Mater. Rev., 2020, 34(): 429 |
| 梁 广, 朱 胜, 王文宇 等. 铝合金腐蚀防护技术研究现状及发展趋势 [J]. 材料导报, 2020, 34(): 429 | |
| [4] | He T, Shi W, Xiang S, et al. Influence of aging on corrosion behaviour of the 6061 cast aluminium alloy [J]. Materials (Basel), 2021, 14: 1821 |
| [5] | Liu Y R, Pan Q L, Li H, et al. Revealing the evolution of microstructure, mechanical property and corrosion behavior of 7A46 aluminum alloy with different ageing treatment [J]. J. Alloys Compd., 2019, 792: 32 |
| [6] | Aust K T. Grain boundary engineering [J]. Can. Metall. Quart., 1994, 33: 265 |
| [7] | Wang W G, Zhou B X, Rohrer G S, et al. Textures and grain boundary character distributions in a cold rolled and annealed Pb-Ca based alloy [J]. Mater. Sci. Eng., 2010, A527: 3695 |
| [8] | Liu Z Q, Wang W G. Study on Σ3 boundaries in an cold rolled and recrystallized Al-Cu alloy [J]. J. Chin. Electron Microsc. Soc., 2018, 37: 232 |
| 刘智强, 王卫国. 冷轧变形Al-Cu合金再结晶Σ3晶界研究 [J]. 电子显微学报, 2018, 37: 232 | |
| [9] | Wang W G, Cai C H, Rohrer G S, et al. Grain boundary inter-connections in polycrystalline aluminum with random orientation [J]. Mater. Charact., 2018, 144: 411 |
| [10] | Yang X M, Wang W G, Gu X F. The near singular boundaries in BCC iron [J]. Philos. Mag., 2022, 102: 440 |
| [11] | Wang W G, Du A H, Yang X M, et al. Quantitative determination of grain boundary inter-connections [P]. Chin Pat, CN2020111-73146.8, 2021 |
| 王卫国, 杜阿华, 杨先明 等. 晶界界面匹配定量表征方法 [P]. 中国专利, CN202011173146.8, 2021) | |
| [12] | Randle V, Rohrer G S, Hu Y. Five-parameter grain boundary analysis of a titanium alloy before and after low-temperature annealing [J]. Scr. Mater., 2008, 58: 183 |
| [13] | Zhang W Z. Application of the O-lattice model to the calculation of the interfacial dislocations [J]. Acta Metall. Sin., 2002, 38: 785 |
| 张文征. O点阵模型及其在界面位错计算中的应用 [J]. 金属学报, 2002, 38: 785 | |
| [14] | Du A H, Wang W G, Gu X F, et al. The dependence of precipitate morphology on the grain boundary types in an aged Al-Cu binary alloy [J]. J. Mater. Sci., 2021, 56: 781 |
| [15] | Wang Z P, Wang W G, Rohrer G S, et al. {111}/{111} Near singular boundaries in a Al-Zn-Mg-Cu Alloy recrystallized after rolling at different temperatures [J]. Acta Metall. Sin., 2023, 59: 947 |
| 王宗谱, 王卫国, Rohrer G S 等. 不同温度轧制Al-Zn-Mg-Cu合金再结晶后的{111}/{111}近奇异晶界 [J]. 金属学报, 2023, 59: 947 | |
| [16] | Takayama A, Yang X, Miura H, et al. Continuous static recrystallization in ultrafine-grained copper processed by multi-directional forging [J]. Mater. Sci. Eng., 2008, A478: 221 |
| [17] | Feng X Z, Wang W G, Rohrer G S, et al. Effects of grain growth on the {111}/{111} near singular boundaries in high purity aluminum [J]. Acta Metall. Sin., 2024, 60: 80 |
| 冯小铮, 王卫国, Rohrer G S 等. 晶粒长大对高纯Al{111}/{111}近奇异晶界的影响 [J]. 金属学报, 2024, 60: 80 | |
| [18] | Tong F, Wang W G, Rohrer G S, et al. Effect of pre-deformation temperature on formation of {111}/{111} near singular boundaries in Al-Mg alloy during subsequent recrystallization [J]. Trans. Mater. Heat Treat., 2023, 44(5): 47 |
| 童 芳, 王卫国, Rohrer G S 等. 预变形温度对Al-Mg合金再结晶{111}/{111}近奇异晶界的影响 [J]. 材料热处理学报, 2023, 44(5): 47 | |
| [19] | Lee Y B, Shin D H, Park K T, et al. Effect of annealing temperature on microstructures and mechanical properties of a 5083 Al alloy deformed at cryogenic temperature [J]. Scr. Mater., 2004, 51: 355 |
| [20] | Chen D, Li W X. Cryogenic treatment of Al and Al alloys [J]. Chin. J. Nonferrous Met., 2000, 10: 891 |
| 陈 鼎, 黎文献. 铝和铝合金的深冷处理 [J]. 中国有色金属学报, 2000, 10: 891 | |
| [21] | Barron R F. Cryogenic treatment of metals to improve wear resistance [J]. Cryogenics, 1982, 22: 409 |
| [22] | Koneshlou M, Asl K M, Khomamizadeh F. Effect of cryogenic treatment on microstructure, mechanical and wear behaviors of AISI H13 hot work tool steel [J]. Cryogenics, 2011, 51: 55 |
| [23] | Molinari A, Pellizzari M, Gialanella S, et al. Effect of deep cryogenic treatment on the mechanical properties of tool steels [J]. J. Mater. Process. Technol., 2001, 118: 350 |
| [24] | Podgornik B, Paulin I, Zajec B, et al. Deep cryogenic treatment of tool steels [J]. J. Mater. Process. Technol., 2016, 229: 398 |
| [25] | Shi J T, Zuo J R, Zhang J S. Microstructure and mechanical properties of 5052 Al alloy by cryogenic rolling [J]. Mater. Sci. Forum., 2020, 993: 86 |
| [26] | Wolf D. Structure-energy correlation for grain boundaries in F.C.C. metals—I. Boundaries on the (111) and (100) planes [J]. Acta Metall., 1989, 37: 1983 |
| [27] | Wright S I, Larsen R J. Extracting twins from orientation imaging microscopy scan data [J]. J. Microsc., 2002, 205: 245 |
| [28] | Wang W G, Lin C, Li G H, et al. Preferred orientation of grain boundary plane in recrystallized high purity aluminum [J]. Sci. Sin. Technol., 2014, 44: 1295 |
| [29] | Krishna N N, Ashfaq M, Susila P, et al. Mechanical anisotropy and microstructural changes during cryorolling of Al-Mg-Si alloy [J]. Mater. Charact., 2015, 107: 302 |
| [30] | Krishna N N, Tejas R, Sivaprasad K, et al. Study on cryorolled Al-Cu alloy using X-ray diffraction line profile analysis and evaluation of strengthening mechanisms [J]. Mater, Des., 2013, 52: 785 |
| [31] | Hou L G, Liu M L, Wang X D, et al. Cryogenic processing high-strength 7050 aluminum alloy and controlling of the microstructures and mechanical properties [J]. Acta Metall. Sin., 2017, 53: 1075 |
| 侯陇刚, 刘明荔, 王新东 等. 高强7050铝合金超低温大变形加工与组织、性能调控 [J]. 金属学报, 2017, 53: 1075 | |
| [32] | Rangaraju N, Raghuram T, Krishna B V, et al. Effect of cryo-rolling and annealing on microstructure and properties of commercially pure aluminium [J]. Mater. Sci. Eng., 2005, A398: 246 |
| [33] | Xiong Y, He T T, Guo Z Q, et al. Effect of severe deformation under different temperatures and annealing on microstructure of commercial pure aluminum [J]. Trans. Mater. Heat Treat., 2011, 32(9): 63 |
| 熊 毅, 贺甜甜, 郭志强 等. 不同温度重度变形及退火对工业纯铝组织的影响 [J]. 材料热处理学报, 2011, 32(9): 63 | |
| [34] | Barrett C S. Recrystallization texture in aluminum after compression [J]. Trans. Aime, 1940, 137: 128 |
| [35] | Engler O, Vatne H E, Nes E. The roles of oriented nucleation and oriented growth on recrystallization textures in commercial purity aluminium [J]. Mater. Sci. Eng., 1996, A205: 187 |
/
| 〈 |
|
〉 |