Research paper

Effect of Mn Segregation on Mechanical Properties of 0.3C-11Mn-2.7Al-1.8Si-Fe Medium Mn Steel and Its Mechanism

  • CAI Xingzhou ,
  • LIU Shengjie ,
  • ZHANG Yusen ,
  • LI Xiaolong ,
  • ZHANG Yuhe ,
  • ZHANG Wenbin ,
  • CHEN Lei ,
  • JIN Miao
Expand
  • 1 Collenge of Mechanical Engineering, Yanshan University, Qinhuangdao 066004, China
    2 Tongyu Heavy Industry Co. Ltd., Yucheng 251200, China

Received date: 2023-10-08

  Revised date: 2024-02-28

  Online published: 2024-03-29

Supported by

National Natural Science Foundation of China(52275388);National Natural Science Foundation of China(52075474);Central Guiding Local Science and Technology Development Fund Projects(236Z1008G);Natural Science Foundation of Hebei Province(E2022203206);Cultivation Project for Basic Research and Innovation of Yanshan University(2021LGZD009);Cultivation Project for Basic Research and Innovation of Yanshan University(2022BZZD002)

Abstract

Improvements in passenger safety and fuel efficiency are crucial issues in the automotive industry. The use of advanced high-strength steel (AHSS) in automotive parts has been suggested as a solution to these issues because it enables large weight reduction and good crash worthiness. Strength and ductility are the key mechanical properties of automotive AHSS. However, high strength is often accompanied by low ductility, resulting in the so-called strength-ductility trade-off dilemma. Currently, there is an increasing demand for automotive AHSS that exhibits a balance between strength and ductility. Lightweight and high-strength medium Mn steel (MMnS with a Mn mass fraction of 3%-12%), as a representative example of the third-generation automotive AHSS, has an excellent combination of strength and plasticity due to the effective usage of the coupled transformation-induced plasticity (TRIP) effect and twinning-induced plasticity (TWIP) effect of the metastable austenite constituent upon deformation. To further improve comprehensive mechanical properties, MMnS with a high Mn content were developed to increase the austenite fraction. Thus, a duplex structure with an ultrafine ferrite and austenite matrix was formed. However, Mn segregation is likely to occur in MMnS with increasing Mn content, especially in the cases of Mn > 10% (mass fraction), which considerably influences MMnS's performance. Therefore, the effects of Mn segregation on the overall mechanical properties, microstructure, and deformation mechanism of MMnS need to be elucidated in more details. In this paper, the influence of Mn segregation on the microstructure and mechanical properties of MMnS with an austenite-ferrite duplex structure and a nominal composition of 0.3C-11Mn-2.7Al-1.8Si-Fe was systemically investigated. Specifically, the underlying mechanism of Mn segregation that affects the mechanical and microstructural behavior of cold-rolled and annealed MMnS was analyzed. The results show that Mn segregation causes the formation of a Mn-rich banded structure, where the grain size of austenite is larger, austenite stability is higher, and fine ferrite is distributed more sparsely on the austenite matrix compared with the case without Mn segregation. The dominant plastic deformation mechanism of austenite in the non-Mn segregation zone involves martensitic transformation and twinning, leading to the coupled TRIP + TWIP effect, while the rate of martensitic transformation is higher than those without Mn segregation. However, the martensitic transformation is inhibited in the austenite of the Mn-rich structure because of its higher stability, limiting the TRIP effect. Consequently, the test MMnS with Mn segregation shows lower ductility and fracture resistance than those without Mn segregation; moreover, its finer austenite enhances the work-hardening capacity.

Cite this article

CAI Xingzhou , LIU Shengjie , ZHANG Yusen , LI Xiaolong , ZHANG Yuhe , ZHANG Wenbin , CHEN Lei , JIN Miao . Effect of Mn Segregation on Mechanical Properties of 0.3C-11Mn-2.7Al-1.8Si-Fe Medium Mn Steel and Its Mechanism[J]. Acta Metall Sin, 2025 , 61(7) : 1024 -1034 . DOI: 10.11900/0412.1961.2023.00410

References

1 Suh D W, Kim S J. Medium Mn transformation-induced plasticity steels: Recent progress and challenges [J]. Scr. Mater., 2017, 126: 63
2 Matlock D K, Speer J G. Third generation of AHSS: Microstructure design concepts [A]. Microstructure and Texture in Steels [M]. London: Springer, 2009: 185
3 Lee Y K, Han J. Current opinion in medium manganese steel [J]. Mater. Sci. Technol., 2015, 31: 843
4 Wang C Y, Chang Y, Zhou F L, et al. M3 microstructure control theory and technology of the third-generation automotive steels with high strength and high ductility [J]. Acta Metall. Sin., 2020, 56: 400
  王存宇, 常 颖, 周峰峦 等. 高强度高塑性第三代汽车钢的M3组织调控理论与技术 [J]. 金属学报, 2020, 56: 400
5 Yan S, Liang T S, Wang Z Q, et al. Novel 1.4 GPa-strength medium-Mn steel with uncompromised high ductility [J]. Mater. Sci. Eng., 2020, A773: 138732
6 Trang T T T, Heo Y U. Effect of solution treatment temperature on microstructure evolution and tensile property of a medium Mn steel having a lamellar structure [J]. Mater. Sci. Eng., 2021, A805: 140578
7 Zhang X L, Yan J H, Liu T, et al. Microstructural evolution and mechanical behavior of a novel heterogeneous medium Mn cold-rolled steel [J]. Mater. Sci. Eng., 2021, A800: 140344
8 Zhang J B, Sun Y R, Ji Z J, et al. Improved mechanical properties of V-microalloyed dual phase steel by enhancing martensite deformability [J]. J. Mater. Sci. Technol., 2021, 75: 139
9 Hu B, He B B, Cheng G J, et al. Super-high-strength and formable medium Mn steel manufactured by warm rolling process [J]. Acta Mater., 2019, 174: 131
10 Sun S H, Cai M H, Ding H, et al. Deformation mechanisms of a novel Mn-based 1 GPa TRIP/TWIP assisted lightweight steel with 63% ductility [J]. Mater. Sci. Eng., 2021, A802: 140658
11 Zhang Y, Ding H, Zhu H K, et al. Influence of microstructural morphology on the continuous/discontinuous yielding behavior in a medium manganese steel [J]. Mater. Sci. Eng., 2021, A824: 141746
12 Mohapatra S, Poojari G, Marandi L, et al. A systematic study on microstructure evolution, mechanical stability and the micro-mechanical response of tensile deformed medium manganese steel through interrupted tensile test [J]. Mater. Charact., 2023, 195: 112562
13 Jia Q X, Chen L, Chen X, et al. Enhancing strength-ductility synergy in medium Mn steel with hetero-structured austenite developed by two-stage cyclic thermomechanical treatment and flash annealing [J]. Scr. Mater., 2023, 226: 115196
14 Jia Q X, Chen L, Xing Z B, et al. Tailoring hetero-grained austenite via a cyclic thermomechanical process for achieving ultrahigh strength-ductility in medium-Mn steel [J]. Scr. Mater., 2022, 217: 114767
15 Patra A K, Athreya C N, Mandal S, et al. High strength-high ductility medium Mn steel obtained through CALPHAD based alloy design and thermomechanical processing [J]. Mater. Sci. Eng., 2021, A810: 140756
16 Xu Y T, Li W, Du H, et al. Tailoring the metastable reversed austenite from metastable Mn-rich carbides [J]. Acta Mater., 2021, 214: 116986
17 De Cooman B C, Estrin Y, Kim S K. Twinning-induced plasticity (TWIP) steels [J]. Acta Mater., 2018, 142: 283
18 Lee H, Jo M C, Sohn S S, et al. Novel medium-Mn (austenite + martensite) duplex hot-rolled steel achieving 1.6 GPa strength with 20% ductility by Mn-segregation-induced TRIP mechanism [J]. Acta Mater., 2018, 147: 247
19 Jo M C, Choi J H, Lee H, et al. Effects of solute segregation on tensile properties and serration behavior in ultra-high-strength high-Mn TRIP steels [J]. Mater. Sci. Eng., 2019, A740-741: 16
20 Sun B H, Palanisamy D, Ponge D, et al. Revealing fracture mechanisms of medium manganese steels with and without delta-ferrite [J]. Acta Mater., 2019, 164: 683
21 Chen X S, Huang X M, Liu J J, et al. Microstructure regulation and strengthening mechanisms of a hot-rolled & intercritical annealed medium-Mn steel containing Mn-segregation band [J]. Acta Metall. Sin., 2023, 59: 1448
  陈学双, 黄兴民, 刘俊杰 等. 一种含富锰偏析带的热轧临界退火中锰钢的组织调控及强化机制 [J]. 金属学报, 2023, 59: 1448
22 He B B, Pan S. Revealing the intrinsic nanohardness of retained austenite grain in a medium Mn steel with heterogeneous structure [J]. Mater. Charact., 2021, 171: 110745
23 Zhang J Y, Xu Y B, Wang Y, et al. Achieving heterogeneous TWIP/TRIP steel with 1 GPa strength and 72% ductility by introducing austenite + martensite lamella structure [J]. Mater. Charact., 2023, 197: 112709
24 Sun S H, Li H Y, Huang H S, et al. Improved Mn-segregation bands and its influence on deformation behavior in a severely warm-rolled 10Mn lightweight steel [J]. Vacuum, 2023, 216: 112428
25 Liu S J. Study on the effect of critical annealing on the microstructure and properties of Fe-11Mn-3Al-2Si-0.3C medium manganese steel and its mechanism [D]. Qinhuangdao: Yanshan University, 2021
  刘胜杰. 临界退火对Fe-11Mn-3Al-2Si-0.3C中锰钢组织性能影响及作用机理研究 [D]. 秦皇岛: 燕山大学, 2021
26 Miller R L. A rapid X-ray method for the determination of retained austenite [J]. Trans. Am. Soc. Met., 1964, 57: 892
27 Krauss G. Solidification, segregation, and banding in carbon and alloy steels [J]. Metall. Mater. Trans., 2003, 34B: 781
28 Hu B J, Zheng Q Y, Lu Y, et al. Recrystallization controlling in a cold-rolled medium Mn steel and its effect on mechanical properties [J]. Acta Metall. Sin., 2024, 60: 189
  胡宝佳, 郑沁园, 路 轶 等. 冷轧中锰钢的再结晶调控及其对力学性能的影响 [J]. 金属学报, 2024, 60: 189
29 Sun B H, Fazeli F, Scott C, et al. Microstructural characteristics and tensile behavior of medium manganese steels with different manganese additions [J]. Mater. Sci. Eng., 2018, A729: 496
30 Lee S, De Cooman B C. Tensile behavior of intercritically annealed 10 pct Mn multi-phase Steel [J]. Metall. Mater. Trans., 2014, 45A: 709
31 Lee S, De Cooman B C. Influence of intra-granular ferrite on the tensile behavior of intercritically annealed 12 pct Mn TWIP + TRIP steel [J]. Metall. Mater. Trans., 2015, 46A: 1012
32 Li S C, Guo C Y, Hao L L, et al. In-situ EBSD study of deformation behaviour of 600 ?MPa grade dual phase steel during uniaxial tensile tests [J]. Mater. Sci. Eng., 2019, A759: 624
33 Alharbi K, Ghadbeigi H, Efthymiadis P, et al. Damage in dual phase steel DP1000 investigated using digital image correlation and microstructure simulation [J]. Modell. Simul. Mater. Sci. Eng., 2015, 23: 085005
34 Lee S, De Cooman B C. Annealing temperature dependence of the tensile behavior of 10 pct Mn multi-phase TWIP-TRIP steel [J]. Metall. Mater. Trans., 2014, 45A: 6039
35 Sohn S S, Choi K, Kwak J H, et al. Novel ferrite-austenite duplex lightweight steel with 77% ductility by transformation induced plasticity and twinning induced plasticity mechanisms [J]. Acta Mater., 2014, 78: 181
36 Pierce D T, Jiménez J A, Bentley J, et al. The influence of manganese content on the stacking fault and austenite/ε-martensite interfacial energies in Fe-Mn-(Al-Si) steels investigated by experiment and theory [J]. Acta Mater., 2014, 68: 238
37 Sun B H, Fazeli F, Scott C, et al. The influence of silicon additions on the deformation behavior of austenite-ferrite duplex medium manganese steels [J]. Acta Mater., 2018, 148: 249
38 Koyama M, Zhang Z, Wang M M, et al. Bone-like crack resistance in hierarchical metastable nanolaminate steels [J]. Science, 2017, 355: 1055
Outlines

/