Research paper

Two-Stage Aging Process of 7A65 Aluminum Alloy Thick Plate Based on In Situ Resistance Method

  • XIAO Wenlong ,
  • ZANG Chenyang ,
  • GUO Jintao ,
  • FENG Jiawen ,
  • MA Chaoli
Expand
  • 1.Tianmushan Laboratory, Hangzhou 311115, China
    2.School of Materials Science and Engineering, Beihang University, Beijing 100191, China
    3.Yunnan Innovation Institute, Beihang University, Kunming 650233, China
XIAO Wenlong, associate professor, Tel: (010)82338631, E-mail: wlxiao@buaa.edu.cn

Received date: 2023-11-28

  Revised date: 2024-03-06

  Online published: 2024-04-19

Supported by

Key Research and Development Program of Zhejiang Privince(2024SSYS0078);Complementary Project of Southwest Aluminum (Group) Co. Ltd(JZKG20190099)

Abstract

With the increasing scarcity of traditional energy sources such as petroleum, the concept of sustainable development has prompted strict demands for energy-saving, economical, and environment-friendly industrial production. As the most important lightweight structural material, the requirements for aluminum alloys in modern industries are also increasing. In particular, 7xxx-series ultrahigh-strength aluminum alloy thick plates have been widely used in aerospace and other fields due to its advantages of lightweight and high specific strength. Currently, the problem of nonuniformity of microstructure and mechanical properties in the thickness direction of the thick plates is still prominent. Therefore, developing a new aging process to overcome the shortcomings of the low efficiency of traditional aging processes and difficult-to-control temperature field is urgently needed. Additionally, the research on aging heat treatment mainly focuses on the performance test and static microstructure characterization. Fewer research works have been carried out on the real-time detection of the transformation of the aging dissolution phase byin situ means. To optimize the two-stage aging process of a 7A65 aluminum alloy thick plate, this study systematically analyzed the aging precipitation behavior of the alloy by in situ electrical resistance analysis, formulated the two-stage aging process of the alloy, and explored the influence law of the aging process on the mechanical properties of the thick plate. The study also explored the strengthening and toughening mechanism of the plate through the microstructure observation and mechanical property test. The isothermal transition curve (i.e., time-temperature-transformation (TTT) curve) of the alloy shows that the “C curve” of η-phase dissolution is observed at 120-220 oC. According to the TTT curve, the optimal conditions for the two-stage aging process for the thick plate are determined to be as follows: heat at 121 oC for 6 h, and then at 152 oC for 19 h. After aging, the electrical conductivity of the plate is higher than 38%IACS, the yield strength is higher than 550 MPa, and the elongation reaches 9%.

Cite this article

XIAO Wenlong , ZANG Chenyang , GUO Jintao , FENG Jiawen , MA Chaoli . Two-Stage Aging Process of 7A65 Aluminum Alloy Thick Plate Based on In Situ Resistance Method[J]. Acta Metall Sin, 2025 , 61(8) : 1153 -1164 . DOI: 10.11900/0412.1961.2023.00461

References

[1] Li S S, Yue X, Li Q Y, et al. Development and applications of aluminum alloys for aerospace industry [J]. J. Mater. Res. Technol., 2023, 27: 944
[2] Heinz A, Haszler A, Keidel C, et al. Recent development in aluminium alloys for aerospace applications [J]. Mater. Sci. Eng., 2000, A280: 102
[3] Rometsch P A, Zhang Y, Knight S. Heat treatment of 7xxx series aluminium alloys—Some recent developments [J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 2003
[4] Zou Y, Wu X D, Tang S B, et al. Investigation on microstructure and mechanical properties of Al-Zn-Mg-Cu alloys with various Zn/Mg ratios [J]. J. Mater. Sci. Technol., 2021, 85: 106
[5] Han B S, Wei L J, Xu Y J, et al. Effect of pre-deformation on microstructure and mechanical properties of ultra-high strength Al-Zn-Mg-Cu alloy after ageing treatment [J]. Acta. Metall. Sin., 2020, 56: 1007
  韩宝帅, 魏立军, 徐严谨 等. 预变形对超高强Al-Zn-Mg-Cu合金时效组织与力学性能的影响 [J]. 金属学报, 2020, 56: 1007
[6] Mishra R S, Komarasamy M. Friction Stir Welding of High Strength 7XXX Aluminum Alloys [M]. Oxford: Butterworth-Heinemann, 2016: 5
[7] Zuo J R, Hou L G, Shi J T, et al. Enhanced plasticity and corrosion resistance of high strength Al-Zn-Mg-Cu alloy processed by an improved thermomechanical processing [J]. J. Alloys Compd., 2017, 716: 220
[8] Xiao Y P, Pan Q L, Li W B, et al. Influence of heat treatment on corrosion behaviour of Al-Zn-Mg-Cu-Zr-Sc alloy [J]. Mater. Corros., 2012, 63: 421
[9] Buha J, Lumley R N, Crosky A G. Secondary ageing in an aluminium alloy 7050 [J]. Mater. Sci. Eng., 2008, A492: 1
[10] Tang J, Liu M C, Bo G W, et al. Unraveling precipitation evolution and strengthening function of the Al-Zn-Mg-Cu alloys with various Zn contents: Multiple experiments and integrated internal-state-variable modeling [J]. J. Mater. Sci. Technol., 2022, 116: 130
[11] Zhang Z, Deng Y L, Ye L Y, et al. Effect of multi-stage aging treatments on the precipitation and mechanical properties of Al-Zn-Mg alloys [J]. Mater. Sci. Eng., 2020, A785: 139394
[12] Li M H, Yang Y Q, Feng Z Q, et al. Precipitation sequence of η phase along low-angle grain boundaries in Al-Zn-Mg-Cu alloy during artificial aging [J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 2061
[13] Yang J L, Deng Y L, Qi X H, et al. Precipitation kinetics of second-phase particles in supersaturated solid solution of 7050 aluminum alloy [J]. J. Cent. South Univ. (Sci. Technol.), 2012, 43: 2528
  杨金龙, 邓运来, 祁小红 等. 过饱和7050铝合金固溶体中第二相粒子的析出动力学[J]. 中南大学学报(自然科学版), 2012, 43: 2528
[14] Wu S Z, Yi Y P, Huang S Q, et al. Research on quench sensitivity and microstructure analysis of 7050 aluminum alloy [J]. Acta Metall. Sin., 2016, 52: 1503
  吴书舟, 易幼平, 黄始全 等. 7050铝合金淬火敏感性研究和微观组织分析 [J]. 金属学报, 2016, 52: 1503
[15] Liu J Z, Chen J H, Yang X B, et al. Revisiting the precipitation sequence in Al-Zn-Mg-based alloys by high-resolution transmission electron microscopy [J]. Scr. Mater., 2010, 63: 1061
[16] Jiang F L, Zurob H S, Purdy G R, et al. Characterizing precipitate evolution of an Al-Zn-Mg-Cu-based commercial alloy during artificial aging and non-isothermal heat treatments by in situ electrical resistivity monitoring [J]. Mater. Charact., 2016, 117: 47
[17] Deschamps A, Brechet Y. Influence of predeformation and ageing of an Al-Zn-Mg alloy—II. Modeling of precipitation kinetics and yield stress [J]. Acta Mater., 1998, 47: 293
[18] Azarniya A, Taheri A K, Taheri K K. Recent advances in ageing of 7xxx series aluminum alloys: A physical metallurgy perspective [J]. J. Alloys Compd., 2019, 781: 945
[19] Yang W C, Ji S X, Zhang Q, et al. Investigation of mechanical and corrosion properties of an Al-Zn-Mg-Cu alloy under various ageing conditions and interface analysis of η′ precipitate [J]. Mater. Des., 2015, 85: 752
[20] Li C, Chen Z, Zhang X Q, et al. Hot deformation behavior of high Zn-containing 7A65 Al alloy [J]. Rare Met., 2023, 42: 302
[21] Li C, Che G Y, Xiao W L, et al. Study on the inhomogeneity of Al-Zn-Cu-Mg aluminum alloy plates with different thickness [J]. J. Mater. Sci., 2022, 57: 21460
[22] Zang C Y, Xiao W L, Fu Y, et al. Enhanced properties and homogeneity of Al-Zn-Mg-Cu alloy thick plate by non-isothermal aging [J]. J. Alloys Compd., 2023, 952: 170023
[23] Liu C L, Wang X, Parson N C, et al. The effect of Mn on the high temperature flow stress of Al-Mg-Si alloys [J]. Mater. Sci. Eng., 2021, A802: 140605
[24] Liu S H, Wang X D, Pan Q L, et al. Investigation of microstructure evolution and quench sensitivity of Al-Mg-Si-Mn-Cr alloy during isothermal treatment [J]. J. Alloys Compd., 2020, 826: 154144
[25] Christian J W. The Theory of Transformations in Metals and Alloys [M]. 3rd Ed., Oxford: Pergamon Press, 2002: 52
[26] She X W, Jiang X Q, Wang P Q, et al. Relationship between microstructure and mechanical properties of 5083 aluminum alloy thick plate [J]. Trans. Nonferrous Met. Soc. China, 2020, 30: 1780
[27] Li J J, Ju J, Zhang Z, et al. Precipitation behavior and mechanical properties of Al-Zn-Mg-Cu matrix nanocomposites: Effects of SiC nanoparticles addition and heat treatment [J]. Mater. Charact., 2021, 172: 110827
Outlines

/